Micro-patterning of Multi-layered Magnetic Metal Films Using Nd:YAG Laser (Nd:YAG Laser를 이용한 자성금속 막의 패턴 식각)

  • Chae, Sang-Hun;Seo, Yeong-Jun;Song, Jae-Seong;Min, Bok-Gi;An, Seung-Jun;Lee, Ju-Hyeon
    • Korean Journal of Materials Research
    • /
    • v.10 no.2
    • /
    • pp.171-174
    • /
    • 2000
  • In this study, the laser patterning of sputter-deposited amorphous CoNbZr films has been tried usig Nd: YAG laser. However, the metal film was not removed because of its high reflectance of the alser on the metal surface. To solve this problem, authors tried to screen-print a block polymer on the metal film and then irradiate the laser on the polymer. This is a new method which was suggested by this study. Using this new method, the metal films were effectively removed with the laser power of 114W even though the metal films was not removed with the laser power of 332W using the conventional method. This result leads to the conclusion that the block polymer acts as a laser energy absorbing and transferring layer.

  • PDF

Corrosion Characteristics of Titanium Alloys for Medical Implant (생체용 Ti 합금의 부식특성)

  • Han, Jun-Hyun;Lee, Kyu Hwan;Shin, Myung Chul
    • Analytical Science and Technology
    • /
    • v.9 no.2
    • /
    • pp.192-197
    • /
    • 1996
  • The purpose of this study is to develop new V-free Ti alloys which have good mechanical properties and corrosion resistance. Although pure Ti has an excellent biocompatibility and corrosion resistance in body, it is inferior to Ti alloys in mechanical properties, and Ti-6Al-4V which has good mechanical properties was known to be cytotoxic due to the alloying element V. New Ti based alloys which do not contain the toxic metallic components were developed by the alloy design technique. Their corrosion and mechanical characteristics were compared with pure Ti and Ti-6Al-4V in this study. The results showed that Ti-20Zr-3Nb-3Ta-0.2Pd-1In and Ti-5AI-4Zr-2.5Mo exhibit good mechanical oroperties and an excellent corrosion resistance in 0.9% NaCl solution.

  • PDF

Microstructures and Mechanical Properties of Beryllium(Be)-free Ni-Cr-Mo based Alloys for Metal-Ceramic Crown (베릴륨(Be)이 미 첨가된 치과도재소부용 Ni-Cr-Mo계 합금의 미세조직 및 기계적 성질 특성)

  • Song, Kyung-Woo;Go, Eun-Kyoung;Lee, Jung-Hwan;Jung, Jong-Hyun;Noh, Hak;Han, Jae-Ick
    • Journal of Technologic Dentistry
    • /
    • v.28 no.2
    • /
    • pp.321-329
    • /
    • 2006
  • The popularity of Ni-Cr-Mo based metal alloys for metal-ceramic crown have increased recently because of low price, superior yield strength and rigidity. the use of these alloys give them the potential advantage of thinner copping with the required rigidity for long span bridges. The purpose of this study was to assess the microstructures and mechanical properties of Ni-Cr-Mo-(Si,Al,Nb,Zr,Ti.Cu,Mm) based Alloys not containing beryllium(Be) related toxic effects. The abtained results indicated that as-cast these specimen alloys showed compositional and microstructural differences, and mechanical properties values of Ni69Cr20Mo5Si2Al4 alloy among these specimen alloys was found to be superior to those of commercial Ni-Cr based alloy using in market place today.

  • PDF

Thermal Stability of $\textrm{Fe}_{80-x}\textrm{P}_{10}\textrm{C}_{6}\textrm{B}_{4}\textrm{M}_{x}$(M=Transition Metal) Amorphous Alloys ($\textrm{Fe}_{80-x}\textrm{P}_{10}\textrm{C}_{6}\textrm{B}_{4}\textrm{M}_{x}$(M=Transition Metal) 비정질합금의 열적안정성)

  • Guk, Jin-Seon;Jeon, U-Yong;Jin, Yeong-Cheol;Kim, Sang-Hyeop
    • Korean Journal of Materials Research
    • /
    • v.7 no.3
    • /
    • pp.218-223
    • /
    • 1997
  • At the aim of finding a Fehased amorphous alloy with a wide supercooled liquid region (${\Delta}T_{x}=T_{x}-T_{g}$) before crystallization, the changes in glass transition temperatudfI$T_{g}$ and crystallization temperature ($T_{x}$) by the dissolution of additional M elements were examined for the $Fe_{80}P_{10}C_{6}B_{4}$(x~6at%. M= transition metals) amorphous alloys. The ${\Delta}T_{x}$ value is 27K for the Fe,,,P,,,C,,R, alloy and increases to 40K for the addition of M=4at%Hf, 4at%Ta or 4at%Mo. The increase in ${\Delta}T_{x}$ is due to the increase of $T_{x}$ exceeding the degree in the increase in $T_{g}$. The $T_{g}$ and $T_{x}$ increase with decreasing electron concentration (e/a) from about 7 38 to 7.05. The decrease of e/a also implies the increase in the attractive bonding state between the M elements and other constitutent elements. It is therefore said that $T_{g}$ and $T_{x}$ increase kith increasing attractive bonding force.