  • In this paper, when the silk fabric was modified by ethylene cyanohydrine, the reaction mechanism between both was studied at various treatment conditions such as curing temperatures and times, ethylene cyanohydrin concentrations and $ZnCl_2$ concentrations. Through the FT-IR and DSC analyses of the treated silk fabrics, we found the results as follows : It was observed in FT-IR analysis of the treated silk fabrics that the -OH characteristic peak($3,450cm^{-1}$)position and shape were all changed when drying and curing treatment conditions were at $80^{\circ}C$ for 3 minute and $110^{\circ}C$ for 2.5 minute, and the concentration of the $ZnCl_2$ was 0.1%. It indicated that the -OH group of the silk participated in the reaction between the silk fabric and ethylene cyanohydrin. From the DSC analysis, it was found that the pyrolysis temperatures of the treated silk fabrics by ethylene cyanohydrin which was processed in the same condition, were all increased from $311^{\circ}C$ to ab. $320^{\circ}C$. From the FT-IR analyses of the silk fabrics treated by ethylene cyanohydrin at the various concentrations of $ZnCl_2$, it was found that the -OH characteristic peaks($3,450cm^{-1}$) were similar to the nontreated one except that of the fabric treated at the $ZnCl_2$ conconcentration of 0.8% when drying and curing treatment conditions were at $80^{\circ}C$ for 3minute and $110^{\circ}C$ for 2.5 minute, and the concentration of the ethylene cyanohydrin was 5%. In the case of the $ZnCl_2$ concentration of 0.8% solution, a lot of change were observed in peak. From the DSC analysis of the treated silk fabrics which was processed in the same condition, it was showed that the pyrolysis temperatures of treated silk fabric were all increased from $311^{\circ}C$ to ab. $320^{\circ}C$, which was no relation with the concentration of $ZnCl_2$.

  • PDF