• 제목/요약/키워드: Erosion rate

검색결과 534건 처리시간 0.031초

포신 마모 예측의 정확도 향상을 위한 실험적 방법 유도 (Derivation of Empirical Method to Enhance the Accuracy of Cannon Tube Erosion Rate)

  • 정동윤;오명호
    • 한국군사과학기술학회지
    • /
    • 제5권3호
    • /
    • pp.23-32
    • /
    • 2002
  • We predict the erosion rate of unknown cannon tubes by substituting measured values of the standard cannon, 155㎜ Howitzer M185 and ballistic data for the erosion equation. We know ten measured erosion values of the standard cannon at every 400 rounds. An approximate formula is derived to interpolate six values up to 2,000 rounds. Numerical example is presented and its results are analyzed. The new erosion equation is also suggested. This equation produces more accurate cannon tube erosion rate than the Rauf Imam's empirical approaches. Computer simulations are presented.

일부 산(Acid)에 폭로된 근로자의 치아산식증에 관한 조사연구 (A STUDY ON THE DENTAL EROSION BY ACID AMONG WORKERS EXPOSED TO ACID)

  • 배정수;이재휘;임현술;정해관;장동수
    • 대한치과보철학회지
    • /
    • 제32권3호
    • /
    • pp.368-377
    • /
    • 1994
  • In order to investigate the oral health status including dental erosion, the authors had surveyed and oral examined 510 male workers, among whom 199 workers were exposed to acids and 311 were not exposed to acids, in a factory using acids during the period from November, 26 to 27 in 1992. The obtained results were as follows ; 1. The positive rate of dental erosion between the acid exposed and non-exposed group didn't show statistical difference. But the positive rate of degree 1 dental erosion by degree was statistically high in the acid exposed group(P<0.05). 2. The acid exposed group showed the higher positive rate of degree 1 dental erosion in lower incisors by site(P<0.01). 3. To the average number of eroded teeth, the acid exposed group showed more degree 1 eroded teeth in lower incisors than the non-exposed(P<0.05). 4. Although the rate of dental erosion was increased according to the increase in tenure in both exposed and non-exposed group(P<0.05), there was no difference in rate of the dental erosion by site among the same tenure group. 5. In the acid exposed group, the rate of dental erosion between protective mask wearer group and non-wearer group was not statistically different, but upper incisors of the protective mask wearer group showed lower rate of dental erosion by site(P<0.05). 6. The positive rate of periodontal diseases was higher in the acid exposed group(P<0.01).

  • PDF

상용 순환 유동층 연소로 수관벽 전열관 마모속도 (Tube Erosion Rate of Water Wall in a Commercial Circulating Fluidized Bed Combustor)

  • 김태우;최정후;선도원;손재익;정봉진;김수섭;김상돈
    • Korean Chemical Engineering Research
    • /
    • 제43권4호
    • /
    • pp.525-530
    • /
    • 2005
  • 상용 순환 유동층 연소로(200 ton steam/hr, $4.97{\times}9.90{\times}28.98m$)의 수관벽에서 전열관의 마모속도를 측정 및 고찰하였다. 전열관의 두께는 초음파 측정방법을 이용하여 측정되었다. Splash 영역에서 윙월을 포함한 모든 수관벽 전열관의 마모속도가 두드러졌다. 전열관의 마모속도는 분배기로부터 높이가 증가함에 따라서 감소한 후 다시 증가하였다. 프리보드 기체출구 부근의 윙월에서는 기체 및 고체흐름의 편향성으로 인한 마모속도의 차이도 나타났다. 윙월의 마모속도는 연소로 단면의 중앙에 위치할수록 크게 나타났다.

선박 슬러지유 환경에서의 캐비티 붕괴유동에 따른 SS400의 침식양상 (A Erosion Aspect of SS400 by Cavity Collapse Fluctuation in Marine Sludge Oil)

  • 한원희;이진열
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제26권3호
    • /
    • pp.328-336
    • /
    • 2002
  • decrease in efficiency due to cavity fluid fluctuation. The purpose of this study is to examine erosion aspect on the SS400 specimen by cavitation and the effect of impact pressure generated from the demolition of the cavity of ultrasonic vibrator horn in the marine sludge oil environment. The erosion damage of specimen was investigated mainly on weight loss, weight loss rate and maximum erosion rate with variation of the vibration amplitude of $50{\mu}m, 24{\mu}m$ as well as the change of space between transducer horn and specimen. The experimental results showed that as the space between ultrasonic vibrator horn and specimen disk increased, the weight loss and weight loss rate decreased and the values were larger in SFO than in SLO. These findings would help interpret the aspect of cavitation erosion damage in metallic materials of different operating environment and material characteristics.

열간가압소결법으로 제조된 Sialon세라믹스의 Erosion특성에 관한 연구 (A Study on Erosion Properties of Hot Pressed Sialon Ceramics)

  • 여인웅;임대순;박동수
    • Tribology and Lubricants
    • /
    • 제13권3호
    • /
    • pp.42-47
    • /
    • 1997
  • Three kinds of the sialon ceramics with and without TiN additions were prepared by hot pressing to investigate the effect of microstructure on erosion behaviors. Hardness and fracture toughness were measured with prepared specimens to study the effect of additives on the mechanical properties. A gas blast type erosion tester was employed to examine erosion behavior of the specimens up to $600^{\circ}C$. Erosion tests showed an increase of erosion rate up to 40$0^{\circ}C$ and a gradual decrease of erosion rate up to 50$0^{\circ}C$ for all kinds of sialon. The results also showed that erosion rates of the sialons were controlled better by microstructural factors than by mechanical properties including fracture toughness and hardness.

질화규소 세라믹스의 강도와 침식도 평가에 관한 연구 (Evaluation for the Strength and Erosion Rate on the Silicon Nitride Ceramics)

  • 김부안
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제27권6호
    • /
    • pp.783-789
    • /
    • 2003
  • An experimental method to investigate the fracture strength and fracture toughness for the silicon nitrides sintered at various sintering temperature is established. The erosion rate for these materials in the various concentration of NaOH solution is also investigated. In result, the fracture strength of Si3N4 is decreased with the increase of sintering temperature. On the other hand, the fracture toughness KIC is increased with the increase of sintering temperature. The erosion rate of silicon nitride in the NaOH solution depend largely on the grain size and the concentration of NaOH solution. The erosion rate of silicon nitride sintered at $1800^{\circ}C$ was much higher than that at $1950^{\circ}C$. These results are due to the unique columnar structure of silicon nitride.

열간가압소결법으로 제조된 Sialon세라믹스의 고온 Erosion 특성에 관한 연구 (A Study on Erosion Properties of Sialon Ceramics by Hot-Pressing)

  • 여인웅;임대순;박동수
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1996년도 제24회 춘계학술대회
    • /
    • pp.20-24
    • /
    • 1996
  • Three kinds of the sialon ceramics with and without TiN additions were hot pressed. Hardness and fracture toughness were measured with prepared specimens to study the effect of additives on the mechanical properties. A gas blast type erosion tester was employed to examine erosion behavior of the specimens up to 600 $^{\circ}$C. Erosion tests showed an increase of erosion rate up to 400 $^{\circ}$C and a gradual decrease of erosion rate 500 $^{\circ}$C for all kinds of sialon. The results also showed that erosion rates of the sialons were controlled better by microstructure factors than by mechanical properties such as fracture toughness.

  • PDF

GPS와 HP법으로 제조된 질화규소의 고온 Erosion 특성 (High Temperature Erosion Properties of Silicon Nitride Fabricated by GPS and HP Method)

  • 최현주;안정욱;임대순;박동수
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2000년도 제32회 추계학술대회 정기총회
    • /
    • pp.304-309
    • /
    • 2000
  • Si$_3$N$_4$-6wt%Y$_2$O$_3$-lwt%Al$_2$O$_3$was prepared by hot pressed and gas pressure sintering to investigate the effect of microstructure on erosion behaviors. Hardness and fracture toughness were measured with prepared specimens to study the high temperature erosion properties. A gas blast type erosion tester was used In examine erosion behavior of the specimens up to 700$^{\circ}C$. In case of GPS silicon nitride, the erosion rate increases up to 500$^{\circ}C$ and decreases over 500$^{\circ}C$. Maximum erosion rate was observed at 300$^{\circ}C$ for HP silicon nitride. The principal factors affecting the high temperature erosive wear of brittle materials are largely dependent on high temperature properties of grain boundaries.

  • PDF

슬러지유 환경에서 진동자 디스크의 침식 특성에 관한 연구 (A study on the Erosion Characteristics of Transducer Horn Disc in Sludge Oil Environment)

  • 정지선;한원희;하만식;이진열
    • 한국마린엔지니어링학회:학술대회논문집
    • /
    • 한국마린엔지니어링학회 2001년도 추계학술대회 논문집(Proceeding of the KOSME 2001 Autumn Annual Meeting)
    • /
    • pp.98-104
    • /
    • 2001
  • Recently, the researches on the prevention of marine oil pollution being strengthened. Sludge oils were unavoidably produced in ship's operations, therefore it is necessary to manage the sludge oils inside the ship itself with the view to prevent marine oil pollution from ship. The present study deals with the ultrasonic breaking systems that recycle the sludge oil from ships into usable oil to be burnt. At the first instanceexperimental studies were carried out to investigate the homogenizing effect of the marine oils and the erosion aspect of horn disc by repeated vibration of ultrasonic transducer. The erosion damages for horn disc SS41 steel with weight loss rate and the irradiation time to max. erosion rate were examined according to the variation of the transducer amplitude, the oil temperature and the immersing depth of horn disc. As the result of it, the erosion aspects of horn disk were varied with oil environments and testing time.

  • PDF

플라즈마 디스플레이 보호막으로 사용되는 마그네슘 산화막(MgO)의 내식각 특성 (The characteristics of anti-erosion for MgO protecting layer in plasma display panel)

  • 최훈영;이석현
    • 한국전기전자재료학회논문지
    • /
    • 제13권2호
    • /
    • pp.163-169
    • /
    • 2000
  • In this paper, we showed the erosion characteristic of MgO protector layer releated to lifetime of plasma display panel(PDP). We observed MgO erosion characteristic as a functions of deposition conditions, pressure and distance between electrodes. In RIE condition of Xe gas, the lowest erosion rate appears in the conditions of no heating bias voltage -30V and pressure 5mtorr. In general, as deposition rate increases, erosion rate decreases. In real panel, when the gap distance between electrodes is narrow and the pressure is low, the heavy plasma damage appears. Also, the surfaces between electrodes and on the bus electrode are extremely damaged.

  • PDF