Torsional strengthening of RC beams using stainless steel wire mesh -Experimental and numerical study

  • Patel, Paresh V.;Raiyani, Sunil D.;Shah, Paurin J.
    • Structural Engineering and Mechanics
    • /
    • v.67 no.4
    • /
    • pp.391-401
    • /
    • 2018
  • Locally available Stainless Steel Wire Mesh (SSWM) bonded on a concrete surface with an epoxy resin is explored as an alternative method for the torsional strengthening of Reinforced Concrete (RC) beam in the present study. An experiment is conducted to understand the behavior of RC beams strengthened with a different configuration of SSWM wrapping subjected to pure torsion. The experimental investigation comprises of testing fourteen RC beams with cross section of $150mm{\times}150mm$ and length 1300 mm. The beams are reinforced with 4-10 mm diameter longitudinal bars and 2 leg-8 mm diameter stirrups at 150 mm c/c. Two beams without SSWM strengthening are used as control specimens and twelve beams are externally strengthened by six different SSWM wrapping configurations. The torsional moment and twist at first crack and at an ultimate stage as well as torque-twist behavior of SSWM strengthened specimens are compared with control specimens. Also the failure modes of the beams are observed. The rectangular beams strengthened with corner and diagonal strip wrapping configuration exhibited better enhancement in torsional capacity compared to other wrapping configurations. The numerical simulation of SSWM strengthened RC beam under pure torsion is carried out using finite element based software ABAQUS. Results of nonlinear finite element analysis are found in good agreement with experimental results.

Effect of the Circular Saw-Blade Type and Wear on the Cutting Quality of a Glass Carbon-Fiber Hybrid Composite (원형 톱날의 형태와 마모가 유리 탄소섬유 하이브리드 복합재료의 절단 품질에 미치는 영향)

  • Baek, Jong-Hyun;Joo, Chang-Min;Kim, Su-Jin;Park, Yoon-Ok
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.20 no.10
    • /
    • pp.72-79
    • /
    • 2021
  • A circular saw is an effective tool for cutting glass and carbon-fiber hybrid composites. This study investigated tool wear and cut quality when reusing saw blades. The carbide saws wear four times faster than the new ones, and polycrystalline diamond (PCD) is very resistant to tool wear, except at the end of its lifespan. The cut cross-section quality is affected by the blade type, tool wear, and spindle speed. Alternate top bevel (ATB)-type blades are suitable for cutting fiber-reinforced plastics, but triple-chip grind (TCG)-type blades are unsuitable because they cause fiber-pullout defects. Tool wear and low spindle speeds increase the occurrence of arc scratches, due to the rear saw blade. A microscopic examination showed that the burr, which is a mixture of fiber chips and epoxy matrix, was bonded on top, and glass-fiber delamination occurred on the bottom glass-fiber-reinforced polymer (GFRP) surface.

Behavior and modeling of RC beams strengthened with NSM-steel technique

  • Md. Akter Hosen;Khalid Ahmed Al Kaaf;A.B.M. Saiful Islam;Mohd Zamin Jumaat;Zaheer Abbas Kazmi
    • Structural Engineering and Mechanics
    • /
    • v.88 no.1
    • /
    • pp.67-81
    • /
    • 2023
  • The reinforced concrete (RC) structures might need strengthening or upgradation due to adverse environmental conditions, design defects, modification requirements, and to prolong the expected lifespan. The RC beams have been efficiently strengthened using the near surface mounted (NSM) approach over the externally bonded reinforcing (EBR) system. In this study, the performance of RC beam elements strengthened with NSM-steel rebars was investigated using an experimental program and nonlinear finite element modeling (FEM). Nine medium-sized, rectangular cross-section RC beams total in number made up for the experimental evaluation. The beams strengthened with varying percentages of NSM reinforcement, and the number of grooves was assessed in four-point bending experiments up to failure. Based on the experimental evaluation, the load-displacement response, crack features, and failure modes of the strengthened beams were recorded and considered. According to the experimental findings, NSM steel greatly improved the flexural strength (up to about 84%) and stiffness of RC beams. The flexural response of the tested beams was simulated using a 3D non-linear finite element (FE) model. The findings of the experiments and the numerical analysis showed good agreement. The effect of the NSM groove and reinforcement on the structural response was then assessed parametrically.

Physical-Mechanical Properties of Laminated Board Made from Oil Palm Trunk (Elaeis guineensis Jacq.) Waste with Various Lamina Compositions and Densifications

  • PRABUNINGRUM, Dita Sari;MASSIJAYA, Muh Yusram;HADI, Yusuf Sudo;ABDILLAH, Imam Busyra
    • Journal of the Korean Wood Science and Technology
    • /
    • v.48 no.2
    • /
    • pp.196-205
    • /
    • 2020
  • The purpose of this study was to investigate a method for improving the physical and mechanical properties of laminated board made from oil palm trunk (OPT). The effects of pretreating the lamina with heat-pressure and altering the lamina composition of the laminated board were investigated. The outer third of OPT in cross-section had high-density wood, while the underlying third had low to medium density. The hot press was applied to pretreat the lamina that had low to medium density. The lamina were 1.5 cm in thickness, 5 cm in width, and 65 cm in length. The hot press was applied at 2.94 MPa or 4.41 MPa at 150 ℃ for 60 minutes, and the target thickness of the lamina was 1 cm. The three layers of the laminated board samples were bonded with isocyanate adhesive at a glue spread of 300 g/㎡ and cold pressed at 0.98 MPa for 3 h. The laminated board samples were tested according to Japanese Agricultural Standard (JAS) 234-2003. The results showed that the densification of the inner lamina did not significantly affect the physical-mechanical properties of the laminated board produced. However, the laminated board made with high-density laminas for the outer layers fulfilled the JAS 234-2003 standard for the modulus of elasticity and the modulus of rupture.

Analytical, experimental and numerical study of timber-concrete composite beams for bridges

  • Molina, Julio C.;Calil, Carlito Junior;de Oliveira, Diego R.;Gomes, Nadia B.
    • Computers and Concrete
    • /
    • v.24 no.2
    • /
    • pp.103-115
    • /
    • 2019
  • In this study, the strength and stiffness (EI) of wood-concrete composite beams for bridges with T-shaped cross section were evaluated. Two types of connectors were used: connectors bonded with epoxy adhesive and connectors attached to the wood just by pre-drilling (without adhesive). The connectors consisted of common steel bars with a diameter of 12.5 mm. Initially, the strength and stiffness (EI) of the beams were analyzed by bending tests with the load applied at the third point of the beam. Subsequently, the composite beams were evaluated by numerical simulation using ANSYS software with focus on the connection system. To make the composite beams, Eucalyptus citriodora wood and medium strength concrete were used. The slip modulus K and the ultimate strength values of each type of connector were obtained by direct shear tests performed on composite specimens. The results showed that the connector glued with epoxy adhesive resulted in better strength and stiffness (EI) for the composite beams when compared to the connector fixed by pre-drilling. The differences observed were up to 10%. The strength and stiffness (EI) values obtained analytically by $M{\ddot{o}}hler^{\prime}$ model were lower than the values obtained experimentally from the bending tests, and the differences were up to 25%. The numerical simulations allowed, with reasonable approximation, the evaluation of stress distributions in the composite beams tested experimentally.

Dismantling and Restoration of the Celadon Stool Treasure with an Openwork Ring Design (보물 청자 투각고리문 의자의 해체 및 복원)

  • KWON, Ohyoung;LEE, Sunmyung;LEE, Jangjon;PARK, Younghwan
    • Korean Journal of Heritage: History & Science
    • /
    • v.55 no.2
    • /
    • pp.200-211
    • /
    • 2022
  • The celadon stools with an openwork ring design which consist of four items as one collection were excavated from Gaeseong, Gyeonggi-do Province. The celadon stools were designated and managed as treasures due to their high arthistorical value in the form of demonstrating the excellence of celadon manufacturing techniques and the fanciful lifestyles during the Goryeo Dynasty. However, one of the items, which appeared to have been repaired and restored in the past, suffered a decline in aesthetic value due to the aging of the treatment materials and the lack of skill on the part of the conservator, raising the need for re-treatment as a result of structural instability. An examination of the conservation condition prior to conservation treatment found structural vulnerabilities because physical damage had been artificially inflicted throughout the area that was rendered defective at the time of manufacturing. The bonded surfaces for the cracked areas and detached fragments did not fit, and these areas and fragments had deteriorated because the adhesive trickled down onto the celadon surface or secondary contaminants, such as dust, were on the adhesive surface. The study identified the position, scope, and conditions of the bonded areas at the cracks UV rays and microscopy in order to investigate the condition of repair and restoration. By conducting Fourier-transform infrared spectroscopy(FT-IR) and portable x-ray fluorescence spectroscopy on the materials used for the former conservation treatment, the study confirmed the use of cellulose resins and epoxy resins as adhesives. Furthermore, the analysis revealed the addition of gypsum(CaSO4·2H2O) and bone meal(Ca10 (PO4)6(OH)2) to the adhesive to increase the bonding strength of some of the bonded areas that sustained force. Based on the results of the investigation, the conservation treatment for the artifact would focus on completely dismantling the existing bonded areas and then consolidating vulnerable areas through bonding and restoration. After removing and dismantling the prior adhesive used, the celadon stool was separated into 6 large fragments including the top and bottom, the curved legs, and some of the ring design. After dismantling, the remaining adhesive and contaminants were chemically and physically removed, and a steam cleaner was used to clean the fractured surfaces to increase the bonding efficacy of the re-bonding. The bonding of the artifact involved applying the adhesive differently depending on the bonding area and size. The cyanoacrylate resin Loctite 401 was used on the bonding area that held the positions of the fragments, while the acrylic resin Paraloid B-72 20%(in xylene) was treated on cross sections for reversibility in the areas that provided structural stability before bonding the fragments using the epoxy resin Epo-tek 301-2. For areas that would sustain force, as in the top and bottom, kaolin was added to Epo-tek 301-2 in order to reinforce the bonding strength. For the missing parts of the ring design where a continuous pattern could be assumed, a frame was made using SN-sheets, and the ring design was then modeled and restored by connecting the damaged cross section with Wood epos. Other restoration areas that occurred during bonding were treated by being filled with Wood epos for aesthetic and structural stabilization. Restored and filled areas were color-matched to avoid the feeling of disharmony from differences of texture in case of exhibitions in the future. The investigation and treatment process involving a variety of scientific technology was systematically documented so as to be utilized as basic data for the conservation and maintenance.

Effects of Thermal and Mechanical Fatigue Stress on Bond Strength in Bracket Base Configurations (열적, 기계적 피로응력이 교정용 브라켓의 결합강도에 미치는 영향)

  • Kim, Jong-Ghee;Kim, Sang-Cheol
    • The korean journal of orthodontics
    • /
    • v.30 no.5 s.82
    • /
    • pp.625-642
    • /
    • 2000
  • The purpose of this study is to evaluate the effects of mechanical and thermal fatigue stress on the shear, tensile and shear-tensile combined bond strengths(SBS, TBS, CBS) in various orthodontic brackets bonded to human premolars with chemically cured adhesive(Ortho-one, Bisco, USA). Five types of commercially available metal brackets with various bracket base configurations of Photoetched base(Tomy, Japan), Non-Etched Foil Mesh base(Dentaurum, Germany), Micro-Etched Foil Mesh base(Ortho Organizers, USA), Chessboard base(Daesung, Korea), and Integral base(3M Unitek, USA) were used. Samples were divided into 3 groups, the first group was acted with shear-tensile combined loads($45^{\circ}$) of 200g for 4 weeks(mechanical fatigue stress), the second group was subjected to the 5,000 thermocycles of 15 second dwell time each in $5^{\circ}C\;and\;55^{\circ}C$ baths(thermal fatigue stress), and the third group was the control. Bond strengths were measured at the crosshead speed of 0.5mm/min. The cross-section of bracket base/adhesive interface and the fracture surface were examined with the stereoscope and the scanning electron microscope. The resin remnant on bracket base surface was assessed by ART(Adhesive Remnant Index). The obtained results were summarized as follows, 1. In static bond strength, Photoetched base bracket showed the maximum bond strength and Integral base bracket showed the minimum bond strength(p<0.05). In all brackets, shear bond strength(SBS) was in the greatest value and shear-tensile combined strength(CBS) was in the least value(p<0.05). 2. After mechanical fatigue test, Photoetched base bracket showed the maximum bond strength and Integral base bracket showed the minimum bond strength(p<0.05). In Photoetched base bracket and Micro-Etched Foil Mesh base bracket, shear bond strength(SBS), tensile bond strength(TBS) and shear-tensile combined strength(CBS) were decreased after mechanical fatigue test(p

  • PDF

Transmitted Noise Reduction Performance of Piezoelectric Single Panel through Piezo-damping (압전감쇠를 통한 압전단일패널의 전달 소음저감성능)

  • 이중근;김재환;김기선;이형식
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.2 no.2
    • /
    • pp.49-56
    • /
    • 2001
  • The possibility of a noise reduction of piezoelectric single Panels is experimentally studied. Piezoelectric single panel is basically a plate structure on which piezoelectric patch with shunt circuit is mounted. The use of piezoelectric shunt damping can reduce the transmission at resonance frequencies of the panel structure. Piezo-damping is implemented by using a newly proposed tuning method. This method is based on electrical impedance model and maximizing the dissipated energy at the shunt circuit. By measuring the electrical impedance at the piezoelectric patch bonded on a structure, an equivalent electrical model is constructed near the system resonance frequency. Resonant shunt circuit for piezoelectric shunt damping is composed of register and inductor in series, and they are determined by maximizing the dissipated energy throughout the circuit. The transmitted noise reduction performance of single Panel is tested on an acoustic tunnel. The tunnel is a tube with a square cross section and a loud speaker is mounted at one side of the tube as a sound source. Panels are mounted in the middle of the tunnel and the transmitted sound pressure across Panels is measured. By enabling the piezoelectric shunt damping noise reduction is achieved at the resonance frequencies as well. Piezoelectric single panel with piezoelectric shunt damping is a promising technology for noise reduction in a broadband frequency.

  • PDF

EFFECT OF CALCIUM HYDROXIDE ON BOND STRENGTH OF DENTIN BONDING SYSTEMS (수산화칼슘 적용에 따른 상아질 접착제의 접착강도 변화에 관한 연구)

  • Park, No-Hoon;Park, Sang-Hyuk;Choi, Gi-Woon;Park, Sang-Jin
    • Restorative Dentistry and Endodontics
    • /
    • v.32 no.3
    • /
    • pp.198-207
    • /
    • 2007
  • The purpose of this study was to investigate the effect of calcium hydroxide on dentin bonding strength of various dentin bonding systems as a function of time in composite resin restoration. Dentin adhesives used in this study were Scotchbond Multipurpose, Single Bond, SE Bond and Prompt L-Pop. Flat dentin surfaces adjacent to pulp chamber were created, then $Ca(OH)_2$ and saline were mixed and applied on dentin surface of experimental group, then IRM was used to cover the mixture on dentin surface and the specimens were stored at $36.5^{\circ}C$ for experiment period (7 days, 30 days). After removing IRM and $Ca(OH)_2$, each dentin adhesives were treated on dentin surfaces. Composite resin (Z-250, 3M) was placed with S mm height and was light-cured for 20 seconds. After stored in distilled water for 24 hours, each dentin-composite bonded spicemen was embedded in epoxy resin and sectioned into $1.0\times1.0mm^2$ cross section composite-dentin beams. Specimen was mounted on zig of Universal testing machine and ${\mu}TBS$ test was performed. SEM analysis was performed to examine the fractured surfaces. The results suggested that applying calcium hydroxide did not show significant difference in dentin bonding strength.

The effect of the strength and wetting characteristics of Bis-GMA/TEGDMA-based adhesives on the bond strength to dentin (2,2-Bis[4-(2-methoxy-3-methacryloyloxy propoxy) phenyl] propane을 함유한 상아질 접착레진의 물성이 접착강도에 미치는 영향)

  • Park, Eun-Sook;Kim, Chang-Keun;Bae, Ji-Hyun;Cho, Byeong-Hoon
    • Restorative Dentistry and Endodontics
    • /
    • v.36 no.2
    • /
    • pp.139-148
    • /
    • 2011
  • Objectives: This study investigated the effect of the strength and wetting characteristics of adhesives on the bond strength to dentin. The experimental adhesives containing various ratios of hydrophobic, low-viscosity Bis-M-GMA, with Bis-GMA and TEGDMA, were made and evaluated on the mechanical properties and bond strength to dentin. Materials and Methods: Five experimental adhesives formulated with various Bis-GMA/Bis-MGMA/TEGDMA ratios were evaluated on their viscosity, degree of conversion (DC), flexural strength (FS), and microtensile bond strength (MTBS). The bonded interfaces were evaluated with SEM and the solubility parameter was calculated to understand the wetting characteristics of the adhesives. Results: Although there were no significant differences in the DC between the experimental adhesives at 48 hr after curing (p > 0.05), the experimental adhesives that did not contain Bis-GMA exhibited a lower FS than did those containing Bis-GMA (p < 0.05). The experimental adhesives that had very little to no TEGDMA showed significantly lower MTBS than did those containing a higher content of TEGDMA (p < 0.05). The formers exhibited gaps at the interface between the adhesive layer and the hybrid layer. The solubility parameter of TEGDMA approximated those of the components of the primed dentin, rather than Bis-GMA and Bis-M-GMA. Conclusions: To achieve a good dentin bond, a strong base monomer, such as Bis-GMA, cannot be completely replaced by Bis-M-GMA for maintaining mechanical strength. For compatible copolymerization between the adhesive and the primed dentin as well as dense cross-linking of the adhesive layer, at least 30% fraction of TEGDMA is also needed.