Purpose: The purpose of this study was to know the physical properties of UDMA dental composite resins containing two photosensitizers, PD, DA, as a photosensitizer instead of CQ. We want to know Remaining Double Bond(RDB) of UDMA unfilled resin and diametral tensile strength and flexural strength of composite resin containing PD and DA were compared with those of CQ, most widely used photosensitizer for dental composite resins. Methods: The RDB of UDMA studied by FT-IR spectroscopy increased with irradiation time. The composite resins were tested for their physical properties. The dental composite resins were made with UDMA as a monomer, silanized silica as filler, N,N-dimethylaminoethyl methacrylate (DAEM) as amine initiator, and one of the two kinds of new photosensitizers. Results: The relative RDB of UDMA was in the order: DA > CQ > PD but the physical properties of the composite resins show PD and DA with higher results compared with that containing CQ. The reason for the results is that PD and DA serve not only as a photosensitizer but also as a photo-crosslinking agent. Conclusion: PD and DA show as effective photosensizers, suitable for UDMA dental composite resin compare with a higher efficiency than CQ.
Purpose: The purpose of this study was to know the availability of two photosensitizers, PD, DA, as a photosensitizer instead of CQ in UDMA dental composite resin. We want to know photopolymerization effect of UDMA unfilled resin and surface hardness of composite resin containing PD and DA were compared with those of CQ, most widely used photosensitizer for dental composite resins. Methods: The photopolymerization effect of UDMA studied by FT-IR spectroscopy increased with irradiation time and the amount of photosensitizer. Knoop hardness of experimental composite resins prepared by the addition of the photosensitizer content and irradiation time. Results: The relative photopolymerization effect of UDMA increased in the order of PD > CQ > DA. The composite resin of UDMA containing DA or PD, which shows better Knoop hardness than that containing CQ. Conclusion: PD and DA show as effective photosensizers, suitable for UDMA dental composite resin compare with a higher efficiency than CQ.
Objectives: The aim of this study is to investigate the mechanical properties and antibacterial effects on Streptococcus mutans of composite resins containing phytoncide. Methods: Phytoncide was mixed with commercial composite resins at 0 (control), 1.25, 2.5, 3.75, and 5.0 weight percentage (wt%). Mechanical properties related to composite resins such as surface hardness, depth of cure, and flexural strength were measured. Antibacterial effects of composite resins were analyzed by using Streptococcus mutans (ATCC 25175). The results were analyzed by one-way analysis of variance followed by Tukey's test (p<0.05). Results: Composite resins that contain low wt% of phytoncide demonstrated no significant difference in surface hardness, depth of cure, and flexural strength (p>0.05). However, composite resins that contain high wt% of phytoncide had significantly decreased mechanical properties (p<0.05). In terms of antibacterial effects, composite resins containing phytoncide inhibited the growth of S. mutans. Conclusions: Our findings suggest that novel composite resins containing phytoncide have effective antibacterial properties while maintaining the originally important mechanical features of composite resins.
Rocha Maia, Rodrigo;Oliveira, Dayane;D'Antonio, Tracy;Qian, Fang;Skif, Frederick
Restorative Dentistry and Endodontics
/
제43권2호
/
pp.22.1-22.9
/
2018
Objectives: To evaluate and compare light-transmittance in dental tissues and dental composite restorations using the incremental double-layer technique with varying layer thickness. Materials and Methods: B1-colored natural teeth slabs were compared to dental restoration build-ups with A2D and B1E-colored nanofilled, supra-nanofilled, microfilled, and microhybrid composites. The enamel layer varied from 0.3, 0.5, or 1.2 mm thick, and the dentin layer was varied to provide a standardized 3.7 mm overall sample thickness (n = 10). All increments were light-cured to $16J/cm^2$ with a multi-wave LED (Valo, Ultradent). Using a spectrophotometer, the samples were irradiated by an RGB laser beam. A voltmeter recorded the light output signal to calculate the light-transmittance through the specimens. The data were analyzed using 1-way analysis of variance followed by the post hoc Tukey's test (p = 0.05). Results: Mean light-transmittance observed at thicker final layers of enamel were significantly lower than those observed at thinner final layers. Within 1.2 mm final enamel resin layer (FERL) thickness, all composites were similar to the dental tissues, with exception of the nanofilled composite. However, within 0.5 mm FERL thickness, only the suprananofilled composite showed no difference from the dental tissues. Within 0.3 mm FERL thickness, none of the composites were similar to the dental tissues. Conclusions: The supra-nanofilled composite had the most similar light-transmittance pattern when compared to the natural teeth. However, for other composites, thicker FERL have a greater chance to match the light-transmittance of natural dental tissues.
The photopolymerization efficiency and surface hardness of composite resin containing 1,2-phenylpropanedione (PD) and diacetyl (DA) as photoinitiators were studied by IR and Vickers hardness and the results were compared with that of camphorquinone (CQ). Relative photopolymerization efficiency of the photoinitiators increased in the order of DA < CQ < PD. Vickers hardness of composite resin containing the photoinitiators increased in the order of CQ < PD < DA. Thus, PD is a new visible light photoinitiator for dental composite resin with higher photopolymerization efficiency and surface hardness than that of CQ. Mechanical properties such as Vickers hardness, diametral tensile strength, and flexural strength of the experimental resin composite prepared by addition of the photosensitizer into a resin of bis-GMA improved with increasing the photosensitizer content and irradiation time. The resin composite of bis-GMA containing DA or PD shows better mechanical properties than that of CQ.
Bending strength, bending elastic modulus ,and fracture toughness of different types of dental composite resins were deter mined. The relationship between bending strength, fracture toughness and filler volume fraction of dental composite resin was understood. In Acoustic Emission(AE) behavior during fracture toughness test, characteristic generation patterns of each type were understood. The fracture toughness values, AE generation patterns, and the nature of fracture surface were analyzed to understand fracture behavior of dental composite resin.
Purpose: The author performed experiments on the microhardness and the marginal fitness of composite resins after polymerizing 4 kinds of composite resins on MOD standard specimens. Methods: For this study, in order to compare the microhardness and the marginal fitness of 4 kinds of composite resins. Results: The results are as follows. 1. In case of the microhardness, Tescera scored the highest among the four kinds of composite resins. 2. In case of the marginal fitness, Premise Indirect scored the highest. However, there was no statistically significant difference, all staying in clinically practical range. 3. Considering the above results, among the four kinds of composite resins, the author advises to use Tescera during teeth restoration which scored the highest in the micro- hardness. Conclusion: Conclusion: All of the composite marginal fitness were within the clinically useful range.
Dental composite resin is a kind of the particle - reinforced composite material, and is widely used in recent dental restoration of anterior and posterior tooth region. The purpose of this study was to investigate the fracture behaviour according to volume fractions and external findings of the filler particles for better interpretation of the fracture characteristics of posterior dental composite resins by analytic method of fracture mechanics. The plane strain fracture toughness($K_{IC}$) and Acoustic Emission were determined with three - point bending test using the single edge notch specimen according to the ASTM - E399, and its analyzed data was compared with filler volume fractions derived from the standard ashing test and scanning electron fractographs of each specimen including the unfilled experimental resin as a control. The results were that the value of fracture toughness of the composite resin material was in the range from 0.85 MPa$\sqrt{m}$ to 1.60 MPa$\sqrt{m}$ and was higher than the value of the unfilled experimental resin, and the fracture behaviours dervied from Acoustic Emission analysis show prominent differences according to the volume fraction and the size of filler particles used in each composite resin. The degree of resistance against crack propagation seems to be increase and the fractographs demonstrate the high degree of surface roughness and irregularity according with the increase of fracture toughness value.
2,2 bis 〔4-(2-hydroxy-3-methacryloyloxypropoxy)phenyl〕propane을 기본 단량체, triethylene glycol dimethacrylate를 희석제로 포함하고 있는 고분자계 치아 수복재는 중합 수축률에서의 문제점으로 인하여 사용에 제약을 받아오고 있다. 본 연구에서는 기존 고분자계 치아 수복제의 문제점인 중합 수축률을 감소시키기 위해 중합시 부피 팽창이 기대되는 비대칭 스파이로 오쏘카보네이트를 합성하고, 이를 포함하는 새로운 치아 수복재를 제조하여 이의 특성을 시험하였다. 스파이로 오쏘카보네이트를 포함하는 새로운 치아 수복재의 중합 수축율은 약45% 감소하여 우수한 체적 안정성을 나타내었다. 그러나 새로운 치아 수복재의 중합특성, 기계적 물성 등은 기존 치아 수복재에 비해 다소 저하되었다.
Background: In our study, a silver diamine fluoride (SDF) compound for the treatment of dental caries was synthesized to characterize its remineralization activity upon direct application to deciduous teeth. This study aimed to use microscopic computed tomography (microCT) and nanoindentation to evaluate whether SDF composite application could effectively arrest dental caries in five exfoliated primary molars. Methods: Carious teeth were extracted and visually examined using quantitative photofluorescence devices (Qraycam and QraypenTM). After performing microCT, the SDF composite was applied to the teeth according to the manufacturer's instructions. The researchers exchanged and precipitated the irritant saliva once daily for 1 week. The teeth were sectioned longitudinally through the centers of the mesial and distal surfaces, embedded, polished, and measured using nanoindentation. Thereafter, microCT was repeated. Statistical analyses were performed using GraphPad Prism software. Results: Following SDF composite application, a remineralized layer was observed on microCT images, and the hardness increased when measured using nanoindentation. We found that demineralized enamel presented with an increased number of irregular crystals in the deep carious lesion group compared with those in the shallow carious lesion group, resulting in a rougher surface. Conclusion: The SDF composite may be used for remineralization of early caries and cessation of advanced caries in primary molars.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.