• Title/Summary/Keyword: Fatigue Crack Growth rate

Search Result 437, Processing Time 0.028 seconds

Influence of overload on the fatigue crack growth retardation and the statistical variation (강의 피로균열지연거동에 미치는 과대하중의 영향과 통계적 변동에 관한 연구)

  • 김선진;남기우;김종훈;이창용;박은희;서상하
    • Journal of Ocean Engineering and Technology
    • /
    • v.11 no.3
    • /
    • pp.76-88
    • /
    • 1997
  • Constant .DELTA.K fatigue crack growth rate experiments were performed by applying an intermediate single and multiple overload for structural steel, SM45C. The purpose of the present study is to investigate the influence of multiple overloads at various stress intensity factor ranges and the effect of statistical variability of crack retardation behavior. The normalized delayed load cycle, delayed crack length and the minimum crack growth rate are increased with increasing baseline stress intensity factor range when the overload ratio and the number of overload application were constant. The crack retardation under low baseline stress intensity factor range increases by increasing the number of overload application, but the minimum crack growth rate decreases by increasing the number of overload application. A strong linear correlation exists between the minimum crack growth rate and the number of overload applications. And, it was observed that the variability in the crack growth retardation behavior are presented, the probability distribution functions of delayed load cycle, delayed crack length and crack growth life are 2-parameter Weibull. The coefficient of variation of delayed load cycle and delayed crack length for the number of 10 overload applications data are 14.8 and 9.2%, respectively.

  • PDF

Fatigue Crack Propagation Characteristics in HAZ of A106 Gr B Steel Weldments (A106 Gr B강 용접열영향부에서의 피로균열성장특성)

  • 김철한;조선영;김복기;배동호
    • Proceedings of the Korean Society of Machine Tool Engineers Conference
    • /
    • 1999.05a
    • /
    • pp.263-268
    • /
    • 1999
  • With HAZ of A 106 Gr B steel weldment, fatigue test in air, electrochemical polarization test and corrosion fatigue test in 3.5wt.% NaCl solution were performed changing load ratio. Obtained results are as follows. 1) K$\sub$op/ was independent of K$\sub$max/ and load ratio in fatigue crack growth. 2) In variation of load ratio, the scatter band of crack growth curve was reduced by half considering crack closure 3) In the result of electrochemical polarization test, current density was increased abruptly when potential was larger than corrosion potential. 4) Fatigue crack growth rate in corrosive environment was markly higher than the rate in air because of corrosion characteristics of the material and anodization of inner surface crack.

  • PDF

A Study on the Fatigue Crack Propagation Behavior of $Al_2O_3/AC4C$ Composites Made by Squeeze Casting Process (용탕단조법으로 제조된 $Al_2O_3/AC4C$ 복합재료의 피로균열 전파거동에 관한 연구)

  • Yeo, In-Dong;Lee, Chi-Hwan
    • Journal of Korea Foundry Society
    • /
    • v.15 no.4
    • /
    • pp.388-396
    • /
    • 1995
  • This study has been conducted with the purpose of examining the fatigue crack growth characteristics of $Al_2O_3$ short fiber reinforced aluminum matrix composites made by squeeze casting process with different applied pressure and binder amount. Fatigue crack growth experiments have been performed under constant load amplitude method with a fixed load ratio. The rate of crack propagation was decreased with binder amount as well as applied pressure. Also fatigue crack growth path in matrix was changed from flat to rough mode with an increase of applied pressure. In the composites, fatigue crack was propagated to interface between matrix and reinforcement at 10MPa, but it was propagated to reinforcement at 20MPa. The major reason of thee result was considered that interfacial bonding force and microstructure of matrix were improved due to an increase of applied pressure. Localized ductile striation in the composites was observed at low growth rate region and such a phenominon was remarkable with an increase of applied pressure. At high growth rate region, the propensity of fracture appearance was changed from interfacial debonding to reinforcement fracture with an increase of applied pressure.

  • PDF

A Study on the Fatigue Crack Growth Behavior of 9% Ni Steels (9% Ni강의 피로균열진전거동에 관한 연구)

  • Shim, Kyue-Taek;Kim, Jae-Hoon;Lee, Kwan-Hee;Ahn, Byung-Wook;Kim, Young-Kyun
    • Proceedings of the KSME Conference
    • /
    • 2008.11a
    • /
    • pp.167-172
    • /
    • 2008
  • This study is to evaluate the fatigue crack growth characteristics for base metals and welded metal of 9% Ni steels. Since this material has very excellent fracture toughness at low temperature, it has been widely used for inner walls of LNG storage tank. These materials to compare fatigue crack growth (FCG) behaviour are treated with heat by the method of quenching and tempering (QT), and quenching, lamellarizing and tempering (QLT). FCG tests using compact temsion (CT) specimen under stress ratio R=0.1, 0.5, and constant load are carried out. K-increasing tests are conducted by the standard test method described in ASTM E 647. To investigate the effect of welded metal on the crack growth rate, the locations of notch tip were chosen at the center of welded metal and heat affected zone (HAZ). Form the results, FCG rate has almost same tendency according to stress ratio, base and welded metal, the locations of welded metal. FCG rate of welded metal is somewhat faster than base metal. Also scanning electron microscope (SEM) is used to observe the striation of the fractured surface after fatigue crack tests.

  • PDF

A Study of Development Methods of Fatigue Life Improvement for the Suspension Material (현가장치재의 피로수명향상 공법개발에 관한 연구)

  • 박경동;정찬기
    • Transactions of the Korean Society of Automotive Engineers
    • /
    • v.12 no.1
    • /
    • pp.196-202
    • /
    • 2004
  • The development of new materials with light weight and high strength has become vital to the machinery, aircraft and auto industries. However, there are a lot of problems with developing such materials that require expensive tools, and a great deal of time and effort. Therefore, the improvement of fatigue strength and fatigue life are mainly focused on adopting residual stress(in this thesis). The compressive residual stress was imposed on the surface according to each shot velocity(57, 70, 83, 96 m/sec) based on Shot-peening, which is the method of improving fatigue life and strength. By using the methods mentioned above, the following conclusions have been drawn. 1. The fatigue crack growth rate(da/dN) of the Shot-peened material was lower than that of the Un-peened material. And in stage I, ΔKth, the threshold stress intensity factor, of the shot-peen processed material is high in critical parts unlike the Un-peened material. Also m, fatigue crack growth exponent and number of cycle of the Shot-peened material was higher than that of the Un-peened material. That is concluded from effect of da/dN. 2. Fatigue life shows more improvement in the Shot-peened material than in the Un-peened material. And compressive residual stress of surface on the Shot-peen processed operate resistance force of fatigue crack propagation.

A Study on the Fatigue Crack Propagation Threshold Characteristic in Steel of Pressure Vessel at Low Temperature (압력용기용 강의 저온 피로크랙전파 하한계 특성에 관한 연구)

  • 박경동;박상오
    • Proceedings of the Korea Committee for Ocean Resources and Engineering Conference
    • /
    • 2001.05a
    • /
    • pp.326-331
    • /
    • 2001
  • In this study. CT specimens were prepared from ASME SA5l6 which was used for pressure vessel plates for room and low temperature service. And we got the following characteristics from fatigue crack growth test carried out in the environment of room and low temperature at $25^{\circ}C$, -3$0^{\circ}C$, -6$0^{\circ}C$, -8$0^{\circ}C$, -10$0^{\circ}C$ and -12$0^{\circ}C$ in the range of stress ratio of 0.1 by means of opening mode displacement. At the constant stress ratio, the threshold stress intensity factor range ΔKsub/th/ in the early stage of fatigue crack growth ( Region I) and stress intensity factor range ΔK in the stable of fatigue crack growth ( Region II) was increased in proportion to descend temperature. It assumed that the fatigue resistance characteristics and fracture strength at low temperature is considerable higher than that of room temperature in the early stage and stable of fatigue crack growth region. The straight line slope relation of logarithm da.dN -ΔK in RegionII, that is, the fatigue crack growth exponent m increased with descending temperature at the constant stress ratio. It assumed that the fatigue crack growth rate da/dN is rapid in proportion to descend temperature in Region II and the cryogenic-brittleness greatly affect a material with decreasing temperature.

  • PDF

A Study on the Fatigue Crack Propagation Behavior by the Variation of Heat Treatment Temperature and Thickness in ATOS 55 Steel (ATOS 55강의 열처리 온도와 두께 변화에 따른 피로균열성장거동에 관한 연구)

  • 오환교
    • Journal of the Korean Society of Safety
    • /
    • v.12 no.4
    • /
    • pp.15-20
    • /
    • 1997
  • This study is to investigate the behavior of fatigue crack growth with ATOS 55 steel which can be applied to the commercial car Dump Frame. It is to obtain the material coefficients after tensile and fatigue crack growth test with the variation of thickness or heat treatment. Also, that is proved the Pari's law by experiment. The summarized results are as follows ; 1) Increasing thickness, tensile and yield strength measured highly regardless to heat treatment and measured lowly as variation of heat treatment temperature. 2) Specimen of thickness 8.0㎜ measured the faster of crack growth rate than another thickness according to the results of experiment. It was the different of stress conditions in crack tip. 3) It was found that the experimental constant m was range of 2∼5 to the relationship between fatigue crack growth rate and stress intensity factor range. Also, it was to prove the Paris's law by the experiment.

  • PDF

Evalustion and Prediction for the Fatigue crack Initiation and Growth Life by Reliability Approach (I) -Statistical Consideration for Fatigue Crack Growth Life- (신뢰성 공학적 피로 균열의 발생, 진전 수명 평가 및 예측에 관한 연구 ( I ) -피로 균열 진전 수명의 통계학적 분포 특성-)

  • 권재도;최선호;황재석;곽상국;전경옥;장재영
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.14 no.6
    • /
    • pp.1583-1591
    • /
    • 1990
  • Life prediction and residual life prediction of structures of machines are one of the most strongly world wide needed problems as requirement in the stage of slowly developing economy which comes after rapidly and highly developing stage. For the purpose of statistical life prediction, fatigue test was conducted under the 4 stress levels, and for each stress level, about 20 specimens are used. The statistical properties of crack growth parameter m and C in the fatigue crack growth law of da/dN=C(.DELTA.K)sup m/, and the relationship between m and C, and the statistical distribution pattern of fatigue crack growth rate can be obtained by experimental results.

Effect of Loading Variables and Temperature on Fatigue Crack Propagation in SA508 Cl.3 Nuclear Pressure Vessel Steel (원자로압력용기강에서 하중변수와 온도가 피로균열진전에 미치는 영향)

  • Kim, B. S.;Lee, B. H.;Kim, I. S.
    • Nuclear Engineering and Technology
    • /
    • v.27 no.6
    • /
    • pp.825-832
    • /
    • 1995
  • The effect of loading variables and temperature on fatigue crack growth rate in SA508 Cl.3 nuclear pressure vessel steel was investigated in air environment Crack growth rate tests on compact tension specimen of thickness 12mm were conducted by using sinusoidal waveform. The crack length was monitored by compliance method. Test conditions were at 0.1 and 0.5 of load ratio, at 1 and 10 Hz of loading frequency, and at room temperature to 40$0^{\circ}C$. At the lower temperatures, the fatigue crack propagation was not affected by the frequency and temperature, while at the higher temperatures above 12$0^{\circ}C$, fatigue crack growth rate increased with decreasing loading frequency and increasing temperature. This accelerated fatigue crack propagation was associated with the increase of oxidation rate at the ahead of crack tip. Fatigue crack growth rate increased with in-creasing the load ratio. The effect of load ratio was more significant at the lower temperature, while the dependence on load ratio decreased with increasing temperature. The sensitivity of load ratio to temperature can be explained by crack closure with the oxidation process.

  • PDF

Analysis of Fatigue Crack Growth Behavior in the Stiffened Panels with Bonded Symmetric Stiffener (접착이음 보강판의 피로거동해석)

  • 이환우;강선규
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.17 no.5
    • /
    • pp.168-172
    • /
    • 2000
  • The stiffened panel is representative of a large portion of aircraft construction and therefore has much practical importance. In this paper, the influence of various shape parameters on the stress intensity factors and the fatigue crack growth in the panels with bonded composite stiffeners are studied experimentally. Results are presented as crack growth rates for various values of crack lengths, stiffness ratios, and stiffening Materials.