• Title/Summary/Keyword: Compressive test

Search Result 3,609, Processing Time 0.037 seconds

Quality Evaluation and Mix Proportion of Antiwashout Underwater Concrete with Mineral Admixture (광물질 혼화재료를 사용한 수중불분리성 콘크리트의 배합 및 품질평가 방안 검토)

  • Park, Yong Kyu;Kim, Hyun Woo;Yoon, Ki Woon
    • Journal of the Korea Concrete Institute
    • /
    • v.26 no.6
    • /
    • pp.679-686
    • /
    • 2014
  • In this research, the mix proportion of the antiwashout underwater concrete with the mineral admixture was evaluated. It can reduce the amount used of the antiwashout admixture (hereinafter referred to as "AWA") and satisfy the properties of concrete. In addition, the review for the difference of the test and practical affairs were conducted. Optimized unit quantity of water of antiwashout underwater concrete and the amount used of AWA was revealed by $190kg/m^3$, 0.9%/W, respectively. In particularly, the mix design is reduced by 5% than the W/B of target strength even though the W and AWA reduced. Therefore, it will have the economical feasibility and qualities including the material separation, resistance characteristic and compressive strength, and etc. The stable value was shown in 1 point of minute passed in the measurement of the turbidity amounts using the turbidimeter after the checker insertion. However, it needs to be reviewed for the interrelationship between turbidity measuring machine and KCI-AD102 standard method. There were no significant differences of compressive strength of specimens in the water depending on the production methods.

Durability Characteristics of Ternary Cement Matrix Using Ferronickel Slag According to the Alkali-Activators (알칼리 활성화제 종류별 페로니켈슬래그를 사용한 3성분계 시멘트 경화체의 내구특성)

  • Cho, Won-Jung;Park, Eon-Sang;Jung, Ho-Seop;Ann, Ki-Yong
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.8 no.2
    • /
    • pp.190-197
    • /
    • 2020
  • This paper evaluates the mechanical properties and durability of cement matrix blended with mineral admixtures and ferronickel slag(FNS) powder which is an industrial b y-product during ferronickel smelting process. The hydration heat, pore structure, compressive strength, length change, rapid chloride penetration test(RCPT), and freezing and thawing resistance of ternary blended cement matrix were investigated and compared with ordinary portland cement matrix. The result showed that the compressive strength of ternary blended cement matrix using ferronickel slag powder and mineral mixture was low in strength compared to the reference concrete, but recovered to a certain extent by using alkali activator. Length change of cement mortar using FNS powder have shown less shrinkage occurs than the reference specimen. In addition, irrespective of using the alkali-activators, all ternary mix are indicative of the 'very low' range for chloride ion penetrability according to the ASTM C 1202, and the freeze-thaw resistance also showed excellent results.

Mechanical Properties of Concrete Using Recycled Coarse Aggregate from Nuclear Power Plant Simulated Concrete (원자력발전소 모의 콘크리트로부터 생산된 순환 굵은 골재 활용 콘크리트 역학적 특성)

  • Lee, Seong-Cheol;Shin, Kyung-Joon;Kim, Chang-Lak
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.8 no.2
    • /
    • pp.167-174
    • /
    • 2020
  • Many researches have been conducted to utilize recycled aggregates in Korea, but since most sources of recycled aggregates are not clear, there is a lot of uncertainty in applying the existing research results on recycle of aggregates generated from nuclear power plants. In this study, therefore, in order to investigate the possibility of recycling coarse aggregates generated through dismantling of nuclear power plants in Korea, recycled coarse aggregates were produced from concrete simulating nuclear power plants in Korea. Using the recycled coarse aggregates, concrete was mixed in consideration of the mixing ratio of the recycled coarse aggregates, and the mechanical properties were experimentally investigated. From the test results, as the mixing ratio of recycled coarse aggregates increased. concrete compressive strength, tensile strength, and elastic modulus generally decreased up to 36, 37, and 27% from the mechanical properties of normal concrete, respectively. Therefore, it can be concluded that limitation on the mixing ratio of recycled coarse aggregates is necessary when coarse aggregates are recycled through dismantling of nuclear power plants.

The Property Evaluation of the Marine Concrete Structure Constructed in the Period of Japanese Occupancy (YoungDo Bridge) (일제시대 건설된 해양 콘크리트구조물의 물성 평가(영도대교))

  • Park, Dong-Cheon;Ahn, Jae-Cheol
    • Journal of Navigation and Port Research
    • /
    • v.37 no.2
    • /
    • pp.165-171
    • /
    • 2013
  • YoungDo bridge is the first suspension bridge in Busan which experienced several times repair and reinforcement after completion in 1934. The bridge is under demolition for extension and restoration work since 2011. The purpose of this research is to establish data base about modern concrete. The mix design of the concrete is like that cement : fine aggregate : coarse aggregate = 1 : 2 : 4 or 1 : 3 : 6 by the parts. The compressive strength is in the ranges from 50 to 55 MPa and the elastic modulus is in the ranges from 25 to 35 GPa. From the fact that the deviation is less than 10 %, considerably high quality control was conducted in those days. The carbonation depth is 5.92 cm at the bridge post and 14.3 cm at the machine room. That is why ocean environment keeps the high humidity. The diffusion coefficient of chloride ion through the pores in concrete is 1.052e-12 $m^2/s$ from the regression analysis using the experiment data. The water cement ration is estimated at approximately 35 % in case if the concrete using ordinary Portland cement.

The Properties of Multi-Component Blended High Fluidity Mortar (다성분계 고유동 모르타르의 특성)

  • Kim, Tae-Wan;Kang, Choonghyun;Bae, Ju-Ryong;Kim, In-Tae
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.22 no.2
    • /
    • pp.124-132
    • /
    • 2018
  • This research presents the results of an investigation on the characteristic of multi-component blended high fluidity mortars. The binder was blended ordinary Portland cement(OPC), ground granulated blast furnace slag(GGBFS), calcium sulfoaluminate(CSA) and ultra rapid setting cement(URSC). The GGBFS was replaced by OPC from 30%(P7 series), 50%(P5 series) and 70%(P3 series), CSA and URSC was 10% or 20% mass. The superplasticizer of polycarboxylate type were used. A constant water-to-binder ratio(w/b)=0.35 was used for all mixtures. Test were conducted for mini slump, setting time, V-funnel, compressive strength and drying shrinkage. According to the experimental results, the contents of superplasticizer, V-funnel and compressive strength increases with an increase in CSA or URSC contents for all mixtures. Moreover, the setting time and drying shrinkage ratio decrease with and increase in CSA or URSC. CSA decreased dry shrinkage but URSC had less effect. However, the mixed binders of CSA and URSC had a large effect of reducing drying shrinkage by complementary effect. This is effective for improving the initial strength of URSC, and CSA is effective for the expansion and improvement of long-term strength.

A Study on the Reinforcement of Bridge Foundation in the Limestone Cavity (석회암 공동지역의 교량기초 보강에 관한 연구)

  • Lee, Sang-Chul;Ryu, Chang-Yeol;Cho, Kook-Hwan
    • Journal of the Korean Society of Hazard Mitigation
    • /
    • v.11 no.1
    • /
    • pp.51-57
    • /
    • 2011
  • Irregular distributions of limestone cavity in Gang-Won province area may cause unexpected accidents from reduced serviceability or failure of structure. It is requested that an appropriate ground reinforcement method should be used to improve bearing capacity of structure, and the method should also be satisfied with environmental requirements. Among several methods used for foundation constructions in cavity area, Rod Jet Pile(RJP) method has been widely used. While the RJP method was used to improve bearing capacity for the railway bridge foundations, water pollutions of drinking water as well as fishery located adjacent to this project area were occurred. The main reason of the water pollution was cement runoff used in cement mortar during injecting material in RJP method. Laboratory tests were performed to prevent water pollution. The compaction mortar method using low movable material was selected for this project. The quality of water at a fishery adjacent to the site and the compressive strength of cores taken from the construction site were measured. Test results show that the water pollutions was minimized, and the average compressive strength of foundation material was over 5 MPa. As a result of this study, compaction mortar method can be used to ensure the bearing capacity of foundation and to prevent environment pollutions.

A Study on Microstructure and Mechanical Properties of TiC/Steel Composites Fabricated by Powder Metallurgy Process (분말야금공정으로 제조된 TiC/steel 금속복합재료의 미세조직 및 기계적 물성 연구)

  • Lee, Jihye;Cho, Seungchan;Kwon, Hansang;Lee, Sang-Kwan;Lee, Sang-Bok;Kim, Daeha;Kim, Junghwan
    • Composites Research
    • /
    • v.34 no.5
    • /
    • pp.311-316
    • /
    • 2021
  • In this study, TiC/steel metal matrix composites were fabricated by powder metallurgy process using Fealloy powders with 3 wt.% Cr and 10 wt.% Cr, respectively, as matrix material. Subsequently, the composite samples were heat treated by the annealing and quenching-tempering(Q-T), respectively, to understand the effect of heat treatment on the mechanical properties of the composites. The correlation between microstructure and structural strength depending on the chromium content and the heat treatment conditions was studied through tensile, compressive, and transverse rupture test and microstructural analysis. In the case of TiC/steel composite containing 10 wt.% Cr, the tensile strength and transverse rupture strength at room temperature were significantly lowered by the influence of coarse chromium carbide formed at the TiC/steel interface. On the other hand, both TiC/steel composites containing 3 wt.% Cr and 10 wt.% Cr showed much higher compressive strength of about 4 GP after quenching-tempering compared to the annealed specimens regardless of the presence of the chromium carbide.

A Study on Strength and Durability of Vibrated and Rolled Method Mortar Mixed with Desulfurized Gypsum and Ferronickel Slag Fine Powder (탈황석고와 페로니켈슬래그 미분말을 혼합한 진동전압방식 모르타르의 강도 및 내구성에 관한 연구)

  • Yoo, Jeong-Hwan;Park, Sang-Soon
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.9 no.4
    • /
    • pp.545-552
    • /
    • 2021
  • In this study, strength and durability evaluations are performed on vibrated-rolled method mortar mixtures containing desulfurized gypsum and ferronickel slag powder. Desulfurized gypsum and ferronickel slag fine powders were substituted for 25% limestone fine powders u sed in the manu factu re of VR tu bes, and mortar specimens were prepared u sing vibrated-rolled method. Accordingly, flexural and compressive strengths were performed to evaluate the strength, and chlorine ion penetration resistance and sulfuric acid resistance tests were performed to evaluate durability. Flexural and compressive strength were improved in the range 20 to 60% of desu lfu rized gypsu m among admixtu res, and the amou nt of passing charge decreased in the choride ion penetration resistance test in the range of 20 to 80% of desulfurized gypsum. As for the resistance to su lfu ric acid, when the proportion of desu lfu rized in the admixtu re was 40%, the strength and weight change rate according to the immersion period was reduced. Appropriate use of desulfurized gypsum and ferronickel slag powder is expected to improve performance in terms of strength and durability.

Strength Characteristics of Sedimentary Rock in Daegu-Gyungbuk Area Followed by Saturation and Crack Initiation (대구경북지역 퇴적암의 포화 및 균열 유발에 따른 강도 특성)

  • Park, Sung-Sik;Kim, Seong-Heon;Bae, Do-Han
    • Journal of the Korean Geotechnical Society
    • /
    • v.34 no.12
    • /
    • pp.29-42
    • /
    • 2018
  • Shale and mudstone in Daegu-Gyungbuk area have low strength and resistance to weathering compared to other rocks. Therefore, it is necessary to evaluate their strength depending on the degree of saturation and crack development. In this study, shales and mudstones were collected from several construction sites in Daegu-Gyungbuk area. Their basic material properties such as porosity, SEM, chemical component, and durability were tested. A porosity (absorptivity) of mudstone was 31% (25%), which was 6 (8) times higher than that of shale. Some mudstone was easily disintegrated with water and it consisted of highly-active clay mineral such as smectite type. These rocks were prepared by small cube specimens for unconfined compression test. An unconfined compressive strength of dry rock was compared with saturated one. Microwave oven was operated step by step to stimulate void water within a saturated rock, which resulted into high temperature and micro crack initiation within rocks. A strength of microwaved rocks was compared with operation time and crack initiation. As a result, the average unconfined compressive strength of dry and saturated shale was 62 and 33 MPa, respectively. The strength of mudstone for each condition was 11 and 4 MPa. When a rock became saturated, its strength decreased by 47% and 64% for shale and mudstone at average. In addition to saturation, a rock was in the microwave for 15 secs, its strength decreased into 49% for shale and 52% for mudstone. When a microwave oven operated up to 20 sec, a rock was crushed into several pieces and its temperature was approximately 200 degrees.

Physiochemical Characteristics and its Applicable Potential of Blast Furnace Slag Grout Mixtures of Sodium Silicate and Calcium Hydroxide (규산소다 및 수산화칼슘을 적용한 고로슬래그 그라우트의 적용성 및 물리화학적 특성)

  • Kim, Joung-Souk;Yoon, Nam-Sik;Xin, Zhen-Hua;Moon, Jun-Ho;Park, Young-Bok;Kim, Young-Uk
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.20 no.1
    • /
    • pp.200-207
    • /
    • 2019
  • Cement is one of the most commonly used materials in the construction and civil engineering industry. However, emissions of carbon dioxide generated during the production of cement have been linked to climate change and environment pollutants. In order to replace cement, many studies have been actively performed research to utilizing Blast Furnace Slag(BFS), which is a byproduct of the steel industry. This study aims to investigate the physiochemical properties of the BFS powder based grout to determine whether it can be used as an environment-friendly grout material. As a fine powder, BSF can be used instead of cement grout due to its potential hydraulic property. BSF has also been known for its ability to strengthen materials long-term and to densify the internal structure of concrete. In order to investigate the physicochemical properties of the BFS powder based grout as a grout material, in this study assessment tests were performed through a gel-time measurement, uniaxial compressive strength, and chemical resistance tests, and heavy-metal leaching test. Characteristics and advantages of the slag were studied by comparing slag and cement in various methods.