• 제목/요약/키워드: Dissimilar metal joining

검색결과 92건 처리시간 0.021초

Review of magnetic pulse welding

  • Kang, Bong-Yong
    • Journal of Welding and Joining
    • /
    • 제33권1호
    • /
    • pp.7-13
    • /
    • 2015
  • Magnetic pulse welding(MPW) is a solid state welding process that is accomplished by a magnetic pulse causing a high-velocity impact on two materials, resulting in a true metallurgical bond. One of the great advantages of MPW is that it is suitable for joining dissimilar metals. No heat affected zones are created because of the negligible heating and the clean surfaces formation that is a consequence of the jet and the metal is not degraded. Also, compared to other general welding processes, this process leads to only a low formation of brittle intermetallic compounds However, although this process has many advantages its application to industrial fields has so far been very low. Therefore, in this study we are presenting the principles, apparatus and application of MPW for application the industrial fields.

HIP DIFFUSION BONDING OF INTRICATE SHAPE COMPONENTS MADE OF LIGHT ALLOYS AND STEELS

  • Guelman, A.A.
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.769-775
    • /
    • 2002
  • The results gained as part of the study on weldability of compositions from steels, aluminium, titanium alloys in various combinations including similar and dissimilar metal bonding variants with reference to solution of specific practical problems are presented in this work. It has been shown that in the case of HIP/DB carried out with direct interaction of bonding surfaces of the most dissimilar material combinations under study, formation of high-quality joints is not assured due to various reasons. That is why development of special bonding techniques was required. The bonding techniques developed and used for HIP/DB of dissimilar steels, "Steel-bronze", "Titanium-niobium"; "Titanium-steel" and other compositions under study ensured vacuum-tight microvoid-free joints strength of a which was equal to the milder parent metal, including those obtained at reduced welding pressures. Examples of new products manufactured by HIP/DB using the technologies developed are presented.

  • PDF

계장핵연료 조사시험용 실튜브 레이저용접기술 (Laser Welding of Seal Tube for Instrumented Irradiation Fuel Test)

  • 김수성;이철용;김웅기;박근일;고진현;서준석
    • Journal of Welding and Joining
    • /
    • 제23권6호
    • /
    • pp.43-48
    • /
    • 2005
  • This work was carried out to obtain sound welds and to select a most suitable binary metal joint among three different dissimilar binary metal combinations such as Zr-4/Ta, Mo/Ta and Ti/Ta(seal tube/sensor sheath) joints fur the instrumented nuclear fuel irradiation test. To do this, Taguchi experimental method was employed to optimize the experimental data. In addition, metallography, micro-focus x-ray radiography and hardness test were conducted to examine the welds. From the weld bead appearance, penetration depth and bead width as well as weld defects standpoint, Zr-4/Ta joint is suggested for the circumferential joining between a seal tube and a sensor sheath. The optimized welding parameters based on Zr-4/Ta joint are suggested as well.

스테인리스강 STS 316L과 탄소강 A516-70의 이종금속 GTA 용접부 특성에 대한 연구 (A Study of Characteristics on the Dissimilar Metals (STS 316L - Carbon Steel: ASTM A516-70) Welds made with GTAW)

  • 김세철;신태우;문인준;장복수;고진현
    • Journal of Welding and Joining
    • /
    • 제33권4호
    • /
    • pp.37-43
    • /
    • 2015
  • Characteristics of dissimilar metal welds between STS 316L and carbon steel ASTM A516 Gr.70 made with GTAW have been evaluated in terms of microstructure, ferrite content, chemical analysis, hardness and corrosion resistance. Three heat inputs of 9.00, 11.25, 13.00kJ/cm were employed to make joints of dissimilar metals with ER309 wire. Based on microstructural examination, the amount of vermicular type of ${\delta}$-ferrite was increased with increasing heat input due to the increase of Creq/Nieq in the second layer of welds. Based on the EDX analysis of weld metals, Cr and Ni content in the 2nd layer increased while those content in the first layer of welds decreased with heat inputs. Cellular solidification mode in the 1st layer and dendritic solidification mode in the 2nd layer due to different cooling rates were prevailed, respectively. Heat affected zone which formed hard microstructure showed higher hardness than the weld metal. The salt spray test of dissimilar metals weld joints showed that the carbon steel surfaces only corroded. The weight loss rate due to corrosion increased up to 100hours but it decreased above 100 hours. There was little difference in the weight loss caused by corrosion regardless of heat inputs.

SPR 과 접착제를 이용한 이종재료 접합의 피로평가 (Fatigue Assessment Using SPR and Adhesive on Dissimilar Materials)

  • 김태현;서정;강희신;이영신;박춘달
    • 한국정밀공학회지
    • /
    • 제28권10호
    • /
    • pp.1204-1209
    • /
    • 2011
  • In this study, fatigue life is evaluated by comparing with lighter car body through the experiment on SPR joints. An experimental activity on sheet metal samples of Aluminum 5J32 and Steel SPRC440 has been conducted to achieve better understanding of the process. In addition, SPR joint used less than the existing Spot Welding improves joint strength and fatigue life is evaluated by using SPR and adhesive joining Hybrid. Joining(bonding) strength and fatigue life on SPR and Hybrid (SPR + adhesive) are evaluated throughout the experiment. With joining strength than 20 % of the aluminum material, dissimilar materials has improved over 2 times as large as the strength In case of dissimilar materials, the fatigue life of aluminum is increased by 1.6 to 2.5 times as large as the life.

마찰교반접합한 오스테나이트계 스테인리스강과 6013알루미늄 합금 이종 접합부의 접합 특성 및 계면 성질 (Joint properties and Interface Analysis of Friction Stir Welded Dissimilar Materials between Austenite Stainless Steel and 6013 Al Alloy)

  • 이원배;;;정승부
    • Journal of Welding and Joining
    • /
    • 제23권5호
    • /
    • pp.61-68
    • /
    • 2005
  • Dissimilar joining of Al 6013-T4 alloys and austenite stainless steel was carried out using friction stir welding technique. Microstructures near the weld zone and mechanical properties of the joint have been investigated. Microstructures in the stainless steel side were composed of the heat affected zone and the plastically deformed zone, while those in the Al alloy side were composed of the recrystallized zone including stainless steel particles, the thermo-mechanically affected zone and the heat affected zone. TEM micrographs revealed that the interface region was composed of the mixed layers of elongated stainless steel and ultra-fine grained Al alloy with lamella structure and intermetallic compound layer. Thickness of the intermetallic layer was approximately 300nm and was identified as the A14Fe with hexagonal close packed structure. Mechanical properties, such as tensile and fatigue strengths were lower than those of 6013 Al alloy base metal, because tool inserting location was deviated to Al alloy from the butt line, which resulted in the lack of the stirring.

페라이트계 및 오스테나이트계 스테인리스강과 IF강의 이종 접합부의 저항 점 용접성 평가 (Assessment of Resistance Spot Weldability of Dissimilar Joints of Austenitic Stainless Steels/IF Steels and Ferritic Stainless Steels/IF Steels)

  • 이진범;김동철;남대근;강남현;김순국;유지훈;임영목;박영도
    • 대한금속재료학회지
    • /
    • 제49권1호
    • /
    • pp.64-72
    • /
    • 2011
  • The spot weldability of dissimilar metal joints between austenitic stainless steels (STS316)/IF steels and ferritic stainless steels (STS430)/IF steels was investigated. This study was aimed to determine the spot welding parameters for a dissimilar metal joint and to evaluate the dissimilar metal joint's weldability, including its welding nugget shape, tensile-shear strength, hardness, and microstructure. The comparison of these results was described in terms of fracture behavior. Compared with the weld lobe of similar metal joints, dissimilar metal joints (STS430/IF) had reduced weld current range. However, the weld lobe of STS316/IF steel joint showed increased weld current range. This is because the dilution of chemical composition in the molten weld pool suppressed the heat input being caused by Joule heat with current flow through the samples. The microstructure of the fusion zone was fully martensite and mixture of ferrite and martensite for austenitic stainless steel/IF steel and ferritic stainless steel/IF steel combination, respectively. The experimental results showed that the shape of nugget was asymmetric, in which the fusion zone of the austenitic and ferritic stainless steel sheet was larger due to the higher bulk-resistance. The predicted microstructure by using the Schaeffler diagram was well matched with experimental results. After peel test, the fracture was initiated from heat affected zone of ferritic stainless steel sheet side, however the final fracture was propagated into the IF steel sheet side due to its lower strength.

원자로 입출구 노즐 Alloy 82/182 이종금속 용접부 Weld Inlay 적용 후 초음파나노표면개질이 잔류응력 완화에 미치는 영향 (The effect of ultrasonic nano crystal surface modification for mitigation of the residual stress after weld inlay on the alloy 82/182 dissimilar metal welds of reactor vessel in/outlet nozzles)

  • 조홍석;박익근;정광운
    • Journal of Welding and Joining
    • /
    • 제33권2호
    • /
    • pp.40-46
    • /
    • 2015
  • This study was performed to investigate the effect of ultrasonic nano crystal surface modification (UNSM) on residual stress mitigation after Weld Inlay repair for butt dissimilar metal weld with Alloy 82/182 in reactor vessel In/Outlet nozzle. As-welded and Weld Inlay specimens were made in accordance with design standard of ASME Code Case N-766, and two planes of their weld specimens were peened by the optimum UNSM process condition. Peening characteristics for weld specimens after UNSM treatment were evaluated by surface roughness and Vickers hardness test. And, residual stress for weld specimens developed from before and after UNSM treatment was measured and evaluated by instrumented indentation technique. Consequently, it was revealed that the mitigation of residual stress in weld metal after Weld Inlay repair of reactor vessel In/Outlet nozzle could be possible through UNSM treatment.

A2024 와 SM45C 마찰용접의 열전달 해석 (Heat Transfer Analysis of Friction Welding of A2024 to SM45C)

  • 이상윤;윤병수
    • 한국공작기계학회논문집
    • /
    • 제10권1호
    • /
    • pp.65-70
    • /
    • 2001
  • The hear transfer mechanism initiating the friction welding is examined and a transient three dimensional heat conduc-tion model for the welding of two dissimilar cylindrical metal bars is investigated. The cylindrical metal bars are made of materials made of A2024 and SM 45C. Numerical simulations of heat flow are performed using the finite volume method. Respectively. Commercial FLUENT code is used in the heat flow simulation and maximum temperature and distribution of temperature are calculated. Temperature of friction welded joining face is compared with the temperature distribution measured by experiment and numerical simulation. The maximum temperature of friction welded joining face is lower than melting point of A2024-T6 aluminum alloy using insert metal. The temperature distribution of friction welded join- ing face with insert metal is more uniform than that of without inset metal.

  • PDF

스테인리스강(ASTM Type 316L)과 탄소강(ASTM A516 Gr.70) 이종금속의 FCA 다층 용접부 특성에 대한 연구 (A Study of Characteristics on the Dissimilar Metals (ASTM Type 316L - Carbon Steel : ASTM A516-70) Welds Made with FCA Multiple Layer Welding)

  • 김세철;현준혁;신태우;고진현
    • Journal of Welding and Joining
    • /
    • 제34권3호
    • /
    • pp.69-76
    • /
    • 2016
  • Characteristics of dissimilar metal welds between ASTM Type 316L and carbon steel ASTM A516 Gr.70 made with FCAW were evaluated in terms of microstructure, ferrite content, EDS analysis, hardness, tensile strength, impact toughness and corrosion resistance. Three heat inputs of 10.4, 16.9, 23.4kJ/cm were employed to make joints of dissimilar metals with E309LMoT1-1 wire. Microstructure of dissimilar weld metals consisted of mostly vermicular type of ${\delta}$-ferrite and some lathy type of ${\delta}$-ferrite, and ${\delta}$-ferrite was transformed into globular type in reheated zone. In all conditions, weld metals were solidified on FA solidification mode. Based on the EDS analysis of weld metals, All Creq/Nieq values were in the range of FA solidification mode, and it was decreased with increasing heat inputs whereas it was increased with increasing layers. The amount of ${\delta}$-ferrite was decreased with increasing heat input due to the difference of cooling rate, and it was increased with increasing layers. Accordingly, hardness and tensile strength of dissimilar metals weld joints was decreased with increasing heat input while impact energy was increased with increasing heat input. Corrosion test of dissimilar metals weld joints showed that weight gain rate of heat input 10.4kJ/cm was the greatest, and that of three heat inputs became constant after certain time.