• Title/Summary/Keyword: Fillet welded joint

Search Result 66, Processing Time 0.038 seconds

A Study on Stree Analysis and Bending Fatigue Strength of One Side Fillet Welded T-joint (T형 평면용접이음재의 응력해석과 굽힘피로강도에 관한 연구)

  • Gang, Seong-Won;Lee, Tae-Hun;Jeon, Jae-Mok;Kim, Chung-Hui
    • Journal of Ocean Engineering and Technology
    • /
    • v.13 no.2 s.32
    • /
    • pp.51-57
    • /
    • 1999
  • In this study, one side fillet welded T-joint, used in box type girder and other welding structure, was investigated by stress analysis and bending fatigue test without edge preparation, with variation of joint shape. The purpose of this study is to give the welding condiltion and design standard on manufacturing one side fillet welded T-joint. As a result, the following conclusions were obtained. 1) In one side fillet welded T-joint, the larger the leg length and the penetration depth, the greater the bending fatigue strength because reduction of stress and strain on toe and root. The increase of the longitudinal leg length rather than vertical leg length contributed to the increase in bending fatigue strength. 2) In one side fillet welded T-joint without edge preparation, both general manual welding and general automatic welding were carried out with same condition. In this case, automatic welding showed deeper penetration and more increased longitudinal leg length than manual welding, so that automatic welding offers greater bending fatigue strength. 3) For one side fillet welded T-joint without edge preparation with automatic welding, the ratio(h/t) of the leg length(h) and the main plate thickness(t) in which toe crake can occur was 1.0 over.

  • PDF

A Study on Bending Fatigue Strength of One Side Fillet Welded T-Joint by SM 490A steel (Sm 490A강으로 제작된 T형 편면용접이음재의 굽힘피로강동에 관한 연구)

  • 엄동석;강성원;이태훈;이해우;조수형
    • Journal of Welding and Joining
    • /
    • v.16 no.5
    • /
    • pp.134-141
    • /
    • 1998
  • In this study, a fillet size for bending fatigue strength of one side fillet welded T-joint, used in box type girder and other welding structure, was investigated by bending fatigue test with or without edge preparation and burn through, with variation of joint shape. As a result, the following conclusions were obtained. (1) In one side fillet welded T-joint, the larger the leg length, the greater the bending fatigue strength. The increase in bending fatigue strength. (2) One side filet welded T-joint with edge preparation showed higher bending fatigue strength than that with twofold-large leg length and without edge preparation. (3) In one side fillet welded T-joint without edge preparation, both manual welding and automatic welding were carried out with same condition. In this case, automatic welding shoed deeper penetration and more increased horizontal leg length than manual welding, so that automatic welding offers grater bending fatigue strength. (4) For one side fillet welded T-joint without edge preparation, the ratio(h/t) of the leg length (h) and the main plate thickness (t) in which toe crack can occur was 1.2 over. (5) In one side fillet welded T-joint with edge preparation, the burn through led to reduced bending fatigue strength. However, this bending fatigue strength was higher than that of one side fillet welded T-joint without edge preparation and with a larger leg length.

  • PDF

A Study of the Thickness Effect using Structural Stress Approach for Fillet Welded Joints (구조 응력 기법을 적용한 필릿 용접부 두께 지수 산정에 관한 연구)

  • Xin, Wen-Jie;Oh, Dong-Jin;Kim, Myung-Hyun
    • Journal of Welding and Joining
    • /
    • v.32 no.2
    • /
    • pp.37-42
    • /
    • 2014
  • In this study, non-load-carrying fillet welded joints fabricated using EH grade-steel are evaluated with the structural stress approach. The thickness effect was investigated by a study on welded steel joints with thickness ranging from 25 to 80mm. As-welded joint for main plate thickness of 25 to 80mm, the fatigue strength is reduced gradually. On the other hand, in case of main plate thickness of 25 to 80mm, the structural stress concentration factor increases gradually. As a result, for structural stress approach, thickness effect is not required for correction. Based on these results, a new evaluation fillet welded joint for fatigue design purposes has been proposed FAT 125.

A study on the fatigue characteristics of SM 490 A material due to the welding type (SM 490 A 재질에 대한 용접 유형에 따른 피로특성 연구)

  • Kim, Jae-Hoon;Goo, Byung-Choon
    • Proceedings of the KSME Conference
    • /
    • 2004.11a
    • /
    • pp.274-278
    • /
    • 2004
  • This study investigates the fatigue characteristics of SM 490 A material specimens for the railway vehicle due to the welding type. The more stress ratio decreases, the more strength of fillet welded specimen decreases. At speciallly, when the stress ratio of TN(Plate with transverse fillet welded rib) specimens decreases 0.5, 0.1, and -0.1, the fatigue limit decreases unifomly. The strength of TN is higher than it of NCN in the compare of fillet welding type, but the strength of NCN(Non load-carrying cruciform fillet welded joint) is higher than it of CN(Load-carrying cruciform fillet welded joint), which these specimens have the rib in the both side. We analysis the strains on the weld positions of the TN specimens during the fatigue test for the investigation of crack initiation and crack growth. In the theses results, we could find the fatigue crack initiation point and time.

  • PDF

Design of Welded Joints Using Stress Intensity Factors (응력확대계수를 이용한 용접이음부 설계 연구)

  • Park, Ji-Woo;Gu, Man-Hoi;Choi, Chang;Sung, Wan
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 1996.11a
    • /
    • pp.1058-1062
    • /
    • 1996
  • The assessments of weld defects by fracture mechanics are performed for design of welded Joints. In general, butt, T-type, and L-type welded joint are useful for welding structure. When linear weld defects are in welded joint, stress intensity factors for each joints are calculated by finite element method. Analysis results are shown for the fracture modes and characteristics of joint types. And they are founded for the weaken order of welded joints being T-type, butt, L-type.

  • PDF

A Study on Stress Concentration Factor at Fillet Welded Joint (필렛용접이음부의 응력집중계수에 관한 연구)

  • S.W. Kang;W.I. Ha;J.S. Shin;J.S. Jae
    • Journal of the Society of Naval Architects of Korea
    • /
    • v.33 no.3
    • /
    • pp.1-7
    • /
    • 1996
  • The stress concentration factor gives the significant effect the fatigue strength of welded joints. The model used herein is the type of the load carrying fillet welded cruciform joint with full or partial penetration. In order to obtain the stress concentration factor at the weld toe of fillet joint, the reasonable element size of the toe part is investigated and the stress analysis for the series models by FEM under tensile load is performed. On the basis of the calculation results, the estimated formulae for the stress concentration factor(Kt) at weld toe part of the fillet welded joint, which the effect of toe radius, flank angle and other parameters are taken into account, is derived.

  • PDF

A Study on Fatigue Design for Welded Joint of STS301L (STS301L 용접종류별 이음재의 피로설계에 관한 연구)

  • Baek, Seung-Yeb
    • Journal of Welding and Joining
    • /
    • v.28 no.3
    • /
    • pp.86-91
    • /
    • 2010
  • Stainless steel sheets are widely used as the structural material for the railroad cars and the commercial vehicles. These kinds structures used stainless steel sheets are commonly fabricated by using the gas welding. For fatigue design of gas welded joints such as fillet and plug type joint, it is necessary to obtain design information on stress distribution at the weldment as well as fatigue strength of gas welded joints. And also, the influence of the geometrical parameters of gas welded joints on stress distribution and fatigue strength must be evaluated. the ${\Delta}P-N_f$ curves were obtained by fatigue tests. Using these results, ${\Delta}P-N_f$ curves were rearranged in the ${\Delta}{\sigma}-N_f$ relation with the maximum stress at the edge of fillet welded joint.

A Study on Fatigue Design for Fillet Welded faint of STS301L (STS301L 필렛 용접이음재의 피로설계에 관한 연구)

  • Baek, Seung-Yeop;Bae, Dong-Ho
    • Proceedings of the KWS Conference
    • /
    • 2006.10a
    • /
    • pp.29-31
    • /
    • 2006
  • Stainless steel sheets are widely used as the structural material for the railroad cars and the commercial vehicles. These kinds structures used stainless steel sheets are commonly fabricated by using the gas welding. For fatigue design of gas welded joints such as fillet and plug type joint, it is necessary to obtain design information on stress distribution at the weldment as well as fatigue strength of gas welded joints. And also, the influence of the geometrical parameters of gas welded joints on stress distribution and fatigue strength must be evaluated. the ${\Delta}P-N_f$ curves were obtained by fatigue tests. Using these results, ${\Delta}P-N_f$ curves were rearranged in the ${\sigma}-N_f$ relation with the maximum stress at the edge of fillet welded joint.

  • PDF

A Study on the Distribution of Residual Stress in Fillet Welds for Thick Mild Steel Plate (두꺼운 연강판(軟鋼板) 필렛 용접(熔接)이음부의 잔류응력분포(殘留應力分布)에 대한 연구(硏究))

  • Dong-Suk,Um;Sung-Won,Kang
    • Bulletin of the Society of Naval Architects of Korea
    • /
    • v.20 no.4
    • /
    • pp.17-24
    • /
    • 1983
  • In this study, it was investigated the distribution of residual stress in the direction of loading between the root and toe the load fillet welds for thick steel plate. Residual stress distributions are measured by sectioning method which is one of stress-relaxation technique in welded joint, and analyzed by two dimensional finite element method on thermo-elasto-plastic theory under plane stress condition. These are compared the results of F.E.M analysis with the experimental result by stress-relaxation techniques. As a results, the following conclusion were obtained. (1) In the no penetration fillet welded joint specimen using mild steel plate with 25mm in thickness, the residual stress of loading direction near the root was about $10kg/mm^2$ tensile. (2) The tensile residual stress has been observed in fillet region of the fillet joint by F.E.M. analysis method. (3) The range of compressive residual stress distribution from the root was largest in the case of 5mm root penetration.

  • PDF