• Title/Summary/Keyword: Dissimilar steel weld

Search Result 114, Processing Time 0.049 seconds

Mechanical Behavior in Buttering Weld Zone between Low Alloy Steel and Austenitic Stainless Steel (저합금강과 오스테나이트 스테인리스강의 버터링 이종용접부에서의 기계적 성질의 거동)

  • Yang, In-Su;Tak, Young-Ji;Kim, Seong-Jae;Oh, Hwan-Sup
    • Proceedings of the KSME Conference
    • /
    • 2003.04a
    • /
    • pp.189-194
    • /
    • 2003
  • It is important to evaluate strength of dissimilar weld zone to use dissimilar materials safely. This study examines mechanical characteristics of dissimilar weld zone between low alloy steel and austenitic stainless steel that satisfies welding related requirements of ASME Code, experimentally reviews metallurgical and mechanical properties at and adjacent to weld interface. It is confirmed that hardness singularity occurs at the weld interface, and that optimum buttering thickness is more than 5㎜ from view points of tensile & yield strength. From a macroscopic view, brittle fracture characteristics is observed in buttering weld zone by tensile test.

  • PDF

A Study on Characteristics of Dissimilar Welds between Super Duplex Stainless Steel UNS S32750 and Carbon Steel A516-70 with FCAW (슈퍼듀플렉스 스테인리스강 UNS S32750과 탄소강 A516-70의 이종금속 FCA 용접 특성에 대한 연구)

  • Moon, In-June;Jang, Bok-Su;Kim, Se-Cheol;Koh, Jin-Hyun
    • Journal of Welding and Joining
    • /
    • v.32 no.4
    • /
    • pp.26-33
    • /
    • 2014
  • The metallurgical and mechanical characteristics, toughness and corrosion resistance of dissimilar welds between super duplex stainless steel UNS S32750 and carbon steel ASTM A516Gr.70 have been evaluated. Three heat inputs of 21.12, 24.00, 26.88kJ/cm were employed to make joints of dissimilar metals with flux cored arc welding(FCAW). Based on microstructural examination, vermicular ferrite was formed in the first layer of weld at low heat input(21.12kJ/cm) and $Cr_{eq}/Ni_{eq}$ of 1.61 while acicular ferrite was formed in last layer of weld at high heat input(26.88kJ/cm) and $Cr_{eq}/Ni_{eq}$ of 1.72. Ferrite percentage in dissimilar welds was lowest in the first layer of weld regardless of heat inputs and it gradually increased in the second and third layers of weld. Heat affected zone showed higher hardness than the weld metal although reheated zone showed lower hardness than weld metal due to the formation of secondary austenite. Tensile strengths of dissimilar welds increased with heat input and there was 100MPa difference. The corrosion test by ferric chloride solution showed that carbon steel had poor corrosion resistance and pitting corrosion occurred in the first layer(root pass) of weld due to the presence of reheated zone where secondary austenite was formed. The salt spray test of carbon steel showed that the surface only corroded but the amount of weight loss was extremely low.

Evaluation of Mechanical Properties with Thermal Aging in CF8M/SA508 Welds (CF8M과 SA508 용접재의 열화거동과 기계적특성 평가)

  • 우승완;최영환;권재도
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.28 no.12
    • /
    • pp.1968-1973
    • /
    • 2004
  • Structural degradations are often experienced on the components of nuclear power plants in reactor pressure vessels (RPV) and steam generators (SG) when these components are exposed to high temperature and high pressure for a long period of time. Such conditions result in the change of microstructures and of mechanical properties of materials, which requires an evaluation of the safeguards related to structural integrity. In a primary reactor cooling system (RCS), a dissimilar weld zone exists between cast stainless steel (CF8M) in a pipe and low-alloy steel (SA508 cl.3) in a nozzle. Thermal aging is observed in CF8M as the RCS is exposed for a long period of time under the operating temperature between 290 and 33$0^{\circ}C$. Under the same conditions, it is well known that degradation is not observed in low alloy steel. An investigation of the effect of thermal aging on the various mechanical properties of the dissimilar weld zone is required. The purpose of the present investigation is to find the effect of thermal aging on the dissimilar weld zone. The specimens are prepared by an artificially accelerated aging technique maintained for various times at 43$0^{\circ}C$, respectively. Then, The various mechanical test for the dissimilar welds are performed.

Residual Stress Analysis of the Overlay Weld on the Dissimilar Metal Butt Weld (이종재이종재료 Butt 용접에 대한 Overlay 용접의 잔류응력해석)

  • Kim, Kang-Soo;Lee, Ho-Jin;Lee, Bong-Sang;Jung, In-Chul;Byeon, Jin-Gwi;Park, Kwang-Soo
    • Proceedings of the KSME Conference
    • /
    • 2008.11a
    • /
    • pp.534-537
    • /
    • 2008
  • In recent years, the dissimilar metal, Alloy 82/182 welds used to connect stainless steel piping and low alloy steel or carbon steel components in nuclear reactor piping system have experienced cracking due to primary water stress corrosion(PWSCC). It is well known that one reason of the cracking is the residual stress by the weld. But, it is difficult to estimate exactly weld residual stress due to many parameters of welding. In this paper, the analysis of 3 FEM models made by ABAQUS Code is performed to estimate exactly the weld residual stress on the dissimilar metal weld. 3 FEM models are Butt model, Repair model and Overlay model and are the plane.strain 2D model. The thermal analysis and the stress analysis are performed on each model and the residual stresses on each model were calculated and compared respectively. Also, the specimen of Butt model was made and the residual stresses were measured by X-Ray method and Hole Drilling Technique. These results were compared with the FEM result of Butt model.

  • PDF

A Study on Weldability and Prediction of Nugget Shape in Dissimilar Metal Arc Spot Weld (이종 금속의 아크 스폿 용접성 및 접합부 형상 예측에 관한 연구)

  • 김기순;장경복;강성수
    • Journal of Welding and Joining
    • /
    • v.18 no.2
    • /
    • pp.57-63
    • /
    • 2000
  • In this study, the lap welding between austenitic stainless steel and carbon steel was carried out using arc spot welding process and weldability of welded specimens was estimated. From the tensile-shear strength test, micro Vickers harness test, and microstructure observation, specimen of $psi6.5mm$(hole of upper plate) showed the best results in terms of tensile-shear strength and nugget shape. And there was an unmix zone in fusion boundary between the carbon steel base metal and bulk weld metal. This zone had very width with the hard microstructure. The shape of weld nugget in arc spot welding of dissimilar metal melds was predicted by searching thermal history of a weld joint through a three-dimensional finite element model. From the numerical analysis, predicted the shape of weld nugget showed good agreement with the experiment.

  • PDF

A Study on the Diffusion Behaviors in Weld Interface of Cr-Mo Steel/Austenitic Stainless Steel (Cr-Mo강/오스테나이트계 스테인리스강 용접재의 용접계면에서의 확산거동에 관한 연구)

  • 김동배;이상율;이종훈;이상용;양성철
    • Journal of Welding and Joining
    • /
    • v.17 no.4
    • /
    • pp.46-52
    • /
    • 1999
  • Some of the pressurized reactor pressure vessels used in many chemical plants are made of low alloy carbon steel plates internally clad with an austenitic stainless steel for improved anti-corrosion properties. In this study, metallurgic structure of the weld interface of A 387 Grade12Class1 low alloy carbon steel claded with A182-F321 austenitic stainless steel after thermal exposure simulation heat treatment was investigated to display a characteristic behavior of dissimilar metal weld interface with thermal exposure during service at high temperature and pressure. EPMA, STEM, vickers-hardness test were performed and the results were correlated with the microstructure. To estimate the depth of the carburized/decarburized bands quantitatively, a model for carbon diffusion was proposed. The validity of the proposed theoretical relationships was confirmed by the directly measured data from the welded parts failed during service.

  • PDF

Evaluation of Mechanical Properties in Inconel 82/182 Dissimilar Metal Welds (인코넬 82/182 이종금속 용접부의 기계물성 평가)

  • Lee, Joung-Hoon;Jang, Chang-Heui;Kim, Jong-Sung;Jin, Tae-Eun
    • Proceedings of the KSME Conference
    • /
    • 2007.05a
    • /
    • pp.244-249
    • /
    • 2007
  • In several locations of the pressurized water reactors, dissimilar metal welds using inconel welding wires are used to join the low alloy steel nozzles to stainless steel pipes. To evaluate the integrity and design the dissimilar welds, tensile and fracture properties variations are needed. In this study, dissimilar metal welds composed of SA508 Gr.3 LAS, inconel 82/182 weld, and TP316 stainless steel were prepared by gas tungsten arc welding and shielded metal arc welding technique. Microstructures were observed using optical and electron microscopes. Different tensile and fracture properties were observed depending on the specimen sampling position at room temperature and $320^{\circ}C,$ and that was discussed based on the microstructure characteristics. It was found that the strength at the bottom of weld was greater than at the top of the weld. Also, from the test data using small punch specimen, more detailed tensile property variations were evaluated.

  • PDF

Distribution Characteristics of Weld Residual Stress on Butt Welded Dissimilar Metal Plate (이종금속 평판 맞대기용접의 용접잔류응력 분포특성)

  • Lee, Kyoung-Soo;Park, Chi-Yong;Kim, Maan-Won;Park, Jai-Hak
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.34 no.9
    • /
    • pp.1317-1323
    • /
    • 2010
  • In this study, the weld residual stress distribution at a dissimilar-metal welded plate of low alloy carbon steel and stainless steel, which are widely used in nuclear power plants, was characterized. A plate mock-up with butt welding was fabricated using SA 508 low alloy steel and Type 304 stainless steel plates and the residual stresses were measured by the X-ray diffraction method after electrolytic polishing of the plate specimen. Finite element analysis was carried out in order to simulate the butt welding of dissimilar metal plate, and the calculated weld residual stress distribution was compared with that obtained from the measured data. The characteristics of the three-dimensional residual stress distribution in a butt weld of dissimilar metal plates were investigated by comparing the measured and calculated residual stress data.

Analysis of Carbon Migration with Post Weld Heat Treatment in Dissimilar Metal Weld. (이종금속 피복용접부의 후열처리에 따른 탄소이동 해석)

  • Kim, Byeong-Cheol;Ann, Hui-Seong;Kim, Seon-Jin;Song, Jin-Tae
    • Korean Journal of Materials Research
    • /
    • v.1 no.1
    • /
    • pp.29-36
    • /
    • 1991
  • Pressurized Water Reactor (PWR) pressure vessels are made of forged low alloy steel plates internally clad with an austenitic stainless steel by welding to improve anti-corrosion properties. They display a characteristic behavior of dissimilar metal weld interface during post weld heat treatment (PWHT) and service at high temperature and pressure. In this Study, Metallugical structure of weld interface of SA 508 Class 3 forged steel clad with 309L, Austenitic stainless steel after PWHT was investigated. To estimate the width of the carburized/decarburized bands quantitatively, a model for carbon diffusion was proposed and a theoretical equation was derived.

  • PDF

A Study of Characteristics on the Dissimilar Metals (Alloy steel : A387 Gr. 91 - Carbon Steel : A516 Gr. 70) Welds Made with FCA Multiple Layer Welding: Part 2 (합금강(ASTM A387 Gr. 91) - 탄소강(ASTM A516 Gr.70) 이종금속의 FCA 다층 용접부 특성 평가 : Part. 2)

  • Shin, Tae Woo;Hyun, Jun Hyeok;Koh, Jin Hyun
    • Journal of Welding and Joining
    • /
    • v.35 no.3
    • /
    • pp.68-74
    • /
    • 2017
  • Characteristics of dissimilar metal welds between alloy steel ASTM A387 Gr. 91 and carbon steel ASTM A516 Gr.70 made with Flux cored arc welding(FCAW) have been evaluated in terms of microstructure, mechanical strength, chemical analysis by EDS as well as corrosion test. Three heat inputs of 15.0, 22.5, 30.0kJ/cm were employed to make joints of dissimilar metals with E71T-1C wire. Post-weld heat treatment was carried out at $750^{\circ}C$ for 2.5 h. Based on microstructural examination, Intragranular polygonal ferrite and grainboundary ferrite were formed only in first layer of weld metal. Another layers consisted of acicular ferrite and $Widmannst{\ddot{a}}tten$ ferrite. The amount of acicular ferrite was increased with decreasing heat input and layer. Heat affected zone of alloy steel showed the highest hardness due to the formation of tempered martensite and lower bainite. Lower and upper bainite were formed in heat affected zone of carbon steel. Tensile strengths of dissimilar metal welds decreased with increasing heat inputs. Dissimilar metal welds showed a good hot cracking resistance due to the low HCS index below 4. The salt spray test of dissimilar metals welds showed that the weight loss rate by corrosion below 170 hours was decreased with increasing heat inputs due to the increase of the amount of acicular ferrite.