• 제목/요약/키워드: Drying schedule

검색결과 44건 처리시간 0.026초

물참나무 판재(板材)두께와 건조(乾燥)스케쥴별 건조(乾燥) 속도(速度), 응력과(應力)과 결함(缺陷)에 관(關)한 연구(硏究) (Studies on drying rate, stress and defect with board thicknesses and drying schedules of Quercus grosseserrata B1.)

  • 이상정;정희석
    • Journal of the Korean Wood Science and Technology
    • /
    • 제18권1호
    • /
    • pp.39-51
    • /
    • 1990
  • This research was carried out to offer the basis data for development of optimum drying schedule for a domestic oak species (Quercus grosseserrata B1.) by investigating drying rate. stress, defect, and moisuture gradient with board thicknesses and drying schedules (code number T4-C2 and T3-B1). The results were obtained as follows: 1. Average drying rate and total drying time from 52.2% to 5.8% were 0.105%/hr and 486 hours for drying schedule T4-C2 and those from 62.1% to 8.3% were 0.070%/hr. and 811 hours for drying schedule T3-B1. 2. Drying rates for 28mm- and 31mm-thick boards showed similar tendency, but were significantly different from 25mm- thick board in drying schedule T4-C2 and those for 22mm-, 25mm- 28mm- and 31mm-thick boards showed similar tendency but were significantly different from 19mm- thick boards in drying schedule T3-B1. 3. The moisture gradients for drying schedule T4-C2 were steeper than those for drying schedule T3-B1 during drying period. and especially in early drying stage slow slope of moisture gradients of drying schedule T3-B1 was effective in preventing serious problem of surface checks. 4. Drying stresses were lower in drying schedule T3-B1 than in drying schedule T4-C2 during drying period. 5. Drying schedule T4-C2 was appropriate for 25mm-thick board but not for 28mm- and 31mm-thick board because of strong drying condition. Drying schedule T3-B1 was appropriate for 28mm- and 31 mm-thick board but not for 19mm-, 22mm-, and 25mm-thick board because of weak drying condition.

  • PDF

국산 소나무재 건조스케줄 개량에 관한 연구 (Improvement of Drying Schedule for Domestic Red Pine Lumber)

  • 이형우;김경용
    • Journal of the Korean Wood Science and Technology
    • /
    • 제33권6호통권134호
    • /
    • pp.25-30
    • /
    • 2005
  • 두께 50 mm 국산 소나무(Pinus densiflora Sieb. et Zucc.) 판재의 건조스케줄 개량을 위해 일반 열기 건조스케줄, 시간 기준 건조스케줄, 연속 온도상승 건조스케줄, 그리고 습구온도 조절 건조스케줄을 적용하여 최종함수율 15% 정도까지 건조한 후 각각의 건조스케줄 적용에 의한 건조특성을 비교분석하였다. 두께 50 mm 국산 소나무의 일반 열기 건조스케줄 적용실험 결과 건조속도는 0.53%/hr, 시간 기준 건조스케줄 적용에 의한 건조속도는 0.9%/hr, 그리고 연속 온도상승 건조스케줄 적용에 의한 건조속도는 2.29%/hr였으며, 습구온도 조절 건조스케줄 적용에 의한 건조속도는 1.52%/hr였다.

미송(美松)의 열기건조(熱氣乾燥)스케쥴 개선(改善)에 관(關)한 연구(硏究) (Study on Kiln-Schedule Modification for Douglas Fir)

  • 정희석;챨리 코즈리크;헬므쓰 레슈
    • Journal of the Korean Wood Science and Technology
    • /
    • 제12권1호
    • /
    • pp.31-37
    • /
    • 1984
  • For the modification of kiln drying schedule, relations between resistance to drying Rd and the moisture content or drying times were found for 4/4, 6/4 and 8/4 green Douglas fir heartwood by the mild drying schedule and the severe drying schedule until the average moisture content was about 10 percent. The results of this study were as follows. 1. Resistance to drying of thicker lumber was higher than that of thinner lumber and resistance to drying of three different thicknesses were negligible between the mild-and the severe drying schedule. The relationships between resistance to drying and two schedules or three thicknesses of lumber were $Rd_1=1.830{\times}10^5\;M^{-2.24}$ for 4/4 lumber by the mild drying schedule, $Rd_2=1.822{\times}10^5\;M^{-2.25}$ for 4/4 lumber by the severe drying schedule, $Rd_3=2.352{\times}10^5\;M^{-2.14}$ for 6/4 lumber by the mild drying schedule, $Rd_4=3.457{\times}10^5\;M^{-2.27}$ for 6/4 lumber by the severe drying schedule, $Rd_5=1.317{\times}10^6\;M^{-2.56}$ for 8/4 lumber by the mild drying schedule, $Rd_6=8.267{\times}10^5\;M^{-2.40}$ for 8/4 lumber by the severe drying schedule. 2. Thinner lumber exhibited lower level of moisture content and shorter drying time required at intersection point between the moisture content and resistance to drying as a function of drying time than those of thicker lumber. Drying time of mild drying was longer than that of severe drying and similar to the level of moisture content at intersection point.

  • PDF

Development of Kiln Schedules to Eliminate the Development of Internal Checking in Radiata Pine Boards

  • Kang, Ho-Yang;Booker, R.E.
    • 한국가구학회지
    • /
    • 제19권2호
    • /
    • pp.116-123
    • /
    • 2008
  • Kiln schedule development was based on two schedule phases, the first being to determine the maximum safe kiln temperature during the check prone initial stage of drying, with the second stage determining how to accelerate drying once the danger of checking had passed. This was achieved by using 38 mm thick boards which were pre-screened for susceptibility to internal checking, and then drying matched sample boards over a range of kiln temperatures. Research has shown that below 50% MC there is no further risk of internal checking. However, difference in drying rate due to board width and the increased occurrence of wet patches in wide boards means that it is essential to modify the basic schedule according to the maximum board width. A condition of 52/40 $^{\circ}C$ was selected for the checking-free initial kiln drying step and a 5-step kiln-schedule dried the boards from 109% to 8% MC for 72.5 hours without internal checking.

  • PDF

단소용 대나무재의 열처리 및 건조 (Heat Treatment and Drying Methods of Small-Notched Bamboo for Vertical Flute)

  • 변희섭;오승원;공태석;김종만
    • 임산에너지
    • /
    • 제21권3호
    • /
    • pp.10-17
    • /
    • 2002
  • 본 연구는 단소용 대나무 악기재를 효과적으로 건조하기 위하여 열처리 및 몇 가지 스케줄에 의한 건조를 실시하였다. 평균 직경 2.2cm, 길이 60cm정도의 솜대를 이용하였다. 열처리 효과를 평가하기 위하여 무처리 및 열처리재로 구분하였으며 적당한 건조 조건 조사를 위해서 20℃, 65%와 40℃, 40% 그리고 대기상태의 3가지 조건으로 실시하였다. 탄화와 재색의 결함이 발생하지 않는 열처리의 최적 온도 조건은 180℃정도가 적당하였으며 열처리가 할렬의 수와 할렬 크기의 발생을 줄였으며 건조결함을 발생하지 않는 최적의 조건은 온도 20℃, 관계습도 65%이지만 건조를 할 때 기간이 너무 많이 소요되는 단점이 있기 때문에 40℃, 40%에서 건조시키는 것이 더욱 효율적이었다.

  • PDF

급속건조법(急速乾燥法)에 의한 은수원사시재(材)의 인공건조(人工乾燥)스케쥴 개발(開發) (Development of Kiln Drying Schedule of Hydrid Aspen (Populus alba × glandulosa) by Oven Drying Method)

  • 이형우
    • Journal of the Korean Wood Science and Technology
    • /
    • 제15권2호
    • /
    • pp.113-119
    • /
    • 1987
  • A study was conducted to determine the kiln drying schedule for hydrid aspen, This kiln drying schedule was found by oven drying method and developed by pilot testing of 2.0cm, 2.5cm, 3.0cm-thick green lumber. The results of this study were as follows: 1. Kiln drying schedule developed by oven-drying method was $T_{12}-E_5$ for 2.5cm-thick green lumber. 2. Drying times for 2.0cm-thick green lumber(127.0 percent moisture content) to 7.3 percent moisture content, for 2.5cm-thick green lumber(95.0 percent moisture content) to 9.7 percent moisture content, and for 3.0cm-thick green lumber(118.5 percent moisture content) to 10.0 percent moisture content were 45 hours, 45 hours, and 54 hours, respectively. 3. Drying rate from 90 to 10 percent moisture content of 2.5cm-thick lumber was about 0.7 times faster than that of 2.0cm-thick lumber and about 1.1 times faster than that of 3.0em-thick lumber. 4. End checks for 2.0cm-, 2.5cm-, and 3.0cm-thick green lumber occurred 95, 74 and 100 percent moisture content, respectively and reached maximum amount in 53, 41, and 60 percent moisture content, respectively. 5. No surface check and no honeycomb occurred. 6. Cupping and collapse slightly occurred and the quality of dry lumber was first.

  • PDF

리기다소나무의 건조저항(乾燥抵抗)을 이용한 건조(乾燥)스케쥴 개량(改良) (Kiln Drying Schedule Modification for Pitch Pine Using Drying Resistance)

  • 이경섭;정희석
    • Journal of the Korean Wood Science and Technology
    • /
    • 제16권2호
    • /
    • pp.69-78
    • /
    • 1988
  • 리기다소나무(Pinus rigida Mill)의 건조(乾燥)스케쥴 개량(改良)을 위해 두께 2.5cm 판재(板材)와 5.0cm 평소각재(平小角材)를 공시하여 각각 관행건조(慣行乾燥)스케쥴을 적용하여 최종함수율(最終含水率) 10% 정도까지 건조(乾燥)하고 함수율(含水率)과 건조저항(乾燥抵抗)의 관계를 측정한 결과는 다음과 같다. 1. 함수율(含水率)과 건조저항(乾燥抵抗)의 관계는 함수율(含水率)이 감소할수록 건조저항(乾燥抵抗)은 곡선적(曲線的)으로 증가하였으며, 건조중(乾燥中) 함수율(含水率)이 동일한 경우 건조저항(乾燥抵抗)은 평소각재(平小角材) 판재(板材)보다 컸다. 목재두께별 적용한 관행건조(慣行乾燥)스케쥴에 따른 함수율(含水率)과 건조저항(乾燥抵抗)의 관계는 다음과 같다. 1) 두께 2.5cm 판재(板材)의 관행건조(慣行乾燥)스케쥴에 따른 건조저항(乾燥抵抗) $R_{2.5}=6.795\times10^3M^{-1.27^{**}}$ 2) 두께 5.0cm 평소각재(平小角材)스케쥴에 따른 건조저항(乾燥抵抗) $R_{5.0}=5.206\times10^4M^{-1.55^{**}}$ 2. 건조시간(乾燥時間)에 따른 함수율(含水率)과 건조저항(乾燥抵抗)의 관계는 건조시간(乾燥時間)이 증가할수록 함수율(含水率)은 감소함과 동시에 건조저항(乾燥抵抗)은 증가하였으며, 평소각재(平小角材)가 판재(板材)보다 곡선변화(曲線變化)가 완만하였다. 3. 함수율(含水率) 10%까지의 관행건조(慣行乾燥)스케쥴에 따른 추정건조시간(推定乾燥時間)은 비교적 작은 오차(誤差)를 나타내며 관행건조시간(慣行乾燥時間)보다 작았다. 4. 목재두께별로 적용한 관행건조(慣行乾燥)을 유발하지 않으면서 최소의 시간에 원하는 최종함수율(最終含水率)에 도달하도록 개량(改良)할 필요가 있다. 5. 관행건조(慣行乾燥)스케쥴에 따른 kiln factor는 두께 2.5cm 판재(板材)의 경우 1.112이었으며, 두께 5.0cm 평소각재(平小角材)의 경우 1.136이었다.

  • PDF

수출용(輸出用) 목재가공품(木材加工品)의 품질개선(品質改善)에 관(關)한 연구(硏究) I. 참나무, 라민 및 나왕의 인공건조(人工乾燥) 스케줄 (A Study on Quality Improvement of Exporting Wood Products I. Kiln Drying Schedules for Oak, Ramin and Meranti)

  • 정병재
    • Journal of the Korean Wood Science and Technology
    • /
    • 제2권1호
    • /
    • pp.3-18
    • /
    • 1974
  • The exports of plywood are increasing annually and it has ranked first in the world market because of the high quality product and manufactured using mordern techniques. However, it is known that the exports of the other wood products, except plywood, is inactive because of their low quality. Accordingly, to increase the exports of various wood products investigations were carried out on kiln drying techniques to improve the quality of the wood. Wet wood should be kiln dried before use to prevent various drying defects such as distortion, shrinkage etc., which would develop after processing,:and also wet wood is not suitable for cutting, gluing and finishing. Therefore, the kiln drying properties of lumber from such species as oak, ramin and meranti which are used in large quantity for manufacturing exporting wood products have been studied. The results of the research are summarized as follows. (1) The end checks and the time for drying from initial moisture content of about 40 percent to 5 percent moisture content in ovendry were investigated as follows: (2) The kiln dried results, for 30mm stock, which are presented by using kiln schedule table 3 are as follows: (3) The kiln schedules for ramin, meranti and oak are given respectively as follows: Ramin kiln schedule: Table 17 and Table 18. Meranti schedule : Table 12. Oak schedule : Table 15.

  • PDF

강원도산(江原道産) 참나무과(科) 4 수종(樹種)의 추정건조(推定乾燥)스케쥴 (The estimated drying schedule of Fagaceae four species grown in Kangwon-Do)

  • 박종수;김수창
    • Journal of Forest and Environmental Science
    • /
    • 제10권1호
    • /
    • pp.38-48
    • /
    • 1994
  • 강원도산(江原道産) 참나무과(科) 4수종(樹種)의 건조특성(乾燥特性)을 파악코져 $100^{\circ}C$에서 급속건조(急速乾燥)를 실시하여 건조중(乾燥中) 함수율(含水率)과 건조경과(乾燥經過), 초기할렬(初期割裂)(목구할렬(목구할렬(木口割裂))과 표면할렬(表面割裂)), 찌그러짐, 내부할렬(內部割裂) 등의 건조결함(乾燥缺陷)을 조사(調査)하여 추정건조(推定乾燥)스케쥴을 작성(作成)한 결과(結果)는 다음과 같다. 건조시간별(乾燥時間別) 건조중(乾燥中) 함수율(含水率)은 초기함수율(初期含水率)이 높은 판재(板材)일수록 급속(急速)한 곡선적(曲線的) 감소(減少)를 나타내었고 건조소요시간(乾燥所要時間)이 길었으며 굴참나무가 건조중(乾燥中) 할렬(割裂)의 발생량(發生量)이 가장 크게 나타났으며 구해진 추정건조(推定乾燥)스케쥴은 $T_5-C_2$였다. 또한 모든 수종(樹種)의 목리방향별(木理方向別) 수축율(收縮率)은 접선방향(接線方向)(T) > 방사방향(放射方向)(R) > 섬유방향(纖維方向)(L)의 순위(順位)였으며 급속건조법(急速乾燥法)에 의한 수축율(收縮率)이 정상적인 수축율(收縮率)보다 크게 나타났다.

  • PDF