High Temperature Oxidation of ${Fe_3}Al-4Cr$ Alloys (${Fe_3}Al-4Cr$ 합금의 고온산화)

  • Kim, Gi-Young;Lee, Dong-Bok
    • Korean Journal of Materials Research
    • /
    • v.11 no.1
    • /
    • pp.34-38
    • /
    • 2001
  • Intermetallics of Fe-28%Al($Fe_3Al$) and Fe-28%Al-4%Cr($Fe_3Al-4Cr$) were oxidized at 1073, 1273 and 1473k in air for up to 17 days. The oxidation resistance of$Fe_3Al-4Cr$ was basically similar to or better than that of $Fe_3Al$. The oxide scales formed on $Fe_3Al$ consisted essentially of pure ${\alpha}-AL_2O_3$, while those formed on $Fe_3Al-4Cr$ consisted of ${\alpha}-AL_2O_3$ having dissolved iron and chromium ions. The preferential outward diffusion of substrate elements to form the outer oxide layer led to the formation of Kirkendall voids at the oxide-matrix interface. The scales formed on $Fe_3Al(-4Cr)$ were thin and dense up to 1273K, but they spalled easily at 1473K, accompanied by more weight gains.

  • PDF

Thermal Stability of Al-Fe-X Alloy System Prepared by Mechanical Alloying and Spark Plasma Sintering: II. Al-Fe-Cr and Al-Fe-Mo (기계적 합금화 및 스파크 플라즈마 소결에 의해 제조된 Al-Fe-X계 합금의 열적 안정성: II. Al-Fe-Cr and Al-Fe-Mo)

  • Lee, Hyun-Kwuon;Lee, Sang-Woo;Cho, Kyeong-Sik
    • Journal of Powder Materials
    • /
    • v.12 no.1
    • /
    • pp.43-50
    • /
    • 2005
  • Mechanical alloying using high-energy ball mill and subsequent spark plasma sintering (SPS) process was applied to Al-Fe-Cr and Al-Fe-Mo powder mixture to investigate effects of Cr and Mo addition on thermal stability of Al-Fe, and thereby to enhance its thermal stability up to $500^{\circC}$. Various analytical techniques including micro-Vickers hardness test, SEM, TEM, X-ray diffractometry and corrosion test were carried out. It was found that addition of Cr and Mo to Al-Fe system played a role of grain growth inhibitor of matrix Al and some precipitates such as $Al_3Fe$ during SPS and subsequent heat treatment. The inhibition of grain growth resulted in increased Vickers hardness and thermal stability up to $500^{\circC}$ comparing to those of Al-Fe alloy system.

Characterization of Oxide Scales Formed on Fe3Al, Fe3Al-Cr, Fe3Al-Cr-Mo, Ni3Al and Ni3Al-Cr Alloys (Fe3Al, Fe3Al-Cr, Fe3Al-Cr-Mo, Ni3Al 및 Ni3Al-Cr 합금표면에 형성된 산화물 특성분석)

  • Shim, Woung-Shik;Lee, Dong-Bok
    • Korean Journal of Materials Research
    • /
    • v.12 no.11
    • /
    • pp.845-849
    • /
    • 2002
  • Alloys of $Fe_3$Al, $Fe_3$Al-6Cr, $Fe_3$Al-4Cr-1Mo, $Ni_3$Al, and $Ni_3$Al-2.8Cr were oxidized at $1000^{\circ}C$ in air, and the oxide scales formed were studied using XRD. SEM, EPMA, and TEM. The oxide scales that formed on $Fe_3$Al-based alloys consisted primarily of $\alpha$-$Al_2$$O_3$ containing a small amount of dissolved Fe and Cr ions, whereas those that formed on $Ni_3$Al-based alloys consisted primarily of $\alpha$-$Al_2$$O_3$, together with a small amount of $NiAl_2$$O_4$, NiO and dissolved Cr ions. For the entire alloys tested, nonadherent oxide scales formed, and voids were inevitably existed at the scale-matrix interface.

Corrosion of AI-Fe Coatings for Wet-Seal Area in Molten Carbonate Fuel Cells

  • Jun, JaeHo;Jun, JoongHwan;Kim, KyooYoung
    • Corrosion Science and Technology
    • /
    • v.3 no.3
    • /
    • pp.98-101
    • /
    • 2004
  • The corrosion behavior of Al-Fe coatings was studied in the wet-seal atmosphere of molten carbonate fuel cells (MCFC). Fe-8Al, Fe-16Al, Fe-25Al, Fe-36Al, and Fe-70Al (in at.%) specimens were tested in Li/K carbonate at $650^{\circ}C$ by a single cell test and an immersion test. In general, the corrosion resistance of the Al-Fe coatings was enhanced due to the formation of a protective $LiAlO_2$ layer. However, when the Al-Fe coatings didn't have sufficient content of aluminum enough for maintaining the protective layer, the corrosion resistance of the Al-Fe coatings was severely degraded by the growth of non-protective scales like $LiAlO_2$. The test results revealed that the aluminum contents in the coatings should be higher than 25 at.% in order to form and maintain the protective $LiAlO_2$ layers.

A Study on the Precipitates in Rapidly Solidified Al-(Fe, Ce) Alloys by Analysis of X-Ray Diffraction (급냉응고된 Al-(Fe, Ce) 합금에서 형성되는 석출상의 X-선적연구)

  • Park, Ik-Min;Lee, Kyu-Han;Choe, Jeong-Cheol;Jo, Hyung-Ho
    • Journal of Korea Foundry Society
    • /
    • v.8 no.4
    • /
    • pp.446-452
    • /
    • 1988
  • To obtain detailed information on the metastable and the equilibrium phases in rapidly solidified Al-(Fe,Ce) alloys, analysis of X-ray diffraction pattern has been carried out. It has been found that the metastable phase formed in Al-Fe alloys including up to 6wt%Fe is $Al_6Fe$ and the equilibrium phase is $Al_3Fe$. Any X-ray diffraction peak corresponding to the equilibrium phase $Al_{13}Fe_4$ has not been observed during aging. In Al-4wt%Fe alloy, which is ribbon shape with thickness less than $70\;{\mu}m$, aged at $400^{\circ}C$ for 1h after rapid solidification, unidentified phase has been found. In Al-4wt%Ce alloy, only X-ray diffraction peak corresponding to the equilibrium phase, $Al_4Ce$ has been observed. It has been found that the metastable phase Formed in Al-Fe-Ce alloys including up to 6wt% Fe and 4wt% Ce is $Al_6Fe$ and the equilibrium phases are $Al_3Fe$ and $Al_{10}CeFe_2$.

  • PDF

Fabrication of$Al_2O_3/Fe$ composite by reaction sintering (반응소결법에 의한 $Al_2O_3/Fe$ 복합재료 제조)

  • 김송희;윤여범
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.9 no.2
    • /
    • pp.185-190
    • /
    • 1999
  • An $Al_2O_3/Fe$ composite was synthesized through the double stage processes by a reaction sintering which requires simple process and equipments but provides near-net-shape, a reduction/oxidation process for 5 hrs at $650^{\circ}C$ was followed by sintering at $1200^{\circ}C$ to form an $Al_2O_3/Fe$ composite. The composite processed through the double stage sintering are mainly consists of $\alpha$-Fe and ${\alpha}Al_2O_3$ with minor amount of $FeAl_2O_4$, a spinnel structure which is known to prevent Fe from filling up the pores and good contact with $Al_2O_3/Fe$ particles.

  • PDF

The Formation Behavior and Thermal Stability of $E_6$ Eutectic Phase in Unidirectionally Solidified Al-Fe Alloys (일방향 응고시킨 Al-Fe계 합금에서 $E_6$ 공정상의 생성특성과 열적안정성)

  • Jung, Hae-Ryong
    • Journal of Korea Foundry Society
    • /
    • v.19 no.1
    • /
    • pp.71-76
    • /
    • 1999
  • Eutectic and off-eutectic Al-Fe alloys were unidirectionally solidified at the solidification rate of $1{\sim}50\;mm/min$ under the temperature gradients $75{\sim}80^{\circ}C/cm$. The investigation has been carried out for the microstructural variation, phase transition, mechanical properties by means of detailed analyses of stress-strain, micro-Vickers hardness and scanning electron micrography. The thermal stability at elevated temperature has been studied on $Al-Al_6Fe$ eutectic alloy held at $600^{\circ}C$ for $0{\sim}150$ hours. When the solidification rate was less than 10mm/min, the X-ray diffraction and EDS analysis showed the presence of $Al_3Fe$ compound. As the solidification rate more than 20 mm/min, $Al-Al_3Fe$ eutectic phase was transfered into $Al-Al_6Fe$ eutectic phase. The mechanical properties of unidirectionally solidified off-eutectic Al-Fe alloy is better than those of unidirectionally solidified eutecic Al-Fe alloy Maximum ultimate tensile strength was obtained in Al-2.25% Fe alloy which was unidirectionally solidified at the solidification rate of 20 mm/min. The metastable $Al-Al_6Fe$ phase was transferred into stable $Al-Al_3Fe$ phase at $600^{\circ}C$ held for 150 hours.

  • PDF

Effect of Fe, Mn Content on the Tensile Property of Al-4 wt%Mg-0.9 wt%Si Alloy System for High Pressure Die Casting (고압 금형 주조용 Al-4 wt%Mg-0.9 wt%Si계 합금의 인장특성에 미치는 Fe, Mn함량의 영향)

  • Kim, Heon-Joo
    • Journal of Korea Foundry Society
    • /
    • v.33 no.3
    • /
    • pp.103-112
    • /
    • 2013
  • Effect of Fe and Mn contents on the tensile properties of Al-4 wt%Mg-0.9 wt%Si alloy system has been studied. Common phases of Al-4 wt%Mg-0.9 wt%Si alloy system were ${\alpha}$-Al, $Mg_2Si$, ${\alpha}-Al_{12}(Fe,Mn)_3Si$ and ${\beta}-Al_5FeSi$. As Fe content of Al-4 wt%Mg-0.9 wt%Si alloy system increased from 0.15 wt% to above 0.3 wt%, ${\beta}-Al_5FeSi$ compound appeared. When Mn content of the alloy increased from 0.3 wt% to 0.5 wt%, morphology of plate shaped ${\beta}-Al_5FeSi$ compound changed to chinese script ${\alpha}-Al_{12}(Fe,Mn)_3Si$. As Fe content of Al-4 wt%Mg-0.9 wt%Si-0.3 wt%Mn alloy increased from 0.15 wt% to 0.4 wt%, tensile strength of the as-cast alloy decreased from 191 MPa to 183 MPa and, elongation of the alloy also decreased from 8.0% to 6.2%. Decrease of these properties can be explained as the formation of plate shape, ${\beta}-Al_5FeSi$ phase with low Mn/Fe ratio of the alloy. However, when Mn content of Al-4 wt%Mg-0.9 wt%Si-0.3 wt%Fe alloy increased from 0.3 wt% to 0.5 wt%, tensile strength of as-cast alloy increased from 181 MPa to 194 MPa and, elongation of the alloy increased from 6.8% to 7.0%. These improvements attribute to the morphology change from ${\beta}-Al_5FeSi$ phase to chinese script, ${\alpha}-Al_{15}(Fe,Mn)_3Si_2$ phase shape-modified from with high Mn/Fe ratio of the alloy.

The Effects of Mn and Cr Additions on the Microstructure of A356 Alloys Containing Impure Fe (불순 Fe를 함유한 A356 주조합금에서 미세조직 형성에 관한 Mn과 Cr의 효과)

  • Han, Sang-Won
    • Journal of Korea Foundry Society
    • /
    • v.25 no.3
    • /
    • pp.128-133
    • /
    • 2005
  • The effects of Mn and Cr on the crystallization behaviors of Fe-bearing intennetallics in A356 alloy were studied. Coarse and acicular ${\beta}-Al_{5}$FeSi phase in A356-0.20wt.%Fe alloy was modified into small ${\alpha}$-Al(Fe,Mn)Si and ${\alpha}$-Al(Fe,Cr)Si phases in response to Mn and Cr addition, respectively. Increasing of Mn addition amount elevates the crystallizing temperature of ${\alpha}$-Al(Fe,Mn)Si and the Mn/Fe ratio in the ${\alpha}$-Al(Fe,Mn)Si. Cr is more effective to modify ${\beta}-Al_{5}$FeSi in comparison with Mn. ${\alpha}$-Al(Fe,Mn)Si phase had BCC/SC dual structure.

Effect of Al and Cr on Oxidation of Fe-Al and Fe-Cr Alloys (Fe-Al과 Fe-Cr계 합금의 내 산화성에 미치는 Al과 Cr의 영향)

  • Kim, Tae-Wan;Jo, Seung-Hoon;Ko, In-Yong;Doh, Jung-Mann;Yoon, Jin-Kook;Shon, In-Jin
    • Korean Journal of Metals and Materials
    • /
    • v.48 no.11
    • /
    • pp.981-988
    • /
    • 2010
  • The effects of Cr and Al contents in Fe-Al and Fe-Cr alloys on oxidation resistance, hardness, and the thermal expansion coefficient were investigated. Fe-Al and Fe-Cr alloys above 10wt.%Al and 20wt.%Cr contents have a high oxidation resistance. The hardness of the Fe-Al and Fe-Cr alloys increased with an increase in Al and Cr contents due to solid solution or formation of an intermetallic compound. The coefficients of thermal expansion of the Fe-Al alloys were higher than those of the Fe-Cr alloys because the coefficient of thermal expansion of Al was higher than that of Fe and Cr.