Temperature-Dependent Mn Substitution Effect on LiNiO2

  • Seungjae Jeon;Sk. Khaja Hussain;Jin Ho Bang
    • Journal of Electrochemical Science and Technology
    • /
    • v.15 no.1
    • /
    • pp.161-167
    • /
    • 2024
  • Despite the important role of manganese (Mn) in cobalt-free, Ni-rich cathode materials, existing reports on the effects of Mn as a substitute for cobalt are not consistent. In this work, we analyzed the performance of cathodes comprised of Li(Ni1-xMnx)O2 (LNMO). Both beneficial and detrimental results occurred as a result of the Mn substitution. We found that a complex interplay of effects (Li/Ni mixing driven by magnetic frustration, grain growth suppression, and retarded lithium insertion/extraction kinetics) influenced the performance and was intimately related to calcination temperature. This indicates the importance of establishing an optimal reaction temperature for the development of high-performance LNMO.

Designing of a Novel Core-Shell-Structured Co-free Cathode Material with Enhanced Thermal and Structural Stability for Lithium Ion Batteries

  • Shin, Ji-Woong;Nam, Yun-Chae;Son, Jong-Tae
    • Journal of the Korean Electrochemical Society
    • /
    • v.22 no.4
    • /
    • pp.172-176
    • /
    • 2019
  • The first commercialized cathode material, $LiCoO_2$, suffers from disadvantages such as high cost and toxicity and also possesses safety problems. The nickel-rich $LiNi_{0.9}Mn_{0.1}O_2$ cathode material, used as an alternative to $LiCoO_2$, has highly reversible capacity and high energy density. So, the nickel-rich $LiNi_{0.9}Mn_{0.1}O_2$ cathode material is widely used as an alternative to $LiCoO_2$ due to its highly reversible capacity and high energy density. However, $LiNi_{0.9}Mn_{0.1}O_2$ has several disadvantages as well, such as poor cycle performance and poor thermal instability. To address these problems, we synthesized a new material, $LiNi_{0.5}Mn_{0.5}O_2$, as a shell on the surface of a core to suppress the surface degradation. The new material showed high structural and thermal stabilities and could also maintain a high capacity. The capacity retention of the core-shell cathode (87.7%) was better than that of the core cathode (76.9%) after 50 cycles. Analysis using differential scanning calorimetry revealed that the heat generation in the core-shell cathode ($65.9Jg^{-1}$) was lower than that in the core cathode ($559.7Jg^{-1}$).

Development of Cobalt-free $La_xSr_{4-x}Fe_6O_{13}$ ($0{\leq}x{\leq}2$) Intergrowth Cathode Material for Solid Oxide Fuel Cells

  • Lee, Seung-Jun;Yong, Seok-Min;Kim, Dong-Seok;Kim, Do-Gyeong
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2011.05a
    • /
    • pp.45.1-45.1
    • /
    • 2011
  • Cobalt-free $La_xSr_{4-x}Fe_6O_{13}$ ($0{\leq}x{\leq}2$) oxide have been synthesized and investigated as a potential cathode material for solid oxide fuel cells (SOFCs). $Sr_4Fe_6O_{13}$ consists of alternating perovskite layers ($Sr_4Fe_2O_8$) containing iron cations in octahedral oxygen coordination and $Fe_4O_5$ layers where iron cations have 5-fold coordination of two types-square pyramids and trigonal bipyramids. Our preliminary electrochemical testes of pristine $Sr_4Fe_6O_{13}$ show a rather high area specific resistance ($0.47{\Omega}cm^2$ at $700^{\circ}C$) for ~20 ${\mu}m$ thick layers with CGO electrolyte. The electrochemical performances are improved by La addition up to x=1 ($La_1Sr_3Fe_6O_{13}$, $0.06{\Omega}cm^2$ at $700^{\circ}C$). In addition, thermal expansion coefficient (TEC) values of $La_1Sr_3Fe_6O_{13}$ specimen demonstrated $15.1{\times}10^{-6}\;^{\circ}C^{-1}$ in the range of 25-900$^{\circ}C$, which provides good thermal expansion compatibility with the CGO electrolyte. An electrolyte supported (300-${\mu}m$-thick) single-cell configuration of $La_1Sr_3Fe_6O_{13}$/CGO/Ni-CGO delivered a maximum power density of 584 $mWcm^{-2}$ at $700^{\circ}C$. In addition, an anode supported single cell by YSZ electrolyte (10-${\mu}m$-thick) with a porous CGO interlayer between the cathode and the electrolyte to avoid undesired interfacial reactions exhibited 1,517 $mWcm^{-2}$ at $800^{\circ}C$. The unique composition of $La_1Sr_3Fe_6O_{13}$ with low thermal expansion coefficient and higher electrochemical properties could be a good cathode candidate for intermediate temperature SOFCs with CGO and YSZ electrolyte.