Fabrication of High Aspect Ratio 100nm-scale Nickel Stamper Using E-beam Lithography for the Injection molding of Nano Grating Patterns (전자빔과 무반사층이 없는 크롬 마스크를 이용한 나노그레이팅 사출성형용 고종횡비 100nm 급 니켈 스템퍼의 제작)

  • Seo, Young-Ho;Choi, Doo-Sun;Lee, Joon-Hyoung;Je, Tae-Jin;Whang, Kyung-Hyun
    • Proceedings of the KSME Conference
    • /
    • 2004.04a
    • /
    • pp.978-982
    • /
    • 2004
  • We present high aspect ratio 100nm-scale nickel stamper using e-beam lithography process and Cr/Qz mask for the injection molding process of nano grating patterns. Conventional photolithography blank mask (CrON/Cr/Qz) consists of quartz substrate, Cr layer of UV protection and CrON of anti-reflection layer. We have used Cr/Qz blank mask without anti-reflection layer of CrON which is non-conductive material and ebeam lithography process in order to simplify the nickel electroplating process. In nickel electroplating process, we have used Cr layer of UV protection as seed layer of nickel electroplating. Fabrication conditions of photolithography mask using e-beam lithography are optimized with respect to CrON/Cr/Qz blank mask. In this paper, we have optimized e-beam lithography process using Cr/Qz blank mask and fabricated nickel stamper using Cr seed layer. CrON/Cr/Qz blank mask and Cr/Qz blank mask require optimal e-beam dosage of $10.0{\mu}C/cm^2$ and $8.5{\mu}C/cm^2$, respectively. Finally, we have fabricated $116nm{\pm}6nm-width$ and $240nm{\pm}20nm-height$ nickel grating stamper for the injection molding pattern.

  • PDF

The Characteristic Variation of Mask with Plasma Treatment (플라즈마 처리에 의한 마스크 특성 변화)

  • Kim, Jwa-Yeon;Choi, Sang-Su;Kang, Byung-Sun;Min, Dong-Soo;An, Young-Jin
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.21 no.2
    • /
    • pp.111-117
    • /
    • 2008
  • We have studied surface roughness, contamination of impurity, bonding with some gas element, reflectance and zeta potential on masks to be generated or changed during photolithography/dry or wet etching process. Mask surface roughness was not changed after photolithography/dry etching process. But surface roughness was changed on some area under MoSi film of Cr/MoSi/Qz. There was not detected any impurity on mask surface after plasma dry etching process. Reflectance of mask was increased after variable plasma etching treatment, especially when mask was treated with plasma including $O_2$ gas. Blank mask was positively charged when the mask was treated with Cr plasma etching gas($Cl_2:250$ sccm/He:20 $sccm/O_2:29$ seem, source power:100 W/bias power:20 W, 300 sec). But this positive charge was changed to negative charge when the mask was treated with $CF_4$ gas for MoSi plasma etching, resulting better wet cleaning. There was appeared with negative charge on MoSi/Qz mask treated with Cr plasma etching process condition, and this mask was measured with more negative after SC-1 wet cleaning process, resulting better wet cleaning. This mask was charged with positive after treatment with $O_2$ plasma again, resulting bad wet cleaning condition.