• 제목/요약/키워드: Dental Scrap

검색결과 2건 처리시간 0.016초

플라즈마 공정으로 구상화된 티타늄 분말과 금속사출성형 공정을 이용한 치과용 부품 제조 (Preparation of Metal Injection Molded Dental Components using Spheroidized Ti Powders by Plasma Process)

  • 곽지나;양상선;윤중열;김주용;박성진;김현승;김용진;박용호
    • 한국분말재료학회지
    • /
    • 제20권6호
    • /
    • pp.467-473
    • /
    • 2013
  • This research presents a preparation method of dental components by metal injection molding process (MIM process) using titanium scrap. About $20{\mu}m$ sized spherical titanium powders for MIM process were successfully prepared by a novel dehydrogenation and spheroidization method using in-situ radio frequency thermal plasma treatment. The effects of MIM process parameters on the mechanical and biological properties of dental components were investigated and the optimum condition was obtained. After sintering at $1250^{\circ}C$ for 1 hour in vacuum, the hardness and the tensile strength of MIMed titanium components were 289 Hv and 584 MPa, respectively. Prepared titanium dental components were not cytotoxic and they showed a good cell proliferation property.

치과용(齒科用) 순(純) 타이타늄 스크랩을 재활용(再活用)한 Ti-6Al-4V 합금(合金)의 제조(製造) 및 산소(酸素) 제어(制御) (Preparation and oxygen control of Ti-6Al-4V alloys by recycling dental pure Ti scraps)

  • 오정민;이백규;최국선;임재원
    • 자원리싸이클링
    • /
    • 제21권1호
    • /
    • pp.60-65
    • /
    • 2012
  • 본 연구는 치과용 순 타이타늄 스크랩을 재활용하여 진공 아크 용해에 의해 Ti-6Al-4V 합금을 제조하였고, 이때 산소함량이 다르게 제조된 Ti-6A1-4V 합금의 물성을 평가하였다. 사용된 타이타늄 스크랩은 치과용 임플란트 재료로써 ASTM G1~G4 등급으로 산소함량이 다르게 진공 아크 용해에 의해 건전한 잉곳을 만든 후 Ti-6Al-4V 합금을 제조하였다. 합금 제조시 875 torr의 가압 아르곤 분위기에서 용해하였을 때 Al 조성의 손실이 방지됨을 확인하였다. 제조된 Ti-6Al-4V의 산소함량이 1170~3340 ppm으로 증가함에 따라 Ti-6Al-4V의 경도가 증가하여 순 타이타늄의 경향과 동일함을 확인하였다. 따라서 본 연구를 통해서 Ti-6Al-4V 합금 제조에 있어서 진공 아크 용해에 의해 치과용 순 타이타늄 스크랩의 재활용 가능성을 확인하였다.