• Title/Summary/Keyword: Electromechanical coupling constant ($K^2$)

Search Result 141, Processing Time 0.024 seconds

Dielectric and Piezoelectric Characteristics of PMW-PNN-PT-PZ Ceramics with addiction of MnO$_2$ (MnO$_2$가 첨가된 PMW-PNN-PT-PZ계 세라믹스의 유전 및 압전 특성)

  • 박석환;윤광희;박정흠;김현재;박창엽
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1996.05a
    • /
    • pp.63-67
    • /
    • 1996
  • In this paper, effect of MnO$_2$ addition(0, 0.1, 0.2, 0.3, 0.5wt%) on the microstructure, dielectric and piezoelectric properties of [xPMW - (0.15-x) PNN] - [yPT-(0.85-y)PZ] (x=0, 0.01, 0.02, 0.03, 0.05, y = 0.35, 0.40, ().425, 0.45, 0.5) were investigated. When Ti/Zr ratio was 1.0, dielectric and piezoelectric properties were highest value. With PMW 2mol%, dielectric constant, dielectric constant (d$\_$33/, d$\_$31/) and electromechanical coupling factor (kp, k$\_$31/) were highest values of 1995, 479, 186(x10$\^$-12/C/N), 0.61, 0.36, respectively. With the addition of MnO$_2$, dielectric constant, electromechanical coupling factor (kp, k$\_$31/) were decreased, but with 0.3wt% MnO$_2$, eletromechanical coupling factor was highest value of 0.63. With the addition of MnO$_2$, mechanical quality(Q$\_$m/ was increased.

  • PDF

Dielectric and Piezoelectric Characteristics of 0.95(K0.5Na0.5)NbO3-0.05Li(Sb0.8Nb0.2)O3 Pb-free Ceramics with amount of Ag2O Addition (Ag2O 첨가량에 따른 0.95(K0.5Na0.5)NbO3-0.05Li(Sb0.8Nb0.2)O3 무연 세라믹스의 유전 및 압전특성)

  • Kim, Do-Hyung;Yoo, Ju-Hyun;Jeong, Yeong-Ho
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.22 no.11
    • /
    • pp.925-929
    • /
    • 2009
  • In this study, $0.95(K_{0.5}Na_{0.5})NbO_3-0.05Li(Sb_{0.8}Nb_{0.2})O_3$ ceramics were investigated as a function of the amount of $Ag_2O$ addition in order to improve dielectric and piezoelectric properties of lead-free piezoelectric ceramics. With increasing the amount of $Ag_2O$ addition, density and electromechanical coupling factor ($k_p$) increased up to 0.2 wt.% $Ag_2O$ and decreased above 0.2 wt.% $Ag_2O$. At the sintering temperature of $1020^{\circ}C$, electromechanical coupling factor ($k_p$), density, dielectric constant (${\varepsilon}r$) and curie temperature (Tc) of ceramics with 0.2 wt% $Ag_2O$ showed the optimal values of 0.42, $4.33\;g/cm^3$, 738 and $393^{\circ}C$, respectively.

A Study on the Low Temperature Sintering Piezoelectric Ceramics for Piezoelectric Actuator Application (압전 액츄에이터에 활용할 저온소결 압전 세라믹스에 관한 연구)

  • Ryu, Sung-Lim;Lee, Yu-Hyung;Lee, Sang-Ho;Yoo, Ju-Hyun
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2007.11a
    • /
    • pp.277-278
    • /
    • 2007
  • In this study, in order to develop multilayer piezo-actuator, PMN-PNN-PZT ceramics were fabricated using $Li_2CO_3,\;Na_2CO_3$, ZnO as sintering aids and their piezoelectric and dielectric properties were investigated according to the Bi substitution. Bi substitution enhanced electromechanical coupling factor$(k_p)$ and dielectric constant$({\varepsilon}_r)$. However, mechanical quality factor was deteriorated. At the sintering temperature of $870^{\circ}C$ and Bi substitution of 1mol%, density, electromechanical coupling factor$(k_p)$, mechanical quality factor$(Q_m)$, Dielectric constant$({\varepsilon}_r)$ and piezoelectric constant$(d_{33})$ of specimen showed the optimum value of $7.878g/cm^3$, 0.608, 835, 1603 and 397pC/N, respectively.

  • PDF

Piezoelectric properties ofPbTi$O_3$ system ceramics for hydrophone (하이드로폰용 PbTi$O_3$계 세라믹스의 압전특)

  • 유주현;홍재일
    • The Transactions of the Korean Institute of Electrical Engineers
    • /
    • v.44 no.4
    • /
    • pp.479-482
    • /
    • 1995
  • In this study, to improve sintering condition, anisotropic properties ( $k_{t}$/ $k_{p}$) of electromechanical coupling coefficient and piezoelectric constant $d_{h}$ and $g_{h}$, Mn $O_{2}$ impurity was added to the (P $b_{0.76}$C $a_{0.24}$)[( $Co_{1}$2/ $W_{1}$2/)$_{0.04}$ $Ti_{0.96}$] $O_{3}$ ceramics for application to hydrophone devices. Electromechanical coupling coefficients of the specimen with 1.5 [mol%] Mn $O_{2}$ sintered at 1150.deg. C were $k_{t}$=49% and $k_{p}$ = O, which exibited the highest value in piezoelectric anisotropic properties (kt/kp). Without relations with sintering temperature, the highest value of hydrostatic piezoelectric constant $d_{h}$ & $g_{h}$ were shown at the specimen with 1.5 [mol%] Mn $O_{2}$. Accordingly, the best addition amount of Mn $O_{2}$ was 1.5 [mol%] and proper sintering temperature was 1150.deg. C. Hydrostatic piezoelectric constant values of $d_{h}$=64.52[10$^{-12}$ C/N], $g_{h}$=35.92[10$^{-3}$ Vm/N] in the above condition were effectiely extended for hydrophone applications.pplications.ons.

  • PDF

Effects of PSN Substitution on the Microstructural and Piezoelectric Characteristics of PNN-PZT Ceramics (PSN 치환이 PNN-PZT 세라믹스의 미세구조 및 압전 특성에 미치는 영향)

  • 윤광희;민석규;류주현;박창엽;정희승
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.14 no.5
    • /
    • pp.356-361
    • /
    • 2001
  • The structureal, dielectric and piezoelectric properties of Pb[(Sb$\_$1/2/Nb$\_$1/2/)$\_$x/-(Ni$\_$1/3/Nb$\_$2/3/)$\_$0.15-x/-(Zr$\_$y/Ti$\_$1-y/)$\_$0.85/]O$_3$(x=0∼0.05, y=0.47∼0.52) ceramics were investigated with the substitution of Pb(Sb$\_$1/2/Nb$\_$1/2/)O$_3$(abbreviated PSN) and the Zr/Ti ratio. At Zr/Ti ratio of 50/50, tetragonality was decreased and grain size abruptly decreased with the increase of PSN substitution. Curie temperature was decreased and dielectric constant increased with the substitution of PSN. The coercive field increased and remnant polarization decreased with the substitution of PSN. Electromechanical coupling factor(k$\_$p/) showed the highest value of 0.622 at 1mol% PSN, but mechanical quality factor(Q$\_$m/) showed the minimum value at that composition. Dielectric constant and electromechanical coupling factor with the Zr/Ti ratio showed maximum values at Zr/Ti ratio of 50/50 and mechanical quality factor showed minimum values near the Zr/Ti ratio of 50/50.

  • PDF

Piezoelectric Properties of Pb-free Bi(Na,K)$TiO_3-SrTiO_3$ Ceramics with the Amount of $CeO_2$ Addition ($CeO_2$첨가에 따른 무연 Bi(Na,K)$TiO_3-SrTiO_3$ 세라믹스의 압전특성)

  • Lee, Hyun-Seok;Yoo, Ju-Hyun;Park, Chang-Yub;Jeong, Yeong-Ho;Hong, Jae-Il;Im, In-Ho;Yoon, Hyun-Sang
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2004.07b
    • /
    • pp.590-594
    • /
    • 2004
  • In this study, lead-free piezoelectric ceramics were investigated for pressure sensor applications as a function of the amount of $CeO_2$ addition at Bi(Na,K)$TiO_3-SrTiO_3$ system. With increasing the amount of $CeO_2$ addition, the density and dielectric constant increased. Electromechanical coupling factor($k_p$) showed the maximum value(kp, 0.39) at 0.1wt% $CeO_2$ addition and decreased above 0.1wt% $CeO_2$ addition., Density, dielectric constant(${\varepsilon}_r$) increased but mechanical quality factor(Qm), piezoelectric constant(d33) decreased in $CeO_2$ addition, respectively.

  • PDF

Poling Effect on Piezoeletric Ceramics for Air Medium (공기 매질에 의한 압전 세라믹스의 분극효과)

  • Kim, Yong-Hyuk
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.23 no.6
    • /
    • pp.464-470
    • /
    • 2010
  • A new method for the poling of piezoelectric ceramics with an air insulation medium in stead of silicon oil is described. A similar variation of electromechanical coupling coefficient $K_t$, for an air medium is observed in comparison to that of the material poled by the conventional poling method using a silicon oil medium. Different poling parameters such as dielectric constant $\varepsilon^T$ and frequency deviation ${\Delta}f$ are studied as well as the influence on the aging effect. The required poling factors to achieve the optimal piezoelectric characteristics are electric field, 2 kV/mm, temperature $100^{\circ}C$, and poling time 30 Min. From this result electric field 3 kV/mm atmosphere airs there being will be able to use with the polarization insulation medium about the piezoelectric material, confirmed.

Piezoelectric and Dielectric Properties of Low Temperature Sintering Pb(Zn1/2W1/2)O3-Pb(Mn1/3Nb2/3)O3-Pb(Zr,Ti)O3 Ceramics

  • Yoo, Ju-Hyun;Lee, Kab-Soo;Lee, Su-Ho
    • Transactions on Electrical and Electronic Materials
    • /
    • v.9 no.3
    • /
    • pp.91-95
    • /
    • 2008
  • In this study, in order to develop the composition ceramics for low loss multilayer piezoelectric actuator application, $Pb(Zn_{1/2}W_{1/2})O_3-Pb(Mn_{1/3}Nb_{2/3})O_3-Pb(Zr,Ti)O_3$ (abbreviated as PZW-PMN-PZT)ceramics according to the amount of $MnO_2$ addition were fabricated using two-stage calcinations method. And also, their dielectric and piezoelectric properties were investigated. At the 0.2 wt% $MnO_2$ added PZW-PMN-PZT ceramics sintered at $930^{\circ}C$, density, electromechanical coupling factor $k_p$, dielectric constant ${\varepsilon}_r$, piezoelectric $d_{33}$ constant and mechanical quality factor $Q_m$ showed the optimum value of $7.84g/cm^3$, 0.543, 1,392, 318.7 pC/N, 1,536, respectively for low loss multilayer ceramics actuator application.

Structure and Dielectric Properties of PMN-PNN-PZT ceramics (PMN-PNN-PZT 세라믹스의 구조 및 유전특성)

  • Lee, Jong-Deok;Park, Sang-Man;Park, Gi-Yup
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2003.05c
    • /
    • pp.257-260
    • /
    • 2003
  • In this study, the structural, dielectric and piezielectric properities of $xPb(Mg_{1/3}Nb_{2/3})O_3-(0.5-x)Pb(Ni_{1/3}Nb_{2/3})O_3-0.5Pb(Zr_{0.3}Ti_{0.7})O_3$ ceramics were investigated with the substitution of $PbMg_{1/3}Nb_{2/3}O_3$. The results showed that the substitution of the $PbMg_{1/3}Nb_{2/3}O_3$ was effective in increasing the dielectric constant and electromechanical coupling factor $(K_p)$. The dielectric constant, dielectric loss and Kp showed the highest values of 4293, 2.4%, 0.59 relatively, when the substitution of amount of $PbMg_{1/3}Nb_{2/3}O_3$ was 5 mol%.

  • PDF

Dielectric and Piezoelectric Characteristics of (Na,K)NbO3 Ceramics System According to Sintering Time (소결시간변화에 따른 (Na,K)NbO3계 세라믹스의 유전 및 압전특성)

  • Kim, Do-Hyung;Yoo, Ju-Hyun;Kim, In-Sung;Song, Jae-Sung
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.21 no.10
    • /
    • pp.901-905
    • /
    • 2008
  • In this study, $0.95(K_{0.5}Na_{0.5})NbO_{3}-0.05Li(Sb_{0.8}Nb_{0.2})O_{3}+0.2\;wt%Ag_{2}O$ were investigated as a variations of sintering times in order to improve dielectric and piezoelectric properties of lead-free piezoelectric ceramics. $Ag_{2}O$ were used as sintering aids and the specimens were sintered during 3, 5, 7, 9 and 11 hours, respectively. At the specimen sintered during 7 hour, Electromechanical coupling factor ($k_p$), density, dielectric constant (${\epsilon}_{\gamma}$), piezoelectric constant ($d_{33}$) and curie temperature ($T_c$) of composition ceramics showed the optimal value of 0.450, 4.274 $[g/cm^3]$, 1007, 257 [pC/N] and $396^{\circ}C$, respectively.