• 제목/요약/키워드: Fiber single crystals

검색결과 11건 처리시간 0.027초

LiNbO3 섬유 단결정의 분극에 관한 연구 (Study on Poling of LiNbO3 Fiber Single Crystals)

  • 강봉훈;장재혁;최덕균;신태희;주기태
    • 한국세라믹학회지
    • /
    • 제46권4호
    • /
    • pp.419-424
    • /
    • 2009
  • Congruent or stoichiometric $LiNbO_3$ fiber single crystals were grown by the $\mu$-PD method, and the grown fiber crystals have the several (2 or 3) ridges with a diameter of $1.35{\sim}1.5\;mm$ and a length of $40{\sim}100\;mm$. In this $\mu$-PD process, different growth rates ($10{\sim}60\;mm/h$) were applied. Pt wire or $LiNbO_3$ crystal was used as a seed. The properties of grown $LiNbO_3$ fiber single crystals having a-axis or c-axis according to seeds were effected by the grown conditions(Pt tube diameter, pulling speed, after heater etc.). Disk-type $LiNbO_3$ samples were poled in condition of DC 5 V/cm at 1050, 1075 or $1100^{\circ}C$. XRD, SEM, conoscope image through the polarized microscope, $T_C$ measuring apparatus, optical transmittance measuring instrument are used to identify the properties of $LiNbO_3$.

(Bi2O3)0.85.(Nb2O5)0.15-6Bi2O3.SiO2계 복합다결정체의 미세구조와 광학적 특성 (Microstructures and Optical Properties of Composite Crystals in the System (Bi2O3)0.85.(Nb2O5)0.15-6Bi2O3.SiO2)

  • 김호건
    • 한국세라믹학회지
    • /
    • 제26권1호
    • /
    • pp.139-145
    • /
    • 1989
  • An eutectic melt in the system(Bi2O3)0.85·(Nb2O5)0.15-6Bi2O3·SiO2 was unidirectionally solidfield at a rate of 0.5mm/h under a thermal gradient of 100℃/cm. Double crucibles and seed crystal plate were used in order to botain the composite crystals which had uniform microstructure throughout the ingot. The obtained composite crystals showed uniform microstructure, in which needle-like δ-(Bi2O3)0.85·(Nb2O5)0.15 crystals were arrayed in parallel in a matrix of γ-6Bi2O3·SiO2 single crystal. It was found that the <110> direction of δ-(Bi2O3)0.85·(Nb2O5)0.15 crystal was essentially parallel to the <111> direction of γ-6Bi2O3·SiO2 crystal in the composite crystals. A transverse thin plate of the composite crystals showed a high resolution optical transmission like an optical fiber array, and sharp chatoyancy was observed in the cabochon shaped composite crystals. Then, this may be useful for applications such as screen of a cathode ray tube or artificial cat's eye gem stones.

  • PDF

${\mu}-PD$ 법으로 성장시킨 near-stoichiometric 조성 $Zn:LiNbO_3$ fiber 단결정 성장 및 광손상 특성 (Crystal growth and optical properties of near-stoichiometric $Zn:LiNbO_3$ fiber single crystal by ${\mu}-PD$ method)

  • 이호준;서중원;신동익;송원영;윤대호
    • 한국결정성장학회지
    • /
    • 제16권6호
    • /
    • pp.235-239
    • /
    • 2006
  • Micro-pulling down$({\mu}-PD)$법을 이용하여 직경 $0.8{\sim}1.0mm$, 길이 $30{\sim}35mm$의 ZnO가 첨가된 near-stoichiometric $LiNbO_3$, 단결정을 성장하였다. 성장된 결정의 결정구조를 powder x-tay diffraction(XRD) patterns으로 확인하였고, electron probe micro analysis(EPMA)를 이용하여 결정내 Zn 이온들이 균일하게 분포되었음을 확인하였다. 또한 2 mol% 이상의 ZnO 첨가시 $OH^-$ 흡수밴드의 특성이 크게 변화함을 관찰함으로써 ZnO 첨가량에 일치한 역치(threshold)가 존재함을 확인하였다.

섬유상 분말로 제조된 배향성을 가진 $BaTiO_3$ 세라믹 (Oriented Barium Titanate Ceramics Made from Fiber State Powder)

  • 서용교;야나기다히로아끼
    • 한국세라믹학회지
    • /
    • 제30권12호
    • /
    • pp.1066-1070
    • /
    • 1993
  • When looked upon as a polycrystalline, ceramics have two basic differences from a single crystal. One is that there exist grain boundaries, the other is that the crystal axes of each small crystal are arranged in random directions. But the crystal axes fo small crystals which compose ceramics may be made to have the tendency of being arranged in a specific direction. This is called that the crystal axes are oriented. The degree of the direction arrangement of the crystal axes is called orientation. In order to orient the crystal axes effectively, the fiberous barium titanates were made through KDC method and the ion exchange method. And then they were arranged through pressing, doctor blade, and syringe. As the result of Lotgering evaluation, the sample oriented through syringe showed the highest orientation. After sintering, though the most particles that had been fiberous shaped became global shape viewed through SEM, the orientation of the crystals was reinforced by means of sintering.

  • PDF

Electrically Controllable Fiber Bragg Gratings with Liquid Crystal Cladding

  • Baek Seungin;Roh Sookyoung;Na Jun-Hee;Kwon Jaejoong;Yoon Ilyong;Chung Seunghwan;Jeong Cherlhyun;Lee Sin-Doo;Lee Byoungho;Jeong Yoonchan
    • Journal of the Optical Society of Korea
    • /
    • 제9권3호
    • /
    • pp.123-128
    • /
    • 2005
  • An electrically controllable fiber Bragg grating inscribed in a hydrogen-loaded standard single-mode fiber with liquid-crystal cladding is presented. Control of the optic axis of liquid crystals by means of external electric fields results in the change of reflectivity and Bragg wavelength of the grating. The increase of surrounding refractive index of a fiber makes effective refractive index of a propagation mode higher, which results in high field confinement and longer Bragg wavelength. The reduction of the fiber diameter by chemical etching process improves the long-range ordering of liquid-crystal molecules and reduces controlling voltage. The tunable ranges of reflectivity and Bragg wavelength of the liquid crystal-cladding fiber Bragg grating were $\~4.6dB\;and\;\~0.3nm$, respectively.

$Er^{3+}$ 첨가 $LiNbO_3$ fiber 단결정의 성장 및 upconversion 특성 (Growth and upconversion properties of erbium doped $LiNbO_3$ single crystal fibers)

  • Yang, Woo-Seok;Suh, Su-Jeong;Lee, Jong-Ho;Tsuguo Fukuda;Yoon, Dae-Ho
    • 한국결정성장학회:학술대회논문집
    • /
    • 한국결정성장학회 1999년도 PROCEEDINGS OF 99 INTERNATIONAL CONFERENCE OF THE KACG AND 6TH KOREA·JAPAN EMG SYMPOSIUM (ELECTRONIC MATERIALS GROWTH SYMPOSIUM), HANYANG UNIVERSITY, SEOUL, 06월 09일 JUNE 1999
    • /
    • pp.321-335
    • /
    • 1999
  • Erbium(Er) doped LiNbO3(Er:LiNbO3) single crystal gibers were grown free of cracks along the c-axis by micro-pulling down method. the Er3+ concentration was distributed homogeneously along the growth axis. The samples for optical characterization were cut from as-grown single crystal fibers and polished. When the 980 nm light was incident on the sample, upconversion phenomena were observed at the green range of wavelength 510~570 nm. In addition, the intensity of upconversion was remarkably increased by increasing the concentration of Er2O3 dopant in as-grown Er:LiNbO3 crystals.

  • PDF

Spinodal Phase Separation and Isothermal Crystallization Behavior in Blends of VDF/TrFE(75/25) Copolymer and Poly(1,4-butylene adipate) (I) -Spinodal Phase Separation Behavior-

  • Kim, Kap Jin;Kyu, Thein
    • Fibers and Polymers
    • /
    • 제4권4호
    • /
    • pp.188-194
    • /
    • 2003
  • Phase behavior and spinodal phase separation kinetics in binary blends of a random copolymer of vinylidene fluoride and trifluoroethylene (75/25) [P(VDF/TrFE)] and poly(l,4-butylene adipate) (PBA) have been investigated by means of optical microscopic observation and time-resolved light scattering. The blends exhibited a typical lower critical solution temperature (LCST)∼${34}^{\circ}C$ above the melting temperature of the P(VDF/TrFE) crystals over the entire blend composition range. P(VDF/TrFE) and PBA were totally miscible in the temperature gap between the melting point of P(VDF/TrFE) and the LCST. Temperature jump experiments of the 3/7 P(VDF/TrFE)/PBA blend were carried out on a light-scattering apparatus from a single-phase melt state (${180}^{\circ}C$) to a two-phase region (205∼${215}^{\circ}C$). Since the late stage of spinodal decomposition (SD) is prevalent in the 3/7 blend, SD was analyzed using a power law scheme. Self-similarity was preserved well in the late stage of SD in the 3/7 blend.

Nd\2O3 첨가에 따른 화학양론조성 LiNbO3 단결정의 성장 및 형광특성 (Crystal Growth and Photoluminescence Property of Stoichiometric LiNbO3 Single Crystal Fiber by Addition of Nd2O3)

  • 서중원;윤석규;이성문;윤대호
    • 한국세라믹학회지
    • /
    • 제39권10호
    • /
    • pp.977-980
    • /
    • 2002
  • Micro-pulling down법을 이용하여 $Nd_2O_3$가 첨가된 crack 등의 결함이 없는 화학양론조성의 $LiNbO_3$ 단결정을 직경 1 mm, 길이 30∼35 mm의 크기로 성장시켰다. Electron probe micro analysis를 이용하여 결정 내에 $Nd_2O_3$가 균일하게 분포되어있음을 확인하였다. 성장된 결정의 $Nd_2O_3$ 첨가에 따른 흡수 band를 관찰하였고 $Nd_2O_3$ 첨가량 변화에 따른 형광특성의 변화를 측정하였다.