• Title/Summary/Keyword: Floor slab cracks

Search Result 6, Processing Time 0.031 seconds

A Study on How to Reduce Vibration in order to Decrease the Cracks that Form on the Upper Floor of a Structure due to Continuous Dynamic Loading (반복되는 동하중에 의한 구조물 상부바닥 균열 감소를 위한 진동저감 연구)

  • Chun, Chong-Keun;Park, Sam-Jin;Park, Sang-Gon;Kim, Do-Young
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.12 no.4
    • /
    • pp.1532-1538
    • /
    • 2011
  • In this study, we investigate the cracks that formed on the upper floor of the structures due to continuous dynamic loading. We explain the cause of floor slab cracks on the upper floor of the distribution center and discuss preventive measures that can enhance the center's functions and security. In order to explain how a forklift's excessive vibration can cause the cracks, we have measured and analyzed the vibration during a forklift's operation and discovered that the cracks form because the vibration exceeds the vibration criteria. Using a finite element modeling on such results, we have come up with optimal methods to reduce the vibration and confirmed their validity by measuring the vibration after implementing our methods.

The Fatigue Performance Evaluation of Concrete Specimen by Using Mineral Admixture (혼화재 사용에 따른 콘크리트 시험체의 피로성능 평가)

  • Kim, Doo-Hwan;Baek, Kyung-Su
    • Journal of the Korean Society of Safety
    • /
    • v.25 no.5
    • /
    • pp.39-43
    • /
    • 2010
  • The surfacing of bridge-decks are object to secure trafficability and to protect bridge face from impact load of traffic volume and other external conditions. But the deformation of pavements and cracks happen due to the damage of the bridge-decks surfacing from the increase of the traffic, short maintenance period and continuous vibration of bridge. This test is to make the 3-type high performance concrete that has different mixing ratio and is added the blast furnace slag, fly ash and silica respectively, and to compare 3-type high performance concrete of normal high strength concrete of $400kgf/cm^2$ strength through the static loading test and fatigue test. And test specimen is united floor slab and pavement for the durability of bridge.

A Study on Creep, Drying Shrinkage, Hydration Heat Produced in Concrete Floor Plate of Steel Box Girdler Bridge (강박스 거더교 콘크리트 바닥판에 발생하는 크리프, 건조수축, 수화열에 관한 연구)

  • 강성후;박선준;김민성
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2003.05a
    • /
    • pp.457-462
    • /
    • 2003
  • It studies the non-structural crack factors that are produced in Steel Box Girder Bridge concrete floor plate using analytical method. It mainly studies humidity and design standard of concrete strength. It used MIDAS CIVIL Ver 5.4.0, a general structure analysis program that applies drying shrinkage rate of domestic road bridge design standard and standard value of creep coefficient, CEF-FIP standard equation and ACI standard equation from the aspect of creep, drying shrinkage and hydration heat to see the effect of the two factors on concrete crack and found the following result. The analytical results of this study showed that the initial stress, which was obtained by ACI standard, exceeds the allowable tensile stress between 5 to 18 days. This result means that even if a bridge is designed and constructed according to design standard, the bridge can have cracks due to various variables such as drying shrinkage, hydration heat and creep that produce stress in slab.

  • PDF

Shrinkage Stress Analysis of Concrete Slab in Multi-Story Building Considering Construction Sequence (시공단계를 고려한 고층건물 콘크리트 슬래브의 건조수축 응력해석)

  • 김한수;정종현;조석희
    • Journal of the Korea Concrete Institute
    • /
    • v.13 no.5
    • /
    • pp.457-465
    • /
    • 2001
  • Shrinkage strains of concrete slab in multi-story building are restrained by structural members such as columns or walls, then can induce cracks due to excessive shrinkage stress over tensile strength of member. In this study, a shrinkage stress analysis method of concrete slab in multi-story building considering not only material properties such as shrinkage, creep and reinforcement effect but also construction sequence is proposed. Tensile stresses of slab due to shrinkage are calculated by converting shrinkage strains into equivalent temperature gradients, creep that can release shrinkage stress can be considered by replacing the modulus of elasticity of concrete, Ec , to the effective secant modulus of elasticity of concrete, E$\_$eff/ Reinforcements are also considered by modeling them as equivalent beam elements in FEM program. Results of step by step analysis reflecting construction sequence summed up to calculate stresses of the whole building considering that shrinkage stresses of the building come from the difference of shrinkage between i-th floor and (i-1)-th floor, named as effecitive shrinkage, and it can be varied by construction sequence. The results of 10-story example building show that shrinkage stresses of lower floors are greater than those of upper floors, that is, stresses of lower floors(1∼2FI.) exceed modulus of rupture of concrete, but stress ratios of higher floors are in the range of 27.9∼92.8%.

Loading capacity of simply supported composite slim beam with deep deck

  • Shi, Yongjiu;Yang, Lu;Wang, Yuanqing;Li, Qiuzhe
    • Steel and Composite Structures
    • /
    • v.9 no.4
    • /
    • pp.349-366
    • /
    • 2009
  • The composite slim beam has become popular throughout Europe in recent years and has also been used on some projects in China. With its steel section encased in a concrete slab, the steel-concrete composite slim beam can provide the floor construction with minimum depth and high fire resistance. However, the design method of the T-shape steel-concrete composite beam is no longer applicable to the composite slim beam with deep deck for its special construction, of which the present design models are not available but mainly depend on experiences. The elevation of the flexural stiffness and bending capacity of composite slim beams with deep deck is rather complicated, because the influences of many factors should be taken into account, such as the variable section dimensions, development of cracks and non-linear characteristics of concrete, etc. In this paper, experimental investigations have been conducted into the flexural behavior of two specimens of simply supported composite slim beam with deep deck. The emphases were laid on the bonding force on the interface between steel beam and concrete, the stress distribution of beam section, the flexural stiffness and bending capacity of the composite beams. Based on the experimental results, the reduction factor of equivalent stress distribution in concrete flange is suggested, and the calculation method of flexural stiffness and bending capacity of simply supported slim beams are proposed.