Concrete structures move wholly with concrete and rebar, so they endure external force, but recently the embedded rebar in concrete has been corroded by environmental, physical and chemical factors, the embedded rebar corrosion influences concrete structure to deteriorate structure capacity. To revaluate effect to deterioration of concrete structure according to corrosion of rebar, the researcher mostly examined into corrosion rebar and complex relation of concrete. In that there are flexural strength deterioration of corrosion concrete structure and the bond strength of concrete. But It has not sufficiently studied about physical characteristic of corrosion rebar itself. In this study I will compare specification of rebar through corrosion experiment with corrosion ratio of rebar according to diameter and revaluate. And will investigate the effect to strength characteristic of rebar according to corrosion ratio.
Proceedings of the Korean Institute of Building Construction Conference
/
2003.05a
/
pp.53-58
/
2003
Concrete structures move wholly with concrete and rebar, so they endure external force, but recently the embedded rebar in concrete has been corroded by environmental, physical and chemical factors. the embedded rebar corrosion influences concrete structure to deteriorate structure capacity. To revaluate effect to deterioration of concrete structure according to corrosion of rebar, the researcher mostly examined into corrosion rebar and complex relation of concrete. In that there are flexural strength deterioration of corrosion concrete structure and the bond strength of concrete. But It has not sufficiently studied about physical characteristic of corrosion rebar itself. In this study I will compare specification of rebar through corrosion experiment with corrosion ratio of rebar according to diameter and revaluate. And I will investigate the effect to strength characteristic of rebar according to corrosion ratio.
In this study, accelerated corrosion tests were conducted on concrete specimens with and without accelerated carbonation beforehand for the purpose of elucidating the effects of carbonation, cover depth, and water-cement ratio (W/C) on the reinforcement corrosion. During testing, the corrosion current between the anode steel and cathode stainless steel was measured to continuously monitor the progress of corrosion throughout the test period, thereby investigating the mechanism of reinforcement corrosion and the relationship between corrosion and crack width, as well as other parameters.
A stainless steel that contains aggressive negative ion was known to decrease the corrosion resistance. Stainless steel with super corrosion resistance was developed for improvement of corrosion resistance. Super duplex stainless steel is widely used under sever environment because of good mechanical properties and corrosion resistance. Also, Super duplex stainless steel has long life in severe environments by showing the enough strength and corrosion resistance. But duplex stainless steel is not stabilized compared to austenite stainless steel in corrosion resistance. In this study, corrosion characteristic were investigated to super duplex stainless steel with additive 0.2% nitrogen with $SiO_2$ thin films coated or no coated by sol-gel method in 3.5% NaCl. From test results, corrosion current density in the heat-treated specimen for ${\sigma}$ phase precipitation was higher than that of different heat-treated specimen. Also, $SiO_2$ colloidal-coated specimen had not occurred almost corrosion.
In order to investigate the corrosion pit occurrence and growth characteristic of M.E.F.(martensite encapsulated islands of ferrite) dual phase steel was made with a suitable heat treatment of raw material(SS41), a corrosion fatigue test was performed under rotary bending in the salt solution having a concentration from 0.01 wt percent to 3.5 wt percent. The fatigue strength of dual phase steel was remarkably decreased with an increase in concentration of salt solution; approximately from 63% to 80% in case of dual phase steel and from 40% to 71% in case of raw material. Corrosion pit occurred in the martensite phase and fatigue cracks from corrosion pits were selectively propagated in martensite phases. In the observation of corrosion pits at the origin of fatigue cracks, it had been found that corrosion pits were grown into hemispherical pits and a/c(the surface diameter, 2c and the depth, a of corrosion pit)was about 1.0-1.5regardless of the variation of salt solution concentration. The difference of corrosion pit depth growth rate was increased with an increase in concentration of salt solution according to an increase in stress level.
In this study, erosion tests and erosion-corrosion tests of Al5083-H321 aluminum alloy were conducted at various flow rates in seawater. The erosion tests were conducted at a flow rate of 0 to 20 m/s, and erosion-corrosion tests were performed by potentiodynamic polarization method at the same flow rate. Characteristic evaluation after the erosion test was conducted by surface analysis. Characteristic evaluation after the erosion-corrosion test was performed by Tafel extrapolation and surface analysis. The results of the surface analysis after the erosion test showed that surface damage tended to increase as the flow rate increased. In particular, intermetallic particles were separated due to the breakdown of the oxide film at 10 m/s or more. In the erosion-corrosion test, the corrosion current density increased as the flow rate increased. Additionally, the surface analysis showed that surface damage occurred in a vortex shape and the width of the surface damage tended to increase as the flow rate increased. Moreover, damage at 0 m/s, proceeded in a depth direction due to the growth of pitting corrosion, and the damaged area tended to increase due to acceleration of the intermetallic particle loss by the fluid impact.
Buried bronze objects are naturally corroded by their surrounding environment, which results in producing corrosion layers containing a number of constituents. Corrosion layers in stable condition protect the objects from the environment and also could provide information in terms of the objects. Characteristic and mechanism of the corrosion layers is likely to be valuable information for the conservation treatment. Many research have been conducted to figure out the formation and characteristic of the corrosion layers, but the more research should be conducted with various approach and analytical methods. Raman spectroscopy is one of the analytical methods to identify microcrystal as a compound while other analytical methods are used to identify element. Therefore, the aim of this research is to identify the characteristic of corrosion layers of both excavated bronze objects through the raman spectroscopy. Two analytical methods, which are raman spectroscopy and SEM~EDS, were used to analyse four excavated bronze bowls. In the case of bronze bowls, malachite was found from the exterior corrosion layer and albite, quartz, and microcline, which are minerals, were also found. Cuprite was detected from the interior corrosion layers illustrating slightly different spectrum due to the combined compound. Lead segregation shows the form of PbO, $PbSO_4$ and $PbCO_3$ or it replaced as cuprite. In this study, small number of samples were analysed. This research is likely to be useful information to figure out not only the characteristic of the corrosion layers but also the authenticity of the artifacts if relevant research will be conducted. Therefore, further comprehensive researches on the various archaeological objects and corrosion environment condition are required in the future.
The objective of this study was to investigate delayed oxygen evolution and localized corrosion resistance of titanium alloys by performing potentiodynamic polarization, potentiostatic polarization, and Mott-Schottky measurements. Delayed oxygen evolution was compared among titanium alloys, 316 stainless steel, and platinum. Difference in delayed oxygen evolution between titanium alloys and other metals was attributed to specific surface characteristic of each metal. Delayed oxygen evolution of titanium alloys resulted from the predominant process of ionic conduction over electronic conduction. The effect of oxygen evolution on localized corrosion of titanium alloys was investigated using electrochemical critical localized corrosion temperature (E-CLCT) technique. Mott-Schottky measurement was performed to clarify the difference in film properties between titanium alloys and stainless steels. Titanium alloys were found to have much lower donor density than stainless steels by 1/28. These results indicate that delayed oxygen evolution has little influence on the concreteness of passive film and the resistance to localized corrosion of titanium alloys.
Kim Yong-Ki;Chang Se-Ky;Oh Chang-Rok;Goo Byeong-Chun
Proceedings of the KSR Conference
/
2004.10a
/
pp.680-685
/
2004
The effects of acid rain and salt content on corrosion behavior were investigated with rolling stock structural steels be caused by environmental. Since these materials are exposed to the corrosive environments like polluted air, acid rain and sea water, it is important to investigate corrosion behaviour in various corrosive environments. The aqueous corrosion of the characteristic materials in aerated acid rain and neutral solution were studied by using immersion tests, electrochemical measurements and analytical techniques. In order to examine corrosion characteristic, structural steels were electrochemically evaluated with respect to the dissolved oxygen content, pH, chloride ion concentration.
The cavity formed by the ultrasonic generation in the fluid with the application of water cavitation peening collides into the metal surface. At this time, the surface modification effect such as the work hardening presents by the compressive residual stress formed due to the localized plastic deformation. In this investigation, the water cavitation peening technology in the distilled water with the lapse of time was applied to 5052-O aluminum alloy for aluminum ship of a high value. So, the optimum water cavitation peening time on the effect for surface hardening and anti-corrosion property was investigated. Consequently, the water cavitatin peening time on excellent hardness and corrosion resistance characteristic presented 3.5 min. and 5.0 min, respectively. The surface hardness in the optimum water cavitation peening time was improved approximately 45% compared to the non-WCPed condition. In addition, corrosion current density was decreased.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.