• 제목/요약/키워드: Cross diffusion

검색결과 334건 처리시간 0.031초

간흡충 감염 가토의 면역진단에 대한 연구 2. 성충 조항원의 정제 및 발육단계별 항원 분석 (Studies on the Immunodiagnosis of Rabbit Clonorchiasis 2. Immunoamnity purification of whole worm antigen and characterization of egg, metacercaria and adult antigens of Clonorchis sinensis)

  • 이옥란;정평림;남해선
    • Parasites, Hosts and Diseases
    • /
    • 제26권2호
    • /
    • pp.73-86
    • /
    • 1988
  • 간흡충(Clonorchis sinensis)의 조항원(WWA), 정제항원(ABA)의 민감도와 특이도를 비교해 보는 한편, 발육단계별로 충란 항원(EGA)-피낭유충 항원(MEA)-성충 항원(WWA)의 단백질 구성물질의 차이를 SDS-polyacrylamide gel electrophoresis(SDS-PAGE)로 관찰하고 이들 항원의 유용성을 효소면역반응(enzyme-linked immunosorbent assay: ELISA)으로 비교하여 다음과 같은 결과를 얻었다. 간흡충의 조항원으로부터 정제된 항원(ABA)은 항체와 결합한 결합항원(affinity-purified antibody(IgG) binding antigen:ABA)으로서 Ouchterlony 반응으로 간흡충 감염 가토혈청과 4개의 침모대 (WWA는 7개)를 형성하였다. WWA의 major protein들은 분자량 16,300∼18,500 및 28,000∼29,000 dalton의 Polypeptide band였고, ABA는 분자량 18,000∼21,000 및 29,000∼31,000 dalton의 단백질로 다소의 차이를 보였다. ELISA시첩에서 ABA는 WWA에 비해 현저히 민감도가 낮았다. WWA와 ABA에 대한 폐흡충 감염 사람혈청의 ELISA 정사에서 WWA는 Ouchterlony 양성자 8예중 3예에서 교차반응을 나타내었으나 ABA는 교차반응을 나타내지 않았다. 간흡충의 발육단계별 항원 단백질의 분자량 범위는 WWA 11,000∼80,000, MEA 15,000∼100,000, EGA 15,000∼200,000 dalton이었다. 주류원 단백질의 분자량은 EGA는 각각 36,600 (band No. 22), 38,500(No. 20), 64,000(No. 9), 62,000(No. 10), 54,500(No. 11), 53,000(No. 12) dalton, MEA는 각각 65,600(No. 3), 44,700 (No.7), 43,900(No. 8) dalton, WWA는 각각 16,300∼18,500(No. 31-32), 28,000∼29,000(No. 25), 11,000w13,000 (No. 35) 및 31,000(No. 24) dalton이었다. 즉, MEA와 EGA가 WWA보다 고분자의 단백질로 구성되어 있었다. 각 발육단계별 항원의 항원성은 ELISA 반응으로 볼 때 WWA가 가장 높았고, MEA는 약한 항원성만을 나타내었으며 EGA는 음성이었다. WWA와 간흡충 감염 가토혈청은 감염 4∼6주에 OD>1.0, 12주 이후 항체가의 plateau를 나타내었으나 MEA는 Ouchterlony 반응에서 EGA와 함께 음성반응을 보였다. ELISA에서도 중감염군(12∼20주)에서만 OD>0.6으로 미약한 항원성이 인정되었으며 경감염군은 전감염기간중 OD<0.6를 나타내었다. 이상의 결과로 보아 성충 항원이 가장 강력한 함원성 물질을 포함하고 있음이 명백하다고 생각된다. 그러나 성충 조항원은 면역진단에 사용할 겹우 타흡충과의 빈번한 교차반응이 예상되므로 민감도 및 특이도가 높은 정제 항원물질을 분리하는 일이 중요하다고 생각된다.

  • PDF

가공의치(架工義齒) 납착부(蠟着部)의 강도(强度)와 내부구조(內部構造)에 관(關)한 실험적(實驗的) 연구(硏究) (An experimental study of the strength and internal structure of solder joint of fixed partial denture)

  • 박상남;계기성
    • 대한치과보철학회지
    • /
    • 제23권1호
    • /
    • pp.39-59
    • /
    • 1985
  • The purpose of this study was to investigate how gap distances of 0.13mm, 0.15mm, 0.20mm, and 0.30mm affects solder joint strength from gold alloys and nickel-chromium base alloys and to examine the composition of solder gold, the solder joint of gold alloys and nickel-chromium base alloys. The tensile test specimens were prepared in the split stainless steel mold with a half dumbbell shape 2.5mm in diameter and l2mm in length. 6 pairs of specimens of each gap distance group of gold alloys and nickel-chromium base alloys were made and 48 pairs of all specimens were soldered with solder gold of 666 fineness. All soldered specimens were machined to a uniform diameter and then a tensile load was applied at a cross-head speed of 0.10mm/min using Instron Universal Testing Machine, Model 1115. The fractured specimens at solder gold of solder joint fracture with each gap distance of 0.13mm, 0.15mm, 0.20mm, and 0.30mm were examined under the Scanning Electron Microscope, JSM-35c and the composition of solder gold, the solder joint of gold alloys and nickel-chromium base alloys was analyzed by Electron Probe Micro Analyzer. The results of this study were obtained as follows: 1. In case of soldering of gold alloys, the tensile strength between gold alloys showed $37.33{\pm}2.52kg/mm^2$ at 0.13, $39.14{\pm}3.35kg/mm^2$ at 0.15mm, $43.76{\pm}2.97kg/mm^2$ at 0.20mm, and $49.18{\pm}4.60kg/mm^2$ at 0.30mm. There was statistically significant difference at each gap distance, and so the greater increase of gap distance showed the greater tensile strength. 2. In case of soldering of nickel-chromium base alloys, the tensile strength between nickel-chromium base alloys showed $34.84{\pm}4.26kg/mm^2$ at 0.13mm, $37.25{\pm}2.49kg/mm^2$ at 0.15mm, $42.91{\pm}4.32kg/mm^2$ at 0.20mm, and $46.93{\pm}4.21kg/mm^2$ at 0.30mm. There was not statistically significant difference only between 0.13mm and 0.15mm and bet ween 0.20 mm and 0.30mm, but generally the greater increase of gap distance showed the greater tensile strength. 3. The greater increase of gap distance shoed less porosities in solder gold at solder joint fracture. 4. In solder gold Au, Cu, Ag, Zn, and Sn were composed and Au and Cu were mostly distributed uniformly. 5. In solder joints of solder gold and gold alloys Au, Cu, Ag, Zn, and Sn were composed in solder gold and Au, Cu, Ag, Pt, and Pd were composed in gold alloys. Au and Cu of solder gold and gold alloys were mostly distributed uniformly and the diffusion of other elements except Pt and Pd around the solder joint was not almost found. In solder joints of solder gold and nickel-chromium base alloys Au, Cu, Ag, Zn, and Sn were composed in solder gold and Ni, Cr, and Al were composed in nickel-chromium base alloys. Au and Cu of solder gold and Ni and Cr of nickel-chromium base alloys were mostly distributed uniformly and the diffusion of other elements except Cr around the solder joint was not almost found.

  • PDF

한강 감조구간에서의 흐름 및 혼합거동 (Flow and Mixing Behavior at the Tidal Reach of Han River)

  • 서일원;송창근;이명은
    • 대한토목학회논문집
    • /
    • 제28권6B호
    • /
    • pp.731-741
    • /
    • 2008
  • 기존의 한강 감조구간 수치모의에 대한 연구는 단면자료 획득의 어려움이나 유도의 조위자료가 없으므로 하류 경계단을 전류지점으로 하여 모의한 논문이 대부분이나 본 연구에서는 수치해도를 바탕으로 곡릉천 합류부 이후와 임진강 하구부의 단면을 가정하고 인천검조소의 조위자료를 유도지점으로 전이시켜 서해안 조위에 의한 한강하류부에서의 수리학적 거동을 해석하였다. 모형의 적용구간은 신곡수중보로부터 한강의 법적 하류단인 김포시 유도까지 총 36.8 km에 이르는 구간으로 흐름 및 혼합거동 해석은 RMA-2 모형과 서일원(2008)이 개발한 2차원 이송-분산 해석모형인 RAM4를 이용하였다. 전류지점에서의 수위 및 종횡방향 유속 실측자료와 수치모의 결과를 비교하여 흐름해석 결과를 검증하였다. 수위 관측소의 자료가 양호하고 인천검조소에서 높은 조차가 발생하는 2006년 6월 23일~25일 동안 모의한 결과 유도지점의 조위에 따라 총 5회의 역방향 흐름이 관찰되었고 최대 역류 길이는 장항 IC까지 총 32.9 km에 이르렀다. 최대 역방향 흐름의 발생 및 소멸 과정, 최고 유속선을 따른 수위 및 유속을 분석하였으며 이에 따른 비보존성 오염물질의 혼합거동을 해석하였다. 굴포천으로부터 유입된 오염물질은 하폭방향 퍼짐이 두드러지게 일어났지만 곡릉천에서 유입된 BOD는 곡릉천 합류부를 전후하여 중앙 및 좌안측 수심이 급격히 깊어지고 최대유속선이 곡릉천 방향인 우안에서 발생하고 있으므로 횡방향 혼합이 빠르게 완료되어 오염운의 반경이 상대적으로 좁은 것을 확인할 수 있었다. 또한 1차원 이송-분산방정식의 해석해를 적용해 유도지점의 염도 값을 인천검조소로부터 추산하여 한강 하류부에서의 수평 2차원 염수 혼합거동을 해석하였다.

Diagram와 Pad의 팽창에 의한 반응도 효과에 대한 연구 (A Study on the Reactivity Effect due to Expansion of Diagrid and Pad)

  • Young In Kim;Keun Bae Oh;Kun Jong Yoo;Mann Cho
    • Nuclear Engineering and Technology
    • /
    • 제16권2호
    • /
    • pp.70-79
    • /
    • 1984
  • 대형 고속증식로용 핵계산 체제(KAERI-26군 단면적 library/1DX/2DB)를 이용하여 SUPER-PHE-NIX I 평형 노심의 초기상태에서의 diagrid 및 Pad팽창에 대한 반응도 계수를 계산, 검토하였다. 노심은 R-Z등가 model로 묘사하고, 2차원 다군 확산 이론 전산코드인 2DB를 사용하여 임계도를 계산하였다. 기초계산으로서 반경방향 및 축방향 균일 괭창에 대한 반응도 계산과 노심구성물질의 원자수 밀도 변화와 노심체적 변화에 대한 반응도 변화량계산을 수행하였다. 균일 팽창으로 고려한 diagrid팽창에 대한 반응도 계수는 -0.553pcm/mil로 계산되었다. 한편 반응도의 온도계수는 -1.0766pcm/$^{\circ}C$로 환산되어 프랑스 발표치 -1.09pcm/$^{\circ}C$와 1.2%오차내로 일치하였다. Diagrid 팽창효과 졔산방법을 활용하여 노심의 불균일 팽창을 유발하는 pad팽창에 대한 반응도 계수 계산을 수행한 바 매우 유용함을 알았다. Pad팽창에 대한 반응도 계수는 평균팽창 model의 경우 -0.2743pcm/mi1, pancake집적 model의 경우 -0.2786pcm/mi1로 각각 계산되었다. 또한 자유팽창 노심에서의 온도변화에 따른 pad 팽창에 대한 반응도 계수는 각 model에 대하여 -0.5766pcm/$^{\circ}C$, -0.5858pcm/$^{\circ}C$로 계산되어 프랑스 발표치 -0.574pcm/$^{\circ}C$와 2% 오차내로 일치하였다.

  • PDF

W 활성소결체의 Ni-rich 상의 양이 응력 파단 성질에 미치는 영향에 관한 연구 (A study on the effect of Ni-rich phase on the stress-rupture properties of Ni microalloyed W)

  • 박대규;김수성;이경섭
    • 한국재료학회지
    • /
    • 제2권4호
    • /
    • pp.270-278
    • /
    • 1992
  • W-0.4wt% Ni, W-0.8wt% Ni 활성 소결체의 Ni rich상의 양이 응력 파단 성질에 미치는 영향을 조사하기 위하여, direct load creep tester를 사용, 100$0^{\circ}C$~120$0^{\circ}C$, 수소 분위기에서 응력 파단시험을 하였다. 100시간 응력 파단 강도는 니켈 함량이 0.4wt%, 0.8wt%로 증가 함에 따라, W-0.2wt% Ni의 경우와 비교하여 100$0^{\circ}C$에서 43%, 90%, $1100^{\circ}C에서$ 35%, 60% 높았으며, 이는 초기 결정립 조대화, 비이론밀도의 상승과 시험 중 결정립 성장 때문으로 생각된다. W-0.4wt% Ni의 크리프변형 활성화 에너지는 81.3kca1/mol으로, 변형기구는 Ni rich 상을 통한 W 확산과 결정립 내부 변형이다. 응력 파단 시험 후, 파단면은 입계 파괴 양상을 나타내었다. 소결시 생성된 고립 기공이 결정입계에 있는 Ni rich상을 따라 전파하였기 때문이다.

  • PDF

확산포집기로 공기중 ppb 농도수준의 휘발성유기물질 포집시 확산길이와 기류변화가 시료포집속도에 미치는 영향 (The effects of face velocity and path length on the uptake rates of volatile organic compounds measured by diffusive samplers)

  • 변상훈;톰 스톡;마리아 모란디;아프샤;제이 크로스
    • 한국산업보건학회지
    • /
    • 제11권1호
    • /
    • pp.34-41
    • /
    • 2001
  • Passive samplers have been used for personal, indoor, and outdoor air monitoring of VOCs at ppb concentrations in community and office environments. The path length of modified passive sampler was shortened, so it was intended to increase an uptake rate. The performance of the modified 3M 3500 organic vapor monitor(OVM) as a tool for assessing exposures to toxic air pollutants in nonoccupational community environments was evaluated using combined controlled test atmospheres of six selected target volatile organic compounds(VOCs): benzene, methyl tert-butyl ether(MTBE), chloroform, 1,4-dichlorobenzene, tetrachloroethylene, and toluene. The experiments were conducted by exposing the dosimeters to concentrations of $50{\sim}100{\mu}g/m^3$ on six face velocity(0.00, 0.02, 0.06, 0.12, 0.20, 0.30 m/sec) for 24 hours. If the uptake rate was increased, that means that we could use the passive sampler more effectively. The uptake rates were increased linearly according to reduce the path length. Although the diffusion path length was shortened, the change of uptake rate was within ${\pm}25%$ of theoretical value, indicating that the modified passive sampler(TM) can be effectively used over the range of concentrations and environmental conditions tested with a 24-h sampling period if the face velocities were over 0.12 m/s for 6 components of VOCs. But when the face velocities were less than 0.12 m/s, uptake rates were reduced more than expected values. So, the passive sampler with the shortened path length should be used at indoor or outdoor environment where the face velocity should be over about 0.10 m/s. If the path length was shortened more, the uptake rate was more effected by starvation.

  • PDF

Immunochemical Studies for the Characterization of Purified $(Na^+,\;K^+)-ATPase$ and Its Subunits with a Special Reference of Their Effect on Monovalent Cation Transport in Reconstituted $(Na^+,\;K^+)-ATPase$ Vesicles

  • Rhee, H.M.;Hokin, L.E.
    • 대한약리학회지
    • /
    • 제26권1호
    • /
    • pp.35-49
    • /
    • 1990
  • A highly purified $(Na^+,\;K^+)-ATPase$ from the rectal gland of Squalus acanthias and from the electric organ of Electrophorus electricus has been used to raise antibodies in rabbits. The 97,000 dalton catalytic subunit and glycoprotein derived from the rectal gland of spiny shark were also used as antigens. The two $(Na^+,\;K^+)-ATPase$ holoenzymes and the two shark subunits were antigenic. In Ouchterlony double diffusion experiments, these antibodies formed precipitation bands with their antigens. Antibodies prepared against the two subunits of shark holoenzyme also formed precipitation bands with their antigens and shark holoenzyme, but not with eel holoenzyme. These observations are in good agreement with inhibitory effect of these antibodies on the catalytic activity of $(Na^+,\;K^+)-ATPase$ both from the shark and the eel, since there is very little cross-reaction between the shark anticatalytic subunit antibodies and the eel holoenzyme. The maximum antibodies titer of the anticatalytic subunit antibodies is found to be 6 weeks after the initial single exposure to this antigen. Multiple injections of the antigen increased the antibody titer. However, the time required to produce the maximum antibody titer was approximately the same. These antibodies also inhibit catalytic activity of $(Na^+,\;K^+)-ATPase$ vesicles reconstituted by a slow dialysis of cholate after solubilization of the enzyme in a presonicated mixture of cholate and phospholipid. In these reconstituted $(Na^+,\;K^+)-ATPase$ vesicles, effects of these antibodies on the fluxes of $Na^+$, $Rb^+$, and $K^+$ were investigated. Control or preimmune serum had no effect on the influx of $^{22}Na^+$ or the efflux of $^{86}Rb^+$. Immunized sera against the shark $(Na^+,\;K^+)-ATPase$ holoenzyme, its glycoprotein or catalytic subunit did inhibit the influx of $^{22}Na^+$ and the efflux of $^{86}Rb^+$. It was also demonstrated that these antibodies inhibit the coupled counter-transport of $Na^+$ and $K^+$ as studied by means of dual labeling experiments. However, this inhibitory effect of the antibodies on transport of ions in the $(Na^+,\;K^+)-ATPase$ vesicles is manifested only on the portion of energy and temperature dependent alkali metal fluxes, not on the portion of ATP and ouabain insensitive ion movement. Simultaneous determination of effects of the antibodies on ion fluxes and vesicular catalytic activity indicates that an inhibition of active ion transport in reconstituted $(Na^+,\;K^+)-ATPase$ vesicles appears to be due to the inhibitory action of the antibodies on the enzymatic activity of $(Na^+,\;K^+)-ATPase$ molecules incorporated in the vesicles. These findings that the inhibitory effects of the antibodies specific to $(Na^+,\;K^+)-ATPase$ or to its subunits on ATP and temperature sensitive monovalent cation transport in parallel with the inhibitory effect of vesicular catalytic activity by these antibodies provide direct evidence that $(Na^+,\;K^+)-ATPase$ is the molecular machinery of active cation transport in this reconstituted $(Na^+,\;K^+)-ATPase$ vesicular system.

  • PDF

고추 역병균에 대한 3-phenylisoxazole과 3-phenyl-2,5-dihydroisoxazol-5-one 유도체들의 살균 활성에 관한 비교 분자장 분석 (CoMFA) (Comparative molecular field analyses (CoMFA) on the antifungal activity against phytophthora blight fungus of 3-phenylisoxazole and 3-phenyl-2,5-dihydroisoxazol-5-one derivatives)

  • 성낙도;이희철
    • 농약과학회지
    • /
    • 제6권2호
    • /
    • pp.72-79
    • /
    • 2002
  • 일련의 3-phenyl-2,5-dihydroisoxazol-5-one(A)과 3-phenylisoxazole(B)유도체 중, 치환-phenyl기가 변화함에 따라 metalaxyl 살균제에 대하여 감수성(SPC:95C C7105)이나 저항성(RPC: 95CC7303)을 나타내는 고추역병균(Phytophthora capsici)의 살균활성 에 관한 비교 분자장 분석(CoMFA) 결과를 검토하였다. 살균활성은 (A)가 (B)보다 큰 경향이었으며 활성을 나타내는 가장 안정한 기질 분자의 형태는 평면성에 가까운 구조이었다. 두 균주를 대상으로 살균 활성에 미치는 CoMFA 장을 계산한 바, 상대적인 기여도는 공히, 정전기장이 가장 우세하였고 소수성장 및 입체장은 비슷한 정도로 기여하였다. 또한, CoMFA 모델은 좋은 상관성과 높은 예측성($q^2>0.570$$r^2>0.968$)을 나타내었다. 등고도 분석으로부터 RPC에 대한 살균활성의 선택성 요소는 benzoyl-기의 ortho, meta(C14 및 C15) 위치에는 부피가 큰 치환체를 그리고 meta, para(C15 및 C16) 위치부근에는 음하전을 생성하는 전자끌게가 도입되어야 할 것으로 판단된다.

$Pt/SrTiO_3/Pb_x(Zr_{0.52}, Ti_{0.48})O_3/SrTiO_3/Si$ 구조의 전기적 특성 분석 및 $SrTiO_3$박막의 완충층 역할에 관한 연구 (Electrical Properties in $Pt/SrTiO_3/Pb_x(Zr_{0.52}, Ti_{0.48})O_3/SrTiO_3/Si$ Structure and the Role of $SrTiO_3$ Film as a Buffer Layer)

  • 김형찬;신동석;최인훈
    • 한국전기전자재료학회논문지
    • /
    • 제11권6호
    • /
    • pp.436-441
    • /
    • 1998
  • $Pt/SrTiO_3/Pb_x(Zr_{0.52}, Ti_{0.48})O_3/SrTiO_3/Si$ structure was prepared by rf-magnetron sputtering method for use in nondestructive read out ferroelectric RAM(NDRO-FEAM). PBx(Zr_{0.52}Ti_{0.48})O_3}$(PZT) and $SrTiO_3$(STO) films were deposited respectively at the temperatures of $300^{\circ}C and 500^{\circ}C$on p-Si(100) substrate. The role of the STO film as a buffer layer between the PZT film and the Si substrate was studied using X-ray diffraction (XRD), Auger electron spectroscopy (ASE), and scanning electron microscope(SEM). Structural analysis on the interfaces was carried out using a cross sectional transmission electron microscope(TEM). For PZT/Si structure, mostly Pb deficient pyrochlore phase was formed due to the serious diffusion of Pb into the Si substrate. On the other hand, for STO/PZT/STO/Si structure, the PZT film had perovskite phase and larger grain size with a little Pb interdiffusion. the interfaces of the PZT and the STO film, of the STO film and the interface layer and $SiO_2$, and of the $SiO_2$ and the Si substate had a good flatness. Across sectional TEM image showed the existence of an amorphous layer and $SiO_2$ with 7nm thickness between the STO film and the Si substrate. The electrical properties of MIFIS structure was characterized by C-V and I-V measurements. By 1MHz C-V characteristics Pt/STO(25nm)/PZT(160nm)/STO(25nm)/Si structure, memory window was about 1.2 V for and applied voltage of 5 V. Memory window increased by increasing the applied voltage and maximum voltage of memory window was 2 V for V applied. Memory window decreased by decreasing PZT film thickness to 110nm. Typical leakage current was abour $10{-8}$ A/cm for an applied voltage of 5 V.

  • PDF

고속철도 터널에서의 미기압파 저감을 위한 모형실험 (The High-speed train model for reducing the micro-pressure wave in railway tunnel)

  • 장용준;박원희;김승태
    • 한국철도학회:학술대회논문집
    • /
    • 한국철도학회 2007년도 추계학술대회 논문집
    • /
    • pp.1330-1336
    • /
    • 2007
  • 본 연구는 미기압파 해석에 필요한 각종계수의 도출 및 해석결과의 신뢰성을 검증하기 위한 목적이 있다. 본 실험에 사용된 터널 주행 열차모형 실험 장치는 1/60축척으로 제작 되었으며, 열차는 KTX 차량 모델의 제원에 맞추어 10량 1편성으로 제작된 모형을 사용하였다. 터널의 다면적은 $107.9m^3$$95.1m^3$를 적용하고, 터널연장은 1km, 0.78km, 0.5km를 적용하였고, 열차속도는 275, 300, 325, 350km/h로 변화시켜 실험 하였다. 실험 장치는 유압발사 시스템으로 열차모델 유압 발사기터널모델 제동장치로 구성된다. 모형열차의 속도는 터널입구 전방 및 출구 부 갱구에서 각각 1.2m지점에서 설치한 속도 감지기에 의해서 측정되며, 터널 내부의 압력변동은 압력센서를 터널의 입구, 중앙, 출구부에 설치하여 연속적으로 측정 하였다. 측정결과 터널입구에서 발생한 압력파의 압력기울기는 터널을 전파하면서 비선형효과에 의해서 증가하거나 확산작용에 의해서 압력기울기가 감소하는 것을 알 수 있었고, 미기압파 저감 대책을 위해 터널입구에 종류별 각각 설치하여 출구부에서 발생되는 미기압파를 비교분석하여보았다.

  • PDF