• Title/Summary/Keyword: Dental Scrap

Search Result 2, Processing Time 0.216 seconds

Preparation of Metal Injection Molded Dental Components using Spheroidized Ti Powders by Plasma Process (플라즈마 공정으로 구상화된 티타늄 분말과 금속사출성형 공정을 이용한 치과용 부품 제조)

  • Gwak, Ji-Na;Yang, Sangsun;Yun, Jung-Yeul;Kim, Ju-Yong;Park, Seongjin;Kim, Hyun-Seung;Kim, Yong-Jin;Park, Yong-Ho
    • Journal of Powder Materials
    • /
    • v.20 no.6
    • /
    • pp.467-473
    • /
    • 2013
  • This research presents a preparation method of dental components by metal injection molding process (MIM process) using titanium scrap. About $20{\mu}m$ sized spherical titanium powders for MIM process were successfully prepared by a novel dehydrogenation and spheroidization method using in-situ radio frequency thermal plasma treatment. The effects of MIM process parameters on the mechanical and biological properties of dental components were investigated and the optimum condition was obtained. After sintering at $1250^{\circ}C$ for 1 hour in vacuum, the hardness and the tensile strength of MIMed titanium components were 289 Hv and 584 MPa, respectively. Prepared titanium dental components were not cytotoxic and they showed a good cell proliferation property.

Preparation and oxygen control of Ti-6Al-4V alloys by recycling dental pure Ti scraps (치과용(齒科用) 순(純) 타이타늄 스크랩을 재활용(再活用)한 Ti-6Al-4V 합금(合金)의 제조(製造) 및 산소(酸素) 제어(制御))

  • Oh, Jung-Min;Lee, Back-Kyu;Choi, Good-Sun;Lim, Jae-Won
    • Resources Recycling
    • /
    • v.21 no.1
    • /
    • pp.60-65
    • /
    • 2012
  • The Ti-6Al-4V alloys were prepared by recycling of dental Ti pure scraps using vacuum arc melting process, and their physical properties were evaluated the Ti-6Al-4V alloys with different oxygen concentrations. For the preparation of Ti-6Al-4V alloys, Ti pure scraps used for dental implant were utilized as a raw material, and their different oxygen concentrations were ranged from G1 to G4 grade in ASTM standards. It was confirmed that the weight loss of Al in the composition of Ti-6Al-4V alloy could be controlled under the Ar pressure of 875 torr during the melting of alloy. The oxygen concentrations of the Ti-6Al-4V alloys were ranged from 1170 to 3340 ppm. The vickers hardness change of the Ti-6Al-4V alloys showed a similar behavior with that of pure Ti. As a result, we confirmed a possibility of preparation of Ti-6Al-4V alloy by recycling of dental Ti scraps using vacuum arc melting process in this study.