• 제목/요약/키워드: Fe-Cr

검색결과 1,717건 처리시간 0.03초

The Effect of Cr Dosage on FePt Nanoparticle Formation

  • Won, C.;Keavney, D.J.;Divan, R.;Bader, S.D.
    • Journal of Magnetics
    • /
    • 제11권4호
    • /
    • pp.182-188
    • /
    • 2006
  • The search for high-density recording materials has been one of most active and vigorous field in the field of magnetism. $FePt-L1_{0}$ nanoparticle has emerged as a potential candidate because of its high anisotropy. In this paper, we provide an overview of recent work at Argonne National Laboratory that contributes to the ongoing dialogue concerning the relation between structure and properties of the FePt nanoparticle system. In particular we discuss the ability to control structure and properties via dosing with Cr. Cr-dosed FePt films were grown via molecular beam epitaxy and annealed at $550^{\circ}C$ in an ultrahigh vacuum chamber, and were studied with the surface magneto-optic Kerr effect (SMOKE), scanning electron microscopy (SEM) and x-ray magnetic circular dichroism (XMCD). We found that small dosage of Cr helps to generate $L1_{0}$ phase FePt magnetic nanoparticles with small size, defined shape and regular spatial distribution on MgO (001) substrate. The nanostructures are ferromagnetic with high magnetic coercivity (${\sim}0.9T$) and magnetic easy axis in the desired out-of-plane orientation. We also show that controlling the lateral region where nanostructures exist is possible via artificial patterning with Cr.

(Cr, Fe)-doped Y2O3-Al2O3계 붉은 안료의 합성과 특성 (Synthesis and Characterization of (Cr, Fe)-doped Y2O3-Al2O3 Red Pigments)

  • 신경현;이병하
    • 한국세라믹학회지
    • /
    • 제46권4호
    • /
    • pp.350-356
    • /
    • 2009
  • Perovskite codoped with chromium and iron have been studied. Samples with $YAl_{0.96}(Cr_{0.04-x}Fe_x)O_3$(x=0.01, 0.02, 0.03, 0.04) were prepared by solid state reaction at $1450^{\circ}C$ for 6 h and were characterized by XRD, FT-IR, Raman spectroscopy, SEM and UV-vis spectrophotometer. The color of the synthesized pigments were from red to dark brown(in bulk). Up to 0.02 mole $Fe_2O_3$ for substituting $Cr_2O_3$ development of color in lime-glaze gives good red color but as increasing amount of $Fe_2O_3$ and decreasing $Cr_2O_3$ proportionally produce from brownish red to brown. Increasing $Fe_2O_3$ amount lead to weaken crystal field relatively due to have smaller ionic radius than $Cr_2O_3$ ionic one. The UV-vis peaks were shifted to lower wavelength.

진해만 퇴적물중의 중금속 함량 (HEAVY METALS IN SEDIMENTS FROM JINHAE BAY, KOREA.)

  • 이수형;이광우
    • 한국해양학회지
    • /
    • 제18권1호
    • /
    • pp.49-54
    • /
    • 1983
  • 진해만의 중금속 오염 현황 파악을 위하여 퇴적물중의 중금속 함량을 조사 하였다. 조사된 중금속은 Cd, Cr, Cu, Fe, Ni, Mn, Pb, Zn등 9가지 원소이며 모두 23개 조사점에서 시료를 채취하여 원자흡수 분광법에 의해 중금속 함량을 분석 하였다. 본 조사 결과로는 Cd, Cr, Cu, Pb, Zn 등의 함량은 마산만이 다른 해역 보다 월등히 높았으며 또 내만에서 외양으로 나갈수록 함량이 뚜렷하게 감소 하였으나 Co, Fe, Ni, Mn 등은 해역간에 별다른 농도 차이를 나타내지 않았다. 중금속의 통계학적 상관 관계를 보면 Cd, Cr, Cu, Pb, Zn group과 co, Fe, Ni group 으로 나뉘어져 각 group 내에서중금속 상호간에 유의성 있는 상관 관계를 나타내었으나 group 간에는 상관 관계를 보이지 않았다.

  • PDF

Precipitation Behavior of ${\gamma}"$ in Severely Plastic Deformed Ni-base Alloys

  • Kim, Il-Ho;Kwun, S.I.
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.962-963
    • /
    • 2006
  • The precipitation behaviors of ${\gamma}"(Ni_3Nb)$ in four Ni-base alloys were investigated. The four alloys were forged Ni20Cr20Fe5Nb alloy, mechanically alloyed Ni20Cr20Fe5Nb alloy, IN 718 alloy and ECAPed(equal channel angular pressing) IN 718 alloy. Aging treatment was employed at either $600^{\circ}C$ or $720^{\circ}C$ for 20 hrs. The TEM observation and hardness test were performed to identify the formation of ${\gamma}"$. The precipitation of ${\gamma}"$ was noticed after aging at $600^{\circ}C$ for 20 hrs in the mechanically alloyed Ni20Cr20Fe5Nb alloy and ECAPed IN 718 alloy, while it was observed after aging at $720^{\circ}C$ for 20 hrs in the forged Ni20Cr20Fe5Nb alloy and IN 718 alloy before ECAP. The lower aging temperature for ${\gamma}"$ precipitation in the mechanically alloyed Ni20Cr20Fe5Nb alloy and ECAPed IN 718 alloy than in the forged Ni20Cr20Fe5Nb alloy and IN 718 alloy before ECAP appeared to be due to the severe plastic deformation which occurred during mechanical alloying or ECAP.

  • PDF

13Cr-1.5Nb-Fe 스텐레스 센서재료의 제조 및 연자기특성 (Fabrication and Magnetic Process of 13Cr-1.5Nb-Fe Stainless Sensors)

  • 윤성호;김택기;조용수
    • 한국자기학회지
    • /
    • 제8권3호
    • /
    • pp.125-130
    • /
    • 1998
  • 13Cr-1.5Nb-Fe합금분말이 수분사법으로 제조되엇다. 제조된 합금뷴말을 압축기를 이용하여 ring현상으로 성형한후, 진공중에서 소결하였다. as-prepared 분말의 현상, 입도분포, 성분분석 및 포화자화물 조사하였으며, 소결된 시편의 투자율, 교류자기이력손실이 조사되었다. as-prepared 13Cr-1.5Nb-Fe합금분말의 포화자화는 160emu/g이었으며, 산소함유량은 약 600ppm이었다. 입도분포는 약 70$\mu$m에서 50%vol.을 나타낸다. 교류투자율은 소결온도 및 성형온도가 증가할수록 증가한다. 주파수 20KHz에서 교류자기이력손실은 12ton/cm2성령압력 및 120$0^{\circ}C$ 소결온도 조건에서 107W/cc로 가장우수하다.

  • PDF

진공다이캐스트법에 의한 Al합금과 Fe-17wt%Cr 강의 주조접합 특성연구 (A Study on the Characteristics of Cast Bonding Aluminium Alloy and Fe-17wt%Cr Steel with Vacuum Die Casting)

  • 김용현;김억수;김흥식;이광학
    • 한국주조공학회지
    • /
    • 제19권5호
    • /
    • pp.410-418
    • /
    • 1999
  • To overcome the undesirable deformation, peeling off and geometrical restrictions which were mainly caused by differences in thermal expansion coefficients during the cladding of aluminum strip and stainless strip, new processing method based on vacuum die casting is designed and implemented in fabricating Fe-17wt%Cr steel (stainless steel). To increase cast-bonding ability, the surface of Fe-17wt%Cr steel is electrochemical etched to have optimum pit size (above 0.2 mm) and pit density (above 30%). The implementation of vacuum die casting by using surface treated stainless steel (Fe-17wt%Cr Steel) produces good trial products having acceptable cast-bonding ability. The enabling conditions for cast-bonding are pouring temperature $690^{\circ}C$, filling speed 30 m/sec and casting pressure $800\;kg/cm^2$. The microscopic observation of cast-bonded Al/Fe-17wt%Cr steel does not show any evidence of intermetallic compounds. The bonding strength of trial products is $150-400\;kg/cm^2$ and this is stronger than conventionally cladded metal having $30-70\;kg/cm^2$.

  • PDF

Fe-16Cr-6Ni-6Mn-1.7Mo 스테인리스 합금의 700~900℃에서의 대기중 산화 (Atmospheric Oxidation of Fe-16Cr-6Ni-6Mn-1.7Mo Stainless Steel between 700 and 900℃)

  • 이동복
    • 대한금속재료학회지
    • /
    • 제49권2호
    • /
    • pp.153-160
    • /
    • 2011
  • The AISI 216L stainless steel with a composition of Fe-16Cr-6Ni-6Mn-1.7Mo (wt.%) was oxidized at $700{\sim}900^{\circ}C$ in air for 100 h. At $700^{\circ}C$, a thin $Mn_{1.5}Cr_{1.5}O_4$ oxide layer with a thickness of $0.4{\mu}m$ formed. At $800^{\circ}C$, an outer thin $Fe_2O_3$ oxide layer and a thick inner $FeCr_2O_4$ oxide layer with a total thickness of $30{\mu}m$ formed. The non-adherent scale formed at $800^{\circ}C$ was susceptible to cracking. At $900^{\circ}C$, an outer thin $Fe_2O_3$ oxide layer and a thick inner $Mn_{1.5}Cr_{1.5}O_4$ oxide layer formed, whose total thickness was $10{\sim}15{\mu}m$. The scales formed at $900^{\circ}C$ were non-adherent and susceptible to cracking. 216 L stainless steel oxidized faster than 316 L stainless steel, owing to the increment of the Mn content and the decrement of Ni content.

선택적 레이저 용융법으로 제조된 CoCrFeMnNi계 고엔트로피합금의 미세조직 및 기계적 물성 연구 동향 (Microstructure and Mechanical Properties of CoCrFeMnNi-type High-entropy Alloy Fabricated by Selective Laser Melting: A Review)

  • 박정민
    • 한국분말재료학회지
    • /
    • 제29권2호
    • /
    • pp.132-151
    • /
    • 2022
  • The CoCrFeMnNi high-entropy alloy (HEA), which is the most widely known HEA with a single face-centered cubic structure, has attracted significant academic attention over the past decade owing to its outstanding multifunctional performance. Recent studies have suggested that CoCrFeMnNi-type HEAs exhibit excellent printability for selective laser melting (SLM) under a wide range of process conditions. Moreover, it has been suggested that SLM can not only provide great topological freedom of design but also exhibit excellent mechanical properties by overcoming the strength-ductility trade-off via producing a hierarchical heterogeneous microstructure. In this regard, the SLM-processed CoCrFeMnNi HEA has been extensively studied to comprehensively understand the mechanisms of microstructural evolution and resulting changes in mechanical properties. In this review, recent studies on CoCrFeMnNi-type HEAs produced using SLM are discussed with respect to process-induced microstructural evolution and the relationship between hierarchical heterogeneous microstructure and mechanical properties.

CoO가 첨가되지 않은 스피넬계 흑색안료의 합성 (Synthesis of Cobalt Oxide Free Black Color Spinel Pigment)

  • 김준호;이성호;서만철;이병하
    • 한국세라믹학회지
    • /
    • 제44권11호
    • /
    • pp.639-644
    • /
    • 2007
  • Spinel pigments, developing black color in high temperature glazes at oxidation or reduction atmosphere, without CoO because of its high price were synthesized by solid solution method. Ten mixed compositions consisted of NiO, MnO, $Fe_2O_3 and $Mn_2O_3$ were fired at $1250^{\circ}C$ for 1h. The resulting pigments were characterized by using XRD, FT-IR, SEM and UV-vis spectrometer. Structure of the pigments are spinel and particles' shape are spherical or cubic. Glazed tiles containing 5 wt% pigments were fired at $1260^{\circ}C$ and $1240^{\circ}C$ in reduction atmosphere. Color in glazes were analyzed by UV-vis spectrometer. Colors of NiO 0.875 MnO $0.125{\cdot}Fe_2O_3$ $0.4875{\cdot}Cr_2O_3$ $0.50{\cdot}Mn_2O_3$ 0.0125 mole% and NiO 0.875 MnO $0.125{\cdot}Fe_2O_3$ $0.3875{\cdot}Cr_2O_3$ $0.50{\cdot}Mn_2O_3$ 0.1125 mole% in lime glaze showed black in oxidation, in reduction NiO 0.875 MnO $0.125{\cdot}Fe_2O_3$ $0.4875{\cdot}Cr_2O_3$ $0.50{\cdot}Mn_2O_3$ 0.0125 mole% and NiO 0.875 MnO $0.125{\cdot}Fe_2O_3$ $0.4375{\cdot}Cr_2O_3$ $0.55{\cdot}Mn_2O_3$ 0.0125 mole% showed black. In case of lime-barium glaze, NiO 0.875 MnO $0.125{\cdot}Fe_2O_3$ $0.3875{\cdot}Cr_2O_3$ $0.50{\cdot}Mn_2O_3$ 0.1125 mole%, NiO 0.975 MnO $0.075{\cdot}Fe_2O_3$ $0.4375{\cdot}Cr_2O_3$ $0.50{\cdot}Mn_2O_3$ 0.0625 mole% and NiO 0.925 MnO $0.075{\cdot}Fe_2O_3$ $0.4375{\cdot}Cr_2O_3$ $0.50{\cdot}Mn_2O_3$ 0.0625 mole% showed black color in oxidation and NiO 0.875 MnO $0.125{\cdot}Fe_2O_3$ $0.3875{\cdot}Cr_2O_3$ $0.50{\cdot}Mn_2O_3$ 0.1125 mole%, NiO 0.925 MnO $0.075{\cdot}Fe_2O_3$ $0.4375{\cdot}Cr_2O_3$ $0.50{\cdot}Mn_2O_3$ 0.0625 mole% and NiO 0.725 MnO $0.275{\cdot}Fe_2O_3$ $0.4375{\cdot}Cr_2O_3$ $0.50{\cdot}Mn_2O_3$ 0.0625 mole% showed black one in reduction.

Fe-(10~40%)Cr강의 800~900℃에서의 Na2SO4 염에서의 부식 (Corrosion of Fe-(10~40)%Cr Steels in Na2SO4 Salts at 800~900℃)

  • 김슬기;이재호;이동복
    • 대한금속재료학회지
    • /
    • 제50권5호
    • /
    • pp.361-368
    • /
    • 2012
  • Fe-(10, 20, 30, 40) wt%Cr alloys were corroded in $Na_2SO_4$ salts ($m.p.=884^{\circ}C$) at $800{\sim}900^{\circ}C$ for 3-300 hrs. Their corrosion resistance increased with an increase in Cr content owing to the formation of slowly growing $Cr_2O_3$. During corrosion, $Na_2SO_4$ dissociated and reacted with the alloys to form $Cr_2O_3$ and $Fe_2O_3$. Since $Fe_2O_3$ dissolved fast into the salts, most of the scales consisted primarily of $Cr_2O_3$. Inside the scale, a small amount of sulfides also existed. The oxidation, dissolution and detachment of the formed scales occurred significantly.