Thermal Properties of Copolyetherester/silica Nanocomposites

  • Baik, Doo-Hyun;Kim, Hae-Young;Kwon, Sun-Jin;Kwon, Myung-Hyun;Lee, Han-Sup;Youk, Ji-Ho;Seo, Seung-Won
    • Fibers and Polymers
    • /
    • v.7 no.4
    • /
    • pp.367-371
    • /
    • 2006
  • Thermal properties of copolyetherester/silica nanocomposites were examined by using DSC and TGA. The segmented block copolyetheresters with various hard segment structures and hard segment contents (HSC) were synthesized and their silica nanocomposite films were prepared by solution casting method. The nano-sized fumed silica particles were found to act as a nucleating agent of the copolyetheresters. The nanocomposites always showed reduced degree of supercooling or faster crystallization than the corresponding copolyetheresters. The nanocomposites also showed increased hard segment crystallinity except HSC 35 sample which had short hard segment length. In case of 2GT [poly(ethylene terephthalate)] copolyetheresters, which were not developed commercially because of their low crystallization rate, the hard segment crystallinity increased considerably. The copolyetherester/silica nanocomposites showed better thermal stability than copolyetheresters.

Mechanical Property of Segmented Block Copolyetherester Effected by Changing the Hard Segment(II) (하드 세그멘트 구조 변화가 세그멘트화 블록 코폴리에테르에스테르의 기계적 성질에 미치는 효과(II))

  • Kim, Hae-Young;Jang, Kyung-Ho;Baik, Doo-Hyun
    • Proceedings of the Korean Fiber Society Conference
    • /
    • 2003.04a
    • /
    • pp.329-330
    • /
    • 2003
  • In general, the thermoplastic elastomers have the elastic recovery property caused by phyical crosslinks after the stress is applied. Segmented block copolyetheresters also have been used as elastomers. Many$\^$l-2/ tried to improve the elastic recovery of those which are less elastic than polyurethane. We confirmed that the copolyetherester based on poly(2,6-butylene naphthalate)(PBN) ha.4 segment had the high melting temperature, whcih was useable at the broader temperature range and the one based on poly(1,3-trimethylene terephthalate)(PTT) the high crystallinity, which would be expected to get the high elastic recovery. (omitted)

  • PDF

Effect of cross-linking agents on the properties of copolyetherester elastomer (코폴리에테르에스테르 고무 탄성체의 물성에 미치는 가교제의 효과)

  • Jang, Young-Joo;Kim, Hae-Young;Baik, Doo-Hyun
    • Proceedings of the Korean Fiber Society Conference
    • /
    • 2001.10a
    • /
    • pp.355-358
    • /
    • 2001
  • Copolyetheresters are us,ed as an engineering thermoplastic elastomer due to their excellent mechanical properties, thermooxidative stability up to high temperatures and a good resistance against many chemicals. However, fibers made from the copolyetheresters exhibited elastic recovery of about 80-85% after being stretched 200%, while spandex fibers usually showed 90-95% recovery. (omitted)

  • PDF

Effect of cross-linking agents on the properties of copolyetherester elastomer(II) (코폴리에테르에스테르 고무 탄성체의 물성에 미치는 가교제의 효과(II))

  • Jang, Young-Joo;Kim, Hae-Young;Baik, Doo-Hyun
    • Proceedings of the Korean Fiber Society Conference
    • /
    • 2002.04a
    • /
    • pp.301-304
    • /
    • 2002
  • In the prior work,$\^$l)/ we introduced several chemical cross-linking agents in order to improve elastic recovery of copolyetheresters, but we are confronted by two difficulties. The first is that cross-linking agents interfere with crystal growth which acts as a physical interlocking. The second is that strain at breaking decreases with the amount of cross-linking agent. It is considered that the chemical interlocking parts couldn't be deformed like crystalline phase. (omitted)