Fatigue resistance, debonding force, and failure type of fiber-reinforced composite, polyethylene ribbon-reinforced, and braided stainless steel wire lingual retainers in vitro

  • Foek, Dave Lie Sam;Yetkiner, Enver;Ozcan, Mutlu
    • The korean journal of orthodontics
    • /
    • v.43 no.4
    • /
    • pp.186-192
    • /
    • 2013
  • Objective: To analyze the fatigue resistance, debonding force, and failure type of fiber-reinforced composite, polyethylene ribbon-reinforced, and braided stainless steel wire lingual retainers in vitro. Methods: Roots of human mandibular central incisors were covered with silicone, mimicking the periodontal ligament, and embedded in polymethylmethacrylate. The specimens (N = 50), with two teeth each, were randomly divided into five groups (n = 10/group) according to the retainer materials: (1) Interlig (E-glass), (2) everStick Ortho (E-glass), (3) DentaPreg Splint (S2-glass), (4) Ribbond (polyethylene), and (5) Quad Cat wire (stainless steel). After the recommended adhesive procedures, the retainers were bonded to the teeth by using flowable composite resin (Tetric Flow). The teeth were subjected to 10,00,000 cyclic loads (8 Hz, 3 - 100 N, $45^{\circ}$ angle, under $37{\pm}3^{\circ}C$ water) at their incisoproximal contact, and debonding forces were measured with a universal testing machine (1 mm/min crosshead speed). Failure sites were examined under a stereomicroscope (${\times}40$ magnification). Data were analyzed by one-way analysis of variance. Results: All the specimens survived the cyclic loading. Their mean debonding forces were not significantly different (p > 0.05). The DentaPreg Splint group (80%) showed the highest incidence of complete adhesive debonding, followed by the Interlig group (60%). The everStick Ortho group (80%) presented predominantly partial adhesive debonding. The Quad Cat wire group (50%) presented overlying composite detachment. Conclusions: Cyclic loading did not cause debonding. The retainers presented similar debonding forces but different failure types. Braided stainless steel wire retainers presented the most repairable failure type.

Shear Bond Strength of Porcelain Repair Systems (도재 수리 시스템의 전단결합강도에 관한 연구)

  • Woo, Soo;Shin, Soo-Youn;Cho, In-Ho
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.22 no.3
    • /
    • pp.211-220
    • /
    • 2006
  • Need of porcelain-repair system is largely demanding as dental porcelain restorations are increased in clinical dentistry. This study investigated shear bond strength of commercial porcelain-repair systems on dental porcelain and their reliability. Experimental groups were as follows; Group A Super Bond C&B, Group B Porcelain repair kit, Group C Ceramic repair, and Group D Spectrum system as a control. Porcelain disks were fired and embedded in epoxy resin. Porcelain surface were ground using 220 grit SiC disk, then cleaned in ultrasonic bath. Then porcelain specimens were treated with each repair system. A clear polystyrene cylinder 3.5 mm in internal diameter was filled with composite resin. Then the resin cylinder was polymerized with a visible light curing unit. Thirty one specimens at each group were prepared and stored at $37^{\circ}C$ distilled water for 48 h. Specimens were tested in an Instron testing machine according to ISO TR 11405. Mean shear bond strength and standard deviation of each group was $15.7{\pm}4.1MPa$ (Group A), $12.8{\pm}4.9MPa$ (Group B), $7.2{\pm}3.0MPa$ (Group C) and $9.6{\pm}2.2MPa$ (Group D). ANOVA and Tukey HSD post-hoc test showed that there were significant differences between groups (p<0.05). Data of bond strength were analyzed with two-parameter Weibull distribution. Confidence interval of Weibull modulus (m-parameter) at 95% of Group A (3.5-6.3) and Group D (3.6-6.0) were significantly higher than Group B (2.2-3.7) and Group C (2.0-3.4). There was little correlation between mean shear bond strength and Weibull modulus. Results indicated that acid-etching of porcelain surface increased porcelain-resin shear bonding strength.

Effects of 3 different light-curing units on the physico-mechanical properties of bleach-shade resin composites

  • Azin Farzad;Shahin Kasraei;Sahebeh Haghi;Mahboubeh Masoumbeigi;Hassan Torabzadeh;Narges Panahandeh
    • Restorative Dentistry and Endodontics
    • /
    • v.47 no.1
    • /
    • pp.9.1-9.11
    • /
    • 2022
  • Objectives: This study investigated the microhardness, flexural strength, and color stability of bleach-shade resin composites cured with 3 different light-curing units. Materials and Methods: In this in vitro experimental study, 270 samples were fabricated of bleach and A2 shades of 3 commercial resin composites (Point 4, G-aenial Anterior, and Estelite Sigma Quick). Samples (n = 5 for each trial) were cured with Bluephase N, Woodpecker LED.D, and Optilux 501 units and underwent Vickers microhardness and flexural strength tests. The samples were tested after 24 hours of storage in distilled water. Color was assessed using a spectrophotometer immediately after preparation and 24 hours after curing. Data were analyzed using 3-way analysis of variance and the Tukey test (p ≤ 0.001). Results: Samples cured with Optilux exhibited the highest and those cured with LED.D exhibited the lowest microhardness (p = 0.023). The bleach shade of Point 4 composite cured with Optilux displayed the highest flexural strength, while the same composite and shade cured with Sigma Quick exhibited the lowest (p ≤ 0.001). The color change after 24 hours was greatest for the bleach shade of G-aenial cured with Bluephase N and least for the A2 shade of Sigma Quick cured with Optilux (p ≤ 0.001). Conclusions: Light curing with polywave light-emitting diode (LED) yielded results between or statistically similar to those of quartz-tungsten-halogen and monowave LED in the microhardness and flexural strength of both A2 and bleach shades of resin composites. However, the brands of light-curing devices showed significant differences in color stability.

Comparison of high molecular coating type dentine hypersensitivity desensitizers (고분자 기반 코팅형 상아질 지각 과민 처치제의 효과에 대한 비교 연구)

  • Roh, Young-Hoon;Lee, Joo-Yeon;Park, Hyun-Jung;Choi, Cha-Nam;Park, Yoon-Jeong;Koo, Ki-Tae;Kim, Tae-Il;Seol, Yang-Jo;Lee, Yong-Moo;Ku, Young;Rhyu, In-Chul;Chung, Chong-Pyoung
    • The Journal of the Korean dental association
    • /
    • v.46 no.11
    • /
    • pp.683-688
    • /
    • 2008
  • Purpose : The aim of this study was to evaluate the clinical efficacy of two commercially available desensitizing agents over 3 weeks on patients with dentin hypersensitivity. Materials and Methods : An oxalate-based solution, Sensblok (NIBEC Inc. Seoul, Korea) & Superseal (Pheonix Inc. Michigan, USA), and a distilled water placebo were compared in a clinical setting. Seven volunteers exhibiting three or more teeth that were sensitive to tactile & air were enrolled in the study (35 teeth total). A visual analog scale (VAS) was used for recording each patient s level of sensitivity to tactile & air stimuli. A Florida probe was rubbed across the exposed dentin three times with a constant pressure 20 grams to measure the tactile stimulus. The air stimulus was generated by dental unit air syringe for 1-second blast from 1/2 inch distance. The desensitizing agents were applied according manufacture s guideline. VAS scores were recorded at baseline, 1 minute after treatment, at 1 week, 2weeks, 3weeks. VAS score were analyzed using a repeated measures ANOVA ( =0.05). Results : The Sensblok, Superseal, and distilled water placebo all decreased dentin sensitivity. A statistically significant difference existed between Sensblok and placebo when tactile stimulus was applied (P<0.05), but no significant difference was found among other desensitizing agents and tactile and air stimuli.

  • PDF

Inhibitory effect on Streptococcus mutans and mechanical properties of the chitosan containing composite resin

  • Kim, Ji-Sun;Shin, Dong-Hoon
    • Restorative Dentistry and Endodontics
    • /
    • v.38 no.1
    • /
    • pp.36-42
    • /
    • 2013
  • Objectives: This study evaluated the antibacterial effect and mechanical properties of composite resins ($L_{CR}$, $M_{CR}$, $H_{CR}$) incorporating chitosan with three different molecular weights (L, Low; M, Medium; H, High). Materials and Methods: Streptococcus (S). mutans 100 mL and each chitosan powder were inoculated in sterilized 10 mL Brain-Heart Infusion (BHI) solution, and was centrifuged for 12 hr. Absorbance of the supernatent was measured at $OD_{660}$ to estimate the antibacterial activities of chitosan. After S. mutans was inoculated in the disc shaped chitosan-containing composite resins, the disc was cleansed with BHI and diluted with serial dilution method. S. mutans was spread on Mitis-salivarius bacitracin agar. After then, colony forming unit (CFU) was measured to verify the inhibitory effect on S. mutans biofilm. To ascertain the effect on the mechanical properties of composite resin, 3-point bending and Vickers hardness tests were done after 1 and 3 wk water storage, respectively. Using 2-way analysis of variance (ANOVA) and Scheffe test, statistical analysis was done with 95% significance level. Results: All chitosan powder showed inhibition effect against S. mutans. CFU number in chitosan-containing composite resins was smaller than that of control resin without chitosan. The chitosan containing composite resins did not show any significant difference in flexural strength and Vickers hardness in comparison with the control resin. However, the composite resin, $M_{CR}$ showed a slightly decreased flexural strength and the maximum load than those of control and the other composite resins $H_{CR}$ and $L_{CR}$. Conclusions: $L_{CR}$ and $H_{CR}$ would be recommended as a feasible antibacterial restorative due to its antibacterial nature and mechanical properties.

A NEW METHOD - REAL TIME MEASUREMENT OF THE INITIAL DYNAMIC VOLUMETRIC SHRINKAGE OF COMPOSITE RESINS DURING POLYMERIZATION (복합레진의 초기 동적 체적 중합수축의 실시간 측정 -새로운 측정장치의 개발에 대한 소고-)

  • 이인복
    • Restorative Dentistry and Endodontics
    • /
    • v.26 no.2
    • /
    • pp.134-140
    • /
    • 2001
  • The polymerization shrinkage of composite resins is an important drawback although the composites have many advantages-more esthetic and conservative than metallic restoratives etc. The purposes of this research were to develop a new measurement method and to manufacture an instrument that can measure the initial dynamic volumetric shrinkage of composite resins during polymerization. The instrument was basically an electromagnetic balance that constructed with a force transducer using position sensitive photo detector(PSPD) and a negative feedback servo amplifier of proportional-derivative(PD) controller. The volumetric change of composites during polymerization was detected continuously as buoyancy change in distilled water by means of Archimedes's principle. It was converted to continuous electrical voltage signal in real time. The signal was properly conditioned and filtered and then it was stored in computer by a data acquisition(DAQ) board. By using this electronic instrument. the dynamic patterns of the polymerization shrinkage of eight commercial(Z-100, DenFil, AeliteFil, Z-250, P-60, SureFil, Synergy compact, and Tetric ceram) composite resins were measured and compared. The results were as follows. 1. From this project of developing instrument, the ability has been achieved that can acquire and process data of electrical signal transformed from various physical phenomenon by using temperature, displacement. photo. and force transducer. As a consequence, the instrumentation and measurement system used to analyze the physical characteristics of various dental materials in dental research field can be designed, manufactured and implemented in lab. 2. This instrument has some advantages. It was insensible to temperature change and could measure true dynamic volumetric shrinkage in real time without complicated process. It showed accuracy and high precision results with small standard deviation. 3. The polymerization shrinkage of composites was significantly different between brands and ranged from 2.47% to 3.89%, The order of polymerization shrinkage was as follows, in order of increasing shrinkage, SureFil, P60, Z250, Z100, Synergy compact. DenFil, Tetric ceram, and AeliteFil. 4. The polymerization shrinkage rate per unit time, dVol%/dt, showed that the instrument can provide an indirect research method for polymerization reaction kinetics.

  • PDF

CLINICAL STUDY OF DESENSITIZER FOR TREATMENT OF DENTINAL HYPERSENSITIVITY (상아질 지각과민 처치제의 임상적 효과에 대한 연구)

  • Cho, Kyung-Mo;Shin, Dong-Hoon
    • Restorative Dentistry and Endodontics
    • /
    • v.25 no.2
    • /
    • pp.219-224
    • /
    • 2000
  • The purpose of this study is for evaluating the effect of MS Coat desensitizing agent in clinical situation. In this study total 60 teeth of 30 patients who is feeling hypersensitivity after periodontal surgery were treated with MS Coat desensitizing agent, and 20 teeth with saline solution for placebo effects and evaluated. All teeth were cleaned with rubber cup and pumice, after then the antibacterial agent was applied for 20 seconds and simply isolated using cotton roll Desensitizing agent was applied with a specific instrument in the manufacturers package by abrading motion for 10 seconds and re-done 8 times. Tactile stimulus with sharp explorer, air stimulus with syringe of dental unit, $7^{\circ}C$ cold water stimulus using micropipette applicator was done to evaluate hypersensitivity before apply test agent, immediate after application, 1 week after, and 3 month after application. The degree of hypersensitivity was recorded using 100mm Visual Analogue Scale and compared between group and evaluation times. From this clinical study sensitivity to the stimulus was significantly induced in both groups and MS Coat made a significant reduction in VAS score than placebo group did(p<.01). The results of this study could demonstrate that MS Coat desensitizing agent can use effectively to heat dentinal hypersensitivity.

  • PDF

Synthesis of Silica Nanoparticles Having the Controlled Size and their Application for the Preparation of Polymeric Composites (크기가 제어된 실리카 나노입자 합성과 제조된 입자의 고분자계 복합재 응용)

  • Kim, Jong-Woung;Kim, Chang-Keun
    • Polymer(Korea)
    • /
    • v.30 no.1
    • /
    • pp.75-79
    • /
    • 2006
  • Silica nanoparticles for polymeric dental restorative composites were prepared by Stober method, and then the effects of surface treatment of silica particles with Lmethacrylofpropyltrimethofsilane $(\gamma-MPS)$ on the dispersity of the silica particles in the organic matrix was investigated. Particles having various average size were prepared by using controlled amounts of tetraethylorthosilicate(TEOS), water, and catalyst and by changing solvent used for reaction. The site of particles prepared by using methanol as solvent was smaller than that prepared by using ethanol as solvent. In addition, the size of particles was increased by decreasing amounts of water and by increasing amounts of TEOS and catalyst. Hydrophobic silica nanoparticles was prepared by reacting hydrophilic nanoparticles with $\gamma-MPS$ to improve interfacial properties with organic matrix. Amounts of $\gamma-MPS$ per unit mass of the particles was increased by decreasing particle size. even though the amount of $\gamma-MPS$ per specific surface area were nearly the same regardless of the particle size. The dispersity of the silica particles in the organic matrix was improved when the surface treated silica particles were used for preparing the polymeric dental restorative composites.

THE COMPARATIVE STUDY FOR THE SHEAR BOND STRENGTH OF DENTAL ADHESIVES CURED WITH VARIOUS LIGHT SOURCES (다양한 광원으로 중합한 치과용 접착제의 전단강도에 관한 비교 연구)

  • Choi, Nam-Ki;Cho, Seong-Hoon;Kim, Seon-Mi
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.38 no.1
    • /
    • pp.33-41
    • /
    • 2011
  • The objective of this study was to compare the shear bond strengths of five dentin adhesive systems cured with three different light curing sources. Seventy five noncarious permanent teeth were collected and stored in an 0.1% thymol solution at room temperature after extraction. The tested adhesives were: Adper Scotchbond Multi-purpose Plus Adhesive (SM) Adper Single bond 2 (SB), Clearfil SE Bond (SE), Adper Prompt L-Pop (PL), G-Bond (GB). And three light curing unit systems were used: Elipar Free light 2(LED), OptiLux 501 (Halogen), Flipo (PAC). For the shear bonding test, the labial and lingual surfaces of permanent teeth were used. To obtain a flat dentin surface, the labial and lingual surfaces of the teeth were sanded on SiO2 with number 600 grit and then divided into 15 groups of 10 surfaces each. All samples were theromocycled in water $5^{\circ}C$ and $55^{\circ}C$ for 1000 cycles. The results were as follows: 1. When cured with Freelight 2, the shear bond strength of SM was significantly higher than that of PL, GB (p<0.05), whereas no significant difference was found among those of any other bonding agents. 2. When cured with Optilux 501, the shear bond strength of SM was significantly higher than those of any other bonding agents (p<0.05), whereas no singnificant difference was found among those of andy other bonding agents. 3. When cured with Flipo, the shear bond strength of SM was significantly higher than those of SB, SE, GB (p<0.05), whereas no significant differences was found among those of any other bonding agents. 4. For comparison according to three different light cure unit system, except SB and GB, each three dentin bonding agents showed no significant difference. For SB, only Freelight 2 was significantly higher than the others, with no significant difference between Optilux 501 and Flip. For GB, Statistically significant difference was found only between Freelight and Flipo.

The Effect of Drinking Water Fluoride on the Fine Structure of the Ameloblast in the Fetal Rat (음용수 불소가 흰쥐태아 법랑모세포의 미세구조에 미치는 영향)

  • Lim, Do-Seon;Jeong, Moon-Jin;Yoe, Sung-Moon
    • Applied Microscopy
    • /
    • v.29 no.2
    • /
    • pp.189-193
    • /
    • 1999
  • The response of ameloblast to long term (3 weeks) exposure to fluoride was examined in continuously erupting mandibular incisors of pregnancy rats as compared to control rats receiving a similar diet (Teklad L-356) but no sodium fluoride in there drinking water. Rats were started on water containing 0 ppm, 100 ppm, 200 ppm, and 300 ppm NaF at the beginning of pregnancy. To examine on the ultrastructural changes of the ameloblast, electron microscopy was used. The results indicated that rat incisors expressed two major changes in normal amelogenesis that could be attributed to chronic fluoride treatment. The fluoride produces marked alteration in the fine structure of ameloblast from teeth of young rats, such as large confluent distensions of the endoplasmic reticulum and swelling of isolated mitochondria, in particular on the morphology of the rough-surfaced endoplasmic reticulum. A graded series of alterations to these organelles were produced, and the severity of the changes would seem to be dependent on dose and time. This experimental data suggested that exposure prolonged of animal to high level of fluoride appears to induce morphological changes in the normal appositional growth and initial mineralization of enamel created during amelogenesis.

  • PDF