일액형 탄소나노튜브/에폭시 바인더 코팅액을 이용한 전도성 필름 제조 및 특성 분석 (Characterization and fabrication of one component solution based CNT/epoxy binder conductive films)

  • 한중탁;우종석;김선영;이건웅
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 추계학술대회 논문집
    • /
    • pp.455-456
    • /
    • 2007
  • Optically transparent, highly conductive coating have been major theme of thin film science efforts for some years. In this work, t-MWNT(thin Multi-walled Carbon Nanotubes) are acid treated, then the stable dispersion of t-MWNTs in polar solvent such as alcohols, was achieved by sonication. The transparent conducting films are prepared using the one component solution of t-MWNT/epoxy binder via spray coating on glass substrate. The characterization of acid treated t-MWNTs was performed by Raman spectrometer. The opto-electrical properties of conducting films are analyzed by the binder concentration, and the effect of co-solvent on the compatibility and dispersibility of one component t-MWNT/epoxy binder solutions are discussed.

  • PDF

Epoxy/BaTiO3 (SrTiO3) composite films and pastes for high dielectric constant and low tolerance embedded capacitors fabrication in organic substrates

  • Paik Kyung-Wook;Hyun Jin-Gul;Lee Sangyong;Jang Kyung-Woon
    • 한국마이크로전자및패키징학회:학술대회논문집
    • /
    • 한국마이크로전자및패키징학회 2005년도 ISMP
    • /
    • pp.201-212
    • /
    • 2005
  • [ $Epoxy/BaTiO_3$ ] composite embedded capacitor films (ECFs) were newly designed fur high dielectric constant and low tolerance (less than ${\pm}15\%$) embedded capacitor fabrication for organic substrates. In terms of material formulation, ECFs are composed of specially formulated epoxy resin and latent curing agent, and in terms of coating process, a comma roll coating method is used for uniform film thickness in large area. Dielectric constant of $BaTiO_3\;&\;SrTiO_3$ composite ECF is measured with MIM capacitor at 100 kHz using LCR meter. Dielectric constant of $BaTiO_3$ ECF is bigger than that of $SrTiO_3$ ECF, and it is due to difference of permittivity of $BaTiO_3\;and\;SrTiO_3$ particles. Dielectric constant of $BaTiO_3\;&\;SrTiO_3$ ECF in high frequency range $(0.5\~10GHz)$ is measured using cavity resonance method. In order to estimate dielectric constant, the reflection coefficient is measured with a network analyzer. Dielectric constant is calculated by observing the frequencies of the resonant cavity modes. About both powders, calculated dielectric constants in this frequency range are about 3/4 of the dielectric constants at 1 MHz. This difference is due to the decrease of the dielectric constant of epoxy matrix. For $BaTiO_3$ ECF, there is the dielectric relaxation at $5\~9GHz$. It is due to changing of polarization mode of $BaTiO_3$ powder. In the case of $SrTiO_3$ ECF, there is no relaxation up to 10GHz. Alternative material for embedded capacitor fabrication is $epoxy/BaTiO_3$ composite embedded capacitor paste (ECP). It uses similar materials formulation like ECF and a screen printing method for film coating. The screen printing method has the advantage of forming capacitor partially in desired part. But the screen printing makes surface irregularity during mask peel-off, Surface flatness is significantly improved by adding some additives and by applying pressure during curing. As a result, dielectric layer with improved thickness uniformity is successfully demonstrated. Using $epoxy/BaTiO_3$ composite ECP, dielectric constant of 63 and specific capacitance of 5.1nF/cm2 were achieved.

  • PDF

Burn Damage에 따른 도막의 방청성 평가 (Evaluation of the Corrosion Protection Coating in Accordance with Burn Damage)

  • 서창호;박진환
    • Corrosion Science and Technology
    • /
    • 제15권6호
    • /
    • pp.290-296
    • /
    • 2016
  • This study was conducted in order to examine the effect of burn damage and the resultant anti-corrosion performance. The breakdown and defect of the paint film caused by burn damage are considered to affect not only the macroscopic appearance but also the adhesive force and the anti-corrosion performance of the paint film. The material of the paint film was epoxy paint that is used most widely for heavy-duty coating, and in order to induce burn damage, heat treatment with a torch was applied to the other side of the paint film. Surface and chemical structure changes according to aging were analyzed using FE-SEM and infrared absorption spectroscopy, and variation in the anti-corrosion performance was analyzed through the AC impedance test.

GIS 절연 신뢰성 향상을 위한 탱크 내면 코팅이 파티클 거동에 미치는 영향 (Effect of the Inner Side Dielectric Coating of the Tank on the Particle Movement for Improving of GIS Insulation Reliability)

  • 이방욱;구자윤;김민규;김익수
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1996년도 추계학술대회 논문집 학회본부
    • /
    • pp.267-269
    • /
    • 1996
  • In this work, the influence of wire type conducting particles on the insulation reliability of GIS has been systematically investigated when outer electrode was dielectric coated by epoxy resin. For this purpose, coaxial cylinder-type electrode was adopted in 362 kV chamber and various size of Cu conducting particle was used and different gas pressure was applied. To prove the coating effect on the gas insulation, different thickness of epoxy coated outer electrode have been considered and the lift-off voltage and flashover voltage have been analyzed. The results show that the dielectric coated electrode has an remarkable influence on the reducing particle behavior in GIS system and enhancing the GIS insulation reliability.

  • PDF

직물형 유리섬유/에폭시 복합재료로 피막된 판유리의 미소강구 충격에 의한 표면파괴거동 (Surface Fracture Response of Glass Eabric/Epoxy Lamina-Bonded Glass Plates to Impact with a Small-Diameter Steel Ball)

  • 김형구;최낙삼
    • Composites Research
    • /
    • 제13권4호
    • /
    • pp.75-82
    • /
    • 2000
  • 유리섬유/에폭시 복합재료로 피막한 유리판의 표면파괴거동을 연구하기 위하여 미소강구 충격실험을 수행하였다. 본 연구에서는 다섯 종류의 재료, 단순소다유리판(soda-lime glass plates), 유리섬유/에폭시박막(glass/epoxy lamina)을 1층 접착, 비접착한 시편과 박막을 3층 접착, 비접착한 시편을 사용하였다. 충격속도 범위 40∼120m/s에서 유리판 배면에서의 최대 응력과 흡수파괴에너지를 측정하였다. 충격 속도증가에 따라 링균열, 콘균열, 레이디얼 균열이 시편 내부에서 발생하였다. 복합재료 박막으로 피막한 결과, 소다유리판의 균열은 현저히 감소하였으며 측정한 최대 응력과 흡수파괴에너지를 이용하여 표면 파괴거동 특성을 평가할 수 있었다.

  • PDF

Effect of Water Impingement Conditions on the Degradation of Epoxy Coatings in Tap Water

  • Kim, D.H.;Yoo, Y.R.;Kim, Y.S.
    • Corrosion Science and Technology
    • /
    • 제21권5호
    • /
    • pp.327-339
    • /
    • 2022
  • The water-jet technique started by Bridgman can cut metal and alloys without harmful gas and fume. However, while this technique is convenient to cut metals and alloys, in the case of coated pipe, water jet induces the degradation of coatings on the pipes, and may facilitate structural failure, leakage, and loss of products. While there are many reports on the effect of water jet on cut metals and the damage of metallic materials, research on the effect of water impingement on the epoxy coatings has been little studied. In this work, we therefore control the velocity of water jet, distance between nozzle and specimen, and water temperature, and discuss the effect of water impingement on the epoxy coatings. Increasing water velocity and water temperature and reducing nozzle distance increased the degradation rates of three epoxy coatings were increased. Among three test parameters - water velocity, nozzle distance and water temperature, water temperature was relatively effective to increase the degradation rate of epoxy coatings.

스테인레스강 316L 상의 New Austrian Tunneling Method Coatings의 수지에 관한 기계적 특성 (Mechanical Properties on Resin of New Austrian Tunneling Coatings on Stainless Steel 316L)

  • 이주엽;성완모;김주한;성민정;김기준
    • 한국응용과학기술학회지
    • /
    • 제37권4호
    • /
    • pp.1034-1040
    • /
    • 2020
  • 스테인레스 스틸에 대한 합성된 폴리우레탄-에폭시 수지의 기계적 특성은 SEM, FT-IR, 인장특성, 그리고 EIS에 의한 특정질량손실량, 입도분석 등에 의해 물성을 측정하였다. 친환경적인 NATM 도료에 관한 관심이 고조됨에 따라 스테인레스 등의 금속에 코팅하는 무용제 도료를 합성하였다. 폴리올, IPDI, 충진제, 실리콘 계면활성제, 촉매 등이 함유된 기존 중방식수지보다 폴리올, MDI, 충진제, 실리콘 계면활성제, 촉매가 함유되어 합성된 중방식수지의 도료가 온도변화에 따른 인장강도가 증가하였고, 전해성이 높은 용액 속에서 저헝력이 크게 측정되었으며, 내구력과 강도가 양호하였다. 견고한 NATM 수지의 기계적 특성은 가교와 부식환경의 차단력이 증가함에 따라 강도가 증가하였다. 결론적으로 중방식의 가교된 미세조직은 방청코팅이 어려운 스테인레스 스틸 같은 금속물질 코팅에도 좋은 실험결과를 보여주었다.

실험과 계산을 통한 에폭시 계열 내화도료의 열분해에 관한 연구 (Experimental and Numerical Study of the Thermal Decomposition of an Epoxy-based Intumescent Coating)

  • 김양균
    • 한국화재소방학회논문지
    • /
    • 제30권1호
    • /
    • pp.31-36
    • /
    • 2016
  • 본 연구는 에폭시 계열 내화 도료의 열분해 특성을 파악하기 위해 열중량분석과 수치해석을 동시에 수행하였다. 에폭시 계열 내화 도료의 질량 감소 양상을 수치적으로 구현하기 위한 계산 모델이 소개되었으며, 계산 모델은 내화 도료의 여러 열분해과정을 단순화하여 4 단계의 순차적인 열분해 형태로 만들었다. 반응 속도는 Arrhenious 형태로 모델 되었고, 열중량분석을 통해 획득된 열분해 현상을 수치적으로 모사하기 위하여 화학 반응 매개변수들이 최적화되었다. 실험 결과 두 단계(two-step)와 세 단계(three-step)의 급격한 질량 감소가 질소와 공기 분위기에서 각각 나타났다. 또한 도료가 공기 분위기에 노출되었을 때 산소의 참여로 발생하는 복합적인 화학 반응들이 내화도료의 안정화를 도와 $200{\sim}500^{\circ}C$ 범위에서 질량 감소율을 낮추었다. 수치해석 결과는 실험과 비교하여 전체적으로 잘 일치하였으며 수치 모델에 포함되지 않은 $800^{\circ}C$ 이후를 제외하면 3% 미만의 오차를 보였다.

Effect of Retained Pre-construction Primer on the Corrosion Protection Properties of Epoxy Coatings

  • Lee, Chul-Hwan;Shin, Chil-Seok;Lee, Ho-Il;Chung, Mong-Kyu;Baek, Kwang-Ki
    • Corrosion Science and Technology
    • /
    • 제6권5호
    • /
    • pp.219-226
    • /
    • 2007
  • Pre-construction primer (PCP), or shopprimer, have been applied to steel plates to control temporary corrosion during ship fabrication. For surface preparation at ship block stage, in common shipyard practices, welding beads, burnt and rusted areas shall be blasted or power tool cleaned and the contamination such as zinc salt shall be removed with blasting or power tool. Whereas, the sound film of PCP needs not to be removed or roughened as the paint having good compatibility with PCP is used for the first coat. In many cases, however, full blasting or sweep blasting on the sound PCP treated block assemblies was requested. There still has been argument about the legitimacy of this practice, thus, it is critical to evaluate the quality of the coating system applied on the sound PCP retained condition, comparing with the one applied on the full blasted or sweep blasted condition. In this study, two different epoxy systems for water ballast tank were applied on the surfaces with sound PCP condition, full blasted condition, and sweep blasted condition. Coating performances such as durability, anti-corrosion, cathodic disbondment resistance were evaluated. The test results clearly indicated that the sound film of PCP needed not to be removed or roughened as the paint having good compatibility with PCP based on inorganic zinc silicate.

해수배관 내부 에폭시 코팅재의 캐비테이션 및 침지 열화에 따른 압입인장특성 (Indentation Tensile Properties of Seawater Piping with Cavitation and Immersion Degradation)

  • 정민재;김수현;전종모;김영식;김영천
    • Corrosion Science and Technology
    • /
    • 제22권6호
    • /
    • pp.419-428
    • /
    • 2023
  • Seawater has been used to cool devices in nuclear power plants. However, the pipes used to transport seawater are vulnerable to corrosion; hence, the inner side of pipelines is coated with an epoxy layer as prevention. Upon coating damage, the pipe becomes exposed, and corrosion progresses. The major cause is widely known as cavitation corrosion, causing the degradation of mechanical properties. In this study, corroded specimens were prepared using cavitation and immersion methods to clarify the degradation trend of mechanical properties with corrosion. Three different types of epoxy coatings were used, and accelerated cavitation procedures were composed of amplitudes of 15 ㎛, 50 ㎛, and 85 ㎛ for 2 h, 4 h, and 6 h. The immersion periods were 3 and 6 weeks. We conducted instrumented indentation tests on all degradation samples to measure mechanical properties. The results showed that higher cavitation amplitudes and longer cavitation or immersion times led to more degradation in the samples, which, in turn, decreased the yield strength. Of the three samples, the C coating had the highest resistance to cavitation and immersion degradation.