• Title/Summary/Keyword: Dental Engineering.

Search Result 1,045, Processing Time 0.025 seconds

EXPRESSION OF BMP-2, -4 DURING DISTRACTION OSTEOGENESIS IN THE RABBIT MANDIBLE (집토끼 하악골에서 신연 골형성술시 BMP-2,-4의 발현)

  • Kim, Sang-Woo;Jee, Yu-Jin;Song, Hyun-Chul
    • Journal of the Korean Association of Oral and Maxillofacial Surgeons
    • /
    • v.30 no.3
    • /
    • pp.193-202
    • /
    • 2004
  • Distraction osteogenesis(DO) is defined as a gradual mechanical process of mechanical stretching two vascularized bone surface apart with a critical rate and rhythm such that new bone forms within the expanding gap, reliably bridges the gap, and ultimately remodels to normal structure. DO has become a mainstay in bone tissue engineering and has significantly improved our armamentarium for reconstructive craniomaxillofacial procedures. But the molecular and biological mechanisms that regulate the formation of new bone during distraction osteogenesis are not completely understood. BMPs are potent osteoinductive agents. Our hypothesis was that BMPs, especially BMP-2 and BMP-4, might play an importent role in the signaling pathways that link the mechanical forces created by distraction to biological responses and in promting new bone formation. Using a rabbit's mandible, we investigated the expression of BMP-2, -4 at different time points during distraction osteogenesis. The purpose of this study is to research the pattern of expression of BMP-2, -4 in new bone formation during distraction osteogenesis of the rabbit mandible. The experimental group was applied gradual distraction (0.7mm a day by twice a day, 4.9mm in total, for 7 days) and the control group was carried out osteotomy alone. They were examined clinically, histologically, and by RT-PCR analysis. On 3 days after osteotomy, the high level of expression of BMP-2, -4 was detected. But, the expression of BMP-4 was decreased during latency period. As distraction was started, its expression was increased and maintained till postoperative 28days. In control group, the expression of BMP-4was remarkably decreased till postoperative 14 days. On the other hand, the expression of BMP-2 was no difference between experimental group and control group. The expression of BMP-4 was maintanined at high level during the entire experimental period in both group. These findings suggested that excellent bone formation during distraction osteogenesis is associated with enhanced expression of BMP-4 genes by mechanical tension stress.

Lateral Cephalometric Measurements of Class I Malocclusion Patients with Uncertainty (불확도를 고려한 Class I 부정교합 환자의 측방두부방사선영상 계측값)

  • Lee, Ji Min;Song, Ji-Soo;Hyun, Hong-Keun;Kim, Young-Jae;Kim, Jung-Wook;Jang, Ki-Taeg;Lee, Sang-Hoon;Kim, Hojae;Cho, Hyo-Min;Shin, Teo Jeon
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.45 no.1
    • /
    • pp.65-74
    • /
    • 2018
  • The aim of this study was to obtain the traceability of the software used to analyze lateral cephalometry and to calculate the uncertainty of the measurements. Furthermore, this study aimed to provide a basis for obtaining standard references for measurement values for orthodontic treatment in children. Cephalometric data were collected from 100 children diagnosed with class I malocclusion between the ages 6 to 13 years who visited the pediatric dentist at Seoul National University Dental Hospital. To ensure traceability, a phantom device was created. Correction values were calculated by measuring the length and angle of the phantom device using the software. Type A uncertainty was calculated by obtaining the standard deviation of cephalometric measurements of 100 persons and the standard error of repeated measurements. Determination of the type B uncertainty was induced by minimum resolution and the position of the head. Using these, the combined standard uncertainty was obtained and the expanded uncertainty was calculated. The results of this study confirm that the currently used software has high accuracy and reliability. Furthermore, the uncertainty of orthodontic measurements in Korean children aged 6 to 13 years was calculated, and distribution range for class I malocclusion with 95% confidence interval was suggested.

MORPHOLOGICAL CHANGES OF DENTIN SURFACE TREATED WITH VARIOUS DENTIN SURFACE CONDITIONERS (수종(數種) 표면처리제(表面處理劑)에 의(依)한 상아질(象牙質) 표면(表面)의 형태(形態) 변화(變化)에 관(關)한 연구(硏究))

  • Cho, Jin-Ho;Choi, Ho-Young;Min, Byung-Soon;Park, Sang-Jin
    • Restorative Dentistry and Endodontics
    • /
    • v.13 no.2
    • /
    • pp.323-334
    • /
    • 1988
  • The purpose of this study was to observe the effect of dentin surface conditioners on the dentin surfaces. Freshly extracted human molars were used in this study. They were stored at $4^{\circ}C$ saline solution before experiment. The crown portions of the teeth were cut in various directions by means of wet diamond point to expose dentin which include transverse, vertical oblique, horizontal and oblique cut to the long axis (Fig. 1). Each tooth was then mounted with self curing acrylic resin in brass ring to expose the flattened dentin surfaces. Final finish was accomplished by grinding the dentin specimens with wet No. 180 and No. 600 grit silicon carbide abrasive paper until a 6.0mm in diameter on a dentin surface was exposed without pulp exposure. The specimens were divided into 9 groups according to the modes of dentin treatment procedure. The following surface treatments were applied on these preparation surfaces; Group 1: unetched (control group) after finish with No. 600 silicon carbide abrasive paper. Group 2: etched with 30% phosphoric acid for 60s Group 3: etched with 10-3 solution for 60s Group 4: Cleaned with 5% NaOCl for 30s Group 5: applied Dentin Adhesit Group 6: cleaned with 5% NaOCl followed by applying the Dentin Adhesit$^{(R)}$ Group 7: applied Photo Bond on the unetched dentin followed by applying the Photo Clearfil Bright Group 8: Etched with 30% phosphoric acid followed by applying Photo Bond and Photo Clearfil Bright Group 9: etched with 10-3 solution followed by applying Photo Bond and Photo Clearfil Bright All the specimens were stored in $37^{\circ}C$ under 50% relative humidity for 24 hours before observations. The specimens in 7, 8, and 9 group, omitting the group 1 to 6, were demineralized in 10% HCl for 10s in order to observe the resin tags. All the specimens in each group were then dried at room temperature. The dried specimens were ion coated with Eiko ion coater (Eiko-engineering Co.), and observed in Hitachi S-430 Scanning electron microscope (Hitachi, Co. Tokyo) at 15KV. The following results were obtained as follows; 1. The smear layers were still remained in group 1,2,4,5, and 6. 2. There is no effect of 5% NaOCl and 30% phosphoric acid on the changes of dentin morphology 3. The dentin treated with 10-3 solution, indicating the tubules opened when the smear layer and the dental plug dissolved. 4. In case of applying the bonding agents the resin tag was not formed at the deep area of dentinal tubules, but in case of applying the Dentin Adhesit$^{(R)}$ that was not.

  • PDF

A STUDY ON THE STRESS DISTRIBUTION OF POSTERIOR FIXED PARTIAL DENTURE WITH VARIOUS ALL-CERAMIC SYSTEMS (구치부 고정성 국소의치에서 전부도재 시스템에 따른 응력분포에 관한 연구)

  • Kang Han-Joong;Dong Jin-Keun;Oh Sang-Chun;Lee Hae-Hyoung;Song Ki-Chang
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.43 no.2
    • /
    • pp.204-217
    • /
    • 2005
  • Purpose. The purpose of this study was to analyze stress distribution of all ceramic posterior fixed partial denture using a three dimensional finite element method. Material and method. A three dimensional finite element model was created to demonstrate all-ceramic posterior fixed partial denture and then this computer model measured the stress distribution of the all ceramic bridges which has a ceramic core materials such as Zirconia, IPS Empress. 2. In-Ceram zirconia, Metal-Ceramic. Also the stress distribution was examined according to loading sites when force was applied to sites such as the central area of second premolar the mesial connector of pontic, the central fossa of pontic, the distal connector of pontic, and the central fossa of second molar. Results. 1. In all the materials of the core in this study, von Mises stress indicated that the stress increased as force was applied to loaded sites, just at those points, on the connector, and the margin in the area adjacent to the connectors. 2. The maximum principal stress was much higher in the lower part of the connectors than in any other region. 3. As the load was applied to the different locations, the research showed a consistent increase of stress in the lower connectors. The maximum value of the von Mises stress was two or three times greater when the load was applied directly to the connectors rather than indirectly through another stressed region. 4. In the case of In-Ceram zirconia, the stress in lower connectors was the highest of all the reference points, the stress showed 75% of all the maximum stress. Ziconia showed 72%, Metal Ceramic 67% and IPS Empress 2 50%. 5. In the case of Ziconia, the stress was well dispersed in each reference point that the stress differences were smaller when compared to In-Cream ziconia.

Effect of microgrooves and fibronectin conjugation on the osteoblast marker gene expression and differentiation

  • Park, Su-Jung;Leesungbok, Richard;Ahn, Su-Jin;Im, Byung-Jin;Lee, Do Yun;Jee, Yu-Jin;Yoon, Joon-Ho;Cui, Taixing;Lee, Sang Cheon;Lee, Suk Won
    • The Journal of Advanced Prosthodontics
    • /
    • v.7 no.6
    • /
    • pp.496-505
    • /
    • 2015
  • PURPOSE. To determine the effect of fibronectin (FN)-conjugated, microgrooved titanium (Ti) on osteoblast differentiation and gene expression in human bone marrow-derived mesenchymal stem cells (MSCs). MATERIALS AND METHODS. Photolithography was used to fabricate the microgrooved Ti, and amine functionalization (silanization) was used to immobilize fibronectin on the titanium surfaces. Osteoblast differentiation and osteoblast marker gene expression were analyzed by means of alkaline phosphatase activity assay, extracellular calcium deposition assay, and quantitative real-time PCR. RESULTS. The conjugation of fibronectin on Ti significantly increased osteoblast differentiation in MSCs compared with non-conjugated Ti substrates. On the extracellular calcium deposition assays of MSCs at 21 days, an approximately two-fold increase in calcium concentration was observed on the etched 60-${\mu}m$-wide/10-${\mu}m$-deep microgrooved surface with fibronectin (E60/10FN) compared with the same surface without fibronectin (E60/10), and a more than four-fold increase in calcium concentration was observed on E60/10FN compared with the non-etched control (NE0) and etched control (E0) surfaces. Through a series of analyses to determine the expression of osteoblast marker genes, a significant increase in all the marker genes except type I collagen ${\alpha}1$ mRNA was seen with E60/10FN more than with any of the other groups, as compared with NE0. CONCLUSION. The FN-conjugated, microgrooved Ti substrate can provide an effective surface to promote osteoblast differentiation and osteoblast marker gene expression in MSCs.

New Approaches to the Control of Pathogenic Oral Bacteria (바이오필름을 생성하는 병원성 구강 세균을 제어하는 새로운 접근법)

  • Cho, Soo Jeong
    • Journal of Life Science
    • /
    • v.31 no.1
    • /
    • pp.100-108
    • /
    • 2021
  • In the oral cavity, there are hundreds of microbial species that exist as planktonic cells or are incorporated into biofilms. The accumulation and proliferation of pathogenic bacteria in the oral biofilm can lead to caries and periodontitis, which are typical oral diseases. The oral bacteria in the biofilm not only can resist environmental stress inside the oral cavity, but also have a 1,000 times higher resistance to antibiotics than planktonic cells by genes exchange through the interaction between cells in the oral biofilm. Therefore, if the formation of oral biofilm is suppressed or removed, oral diseases caused by bacterial infection can be more effectively prevented or treated. In particular, since oral biofilms have the characteristic of forming a biofilm by gathering several bacteria, quorum sensing, a signaling system between cells, can be a target for controlling the oral biofilm. In addition, a method of inhibiting biofilm formation by using arginine, an alkali-producing substrate of oral bacteria, is used to convert the distribution of oral microorganisms into an environment similar to that of healthy teeth or inhibit the secretion of glucosyltransferase by S. mutans to inhibit the formation of non-soluble glucans. It can be a target to control oral biofilm. This method of inhibiting or removing the oral biofilm formation rather than inducing the death of pathogenic bacteria in the oral cavity will be a new strategy that can selectively prevent or therapeutic avenues for oral diseases including dental caries.

Recovery of Metallic Pd with High Purity from Pd/Al2O3 Catalyst by Hydrometallurgy in HCl (염산 침출용액을 이용한 Pd/Al2O3 촉매에서 고순도 팔라듐 회수)

  • Kim, Ye Eun;Byun, Mi Yeon;Baek, Jae Ho;Lee, Kwan-Young;Lee, Man Sig
    • Clean Technology
    • /
    • v.26 no.4
    • /
    • pp.270-278
    • /
    • 2020
  • Palladium (Pd) has been widely used in various industrial applications such as jewelry, catalyst, and dental materials despite its limited resources. It has been gaining attention to recover Pd with high purity from the spent materials. This study investigated the optimum conditions for the leaching and recovery of metallic Pd. The leaching parameters are HCl concentration, temperature, time, concentration of oxidants, and pulp density. 97.2% of Pd leaching efficiency was obtained in 3 M HCl with 3 vol% oxidants at 80℃ for 60 min. The ratio of hydrogen peroxide to sodium hypochlorite played a critical role in the leaching efficiency due to the supply of Cl- ions in the leachate. Moreover, the complete recovery of Pd in the leachate was achieved at 80℃ with 0.3 formic acid/leachate after adjusting the pH value of 7. This situation was ascribed to the decomposition of formic acid into hydrogen gas and carbon dioxide at 80℃. ICP-AES and XRD characterized the recovered Pd powder, and the purity of the recovered powder was found to be 99.6%. Consequently, the recovered Pd powder with high purity could be used in circuits, catalyst precursors, and surgical instruments.

Physicochemical properties of a calcium aluminate cement containing nanoparticles of zinc oxide

  • Amanda Freitas da Rosa;Thuany Schmitz Amaral;Maria Eduarda Paz Dotto;Taynara Santos Goulart;Hebert Luis Rossetto;Eduardo Antunes Bortoluzzi;Cleonice da Silveira Teixeira;Lucas da Fonseca Roberti Garcia
    • Restorative Dentistry and Endodontics
    • /
    • v.48 no.1
    • /
    • pp.3.1-3.14
    • /
    • 2023
  • Objectives: This study evaluated the effect of different nanoparticulated zinc oxide (nano-ZnO) and conventional-ZnO ratios on the physicochemical properties of calcium aluminate cement (CAC). Materials and Methods: The conventional-ZnO and nano-ZnO were added to the cement powder in the following proportions: G1 (20% conventional-ZnO), G2 (15% conventional-ZnO + 5% nano-ZnO), G3 (12% conventional-ZnO + 3% nano-ZnO) and G4 (10% conventional-ZnO + 5% nano-ZnO). The radiopacity (Rad), setting time (Set), dimensional change (Dc), solubility (Sol), compressive strength (Cst), and pH were evaluated. The nano-ZnO and CAC containing conventional-ZnO were also assessed using scanning electron microscopy, transmission electron microscopy, and energy-dispersive X-ray spectroscopy. Radiopacity data were analyzed by the 1-way analysis of variance (ANOVA) and Bonferroni tests (p < 0.05). The data of the other properties were analyzed by the ANOVA, Tukey, and Fisher tests (p < 0.05). Results: The nano-ZnO and CAC containing conventional-ZnO powders presented particles with few impurities and nanometric and micrometric sizes, respectively. G1 had the highest Rad mean value (p < 0.05). When compared to G1, groups containing nano-ZnO had a significant reduction in the Set (p < 0.05) and lower values of Dc at 24 hours (p < 0.05). The Cst was higher for G4, with a significant difference for the other groups (p < 0.05). The Sol did not present significant differences among groups (p > 0.05). Conclusions: The addition of nano-ZnO to CAC improved its dimensional change, setting time, and compressive strength, which may be promising for the clinical performance of this cement.

Comparative Analysis of the Physical and Biochemical Properties of Light-cure Resin-modified Pulp Capping Materials

  • Tae Gyeom Kim;Jongsoo Kim;Joonhaeng Lee;Jisun Shin;Mi Ran Han;Jongbin Kim;Yujin Kim;Jae Hee Park
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.51 no.2
    • /
    • pp.149-164
    • /
    • 2024
  • This study compared the solubility, water absorption, dimensional stability, release of various ions (hydroxyl, calcium, sulfur, strontium, and silicon), and cytotoxicity of light-cured resin-modified pulp-capping materials. Resin-modified calcium hydroxide (Ultra-blendTM plus, UBP), light-cured resin-modified calcium silicate (TheraCal LCTM, TLC), and dual-cure resin-modified calcium silicate (TheraCal PTTM, TPT) were used. Each material was polymerized; solubility, 24-hour water absorption, and 30- day dimensional stability experiments were conducted to test its physical properties. Solubility was assessed according to the ISO 6876 standard, and 24 hours of water absorption, 30 days of dimensional stability were assessed by referring to the previous protocol respectively. Eluates at 3 and 24 hours and on 7, 14, and 28 days were analyzed according to the ISO 10993-12 standard. And the pH, Ion-releasing ability, cell proliferation rate, and cell viability were assessed using the eluates to evaluate biochemical characteristics. pH was measured with a pH meter and Ion-releasing ability was assessed using inductively coupled plasma atomic emission spectrometry (ICP-AES). Cell proliferation rate and cell viability were assessed using human dental pulp cells (hDPCs). The former was assessed by an absorbance assay using the CCK-8 solution, and the latter was assessed by Live and Dead staining. TPT exhibited lower solubility and water absorption than TLC. UBP and TPT demonstrated higher stability than TLC. The release of sulfur, strontium, calcium, and hydroxyl ions was higher for TLC and TPT than for UBP. The 28-day release of hydroxyl and silicon ions was similar for TLC and TPT. TLC alone exhibited a lower cell proliferation rate compared to the control group at a dilution ratio of 1 : 2 in cell proliferation and dead cells from Live and Dead assay evaluation. Thus, when using light-cure resin-modified pulp-capping materials, calcium silicate-based materials can be considered alternatives to calcium hydroxide-based materials. Moreover, when comparing physical and biochemical properties, TPT could be prioritized over TLC as the first choice.

MICROLEAKAGE OF MICROFILL AND FLOWABLE COMPOSITE RESINS IN CLASS V CAVITY AFTER LOAD CYCLING (Flowable 및 microfill 복합레진으로 충전된 제 5급와동에서 load cycling 전,후의 미세변연누출 비교)

  • Kang, Suk-Ho;Kim, Oh-Young;Oh, Myung-Hwan;Cho, Byeong-Hoon;Um, Chung-Moon;Kwon, Hyuk-Choon;Son, Ho-Hyun
    • Restorative Dentistry and Endodontics
    • /
    • v.27 no.2
    • /
    • pp.142-149
    • /
    • 2002
  • Low-viscosity composite resins may produce better sealed margins than stiffer compositions (KempScholte and Davidson, 1988: Crim, 1989). Plowable composites have been recommended for use in Class V cavities but it is also controversial because of its high rates of shrinkage. On the other hand, in the study comparing elastic moduli and leakage, the microfill had the least leakage (Rundle et at. 1997) Furthermore, in the 1996 survey of the Reality Editorial Team, microfills were the clear choice for abfraction lesions. The purpose of this study was to evaluate the microleakage of 6 compostite resins (2 hybrids, 2 microfills, and 2 flowable composites) with and without load cycling. Notch-shaped Class V cavities were prepared on buccal surface of 180 extracted human upper premolars on cementum margin. The teeth were randomly divided into non-load cycling group (group 1) and load cycling group (group 2) of 90 teeth each. The experimental teeth of each group were randomly divided into 6 subgroups of 15 samples. All preparations were etched, and Single bond was applied. Preparations were restored with the following materials (n=15) : hybrid composite resin [Z250(3M Dental Products Inc. St. Paul, USA), Denfil(Vericom, Ahnyang, Korea)], microfill [Heliomolar RO(Vivadent, Schaan, Liechtenstein), Micronew(Bisco Inc. Schaumburg, IL, USA)], and flowable composite[AeliteFlo(Bisco Inc. Schaumburg, IL, USA), Revolution(Kerr Corp. Orange, CA, USA)]. Teeth of group 2 were subjected to occlusal load (100N for 50,000 cycles) using chewing simulator(MTS 858 Mini Bionix II system, MTS Systems Corp. Minn. USA). All samples were coated with nail polish 1mm short of the restoration, placed in 2% methylene blue for 24 hours, and sectioned with a diamond wheel. Enamel and dentin/cementum margins were analyzed for microleakage on a sclale of 0 (no leakage) to 3 (3/3 of wall). Results were statistically analyzed by Kruscal-Wallis One way analysis, Mann-Whitney U-test, and Student-Newmann-Keuls method. (p = 0.05) Results : 1. There was significantly less microleage in enamel margins than dentinal margins of all groups (p<0.05) 2. There was no significant between six composite resin in enamel margin of group 1. 3. In dentin margin of group 1, flowable composite had more microleakage than others but not of significant differences. 4. there was no significant difference between six composite resin in enamel margin of group 2. 5. In dentin margin of group 2, the microleakage were R>A =H=M>D>Z. But there was no significant differences. 6. In enamel margins, load cycling did not affect the marginal microleakage in significant degree. 7. In enamel margins, load cycling did affect the marginal microleakage only in Revolution. (p<0.05).