• Title/Summary/Keyword: Flame retardants

Search Result 131, Processing Time 0.021 seconds

Studies on Press Drying of Fire-Retardant Treated Plywood (내화처리합판(耐火處理合板)의 열판건조(熱板乾燥)에 관(關)한 연구(硏究))

  • Kim, Jong Man
    • Journal of Korean Society of Forest Science
    • /
    • v.56 no.1
    • /
    • pp.1-25
    • /
    • 1982
  • Plywood used for construction as a decorative inner material is inflammable and can cause fire accidents. causing destruction of human life and property. To diminish the fire disaster, fire retardant plywood is indeed required. In the methods of manufacturing the fire retardant plywood, a soaking method is occasionally used. However after soaking plywood into fire retardant chemical solutions redrying of soaked plywood is of the utmost importance. In this study 3.5mm and 5.0mm thickness plywoods were selected for fire retardant treatment. Treating solutions were prepared for 20% dilute solutions of ammonium sulfate, monoammonium phosphate, diammonium phosphate, borax-boric acid minalith, and water solution, 1-, 3-, 6-, and 9 hour-soaking treatments in borax-boric acid and minalith, and 6- and 9 hours in the other chemicals were applied and after the treatment hot drying was applied to treated plywoods at $90^{\circ}C$, $120^{\circ}C$ and $150^{\circ}C$ of press temperature. Drying rates, drying curves, water absorption rates of fire retardant chemicals, weight per volume and fire retardant degree of plywood were investigated. The results may be summarized as follows: 1) In the 9 hours-soaking treatment of fire retardants by hot and cold bath method, the chemical retentions of 3.5mm thickness plywood could be attained within the range ($1.125-2.25kg/(30cm)^3$) of minimum retention specification as follows: $1.353kg/(30cm)^3$ in monoammonium phosphate, $1.331kg/(30cm)^3$ in diammonium phosphate, $1.263kg/(30cm)^3$ in ammonium sulfate, $1.226kg/(30cm)^3$ in borax-boric acid. But the chemical retention, $0.906kg/(30cm)^3$, in minalith could not be attained within the range of minimum retention specification. And also in case of 5.0mm thickness plywood, chemical retentions, as $1.356kg/(30cm)^3$ and $1.166kg/(30cm)^3$ respectively, of ammonium sulfate and diammonium phosphate could be attained within the range minimum retention specification, but the other fire retardant chemicals could not. 2) In the 6- and - hours-soaking treatments of 3.5mm and 5.0mm thickness plywood, the drying curve sloped of chemical treated plywood was smaller than that of water treated. The drying rate related to thickness of treated plywood, was about three times as fast in 3.5mm thickness plywood compared with 5.0mm thickness plywood. 3) In the treatment at $120^{\circ}C$ of hot platen temperature, the drying rates of chemical-treated plywood showed the highest quantity in diammonium phosphate of 3.5mm and 5.0mm thickness plywood. But the drying rate of water treated plywood was highest during the 6- and 9 hours-soaking treatments. 4) The drying rate remarkably increased with proportion to increase of the platen temperature, and the values were respectively 1.23%/min., 6.54%/min., 25.75%/min. in hot platen temperature of $90^{\circ}C$, $120^{\circ}C$, $150^{\circ}C$ in 3.5mm thickness plywood and 0.55%.min., 2.49%/min., 8.19%/min. in hot platen temperature of $90^{\circ}C$, $120^{\circ}C$, $150^{\circ}C$ in 5.0mm thickness plywood. 5) In the fire retardant degree of chemical treated plywood, the loss in weight was the smallest in diammonium phosphate, next was in monoammonium phosphate and ammonium sulfate, and the greatest was in borax-boric acid and minalith. And the fire-retardant effect in burning time, flame-exhausted time and carbonized area were greatest in diammouniun phosphate, next were in monoammonium phosphate and ammonium sulfate, and the weakest were in borax-boric acid and minalith.

  • PDF