탄소섬유 복합재료의 AE에 충격손상재강도와 손상특성 평가 (The Evaluation of Strength and Damage Characteristics by AE in Impact Test of CFRP)

  • 이상국;오세규;남기우;김옥균
    • 한국해양공학회지
    • /
    • 제9권1호
    • /
    • pp.47-56
    • /
    • 1995
  • This study is aimed to have a database of system development for the prediction, monitoring, analyzing, and evaluation of tensile strength and damage characteristics through AE technique for CFRP. Therefore the correlations between impact characteristics (such as impact velocity, impact energy, delamination area etc) and AE signals for CFRP laminates were investigated. And also it were accomplished the evaluation of tensile strength and the investigation on correlation with AE signals for impact damaged specimen of CFRP laminates.

  • PDF

온도변화가 CF/PEEK 적층재의 충격 후 굽힘강도에 미치는 영향 (The Effects of Temperature Change on the Bending Strength of CF/PEEK Laminates after Impact)

  • 양인영;정종안;나승우
    • 한국안전학회지
    • /
    • 제18권2호
    • /
    • pp.34-39
    • /
    • 2003
  • In this paper, when CF/PEEK laminates for high efficiency space structure are subjected to FOD(Foreign Object Damage), the effects of temperature change on the impact damages(interlaminar separation and transverse crack) of CF/PEEK laminates and the relationship between residual lift and impact damages are experimentally investigated. Composite laminates used in this experiment are CF/PEEK orthotropic laminated plates, which have two-interlaces [$0^{\circ}_4/90^{\circ}_8/0^{\circ}_4$]. A steel ball launched by the air gun collides against CF/PEEK laminates to generate impact damages. And then CF/PEEK specimens with impact damages are observed by a scanning acoustic microscope under room and high temperatures. In this experimental results, various relations are experimentally observed including the delamination area vs. temperature change, the bending strength vs. impact energy and the residual bending strength vs. impact damage of CF/PEEK laminates.

인공발(Prosthetic Foot) 스프링용 유리섬유강화 적층재의 적층배향에 따른 층간분리거동 해석 (Analysis of Delamination Behavior on the Stacking Sequence of Prosthetic Foot Keel in Glass fiber Reinforced Laminates)

  • 송삼홍;김철웅
    • 대한기계학회논문집A
    • /
    • 제27권4호
    • /
    • pp.623-631
    • /
    • 2003
  • It is considered that the application of advanced composite materials to the prostheses for the disables is important to improve their bio-mechanical performance. Particularly, energy storing foot prosthesis is mostly important to restore gait ability of the disables with low-extremity amputation since it could provide propulsion at terminal stance enhancing the disables ability to walk long distance even run and jump. Therefore, the energy storing spring of Prosthetic foot keel under cyclic bending moment use mainly of high strength glass fiber reinforced plastic. The main objective of this study was to evaluate the stacking sequence effect using the delamination growth rate(dA$_{D}$/dN) of energy storing spring in glass fiber reinforced plastic under cyclic bending moment. The test results indicated that the shape of delamination zone depends on stacking sequence in GFRP laminates. Delamination area(A$_{D}$) turns out that variable types with the contour increased non-linearly toward the damage zones.nes.

반도체 패키지의 층간박리 파괴역학인자 해석 및 균열진전경로 예측 (Analyses of Fracture Parameters and Prediction of Crack Propagation Path on Delamination in the LSI Package)

  • 정남용;박철희
    • 한국생산제조학회지
    • /
    • 제18권4호
    • /
    • pp.401-409
    • /
    • 2009
  • This paper presents a method of calculating the stress intensity factor (K) and crack propagation direction (${\theta}_0$) at the crack-tip that is associated with delamination in the large scale integration(LSI) package. To establish a reasonable strength evaluation method and life prediction, it is necessary to assess fracture parameters under various fracture conditions. Therefore, we conducted quantitative stress singularity analysis considering thermal stress simulating the changes of crack length (a), (h) and (v) in delamination using the 2-dimensional elastic boundary element method (BEM), and from these results predicted crack propagation direction and path.

  • PDF

펄라이트 강선의 어닐링 조건이 딜라미네이션 발생에 미치는 영향 (The Effect of Annealing Condition on the Occurrence of the Delamination in Pearlitic Steel Wires)

  • 박대범;이중원;남원종
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2007년도 추계학술대회 논문집
    • /
    • pp.120-123
    • /
    • 2007
  • The effects of annealing condition on the occurrence of the delamination in cold drawn hyper-eutectoid steel wires, were investigated. Annealing treatment was performed on cold drawn steel wires for temperature range of $425^{\circ}C\sim500^{\circ}C$ with the variation of annealing time from 30sec to 15min. The increase of annealing temperature and time would cause the decrease of tensile strength and the increase of ductility. However, the occurrence of the delamination, representing torsional ductility, showed the different way from the variation of ductility.

  • PDF

CFRP의 드릴작업시 AE적용에 의한 손상평가 (The Damage Evaluation for the Application of Acoustic Emission in a Drilling Procedure of the CFRP Composite Materials)

  • 최병국;윤유성
    • 한국안전학회지
    • /
    • 제16권4호
    • /
    • pp.47-51
    • /
    • 2001
  • The carbon fiber reinforced plastics(CFRP) have been widely used in aircraft and spacecraft structures as well as sports goods because it has high specific strength, high specific stiffness and low coefficient of thermal expansion. Machining of CFRP poses problems not frequently seen for metals due to the nonhomogeneity, anisotropy, and abrasive characteristics of CFRP. Delamination is a common problem faced while drilling holes in CFRP using conventional drilling. Therefore, AE characteristics related to drilling damage process of unidirectional and [0/90/]s crossply laminate composite was studied. Also drilling damage like the delamination was observed by video camera in real time monitoring technique. From the results, we basically found the relationships between the delamination from drilling and AE characteristics for CFRP composites.

  • PDF

CFRP 적층판의 충격손상이 잔류 굽힘 피로강도에 미치는 영향 (Influence of Residual Bending Fatigue Strength on Impact Damage of CFRP Composites)

  • 양용준;양인영
    • 한국안전학회지
    • /
    • 제30권3호
    • /
    • pp.7-12
    • /
    • 2015
  • CFRP composites are used as primary structural members in various industrial fields because their specific strength and specific stiffness are excellent in comparison to conventional metals. Their usage is expanding to high added-value industrial fields because they are more than 50% lighter than metals, and have excellent heat resistance and wear resistance. However, when CFRP composites suffer impact damage, destruction of fiber and interface delamination occur. This causes an unexpected deterioration of strength, and for this reason it is very difficult to ensure the reliability of the excellent mechanical properties. Therefore, for the destruction mechanism in bending with impact damage, this study investigated the reinforcement data regarding various external loads by identifying the consequential strength deterioration. Specimens were damaged by impact with a steel ball propelled by air pressure. Decrease in bending strength caused by the tension and compression of the impact side, and depending on the lamination direction of fiber and interface inside the specimen. From the bending test it was found that the bending strength reduced when the impact energy increased. Especially in the case of compression on the impact side, as tensile stress occurred at the damage starting point, causing rapid failure and a substantially reduced failure strength.

일방향 복합재료 Single Lap접합 조인트의 파손 모드 및 강도 I. 실험 (Failure Mode and Strength of Unidirectional Composite Single Lap Bonded Joints I. Experiments)

  • 김광수;유재석;안재모;장영순
    • Composites Research
    • /
    • 제17권6호
    • /
    • pp.14-21
    • /
    • 2004
  • 본 연구에서는 몇 가지 접합 방법에 따라 일방향 복합재료 단일 겹치기 접합 조인트의 파손 과정, 모드 및 강도를 실험적으로 평가하였다 접합 방법으로는 접착제 없는 동시성형, 접착제를 사용한 동시성형 및 이차 접합의 세 가지를 고려하였다 또한 이차 접합 조인트에서 몇 가지 파라미터의 영향도 살펴보았다. 접착제 없는 동시성형 시편은 가장 우수한 조인트 강도를 나타내었다. 이차접합 조인트에서는 접착제 층의 점진적인 파손이 발생하였다. 접착제의 재료 및 접합 강도가 상대적으로 강한 필름 접착제의 동시성형 조인트는 갑작스런 층간분리 파손이 발생하였으며 이차 접합 조인트보다 더 낮은 파손 강도를 나타내었다. 이차 집합 조인트에서 층간분리 파손이 발생하지 않은 것은 접착제 층에서의 균열 진전 및 점진적 파손이 층간분리 파손을 방지한 것으로 보인다. 따라서 복합재료 접합 조인트의 파손 강도는 접착제의 재료 강도 또는 접착 성능과 항상 비례하지 않으며 이것은 복합재료가 층간 분리 파손에 약하기 때문이다.

알루미나 분말 혼합 비율에 따른 GFRP의 기계적 강도 특성 (Mechanical Behaviour of GFRP Composites according to Alumina Powder Impregnation Ratios in Resin)

  • 강대곤;박재학
    • 한국재료학회지
    • /
    • 제30권1호
    • /
    • pp.22-30
    • /
    • 2020
  • Small fishing vessels are manufactured using FRP. Various studies have been conducted to increase the strength of the composite material by mixing alumina powder with resin. Tensile tests and flexural strength tests are conducted to examine the effect of alumina powder on the strength of GFRP. In the current study, resin/alumina composites at different alumina contents (i.e., 0, 1, 5, and 10 vol%) have been prepared. The physical and mechanical properties of the prepared composites have been investigated. From the results, the tensile strength of the specimen with alumina powder mixed in at 10% shows the highest value of 155.66 MPa. The tensile strength of the specimen mixed with alumina powder increases with the amount of alumina powder impregnated. In the flexural strength test, the flexural strength of neat resin without alumina powder has a highest value of 257.7 MPa. The flexural modulus of ALMix-5 has a highest value of 12.06 GPa. Barcol hardness of ALMix-10 has a highest value of 51. We show that alumina powder leads to decreasing cracks on the surface and decreasing length area of delamination.

초기 균열길이 및 섬유방향이 CFRP/GFRP 하이브리드 적층재의 층간 파괴에 미치는 영향 (The Effects of the Initial Crack Length and Fiber Orientation on the Interlaminar Delamination of the CFRP/GFRP Hybrid Laminate)

  • 권오헌;권우덕;강지웅
    • 한국안전학회지
    • /
    • 제28권1호
    • /
    • pp.12-17
    • /
    • 2013
  • Considering the wind power system and the rotor blades which are composed of much technology, the wind power blade would be the most dangerous part because it revolves at high speed and weighs about dozens of tons, if the accident happens. Therefore, the light weight composite materials have been replacing as substitutional materials. The object of this study is to examine the delamination and damage for CFRP/GFRP hybrid composite that is used for strength improvement of a wind power blade. The influence of the initial crack length and fiber orientation for the interlaminar delamination was exposed for the blade safety. Plain woven CFRP instead of GFRP was inserted into the layer of the box spar for improving the strength and blade life. DCB(Double Cantilever Beam) specimen was used for evaluating fracture toughness and damage evaluation of interlaminar delamination. The material used in the experiment is a commercial material known as CF 3327 EPC in plain woven carbon prepreg(Hankuk Carbon Co.) and UD glass fiber prepreg(Hyundai Fiber Co.). From the results, crack growth rate is not so different according to the variation of the initial crack length. Mode I interlamainar fracture toughness of fiber direction $0^{\circ}$ is higher than that of $45^{\circ}$. Interlaminar fracture has an effect on fiber direction and K decreased with lower value according to increasing initial crack length. Also energy release rate fracture toughness was evaluated because CFRP/GFRP hybrid composite with a different thickness is under the mixed mode loading condition. The interlaminar fracture was almost governed by mode I fracture even though the mixed mode.