• 제목/요약/키워드: Co-Cr dental alloy

검색결과 73건 처리시간 0.096초

도재용착용 Ni-Cr계 합금의 이트륨 첨가물이 도재전단결합강도에 미치는 영향 (Effect of yttrium additives on the shear bond strength of porcelain fused to Ni-Cr alloy for porcelain fused metal crown)

  • 우제승;노세라;노형록;임청하;이정환
    • 대한치과기공학회지
    • /
    • 제41권2호
    • /
    • pp.71-80
    • /
    • 2019
  • Purpose: In this study, to evaluate the effect of oxide changes on the shear bond strength according to the composition of Ni-Cr alloys for porcelain fused matal crown, T-4 alloys, Zeroy alloys and Zeroy-X alloys were selected. Methods: 20 specimens were fabricated using selected Ni-Cr alloys and porcelain powders. A Ni-Cr alloy having a diameter of 5 mm and a height of 25 mm was produced and the metal surface was polished. Porcelain powder was fired on the polished metal surface to a diameter of 5 mm and a height of 3 mm. The experiment group consisted of three groups, T-4(TNA), Zeroy(ZNA) and Zeroy-X(ZXA). The fabricated specimens were mounted on a jig of a universal testing machine(UTM) and fracture strength was measured by applying a shear force at a UTM crosshead speed of 0.5 mm/min. The fracture strength was calculated as the bond strength between the porcelain and the alloy. The surface of the fractured alloy was analyzed by X-ray diffraction(XRD) and scanning electron microscopy(SEM), and the components of the oxide were measured by energy dispersive X-ray spectroscopy(EDX) line profile method. Results: In SEM, XRD and EDX analysis, yttrium tended to increase the mechanical and chemical bonding forces. The shear bond strength of ZXA group containing yttrium showed the highest value at 27.53 MPa. Conclusion: Based on the results of this study, it is considered that the yttrium-added Ni-Cr alloy is clinically acceptable in porcelain shear bond strength.

Comparison of the bond strength of ceramics to Co-Cr alloys made by casting and selective laser melting

  • Lawaf, Shirin;Nasermostofi, Shahbaz;Afradeh, Mahtasadat;Azizi, Arash
    • The Journal of Advanced Prosthodontics
    • /
    • 제9권1호
    • /
    • pp.52-56
    • /
    • 2017
  • PURPOSE. Considering the importance of metal-ceramic bond, the present study aimed to compare the bond strength of ceramics to cobalt-chrome (Co-Cr) alloys made by casting and selective laser melting (SLM). MATERIALS AND METHODS. In this in-vitro experimental study, two sample groups were prepared, with one group comprising of 10 Co-Cr metal frameworks fabricated by SLM method and the other of 10 Co-Cr metal frameworks fabricated by lost wax cast method with the dimensions of $0.5{\times}3{\times}25\;mm$ (following ISO standard 9693). Porcelain with the thickness of 1.1 mm was applied on a $3{\times}8-mm$ central rectangular area of each sample. Afterwards, bond strengths of the samples were assessed with a Universal Testing Machine. Statistical analysis was performed with Kolmogorov-Smirnov test and T-test. RESULTS. Bond strength in the conventionally cast group equaled $74.94{\times}16.06\;MPa$, while in SLM group, it equaled $69.02{\times}5.77\;MPa$. The difference was not statistically significant ($P{\leq}.05$). CONCLUSION. The results indicated that the bond strengths between ceramic and Co-Cr alloys made by casting and SLM methods were not statistically different.

아말감과 이종(異種)금속의 거리에 따른 부식에 대한 고찰 (A Study on Corrosion according to Distance between Amalgam and Dissimilar Metals)

  • 김주원;정은경
    • 치위생과학회지
    • /
    • 제4권3호
    • /
    • pp.103-109
    • /
    • 2004
  • 본 실험은 제조회사 매뉴얼과 통법에 의해서 Amalgam 합금, Ni-Cr alloy의 Crown용 Verabond, Denture용 Talladium $^{TM}alloy$로 각각 24개의 총 72의 시편을 하악 제1대구치근 원심 치관 폭경과 임상에서의 MOD cavity를 고려하여 제작하였고 인공 타액 80ml를 담은 200ml 용 비이커에 시편을 넣어 0mm, 7mm, 40mm 거리에서 7일 후 갈바닉 부식을 측정하였다. 유리금속은 유도 플라즈마 방출 분광기(Inductively Coupled Plasma - Atomic Emission Spectrometer(ICP-AES, JY-50P, VG Elemental Co. France)로 전해액내의 Cu, Ag, Ni, Cr, Sn, Zn, Hg를 정량 분석했으며 그 결과 다음과 같은 결론을 얻었다. 첫째, Cu, Sn, Ag, Hg, Zn은 아말감이 금 합금과 접촉했을 때가 크라운용 Ni-Cr alloy와 덴쳐용 Talladium alloy 보다 아주 많이 유리 했으며 금 합금이 구강조직과 생체 적합성이 가장 좋다지만 아말감과 함께 있을 때 가장 불리 했슴을 알 수 있었다. 둘째, 아말감이 금 합금과 접촉했을 때, 금 합금의 조성에서 Ni, Cr 같은 중금속이 함유되지 않았기 때문인지 전혀 유리되지 않았으나 Sn은 조성에는 없었지만 $227.1{\pm}18.0035{\mu}g/cm^2$나 유리 되었고 Hg도 유리되었는데 이는 아말감 자체의 유리 물질임을 추측할 수 있었다. 셋째, 아말감 합금과 금 합금 사이에서의 0mm, 7mm, 40mm 거리에서는 Cu, Ag는 유의성이 있었으며 Hg는 유의성이 없었다. 이는 금합금은 절대 아말감과 같이 사용해서 안되며 이종 보철물 사이의 거리에 관계없이 사용을 금해야 하는 것으로 사료된다. 넷째, 아말감합금이 Crown용 Ni-Cr 합금과 접촉했을 때 아말감의 Ag이 유리 되지 않았으며 Zn, Ni, Sn, Hg, Cu의 순으로 유리되었다. 0mm, 7mm, 40mm 거리에 따라서 유의성이 있었다. Hg는 유리 되지 않았지만 중금속인 Ni, Cr은 유리되었고 반대 악궁이나 거리가 떨어져 있으면 접촉보다 Hg의 유리가 적었다. 다섯째, 아말감합금이 Denture용 Talladium alloy 합금과 접촉했을 때 0mm, 7mm, 40mm 거리에서도 유의성이 있었다. 0mm, 7mm, 40mm 거리에 따라서 유의성이 있었다. Hg는 유리 되지 않았지만 중금속인 Ni, Cr은 유리되었고 반대 악궁이나 거리가 떨어져 있으면 접촉보다 Hg의 유리가 적었다. 여섯째, 인공 타액에서 접촉 시 Amalgam alloy와 Gold, Verabond, Talladium alloy의 Cu, Sn, Ag, Hg, Zn, Ni, Cr의 ICPES 검사 결과 Cu, Hg가 유의성을 있었다. 일곱째, 인공타액에서 아말감합금과 두 비귀금속인 Ni-Cr alloy(crown용), Denture용 Talladium alloy가 접촉한 경우 거리에 따른 Hg, Ni, Cr의 유리 부산물에서 유의성을 확인했다.

  • PDF

용출법을 이용한 치과용 base metal alloy의 세포독성에 관한 실험적 연구 (An Experimental Study on The Cytotoxicity of Dental Base Metal Alleys by Extraction Method)

  • 윤민의;진태호;동진근
    • 대한치과보철학회지
    • /
    • 제27권2호
    • /
    • pp.123-130
    • /
    • 1989
  • In order to investigate the biocompatibility of base metal alloys in dental prosthesis, the 3 types of Ni-Cr alloys and the 3 types of Co-Cr alloys were collected and each alloy was extracted in the culture medium. L-cells derived from the subcutaneous tissue of mouse and extracted medium were cultivated. The relative growth rate of L-cells in the tissue culture was calculated with N-R assay. The obtained results were as follows: 1. In the case of the Co-Cr alloys tested, its cytotoxicity proved weak. 2. In the case of the Ni-Cr alloys tested, there was no significant degree of cytotoxicity, especially 25% Victory was proved noncytotoxicity.

  • PDF

베릴륨(Be)이 미 첨가된 치과도재소부용 Ni-Cr-Mo계 합금의 미세조직 및 기계적 성질 특성 (Microstructures and Mechanical Properties of Beryllium(Be)-free Ni-Cr-Mo based Alloys for Metal-Ceramic Crown)

  • 송경우;고은경;이정환;정종현;노학;한재익
    • 대한치과기공학회지
    • /
    • 제28권2호
    • /
    • pp.321-329
    • /
    • 2006
  • The popularity of Ni-Cr-Mo based metal alloys for metal-ceramic crown have increased recently because of low price, superior yield strength and rigidity. the use of these alloys give them the potential advantage of thinner copping with the required rigidity for long span bridges. The purpose of this study was to assess the microstructures and mechanical properties of Ni-Cr-Mo-(Si,Al,Nb,Zr,Ti.Cu,Mm) based Alloys not containing beryllium(Be) related toxic effects. The abtained results indicated that as-cast these specimen alloys showed compositional and microstructural differences, and mechanical properties values of Ni69Cr20Mo5Si2Al4 alloy among these specimen alloys was found to be superior to those of commercial Ni-Cr based alloy using in market place today.

  • PDF

비귀금속 산화물이 치과용 합금과 도재의 화학적 결합에 미치는 영향 (Effects of Nonprecious Metallic Oxide on the Chemical Bonding Between Dental Alloy and Porcelain)

  • 김광남;조성암
    • 대한치과보철학회지
    • /
    • 제25권1호
    • /
    • pp.317-325
    • /
    • 1987
  • A study on the shear bonding strength between dental alloy and porcelain according to various kidns of sputtered metallic thin films was established by Ingtron universal testing machine, and the change of the elemental weight % at the surface of dental alloy was studied by E.D.S. The kind of metallic thin films were Al, Ni, In, Cr. Ti and Sn with $0.3{\mu}m$ thickness. The dental alloys were Verabond made by Aalba Dent. Co. and Degudent H manufactured by Degussa Co. The control groups were Verabond and Degudent H. The obtained results were as follows; 1. The shear bonding strength of Al plated sample was the strongest of all. 2. The shear bonding strength of Ni plated sample was stronger than that of Degudent H, Sn plated samples. 3. The shear bonding strength of Verabond was weaker than that of Al, Ni, In, Cr, plated samples. 4. After degassing, it is more weight % of Ni at the alloy surface of the Ni sputtered specimen than the Sn sputtered sample.

  • PDF

The effect of repeated porcelain firings on corrosion resistance of different dental alloys

  • Tuncdemir, Ali Riza;Karahan, Ismail;Polat, Serdar;Malkoc, Meral Arslan;Dalkiz, Mehmet
    • The Journal of Advanced Prosthodontics
    • /
    • 제5권1호
    • /
    • pp.44-50
    • /
    • 2013
  • PURPOSE. The aim of this study was to evaluate the effects of repeated porcelain firing process on the corrosion rates of the dental alloys. MATERIALS AND METHODS. Cr-Co, Cr-Ni and Pd-Ag alloys were used for this study. Each metal supported porcelain consisted of 30 specimens of 10 for 7, 9 and 11 firing each. Disc-shaped specimens 10 mm diameter and 3 mm thickness were formed by melting alloys with a propane-oxygen flame and casted with a centrifuge casting machine and then with the porcelain veneer fired onto the metal alloys. Corrosion tests were performed in quintuplicate for each alloy (after repeated porcelain firing) in Fusayama artificial saliva solution (pH = 5) in a low thermal-expansion borosilicate glass cell. Tamhane and Sheffe test was used to compare corrosion differences in the results after repeated firings and among 7, 9 and 11 firing for each alloy. The probability level for statistical significance was set at ${\alpha}$=0.05. RESULTS. The corrosion resistance was higher (30 mV), in case of 7 times firing (Commercial). On the other hand, it was lower in case of 11 times firing (5 mV) (P<.05). Conclusion. Repeated firings decreased corrosion resistance of Pd-Ag, Cr-Co and Cr-Ni alloys. The Pd-Ag alloy exhibited little corrosion in in vitro tests. The Cr-Ni alloy exhibited higher corrosion resistance than Cr-Co alloys in in vitro tests.

Co-Cr alloy의 전해연마에 따른 부식의 영향 (Effect of Electropolishing Process on Corrosion Resistance of Co-Cr Alloy)

  • 박제민;김완철
    • 한국표면공학회지
    • /
    • 제43권4호
    • /
    • pp.199-204
    • /
    • 2010
  • The Co-Cr alloys have clinical histories as dental and orthopaedic implants, and recently as cardiovascular stent applications because they exhibit a high elastic modulus and radiopacity. In order to improve their mechanical and corrosion resistance, electropolishing is employed as the final process. Electropolishing, an anodic dissolution process in the transpassive state, is sensitively affected by process conditions such as current density, machining time, and electrode gap. In this study, the effect of the electropolishing conditions on surface roughness and corrosion resistance is investigated for Co-Cr alloys (L605). The most smooth surface is obtained when electropolishing is performed at 15-20 V for 15-30 sec with a electrode gap of 3.5 mm. It is found out that electropolishing reduces corrosion rate about one-tenth as much.

비귀금속 주조 맞춤형 지대주를 이용한 상악 전치부 임플란트 보철수복 증례 (Maxillary anterior fixed implant prosthesis using customized nonprecious metal casting abutment: a case report)

  • 이재인
    • 구강회복응용과학지
    • /
    • 제31권1호
    • /
    • pp.50-59
    • /
    • 2015
  • 임플란트를 이용하여 심미 영역인 상악 전치부를 심미적, 기능적으로 수복하고 유지 관리하는 것은 어려운 일이다. 임플란트 주위염으로 인하여 치조골의 흡수, 치간유두의 수축 등과 같은 임플란트 주위 조직 문제와 금속 지대주의 노출로 인한 심미적 문제가 발생할 수 있기 때문이다. 본 증례에서는 기성지대주의 단점을 보완 가능한 맞춤형 지대주를 전통적인 제작 방식인 주조 방식으로 Co-Cr 합금을 이용하여 제작하고, 시멘트 유지형 보철물을 제작한 증례에 대해 보고하고자 한다.

Evaluation of marginal and internal gaps of Ni-Cr and Co-Cr alloy copings manufactured by microstereolithography

  • Kim, Dong-Yeon;Kim, Chong-Myeong;Kim, Ji-Hwan;Kim, Hae-Young;Kim, Woong-Chul
    • The Journal of Advanced Prosthodontics
    • /
    • 제9권3호
    • /
    • pp.176-181
    • /
    • 2017
  • PURPOSE. The purpose of this study was to evaluate the marginal and internal gaps of Ni-Cr and Co-Cr copings, fabricated using the dental ${\mu}-SLA$ system. MATERIALS AND METHODS. Ten study dies were made using a two-step silicone impression with a dental stone (type IV) from the master die of a tooth. Ni-Cr (NC group) and Co-Cr (CC group) alloy copings were designed using a dental scanner, CAD software, resin coping, and casting process. In addition, 10 Ni-Cr alloy copings were manufactured using the lost-wax technique (LW group). The marginal and internal gaps in the 3 groups were measured using a digital microscope ($160{\times}$) with the silicone replica technique, and the obtained data were analyzed using the non-parametric Kruskal-Wallis H test. Post-hoc comparisons were performed using Bonferroni-corrected Mann-Whitney U tests (${\alpha}=.05$). RESULTS. The mean (${\pm}$ standard deviation) values of the marginal, chamfer, axial wall, and occlusal gaps in the 3 groups were as follows: $81.5{\pm}73.8$, $98.1{\pm}76.1$, $87.1{\pm}44.8$, and $146.8{\pm}78.7{\mu}m$ in the LW group; $76.8{\pm}48.0$, $141.7{\pm}57.1$, $80.7{\pm}47.5$, and $194.69{\pm}63.8{\mu}m$ in the NC group; and $124.2{\pm}52.0$, $199.5{\pm}71.0$, $67.1{\pm}37.6$, and $244.5{\pm}58.9{\mu}m$ in the CC group. CONCLUSION. The marginal gap in the LW and NC groups were clinically acceptable. Further improvement is needed for CC group to be used clinical practice.