Microwave Dielectric Properties of the $MgTiO_3-SrTiO_3$ Ceramics ($MgTiO_3-SrTiO_3$ 세라믹스의 마이크로파 유전특성)

  • 배경인;이상철;최의선;배선기;이영희
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.50 no.8
    • /
    • pp.376-381
    • /
    • 2001
  • The(1-x) MgTiO$_3$-xSrTiO$_3$(x=0.03~0.04) ceramics were fabricated by the conventional mixed oxide method. The structural and microwave dielectric properties were investigated by XRD, SEM, EDS and network analyzer. The sintering temperature and time were 1275$^{\circ}C$~135$0^{\circ}C$ and 2hours, respectively. In the XRD results of 0.96MgTiO$_3$-0.04SrTiO$_3$ceramics, the perovskite structure of SrTiO$_3$and ilmenite structure of MgTiO$_3$phase were coexisted. The dielectric constant($\varepsilon$(sub)${\gamma}$) and temperature coefficient of resonant frequency($\tau$(sub)f) were increased with addition of SrTiO$_3$. In thie case of 0.96MgTiO$_3$-0.04SrTiO$_3$ ceramics sintered at 13$25^{\circ}C$, the dielectric constant, quality factor(Q) and temperature coefficient of resonant frequency($\tau$(sub)f) were 20.13, 7956(at 7.27GHz), and +1.76ppm/$^{\circ}C$, respectively.

  • PDF

Microstructure and Microwave Dielectric Properties of (1-x)Mg4Ta2O9-xTiO2(x=0\sim0.9) Ceramics ((1-x)Mg4Ta2O9-xTiO2(x=0\sim0.9)세라믹스의 미세구조와 마이크로파 유전 특성)

  • 김재식;최의선;이문기;류기원;이영희
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.17 no.8
    • /
    • pp.840-845
    • /
    • 2004
  • The microstructure and microwave dielectric properties of $(1-x){Mg}_4{Ta}_2{O}_9-xTi{O}_2(x=0\sim0.9)$ ceramics were investigated. The specimens were prepared by the conventional mixed oxide method with sintering temperature of 140$0^{\circ}C$∼150$0^{\circ}C$. To improve the quality factor and the temperature coefficient of resonant frequency,$ Ti{O}_2(\varepsilon\Gamma=100, Q\times f_\Gamma=40,000 GHz,\ta_f= +450 ppm\diagup^{\circ}C $ was added in ${Mg}_4{Ta}_2{O}_9$ceramics. The dielectric and structural properties were investigated. According to the XRD patterns, $(1-x){Mg}_4{Ta}_2{O}_9-xTi{O}_2(x=0\sim0.9)$ ceramics had the ${Mg}_4{Ta}_2{O}_9$ phase(hexagonal) and ${MgTi}_2{O}_5$phase(orthorhombic). The dielectric constant($\varepsilon_r$). quality($Qtimes{f}_r$${\tau}_f$) of the $(1-x){Mg}_4{Ta}_2{O}_9-xTi{O}_2(x=0\sim0.9)$ ceramics were 8.12∼18.59, 18,750∼186,410 GHz and -36.02∼+3.46 ppm/$^{\circ}C$, respectively.

Piezoelectric Properties of Pb-free Bi(Na,K)TiO3-SrTiO3 Ceramics with the Amount of La2O3 Addition (La2O3첨가에 따른 무연 Bi(Na,K)TiO3-SrTiO3 세라믹스의 압전 특성)

  • 류주현;이현석;박창엽;정광현;이덕출;정영호;홍재일
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.17 no.8
    • /
    • pp.830-834
    • /
    • 2004
  • In this study, lead-free pirzoelectric ceramics were investigated for pressure sensor applications as a function of the amount of ${La}_2{O}_3$ addition at $Bi(Na, K)Ti{O}_3-SrTi{O}_3$system. With increasing the amount of addition, the density and dielectric constant increased up to 0.9 wt% ${La}_2{O}_3$ addition and decreased above 0.9 wt% ${La}_2{O}_3$addition. Electromechanical coupling factor( $K_{P}$) showed the maximum value at 0.2 wt% ${La}_2{O}_3$addition and decreased above 0.2 wt% ${La}_2{O}_3$ addition. Electromechanical coupling $factor{(K)}_P$, density, dielectric constant$(\varepsilon_\Gamma)$, piezoelectric constant$(d_33)$ and curie temperature$(T_C)$ showed optimum value of 0.40, 5.75 g/㎤, 768, 215 pC/N and 320 $^{\circ}C$ at 0.2 wt%${La}_2{O}_3$addition, respectively.