• Title/Summary/Keyword: Coated tool

Search Result 258, Processing Time 0.022 seconds

The Effect of TiAlN coated Ball End Mill on Cutting characteristic of High Hardness Steels in Dry Condition (초경 볼 엔드밀의 TiAlN 코팅 처리조건이 건식가공환경에서 고경도 강재의 절삭 특성에 미치는 영향)

  • Park D. S.;Won S. T.;Lee Y. J.;Hur J. H.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2005.10a
    • /
    • pp.344-349
    • /
    • 2005
  • This paper is studied on the effect of TiAlN coated ball end mill on cutting characteristic of high hardness steels in dry cutting condition without coolant. KP4 steels[HRC32] and STD11[HRC60] heat treated steels wert: used as the workpiece and WC-Co ball end mill and single and multi layer TiAlN coated ball end mill were utilized. Results showed that TiAlN coated ball end mill were increased the cutting length than WC-Co ball end mill in the cutting speed$[245\~320m/min]$ about $2\~5$ times for KP4 steels and about $2.7\~4.3$ times for STD11 heat treated steels. The multi layer TiAlN coated ball end mill is good about $1.2\~1.7$ times for KP4 steels and STD11 steels than single layer coated.

  • PDF

Development and validation of FRAT code for coated particle fuel failure analysis

  • Jian Li;Ding She;Lei Shi;Jun Sun
    • Nuclear Engineering and Technology
    • /
    • v.54 no.11
    • /
    • pp.4049-4061
    • /
    • 2022
  • TRISO-coated particle fuel is widely used in high temperature gas cooled reactors and other advanced reactors. The performance of coated fuel particle is one of the fundamental bases of reactor safety. The failure probability of coated fuel particle should be evaluated and determined through suitable fuel performance models and methods during normal and accident condition. In order to better facilitate the design of coated particle fuel, a new TRISO fuel performance code named FRAT (Fission product Release Analysis Tool) was developed. FRAT is designed to calculate internal gas pressure, mechanical stress and failure probability of a coated fuel particle. In this paper, FRAT was introduced and benchmarked against IAEA CRP-6 benchmark cases for coated particle failure analysis. FRAT's results agree well with benchmark values, showing the correctness and satisfactory applicability. This work helps to provide a foundation for the credible application of FRAT.

Wear Behavior of TiN Coatings Deposited on High Speed Steel and Alloy Tool Steel (TiN 코팅된 고속도강과 합금공구강의 마멸거동)

  • 김석삼;서창민;박준목
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.19 no.3
    • /
    • pp.705-712
    • /
    • 1995
  • The wear characteristics and wear mechanisms in TiN coating deposited on high speed steel and alloy tool steel by ion plating were investigated. Pin on V-block wear tester was used for a wear test method. The specimen was composed of three kinds of high speed steel and alloy tool steel which had different hardness by changing the heat treating condition. Three kinds of coating thickness were also applied to each specimen. Microscopic observation of worn surfaces was made by SEM. The scratch test of coating surface by the ion plating showed that critical load to break the coating interface was greater than 50N. The critical load increased with both substrate hardness and coating thickness. The wear resistance of TiN coated high speed steel became 10 times greater than that of non-coated ones. SEM observation showed that leading edge of contact was compressive and trailing edge was under maximum tensile stress and then surface cracking broke out perpendicular to sliding direction.

Regression Equation Deduction for Cutting Force Prediction during Interrupted Cutting of Carbon Steel for Machine Structure (SM45C) (기계구조용 탄소강(SM45C)의 단속절삭 시 절삭력예측을 위한 회귀방정식 도출)

  • Bae, Myung-Il;Rhie, Yi-Seon
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.15 no.4
    • /
    • pp.40-45
    • /
    • 2016
  • Interrupted cutting has different cutting characteristics compared with continuous cutting. In interrupted cutting, the workpiece has a groove that regularly impacts the cutting tool and workpiece. Therefore, tool damage occurs rapidly, and this increases the cutting force and surface roughness. In this study, we performed interrupted cutting of carbon steel for machine structure (SM45C) using a coated carbide tool (TT7100). To predict the cutting force, we analyzed the experimental results with a regression analysis. The results were as follows: We confirmed that the factors affecting the principal force and radial force were cutting speed, depth of cut, and feed rate. From the multi-regression analysis, we deduced regression equations, and their coefficients of determination were 89.6, 89.27, and 28.27 for the principal, radial, and feed forces, respectively. This means that the regression equations were significant for the principal and radial forces but not for the feed force.

The Effect of TiAlN coated Ball End Mill and MQL Cutting Condition on Cutting characteristic of High Hardness Steels (고경도 강재의 MQL 가공시 초경 볼 엔드밀의 TiAlN 코팅 조건이 절삭 특성에 미치는 영향)

  • Park D. S.;Won S. T.;Lee Y. J.;Hur J. H.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2004.10a
    • /
    • pp.245-251
    • /
    • 2004
  • This paper is studied on the effect of TiAlN coated Ball End Mill and MQL(Minimum Quantity Lubrication) cutting condition on cutting characteristic of high hardness steels. KP4 steels[HRC32] and STD11[HRC60] heat treated steels were used as the workpiece and WC-Co ball end mill and single and multi layer TiAlN coated ball end mill were utilized in the cutting tests. MQL device was used to spray botanical oil coolant. Result showed that TiAlN coated ball end mill were increased the cutting length than WC-Co ball end mill in the cutting speed[$245{\sim}320m/min$] about $2.3{\sim}5.7$ times for KP4 steels and about $2.5{\sim}4.3$ times far STD11 heat treated steels. The multi layer TiAlN coated ball end mill is good for KP4 steels than single layer coated.

  • PDF

The effect of particle size on tool wear of SiCp-reinforced metal matrix composite

  • Sahin, Y.;Sur, G.
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 2002.10b
    • /
    • pp.237-239
    • /
    • 2002
  • The effect of particle sizes of the metal matrix composites containing 10 wt.%SiCp was investigated with using various tools. The results showed that tool life decreased considerably with increasing particle size and cutting speed. The wear resistance of TiC-coated tools was considerably higher than that of the other tools. It was observed that abrasive wear was the main responsible mechanism for wear of the tool thermal cracks were at high speed while a built-edge formation was also evident at lower speed.

  • PDF

Optimal Air Jet System Design for the Turning of Hardened Material (고경도재료 선삭시 최적 에어제트 냉각시스템 설계)

  • 정보구
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 1996.04a
    • /
    • pp.58-62
    • /
    • 1996
  • In case of hard turning, tool wear is acclerated by heat. So we intend to decrease tool wear by using an air-jet cooling system. Before constructing the air-jet cooling system, no chipping conditions were selected through a statistical method, so called 'Taguchi method', and then the air-jet cooling system was developed by synthesizing and analyzing the results of experimental data through Taguchi method. The air-jet cooling system actually reduced flank wear of TiN coated tool by 25%.

  • PDF

Machinability investigation and sustainability assessment in FDHT with coated ceramic tool

  • Panda, Asutosh;Das, Sudhansu Ranjan;Dhupal, Debabrata
    • Steel and Composite Structures
    • /
    • v.34 no.5
    • /
    • pp.681-698
    • /
    • 2020
  • The paper addresses contribution to the modeling and optimization of major machinability parameters (cutting force, surface roughness, and tool wear) in finish dry hard turning (FDHT) for machinability evaluation of hardened AISI grade die steel D3 with PVD-TiN coated (Al2O3-TiCN) mixed ceramic tool insert. The turning trials are performed based on Taguchi's L18 orthogonal array design of experiments for the development of regression model as well as adequate model prediction by considering tool approach angle, nose radius, cutting speed, feed rate, and depth of cut as major machining parameters. The models or correlations are developed by employing multiple regression analysis (MRA). In addition, statistical technique (response surface methodology) followed by computational approaches (genetic algorithm and particle swarm optimization) have been employed for multiple response optimization. Thereafter, the effectiveness of proposed three (RSM, GA, PSO) optimization techniques are evaluated by confirmation test and subsequently the best optimization results have been used for estimation of energy consumption which includes savings of carbon footprint towards green machining and for tool life estimation followed by cost analysis to justify the economic feasibility of PVD-TiN coated Al2O3+TiCN mixed ceramic tool in FDHT operation. Finally, estimation of energy savings, economic analysis, and sustainability assessment are performed by employing carbon footprint analysis, Gilbert approach, and Pugh matrix, respectively. Novelty aspects, the present work: (i) contributes to practical industrial application of finish hard turning for the shaft and die makers to select the optimum cutting conditions in a range of hardness of 45-60 HRC, (ii) demonstrates the replacement of expensive, time-consuming conventional cylindrical grinding process and proposes the alternative of costlier CBN tool by utilizing ceramic tool in hard turning processes considering technological, economical and ecological aspects, which are helpful and efficient from industrial point of view, (iii) provides environment friendliness, cleaner production for machining of hardened steels, (iv) helps to improve the desirable machinability characteristics, and (v) serves as a knowledge for the development of a common language for sustainable manufacturing in both research field and industrial practice.

A Study on the High Speed Characteristics of Plastic Mould Steel using Ball End Mill AlTiN Coated Layers (볼 엔드밀 AlTiN코팅 층수에 따른 플라스틱금형강의 고속가공에 관한 연구)

  • Lee, Seung-Chul;Cho, Gyu-Jin
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.9 no.1
    • /
    • pp.81-86
    • /
    • 2010
  • This paper investigated into process characteristics of AlTiN coated layers for machining to the direction of upper and lower in plastic mold material (KP-4) with the cemented carbide ball endmill with the diameter of 8mm coated AlTiN layers (1~4) step by step using machining center. The material used in experiments was KP-4 that was machined by three types of inclined angles; $15^{\circ}$, $30^{\circ}$ and $45^{\circ}$ As estimated mechanical properties of AlTiN coated layers, it was shown the most result in the condition of three layered coating that the coating that the coating depth, the hardness of the coated layer and the surface roughness of the coated layer were $13{\mu}m$, Hv 3027.3 and $0.042{\mu}m$, respectively. The cutting component was better at the condition of upper direction than that of lower direction in all experimental conditions and indicated to be less which the bigger angle of the material was increased the effective diameter of the tool.

A Study on the Coated Characteristics of Ceramic Tools (코팅공구의 절삭성능에 관한 연구)

  • 유봉환
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.9 no.1
    • /
    • pp.96-101
    • /
    • 2000
  • Ceramic, PCD and CBN tools are available for the difficult-to-cut-materials such as hardened carbon tool steel, stainless steel, Inconel 718 and etc.. Ceramic toolsare likely to be chipped and abruptly broken before the appearance of normal wear in turning. Ther2efore ceramic tools are suitable for continuous cut in turning not for intermittent in milling. In this study, TiN/TiCN multi-layer coated ceramic tools were found to restrain the chipping, breaking and early fracture and to increase the critical cutting speed owing to TiN/TiCN multi-layer coating in Arc Ion Plating of PVD method.

  • PDF