$Li_2O$의 삼출이 없는 $LiNbO_3$ 광도파로의 제조방법 (New Fabrication Method of $Ti:LiNbO_3$ Waveguide with Suppressed Out-Diffusion)

  • 김상혁;김상국;조재철;최상삼
    • 한국광학회지
    • /
    • 제2권3호
    • /
    • pp.149-152
    • /
    • 1991
  • 리튬나이오베이트 결정에 Ti를 열확산시켜 광도파로를 만드는 방법에서 문제가 되는 out-diffusion(삼출) 문제를 해결하는 방안으로 확산과정 이전에 $SiO_2$ 박막을 시료 위해 입히고 Ti을 열확산시켜 광도파로를 제조하는 방법을 제안하였으며, 기존의 방법에 의해서 만들어진 광도파로와 본 연구의 방법에 의해서 만든 광도파로의 근시야상(near field pattern)을 비교하였다.

  • PDF

이온교환 평판도파로의 실효굴절율 측정 및 해석 (Analysis and Measurement of Effective Refractive Indices with Ion-exchanged Slab Waveguide)

  • 천석표;박정일;박태성;정홍배
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1995년도 춘계학술대회 논문집
    • /
    • pp.73-76
    • /
    • 1995
  • In this study, the slab waveguide was fabricated using potassium-nitride(KNO$_3$) or silver-nitride (AgNO$_3$) molten sources by ion-exchange process. The effective refractive indices of waveguide were measured by Prism-Coupling method. and The characteristics of waveguide(mode dispersion, effective diffusion depth. surface refractive index, diffusion coefficient, and refractive index profile etc,) were investigated by WKB method, In the case of potassium ion-exchange, the computer calculation showed that the refractive index profile of waveguide followed Gaussian function, the surface refractive index increased with ion-exchange time and the effective diffusion depth increased a little as ion-exchange time increased, while the surface refractive index of silver ion-exchanged waveguide decreased with ion-exchange time because of the ion depletion on the surface of waveguide, and the effective diffusion depth seriously with ion-exchange tim. Double ion-exchanged waveguide was fabricated by performing silver ion-exchange after potassium ion-exchange. Double ion-exchanged waveguide had a tight mode binding force since the surface refractive index was larger than single step ion-exchanged waveguide.

  • PDF

저손실 $Ti:LiNbO_3$ 광도파로제작 및 BPM 해석 (BPM Analysis and Preparation of Low Loss $Ti:LiNbO_3$ Optical Waveguide)

  • 김성구;윤형도;윤대원;박계춘;이진
    • 한국전기전자재료학회논문지
    • /
    • 제11권5호
    • /
    • pp.400-406
    • /
    • 1998
  • We investigated the preparation and guided-mode properties of $Ti:LiNbO_3$ waveguides which were fabricated by Ti in-diffusion. The diffusion method to reduce the Li out-diffusion was proposed. The optical guided-mode and propagation loss based on butt-coupling pigtailed with PMF-input were measured. How to improve the polishing grade of waveguide endfaces is newly proposed in this paper. To show the mode propagations, the BPM simulations of channel waveguide are described.

  • PDF

Air 분위기로 제작한 Ti:$LiNbO_3$ 도파로 특성 및 폴리싱 방법제안 (Properties of Ti:$LiNbO_3$ Optical Waveguide by Diffusion in Air Atmosphere and Proposal of a Polishing Method)

  • 김성구;윤형도;윤대원;한상필;박계춘;유용택
    • E2M - 전기 전자와 첨단 소재
    • /
    • 제10권7호
    • /
    • pp.682-691
    • /
    • 1997
  • We have investigated the guided optical properties of a Ti:LiNbO$_3$optical waveguide which was fabricated by Ti-diffusion in an air atmosphere and proposed an effective polishing method of waveguide endfaces. And the results of guided optical mode and fabrication condition were obtained as follows; \circled1 propagation loss : 0.53 dB/cm \circled2 mode size : horizontal/vertical=12.5${\mu}{\textrm}{m}$ \circled3 mode mismatch : 1.7 dB \circled4 diffusion temperature : 105$0^{\circ}C$, time : 8 hours \circled5 atmosphere : air

  • PDF

Total Fiber-to-fiber Insertion Loss가 <6dB 인 Ti:$LiNbO_3$ 과도파로 Pigtailing 및 손실분석 (The Pigrailing and The Loss Analysis of low loss LiNbO$_3$ Optical Waveguide with Fiber-to-fiber Insetion Loss<6dB)

  • 김성구;박계춘;조재철
    • 한국전기전자재료학회논문지
    • /
    • 제11권7호
    • /
    • pp.557-564
    • /
    • 1998
  • A low loss x-cut $LiNbO_3$optical waveguide was fabricated by Yi in-diffusion, and the properties of guided-mode and the total insertion loss of the pigtailed waveguide with polarization maintaining fiber(PMF) were measured at optical wavelength 1550nm. for forming the waveguides, the parameters of diffusion, Ti thickness, waveguide line-width, length, diffusion temperature, time and atmosphere were set $1400{\AA}$, $8{\mu}m$, 3.3cm, $1050^{\circ}C$, 8 hours and wet bubbled oxygen, respectively. And then after the polishing and piatailing, it showed that the total insertion loss was -4.1dB for TM mode, -5.5dB for TE mode, and mode size, that is, the horizontal/ vertical size were $13.8{\mu}m/18{\mu}m$ for TM mode, $9.6{\mu}m/6.5{\mu}m$ for TE mode.

  • PDF

Fiber-to-fiber Total Insertion Loss가 <6d8인 Ti:LiNbO$_3$ 광도파로 Pigtailing 및 도파모드특성

  • 김성구;윤형도;임영민;윤대원;한상필
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1997년도 추계학술대회 논문집
    • /
    • pp.73-76
    • /
    • 1997
  • A low loss x-cut LiNbO$_3$ optical waveguide was fabricated by Ti in-diffusion and the guided-mode properties and total insertion loss of pigtailing with polarization maintaining fiber(PMF) were investigated and measured at optical wavelength 15507. For formaing the waveguide, the parameters of diffusion Ti thickness, waveguide line-width, length, diffusion temperature, time and atmosphere were set 1400$\AA$, 8${\mu}{\textrm}{m}$, 3.3cm, 105$0^{\circ}C$, 8 hours and wet bubbled oxygen, respectively. and then After the polishing and pigtailing, it showed that total insertion loss was -4.1dB for TM mode, -5.5dB for TE mode, and mode size, that is, horizontal/vertical sizes were 13.87/18${\mu}{\textrm}{m}$ for TM mode, 9.61${\mu}{\textrm}{m}$/6.5${\mu}{\textrm}{m}$ for TE mode.

  • PDF

Ti:LiNbO$_{3}$ 광도파로 제작 및 특성분석 (Fabrication and Characteristics Analysis of Ti:LiNbO$_{3}$ Optical Waveguide)

  • 윤형도;김성구;이한영;윤대원
    • 전자공학회논문지D
    • /
    • 제35D권7호
    • /
    • pp.109-116
    • /
    • 1998
  • In this work was produced and analyzed a z-cut Ti:LiNbO$_{3}$ optical waveguide which applies for various optical devices.A waveguide channel with a thickness 8 .mu.m and a length 66,000.mu.m and a mach-zehnder interferometer type waveguide were fabricated at a diffusion temperature 1050.deg. C for 6-8hours in a wet $O_{2}$ environment. The resulting Ti:LiNbO$_{3}$ optical waveguide was measured to have a Ti-strip thickness of 950.angs. and low loss. Surfaces and cross-sections of a fabricated waveguide were analysed. The mode pattern anaysis revealed that the waveguide showed a single mode at a 1550nm wavelength. The effective dimension of the waveguide was calculated by measuring a gaussian profile; Wx=10.95.mu. and Wy=9.14.mu.m. a propagation loss, of 0.50dB/cm for a TM mode and 0.45dB/cm for a TE mode, was low enough to be accepatable for optical devices.

  • PDF

高 굴절율화된 z-cut LiNbO$_3$ 광도파로 제작 및 Ti 두께에 따른 삽입손실특성 (Preparations of z-cut LiNbO$_3$ Optical Waveguide for High Refractive Index Change and Properties of Insertion Loss as a Function of Ti Thickness)

  • 김성구
    • 전자공학회논문지D
    • /
    • 제36D권5호
    • /
    • pp.69-79
    • /
    • 1999
  • 본 연구에서는 Ti 확산 lithium niobate 광도파로의 고굴절율 제작하기 위한 확산모델을 제시하고, 기존 확산방법과 비교하였다. 그리고 광파장 λ=1.55㎛에서 단일모드 광섬유와 광도파로를 피그테일링하여 두께에 따른 전체삽입손실을 논의하였다. 본 연구에서는 제안한 확산방법은 기존 확산방법보다도 광도파로의 고굴절율을 도모하는 것으로 분석되었으며, 제안된 확산방법으로 Ti 두께 1000Å∼1400Å범위에서 제작한 마크젠다 간섭기형 광도파로를 제작한 결과, TE 및 TM 전체삽입손실을 z-cut 인 경우0.5㏈/㎝ 수준이었고 x-cut인 경우 1±0.5㏈/㎝를 나타내었다. 이러한 결과로부터 이 확산모델은 저전력형 광변조기나 스위치 등의 제작에 활용할 수 있을 것이다.

  • PDF

LiNbO3 integrated optic devices with an UV-curable polymer buffer layer

  • Jeong, Woon-Jo;Kim, Seong-Ku;Park, Gye-Choon;Lee, Jin
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 춘계학술대회 논문집 센서 박막재료 반도체재료 기술교육
    • /
    • pp.111-118
    • /
    • 2002
  • A new lithium niobate optical modulator with a polymer buffer layer on Ni in-diffused optical waveguide is proposed for the fist time, successfully fabricated and examined at a wavelength of 1.3 mm. By determining the diffusion parameters of Ni in-diffused waveguide to achieve more desirable mode size which is well matched to the mode in the fiber, the detailed results on the achievement of high optical throughput are reported. In addition, the usefulness of polymer buffer layer which can be applicable to a buffer layer in Ni in-diffused waveguide devices is demonstrated. Several sets of channel waveguides fabricated on Z-cut lithium niobate by Ni in-diffusion were obtained and on which coplanar traveling-wave type electrodes with a polymer-employed buffer layer were developed by a conventional fabrication method for characterizing of electro-optical performances of the proposed device. The experimental results show that the measured half-wave voltage is of ~10 V and the total measured fiber-to-fiber insertion loss is of ~6.4 dB for a 40 mm long at a wavelength of =1.3 mm, respectively. From the experimental results, it is confirmed that the polymer-employed buffer layer in LiNbO3 optical modulator can be a substitute material instead of silicon oxide layer which is usually processed at a high temperature of over $300^{\circ}C$. Moreover, the fabrication tolerances by using polymer materials in LiNbO3 optical modulators are much less strict in comparison to the case of dielectric buffer layer.

  • PDF

Wet Oxygen 분위기로 제작한 z-cut $Ti;LiNbO_3$도파로 광특성 및 두께에 따른 삽입손실 (z-cut $Ti;LiNbO_3$ Waveguide Optical Properties and lnsertion Loss As a Function of $Ti;LiNbO_3$thickness Fabricated by wet Oxygen Atmosphere)

  • 김성구;윤형도;윤대원;박계춘;정해덕;이진
    • 한국전기전자재료학회논문지
    • /
    • 제11권10호
    • /
    • pp.903-910
    • /
    • 1998
  • Ti:LiNbO$_3$ optical waveguides have been fabricated by Ti-diffusion in wet oxygen atmosphere. The fabrication conditions of furnace temperature, diffusion time and bubbler temperature were 105$0^{\circ}C$, 8 hours and 9$0^{\circ}C$, respectively and Ti thickness was varied from 700$\AA$ to 1500$\AA$. In this paper, the nearfield patterns, mode sizes (hirizontal/vertical) and insertion loss of waveguides were discussed at wavelength 1550 nm ad function of Ti thickness. With the planar waveguide, the effective index change and diffusion depth were calculated at 632.8nm using the prism coupling method. From these results, the best Ti thickness in our conditions seems like to by 1200$\AA$~1300$\AA$.

  • PDF