3차원 미세조직에 기반한 잔류응력 하의 이상 조직강의 소성변형률비 예측 (Prediction of the Plastic Strain Ratio Evolution of a Dual-phase Steel)

  • 하진진;이진우;이명규;;김지훈
    • 소성∙가공
    • /
    • 제24권6호
    • /
    • pp.395-399
    • /
    • 2015
  • A microstructure-based finite element simulation was conducted to predict the plastic strain ratio (R-value) of a dual-phase (DP) steel. The representative volume elements (RVEs) concept was adopted for the image-based FE modeling and a 3D model was constructed using sequential 2D images. Each phase was considered with the von-Mises yield criterion and the Swift model. The Swift parameters were defined by the empirical equations based on the chemical composition. The developed model was applied to analyze the effect of residual stress on the R-value and stress distribution. In order to consider the residual stress development after cold rolling, 10 % compression was applied in the thickness direction and unloaded before the tensile stress was applied in the rolling direction. The results showed a reasonable prediction for the R-value evolution: a sharp increase at small strains was well described and a transition followed in the downward direction. The R-value evolution was analyzed using the stress distribution change on the π-plane

신선 가공된 열처리 생략강의 냉간 성형성에 대한 연구 (Study on the Cold Formability of Drawn Non-heat Treated Steels)

  • 박경수;박용규;이덕락;이종수
    • 소성∙가공
    • /
    • 제12권4호
    • /
    • pp.364-369
    • /
    • 2003
  • Non-heat treated steels are attractive in the steel-wire industry since the spheroidization and quenching-tempering treatment are not involved during the processing. However, non-heat treated steels should satisfy high strength and good formability without performing heat treatment. Therefore, it is important to investigate optimum materials showing a good combination of strength and formability after the drawing process. In this study, three different steels such as dual phase steel, low-Si steel, and ultra low carbon bainitic steel were used to study their mechanical properties and the cold formability. The cold formability of three steels was investigated by estimating the deformation resistance and the forming limit. The deformation resistance was estimated by calculating the deformation energy, and the forming limit was evaluated by measuring the critical strain revealing crack initiation at the notch tip of the specimens. The results showed that deformation resistance was the lowest in the low-Si steel, and the forming limit strains of ultra low carbon bainitic steel and low-Si steel were higher than that of commercial SWRCH45F steel.

수소주입시킨 DP박강판의 SP시험과 수소취성 관계 해석 (Analysis of Correlation between the Hydrogen Embrittlement and the Small Punch Test for Hydrogen-charged Dual Phase Steels)

  • 박재우;강계명
    • 한국가스학회지
    • /
    • 제18권1호
    • /
    • pp.61-67
    • /
    • 2014
  • 고강도 DP강의 수소취성 거동을 소형펀치시험을 통해 평가하였다. 이를 위해 첨가원소가 각기 다른 3종의 DP강 시험편에 전기화학적 방법으로 수소를 강제 주입시켰다. 수소주입 후, 수소주입량을 측정하였다. 수소주입량은 마르텐사이트 부피분율에 크게 의존하는 것으로 조사되었다. 전류밀도 150, $200mA/cm^2$ 조건에서 25시간이 포화상태에 도달하는 수소주입조건으로 나타났다. SP시험 후 SP에너지와 SP bulb 형상을 비교한 결과, 수소주입량의 증가에 따라 SP에너지와 SP bulb 높이가 감소하는 것으로 나타났다. 또한 SP bulb 파단면에서는 뚜렷한 facet와 층상형태의 벽개 파단면이 관찰되어 수소취성화를 관찰할 수 있었다.

영구 연화 거동을 고려한 마찰교반용접(FSW) 된 DP강 판재의 탄성 복원 예측 (Springback prediction of friction stir welded DP590 steel sheets considering permanent softening behavior)

  • 박태준;이원오;정경환;김준형;김대용;;;;정관수
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2008년도 추계학술대회 논문집
    • /
    • pp.304-307
    • /
    • 2008
  • In order to evaluate the effect of permanent softening behavior on springback prediction, 2D-draw bending simulations were compared with experiments for friction stir welded DP590 steel sheets. To account fur the nonlinear hardening behavior, the combined isotropic-kinematic hardening law was utilized with and without considering the permanent softening behavior during reverse loading. Also, the non-quadratic orthotropic yield function, Yld2000-2d, was used to describe the anisotropic initial-yielding behavior of the base sheet while anisotropic properties of the weld zone were ignored for simplicity.

  • PDF

고Si DP980강 스폿 용접 특성에 미치는 Phosphorus (P) 및 in-situ 후열처리 펄스 조건의 영향 (Effects of Phosphorus and in-situ Post-heat Pulse Conditions on Resistance Spot Weldability of High Si DP980 Steel Sheet)

  • 최두열
    • Journal of Welding and Joining
    • /
    • 제33권6호
    • /
    • pp.21-26
    • /
    • 2015
  • Recently, application of UHSS(Ultra High Strength Steels) whose tensile strength is over 1000MPa to car body structure are growing due to great needs for light weighting and improved crash worthiness. However, their poor weldability is one of obstacles to expand selecting to car body. In this study, effect of Phosphorus contents on resistance spot weldability of high elongation DP980 steel whose Si content is over 1% was investigated. The cross tension strength (CTS) was decreased showing partial interface fracture as Phosphorus content increase because of solidification segregation of Phosphorus. In order to improve resistance spot weldability by modification of welding condition, in-situ post-weld heating pulse was introduced after main pulse. The optimum cooling time between main and post pulse and post-pulse current condtion were determined through FEM welding simulation and DOE tests. The CTS was increased about 1.5 time showing plug fracture. The decrease of Phosphorus segregation was found to be a major reason for weld ductility and CTS improvement.

디프도로잉 시 DP강의 집합조직 및 이방성 거동 모사 (Simulation of Texture Evolution and Anisotropic Properties in DP Steels during Deep Drawing Process)

  • 송영식;김병진;한성호;진광근;최시훈
    • 소성∙가공
    • /
    • 제17권7호
    • /
    • pp.517-522
    • /
    • 2008
  • A visco-plastic self-consistent (VPSC) polycrystal model has been applied to simulate texture simulation and anisotropic properties of DP steels during deep drawing process. In order to evaluate the strain path during deep drawing, a steady state was assumed in the flange part of deep drawn cup. The final stable orientations were strongly dependent on the initial location in the blank. The evolution of anisotropy of DP steel sheets has been demonstrated through comparison of plastic strain rate vector at the different plastic strain levels.

자동차 차체용 냉연 DP강 저항점용접부의 너깃경과 인장전단강도에 미치는 Si 함유량의 영향 (Effect of Si contents on Tensile-Shear Peak Load and Nugget Diameter in the Resistance Spot Welded of Dual Phase Steel for Automotive Body Applications)

  • 공종판;박태준;한태교;진광근;강정윤
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2009년 추계학술발표대회
    • /
    • pp.45-45
    • /
    • 2009
  • 원가 측면에서 유리한 저항점용접(Resistance Spot Welding)이 차체 용접에 80%이상으로 가장 많이 적용되고 있다. 첨단고강도강(Advanced High Strength Steel)의 저항점용접성 및 용접부 특성에 미치는 공정 변수의 영향에 대한 연구결과는 많으나, 합금원소의 영향에 대해서는 전무하다. 특히, Si는 DP(Dual Phase)강에 첨가 시 균일한 마르텐사이트의 분포를 촉진하는 원소로 저항 점용접성 및 용접부 특성에 영향을 미칠 것으로 예상되며, 이에 대한 연구는 보고된바 없다. 본 연구에서는 냉연 DP강의 저항 점용접시 중요한 인자 중 하나인 너깃경과 전단인장강도에 미치는 Si함유량의 영향을 검토하였다. 사용된 강재 및 용접기는 1.2mm 두께의 Si함유량(0, 0.5, 1.0, 1.5wt%)이 다른 인장강도 780~1000MPa급 냉연 DP강과 단상 AC용접기를 사용하였다. 용접조건은 ISO 18278-2규격에 따라 가압력 4kA, 초기가압시간 40cycle, 유지시간 17cycle로 고정하고, 용접전류만 변화하여 용접을 실시하였다. 너깃경은 용접부 단면을 컷팅 후 폴리싱 하여, 광학현미경과 Image Pro plus를 이용하여 측정했으며, 인장시편규격은 JIS Z 3137를 이용하였다. Si함유량이 증가에 따라 스패터 발생 전류는 감소했고, 너깃경은 직선적으로 증가했다. Si함유량 증가에 따른 너깃경 증가 이유는 저항(R) 측정결과, Si함유량 증가에 따라 모재의 저항이 높아져, 따라서 입열량($Q=I^2Rt$)이 많아지기 때문으로 판단되었다. 인정전단강도는 Si함유량 증가에 따라 직선적으로 증가했다. 이러한 이유는 Si함유량 증가에 따라 너깃경이 증가되기 때문으로 판단되었고, 너깃경과 인장전단강도 사이에 직선적 관계(PL(kN)=$3.2N_{dia.}$-0.81, $R^2$=0.93)를 가지고 있었다. 파단양상은 Si함유량에 상관없이 5.4kA이하에서는 계면파단이 일어났고, 6.0kA이상에서는 풀 아웃 파단이 일어났다. 계면파단주원인은 용접부 가장자리에 지름이 약 $5{\mu}m$이하의 예리한 노치가 존재하여 노치응력집중과 HAZ계면 근처에 미접합부가 존재하기 때문으로 판단되었다. 6.0kA이상에서는 예리한 노치가 없었고, HAZ부가 완전히 접합되어 있기 때문에 풀 아웃 파단이 일어난 것으로 판단되었다. 따라서, Si함유량 증가에 따라 적정용접전류 구간은 감소했고, 너깃경은 직선적으로 증가했다. 또한, Si함유량 증가에 따라 인장전간강도는 증가 했으며, 너깃경과 인장전단강도 사이에 직선적 관계를 가지고 있었다. 파단 양상은 Si함유량에 상관없이 5.2kA이하에서는 계면파단이, 6.0kA이상에서는 풀 아웃 파단이 일어났다.

  • PDF

수소주입된 고강도 DP 박강판의 소형펀치시험결과 분석 (An Analysis of Small Punch Test Conducted with the High Strength Dual Phase Sheet Steels Charged with Hydrogen)

  • 최영철;박재우;강계명
    • 한국표면공학회지
    • /
    • 제46권5호
    • /
    • pp.229-233
    • /
    • 2013
  • The small punch(SP) tests that can be applied to high strength sheet steel in automobile were carried out to evaluate the behavior of hydrogen embrittlement of DP sheet steels. In order to charge hydrogen at DP sheet steels, DP sheet steels were treated by the electrochemical hydrogen charging method under the charging conditions of current densities of 100, 150 and 200 $mA/cm^2$ for charging times of 5, 10, 25 and 50 hrs. Respectively, After hydrogen charging with experimental conditions, SP tests were performed. From the SP results, the correlations between the variation of bulb diameters and bulb heights with the hydrogen charging conditions were analysed. It was shown that the variation of bulb diameters were not significant with the hydrogen embrittlement due to the amounts of hydrogen charging. On the other hand, the bulb heights were observed to decrease with increasing hydrogen contents. It was thought that these results of the variation of bulb shapes after SP tests would be estimated as the index of evaluation of hydrogen embrittlement.

1GPa급 DP강 전기저항점용접부의 경도분포와 미세조직의 상관관계 (Hardness Distribution and Microstructures of Electric Resistance Spot Welded 1GPa Grade Dual Phase Steel)

  • 나혜성;공종판;한태교;진광근;강정윤
    • Journal of Welding and Joining
    • /
    • 제30권2호
    • /
    • pp.76-80
    • /
    • 2012
  • In this study, the effect of the welding current on the hardness characteristics and microstructure in the resistance spot welding of 1GPa grade cold-rolled DP steel was investigated, Also, correlation between the hardness and microstructure was discussed. In spite of the change in the welding current, the hardness distributions near weld was similar. the hardness in the HAZ and the fusion zone was higher than that of the base metal and the hardness in the fusion zone was variated with the location. Especially, the hardness of HAZ adjacent to the base metal showed maximum value, and softening zone in the base metal adjacent to HAZ was found. With the increasing of welding current, there were no difference in maximum hardness and average hardness in the fusion zone were, but the hardness of the softening zone reduced. The difference in the hardness in each location of weld due to grain size of prior austenite. The softening of the base metal occurred by tempering of the martensite.

자동차용 고강도 냉연강판 개발 (Development of Austomtive Cold-roiled High Strength Steel Sheets)

  • 김성주;진광근
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2004년도 춘계학술대회 논문집
    • /
    • pp.349-356
    • /
    • 2004
  • 자동차의 외관품질과 관련된 외판재용 고강도강으로는 내 dent성을 향상을 위해서 IF-HSS강과 BH강의 사용량이 크게 증가하였으며, 최근에는 490MPa급 DP강이 적용되기 시작하고 있다. 그리고 내판 판넬의 경우에는 고가공성 을 갖는 고강도강의 개발으로 고강도강의 사용량이 늘어나고 있다. 내판재 중 승객의 안전과 관련된 멤버, 필라와 같은 구조부재는 중간 정도의 강도를 갖는 고강도강을 주로 적용되어 왔으나, 최근 차체경량화 요구의 증가로 590MPa급 이상 고강도강이 적용되기 시작하였으며, 특히 고속변형에서 에너지 흡수능이 우수한 TRIP (Trans-formation Induced Plasticity)강 및 DP(Dual Phase)강에 대한 관심이 크게 증대되고 있다. 저속충돌에서 차체를 보호하는 범퍼보강재는 고강도화가 빠르게 진행되어, 현재는 석출경화강에 변태 조직 강화를 더한 780MPa급 이상의 초고강도강을 주로 사용하고 있으며, 1370MPa급 까지 적용하고 있다.

  • PDF