극저온 압연 및 온간 압연 기술을 이용한 5052 알루미늄 합금의 기계적 성질의 향상 (Large enhancement in mechanical properties of the 5052 Al alloys by cryogenic and warm rolling)

  • 강의구;이상훈;이종철;남원종
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2007년도 추계학술대회 논문집
    • /
    • pp.81-83
    • /
    • 2007
  • Cryogenic rolling combined with warm rolling has been found to be more effective than only cryogenic rolling procedure in improving the strength of a 5052 Al alloy. In this study, cryo-rolled 5052 Al alloys were aged at $175^{\circ}C$. Warm rolling was conducted after dipping plates into silicon oil bath. A notable increase of tensile strength is achieved by the precipitation during warm rolling. The mechanical behavior of this alloy was investigated by hardness and tensile tests. The microstructure was investigated by transmission electron microscopy. It was found that the cryogenic rolling combined with warm rolling was very effective in improving tensile strength.

  • PDF

극저온 압연 및 온간 압연 기술을 이용한 5052 알루미늄 합금의 기계적 성질의 향상 (Enhancement of Mechanical Properties of 5052 Al Alloy by Cryogenic and Warm rolling)

  • 강의구;이상훈;이종철;남종원
    • 소성∙가공
    • /
    • 제17권2호
    • /
    • pp.102-106
    • /
    • 2008
  • Cryogenic rolling combined with warm rolling has been found more effective than a single cryogenic rolling process in improving the strength of a 5052 Al alloy. In this study, cryo-rolled 5052 Al alloys were warm-rolled at $175^{\circ}C$. A notable increase of tensile strength was achieved by the precipitation during warm rolling process. Mechanical behavior of this alloy was investigated using hardness and tensile tests. It was found that the cryogenic rolling process combined with warm rolling process was very effective in improving tensile strength.