Recovery of Mo by liquid-liquid extraction from synthetic leaching solution of spent Inconel 713C super alloy and preparation of Mo compounds (폐 인코넬계(Inconel 713C)내열합금 모의 침출액으로부터 액-액 추출법에 의한 Mo의 회수 및 Mo 화합물 제조)

  • Ahn, Jong-Gwan;Kim, Da-young;In, Yong-Hyeon
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.19 no.8
    • /
    • pp.403-409
    • /
    • 2018
  • Inconel 713C which of a commercial Ni super alloy have the composition of 70 % Ni, 12 % Cr, 6 % Al and 4 % Mo. Mo is very expensive and have some economic value to recover in the alloy. In this study, liquid-liquid exraction(solvent extraction and stripping) has been performed to separate Mo from the synthetic leaching solution of spent Inconel 713C alloy and prepare to Mo powder by dying, evaporation and heat treatment. The experiments were conducted by using synthetic leaching solution which was prepared $NaMoO_4$ $2H_2O$ by dissolved in distilled water. Alamine336 and Cyanex272 dissolved in kerosene were used as extractants. The extraction percentage of Mo by Alamine336 is 99 % in the condition of the range of pH 1 to 4 and 1 % of concentration of Alamine336. The stripping solutions are used by HCl, $H_2SO_4$ and $HNO_3$ solutions and the concentrations were controlled by distilled water. The concentrations of HCl, $H_2SO_4$ and $HNO_3$ as stripping solutions are increased, the stripping percentages of Mo are increased and the stripping percentage of Mo by $HNO_3$ is higher than other stripping solutions. After liquid-liquid extraction and heat treatment, $MoO_3$ powder which of the purity of 97.5 % was prepared.

Recovery of Cobalt from Synthetic Leaching Solution of Manganese Nodule Matte by Solvent Extraction-electrowinning (용매추출-전해채취법에 의한 망간단괴 매트상 모의 침출용액으로부터 코발트 회수)

  • Kim, Hyun-Ho;Nam, Chul-Woo;Park, Kyung-Ho;Yoon, Ho-Sung;Kim, Min-Seuk;Kim, Chul-Joo;Park, Sang-Woon
    • Resources Recycling
    • /
    • v.25 no.2
    • /
    • pp.33-41
    • /
    • 2016
  • A scale up tests (380 kg/day) using a continuous solvent extraction and electro-winning system was carried out to separate and recover cobalt from a solution containing 1.91 g/L Co and 14.65 g/L Ni. The solution was obtained during a process including solvent extraction and precipitation stages for removal of Cu and Fe from a synthetic sulfuric acid solution of manganese nodule matte. The optimal condition for solvent extraction was : solvent concentration of 0.22M Na-Cyanex 272 (45% saponified with NaOH) and O:A phase ratios of 1:1.5, 10:1 and 1.5:1 used in extraction, scrubbing and stripping stages, respectively. The extraction and stripping efficiencies were found to be 99.8% and 99.88%, respectively. The stripped solution contained 40.27 g/L Co with 4 ppm Ni. Cobalt metal of 99.963% purity was yielded with current efficiency of 67% and current density of $0.563A/dm^2$ during the electro-winning process.

Recovery of the Vanadium and Tungsten from Spent SCR Catalyst Leach Solutions by Hydrometallurgical Methods (SCR 폐촉매 침출액으로부터 습식제련법에 의한 바나듐, 텅스텐의 회수)

  • Choi, In-Hyeok;Moon, Gyeonghye;Jeon, Jong-Hyuk;Lee, Jin-Young;Jyothi, Rajesh Kumar
    • Resources Recycling
    • /
    • v.29 no.2
    • /
    • pp.62-68
    • /
    • 2020
  • In new millennium, wide-reaching demands for selective catalytic reduction (SCR) catalyst have been increased gradually in new millennium. SCR catalyst can prevent the NOx emission to protect the environment. In SCR catalyst the main composition of the catalyst is typically TiO2 (70~80%), WO3 (7~10%), V2O5 (~1%) and others. When the SCR catalysts are used up and disposed to landfills, it is problematic that those should exist in the landfill site permanently due to their extremely low degradability. A new advanced technology needs to be developed primarily to protect environment and then recover the valuable metals. Hydrometallurgical techniques such as leaching and liquid-liquid extraction was designed and developed for the spent SCR catalyst processing. In a first stage, V and W selectively leached from spent SCR catalyst, then both the metals were processed by liquid-liquid extraction process. Various commercial extractants such as D2EHPA, PC 88A, TBP, Cyanex 272, Aliquat 336 were tested for selective extraction of title metals. Scrubbing and stripping studies were tested and optimized for vanadium and tungsten extraction and possible separation. 3rd phase studies were optimized by using iso-decanol reagent.

Behavior of Cobalt Extraction from Cobalt Sulphate solution using Supercritical 2 (황산코발트용액(溶液)으로부터 초임계(超臨界CO2에 의한 코발트 추출거동(抽出擧動))

  • Shin, Shun-Myung;Joo, Sung-Ho;Sohn, Jeong-Soo;Kang, Jin-Gu
    • Resources Recycling
    • /
    • v.20 no.6
    • /
    • pp.78-82
    • /
    • 2011
  • Supercritical $CO_2$($scCO_2$) extraction has a great possibility to be a new process to recover metal and to replace the existing leaching/solvent extraction processes. The cobalt extraction was carried out using $scCO_2$ from cobalt sulphate solution. The bis (2,4,4-trimethylpentyl) phosphinic acid and diethylamine ligands were used to extract cobalt ion in $scCO_2$. The recommended method consists of $scCO_2$/extractants complexation process and metal extraction process at 60, 200bar. Experimental results showed that the extraction efficiency of Co was increased by 16-99% with increasing the ligand amount.

A Synthesis of LiCoO2 using the CoSO4 Recovered from Cathode Material Scrap and its Electrochemical Properties (폐 리튬 이차전지로부터 회수된 황산코발트 제조 및 이를 이용해 합성된 산화리튬코발트 양극활물질의 전기화학적 특성)

  • Kim, Mi-So;Ha, Jong-Keun;Park, Se-Bin;Ahn, Jou-Hyeon;Choi, Im-Sic;Cho, Kwon-Koo
    • Journal of the Korean Electrochemical Society
    • /
    • v.17 no.2
    • /
    • pp.111-118
    • /
    • 2014
  • The electrochemical properties using the cells assembled with the synthesized $LiCoO_2$(LCO) were evaluated in this study. The LCO was synthesized from high-purity cobalt sulfate($CoSO_4$) which is recovered from the cathode scrap in the wastes lithium ion secondary battery(LIB). The leaching process for dissolving the metallic elements from the LCO scrap was controlled by the quantities of the sulfuric acid and hydrogen peroxide. The metal precipitation to remove the impurities was controlled by the pH value using the caustic soda. And also, D2EHPA and $CYANEX^{(R)}272$ were used in the solvent extraction process in order to remove the impurities again. The high-purity $CoSO_4$ solution was recovered by the processes mentioned above. We made the 6 wt.% $CoSO_4$ solution mixed with distilled water. And the 6 wt.% $CoSO_4$ solution was mixed with oxalic acid by the stirring method and dried in oven. $LiCoO_2$ as a cathode material for LIB was formed by the calcination after the drying and synthesis with the $Li_2CO_3$ powder. We assembled the cells using the $LiCoO_2$ powders and evaluated the electrochemical properties. And then, we confirmed possibility of the recyclability about the cathode materials for LIBs.

Recycling of end-of-life LiNixCoyMnzO2 batteries for rare metals recovery

  • Sattar, Rabia;Ilyas, Sadia;Kousar, Sidra;Khalid, Amaila;Sajid, Munazzah;Bukhari, Sania Iqbal
    • Environmental Engineering Research
    • /
    • v.25 no.1
    • /
    • pp.88-95
    • /
    • 2020
  • An investigation of rare metals recovery from LiNixCoyMnzO2 cathode material of the end-of-life lithium-ion batteries is presented. To determine the influence of reductant on the leach process, the cathode material (containing Li 7.6%, Co 20.4%, Mn 19.4%, and Ni 19.3%) was leached in H2SO4 solutions either with or without H2O2. The optimal process parameters with respect to acid concentration, addition dosage of H2O2, temperature, and the leaching time were found to be 2.0 M H2SO4, 4 vol.% H2O2, 70℃, and 150 min, respectively. The yield of metal values in the leach liquor was > 99%. The leach liquor was subsequently treated by precipitation techniques to recover nickel as Ni(C4H7N2O2)2 and lithium as Li2CO3 with stoichiometric ratios of 2:1 and 1.2:1 of dimethylglyoxime:Ni and Na2CO3:Li, respectively. Cobalt was recovered by solvent extraction following a 3-stage process using Na-Cyanex 272 at pHeq ~5.0 with an organic-to-aqueous phase ratio (O/A) of 2/3. The loaded organic phase was stripped with 2.0 M H2SO4 at an O/A ratio of 8/1 to yield a solution of 114 g/L CoSO4; finally recovered CoSO4.xH2O by crystallization. The process economics were analyzed and found to be viable with a margin of $476 per ton of the cathode material.