마찰교반접합한 오스테나이트계 스테인리스강과 6013알루미늄 합금 이종 접합부의 접합 특성 및 계면 성질 (Joint properties and Interface Analysis of Friction Stir Welded Dissimilar Materials between Austenite Stainless Steel and 6013 Al Alloy)

  • 이원배;;;정승부
    • Journal of Welding and Joining
    • /
    • 제23권5호
    • /
    • pp.61-68
    • /
    • 2005
  • Dissimilar joining of Al 6013-T4 alloys and austenite stainless steel was carried out using friction stir welding technique. Microstructures near the weld zone and mechanical properties of the joint have been investigated. Microstructures in the stainless steel side were composed of the heat affected zone and the plastically deformed zone, while those in the Al alloy side were composed of the recrystallized zone including stainless steel particles, the thermo-mechanically affected zone and the heat affected zone. TEM micrographs revealed that the interface region was composed of the mixed layers of elongated stainless steel and ultra-fine grained Al alloy with lamella structure and intermetallic compound layer. Thickness of the intermetallic layer was approximately 300nm and was identified as the A14Fe with hexagonal close packed structure. Mechanical properties, such as tensile and fatigue strengths were lower than those of 6013 Al alloy base metal, because tool inserting location was deviated to Al alloy from the butt line, which resulted in the lack of the stirring.

이종 마찰용접 강봉재의 후열처리에 따른 기계적 특성 (Mechanical Properties of Dissimilar Friction Welded Steel Bars in Relation to Post Weld Heat Treatment)

  • 공유식;김선진
    • 대한기계학회논문집A
    • /
    • 제30권4호
    • /
    • pp.402-408
    • /
    • 2006
  • Dissimilar friction welding were produced using 15(mm) diameter solid bar in chrome molybedenum steel(KS SCM440) to carbon steel(KS S45C) to investigate their mechanical properties. The main friction welding parameters were selected to endure good quality welds on the basis of visual examination, tensile tests, Vickers hardness surveys of the bond of area and H.A.Z and microstructure investigations. The specimens were tested as-welded and post-weld heat treated(PWHT). The tensile strength of the friction welded steel bars was increased up to 100% of the S45C base metal under the condition of all heating time. Optimal welding conditions were n=2,000(rpm), $P_1=60(MPa),\;P_2=100(MPa),\;t_1=4(s),\;t_2=5(s)$ when the total upset length is 5.4 and 5.7(mm), respectively. The peak of hardness distribution of the friction welded joints can be eliminated by PWHT. Two different kinds of materials are strongly mixed to show a well-combined structure of macro-particles without any molten material and particle growth or any defects.

유공압 밸브 스풀용 강재의 관 대 봉 이종재 마찰용접의 최적화와 용접강도특성 및 AE평가 (Optimization of tube-to-bar dissimilar FRW of hydraulic valve spool steels and the weld strength properties and its AE evaluation)

  • 오세규;김현필;장홍근;오명석
    • 한국해양공학회지
    • /
    • 제11권1호
    • /
    • pp.24-35
    • /
    • 1997
  • The hydraulic or pneumatic valve spools become essential as the important components on the production of automatic hydraulic or pneumatic as mechanical industry has been rapidly developed. The machining precision is in necessity for manufacturing the valve spools. They could be unstable in the quality by the conventional are welding. And also they have a lot of technical problems in manufacturing because their shapes are generally small. By the precision casting process such as lost wax process, the production cost may be increased. But by the friction welding technique, they will be able to be manufactured without such problems. This paper deals with the development of dissimilar friction welding optimization for the hydraulic or pneumatic valve spool by friction welding and a new approach of on real-time qualify evaluation by AE techniques.

  • PDF

이종재(SKNM50-SCM440) 금형펀치의 마찰용접과 AE품질평가 (Friction Welding of Dissimilar Press Punch Materials and Its Evaluation by AE)

  • 오세규;박일동;전태언;이원석;이향동
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 1995년도 특별강연 및 추계학술발표 개요집
    • /
    • pp.165-169
    • /
    • 1995
  • This paper deals with determining the proper friction welding condition and analyzing mechanical in of friction welded joints of sintered carbide tool materials (SKNM50 for the blade part of press punch) to alloy steel (SCM440 for the shank part of press punch), the alloy steel to aluminum(A6061 for the interlayer material between the blade part and the shank) and sintered carbide tool materials to aluminum. And also acoustic emission test will be carried out during fiction welding to evaluate the weld quality.

  • PDF

열간 금형재의 마찰용접 최적화와 AE평가 (Friction Welding Optimization of Hot Die Punch Materials and Its AE Evaluation)

  • 오세규;공유식;박일동;유인종
    • 동력기계공학회지
    • /
    • 제4권4호
    • /
    • pp.54-58
    • /
    • 2000
  • The complete joining method for dissimilar hot die punch materials and its real-time evaluation method are not available at present. Brazing method has been used for joining them, but it is known that the welded joint by the brazing has the lower bonding efficiency and reliability than the diffusion welding. The friction welding with a diffusion mechanism in bonding was applied in this study. So, this work was carried out to determine the optimal friction welding conditions and to analyze mechanical properties of friction welded joints of hot die punch materials (STD61 for the blade part of hot die punch) to alloy steel (SCM440 for the shank part of hot die punch) such as plunger. In addition, acoustic emission test was carried out during friction welding to evaluate the weld quality.

  • PDF

스프링강(SUP9A)-SM25C의 이종재 마찰용접 피로특성에 관한 연구 (A Study on Fatigue Characteristics of Dissimilar Spring Steel(SUP9A)-SM25C by Friction Welding)

  • 정석주;이기중
    • 한국안전학회지
    • /
    • 제16권3호
    • /
    • pp.19-25
    • /
    • 2001
  • The friction-welding SM25C is a substitute for the suing steel that is utilized in the machinery, airplane, and automobile, ok. This substitution would provide reduction of material and weight of welding parts. From the result we found that the strength of the friction welded joint was 529-617MPa and the toughness 1.2 times higher than that of the base metal. The optimal condition of friction welding was found as follows : n=2000rpm, $P_1$=68㎫, $P_2$=137MPa, $t_2$=2sec, $t_1$=2-4sec, Considering the strength, the hardness, and the reduction of area in the friction welding, the fiction welding using SUP9A and SM25C was found to cause no problem in on-the-job application.

  • PDF

Turning Vane Bolt의 이종재(STS316L/IN X-750) 마찰용접에 관하여 (On Dissimilar Friction Welded Joints(STS316L/IN X-750) of Turning Vane Bolt)

  • 신기석;공유식;김선진;류인일
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2004년도 학술대회지
    • /
    • pp.331-336
    • /
    • 2004
  • Dissimilar friction welding were produced using 10mm and 11mm diameter solid bar in Inconel ally(IN X-750) to Stainless steel(STS316L) to investigate their mechanical properties. The main friction welding parameters were selected to endure good quality welds on the basis of visual examination, tensile tests, Virkers hardness surveys of the bond of area and HAZ and macro-structure investigations. The specimens were tested as welded, not heat-treated. The tensile strength of the friction welded steel bars was increased up to $95\%$ of the STS316L base metal under the condition of all heating time. Optimal welding conditions were n=2,000(rpm), $P_1=220(MPa),\;P_2=260(MPa),\;t_1=4(s),\;t_2=4(s)$ when the total upset length is 7(mm).

  • PDF

철도차량 적용을 위한 Al alloy(A6005)-Mg alloy(AZ61) 이종소재 마찰교반용접 특성 연구 (Characteristics of Dissimilar Materials Al alloy(A6005)-Mg alloy(AZ61) Under Friction Stir Welding for Railway Vehicle)

  • 이우근;김정석;선승주;임재용
    • 한국산학기술학회논문지
    • /
    • 제17권8호
    • /
    • pp.706-713
    • /
    • 2016
  • 본 연구에서는 이종소재 A6005-AZ61 접합을 위하여 마찰교반용접의 툴 삽입 위치와 모재의 냉각 유 무에 따라 용접부 특성을 분석하였다. 다른 용접 조건들인 툴 회전속도와 이송속도는 500rpm-30mm/min으로 고정하고 Advancing side에 알루미늄 합금(A6005), Retreating side에 마그네슘 합금(AZ61)을 배치하여 용접을 진행하였다. 용접은 여섯 가지 케이스를 진행하였다. 용접부 특성을 관찰하기 위하여 인장 시험을 진행하고, 광학현미경을 사용하여 용접부의 미세조직을 관찰하였다. 인장시험 결과 마그네슘 합금 방향으로 툴을 1mm 이동시키고 모재에 냉각을 시킨 조건에서 강도가 가장 높게 나타났다. 동일한 용접 조건에서 냉각을 한 경우에 냉각을 하지 않은 것 보다 강도가 약 2배 높게 측정되었다. 툴의 위치는 용접부 중심에서 알루미늄 합금 방향으로 1.7mm, 마그네슘 합금 방향으로 1.7mm 이동시켜 과도한 편심을 적용한 용접 조건에서는 교반이 잘 이루어지지 않아 용접부의 건전성이 가장 좋지 않았다. 과도한 편심을 적용한 용접 조건에서는 교반이 잘 이루어지지 않아 용접부의 건전성이 가장 좋지 않았다. 본 연구를 통해 A6005-AZ61 이종 마찰교반용접시 용접속도와 툴 회전속도만큼 모재의 온도 조절과 툴 삽입위치가 중요한 용접변수임을 확인 하였다.