• 제목/요약/키워드: Co-22%Cr

검색결과 124건 처리시간 0.024초

기판온도에 따른 Co-22%Cr 합금박막의자가정렬형 나노구조 (Self-Organized Nano Structure in Co-22% Cr Alloy Thin Films with Substrate Temperatures)

  • 송오성;이영민
    • 한국표면공학회지
    • /
    • 제34권6호
    • /
    • pp.531-536
    • /
    • 2001
  • Co-22 %Cr alloy films are promising for high-density perpendicular magnetic recording media with their perpendicular anisotropy and large coercivity of 3000 Oe. We observed that a self organized nano structure (SONS) of fine ferromagnetic Co-enriched phase and paramagnetic Cr-enriched phase appears inside the grain of Co-Cr magnetic alloy thin films at the elevated substrate temperature after do-sputtering. The periodic fine Co-enriched phase and Cr-enriched phase is the plate shape of 80 (equation omitted)-wide and 1000 (equation omitted)-long. Cr-enriched phases are located at the center of grains. We prepared 5000 (equation omitted) -thick Co-22 %Cr films on polyimide substrate with varying substrate temperature of $ 30^{\circ}C$, $ 150^{\circ}C$ ,200 $^{\circ}C$, $300^{\circ}C$, and $400^{\circ}C$, respectively. A transmission electron microscope equipped with energy dispersive X-ray analyzer is employed to observe the microstructure of each samples after Co-enri-ched phase are etched selectively. The self organized nano structure of Co-enriched and Cr-enriched lamellar is observed above the substrate temperture of $150^{\circ}C$. No compositional change is observed with substrate temperature. The compositional phase separation in self organized structure becomes clear as the substrate temperature increases. Our results implies that the self organized nano structure in Co-22 %Cr film is ideal for ultra high density recording media by recording selectively on Co-enri-ohed phase.

  • PDF

Fe-Cr-Mn-X계 합금의 감쇠능 및 플라즈마 이온 질화특성에 미치는 합금원소의 영향 [II플라즈마 이온 질화특성] (The Effect of Alloy Elements on the Damping Capacity and Plasma Ion Nitriding Characteristic of Fe-Cr-Mn-X Alloys. [II Plasma Ion Nitriding Characteristic])

  • 손동욱;이해후;성장현;박규섭;김창규;강창룡
    • 동력기계공학회지
    • /
    • 제9권1호
    • /
    • pp.76-81
    • /
    • 2005
  • The effect of micro-pulse plasma nitriding temperature and time on the case thickness, hardness and nitride formation in the surface of Fe-12Cr-22Mn-X alloy with 3% Co and 1% Ti alloys elements investigated. External compound layer and internal diffusion layer was constituted in plasma nitride case of Fe-12Cr-22Mn-X alloys and formed nitride phase such as ${\gamma}'-Fe4N\;and\;{\varepsilon}-Fe2-3N$. Case depth increased with increasing the plasma nitriding temperature and time. Surface hardness of nitrided Fe-12Cr-22Mn-X alloys obtained the above value of Hv 1,600 and case depth obtained the above value of $45{\mu}m$ in Fe-12Cr-22Mn-3Co alloy and $60{\mu}m$ in Fe-12Cr-22Mn-1Ti alloy. Wear-resistance increased with increasing plasma nitriding time and showing the higher value in Fe-12Cr-22Mn-1Ti alloy than Fe-12Cr-22Mn-3Co alloy.

  • PDF

Co-22%Cr 합금박막의 자가정렬형 나노구조에 의한 자기적 물성 (Magnetic Property Evolution of Co-22%Cr Alloy Thin Films with Self-Organized Nano Structure Formation)

  • 송오성;이영민
    • 한국재료학회지
    • /
    • 제11권12호
    • /
    • pp.1042-1046
    • /
    • 2001
  • Co-22%Cr alloy films are promising for high-density perpendicular magnetic recording media with their perpendicular anisotropy and large coercivity of 3000 Oe. We observed that a self organized nano structure(SONS) of fine ferromagnetic Co-enriched phase and paramagnetic Cr-enriched phase appears inside the grain of Co-Cr magnetic alloy thin films at the elevated substrate temperature after do-sputtering. We prepared 1000 $\AA$-thick Co-22%Cr films on 2000 $\AA$- SiO$_2$/Si(100) substrates at the deposition rate of 100 $\AA$/min with substrate temperatures of 3$0^{\circ}C$, 10$0^{\circ}C$, 15$0^{\circ}C$, 20$0^{\circ}C$, 30$0^{\circ}C$, and 40$0^{\circ}C$, respectively. We employed a vibrating sample magnetometer(VSM) to measure the B-H loops showing the saturation magnetifation, coercivity, remanence in in- plane and out- of- plane modes. In- plane coercivity, perpendicular coercivity, and perpendicular remanence increased as substrate temperature increased, how-ever they decreased after 30$0^{\circ}C$ slowly. Transmission electron microscope (TEM) characterization revealed that the self organized nano structure (SONS) appears at the elevated substrate temperature, which forms fine Co-enriched phases inside a grain, then it eventually affect the perpendicular magnetic property. Our results imply that we may tune the perpendicular magnetic properties with SONS obtained at appropriate substrate temperature.

  • PDF

가스터빈 엔진부품용 NiCoCrAlY-(Ta, Re, Ir) 코팅의 고온산화특성 (High Temperature Oxidation of NiCoCrAlY-(Ta, Re, Ir) Coatings for Gas Turbines)

  • 최정호;이동복
    • 한국표면공학회지
    • /
    • 제39권3호
    • /
    • pp.129-136
    • /
    • 2006
  • The high velocity oxy-fuel sprayed coatings of 38Ni-23Co-20Cr-11Al-3Y-5Ta, 25Ni-34Co-20Cr-11Al-3Y-2Re and 32Ni-34.5Co-22Cr-11Al-0.5Ir (in wt%) were oxidized at 1000 and $1100^{\circ}C$ in air in order to find the alloying effect of Ta, Re and Ir on the oxidation properties of the NiCoCrAlY-base coatings. The primary phase of the coatings was $Ni_3Al$. The oxides formed on the coatings consisted primarily of ${\alpha}-Al_2O_3$, together with some $CoCr_2O_4,\;CoAl_2O_4$, and $Al_5Y_3O_{12}$. Tantalum oxidized to $Ta_2O_5$ and $Ta_2O_{22}$. However, no oxides of Re and Ir were detected by XRD owing to their thermodynamic inertness and/or their small amount.

Co-22%Cr 자성합금박막에서 박막두계에 따른 자기미세구조 변화 (The change of magnetic microstructure with Co-22%Cr film thicknesses)

  • 송오성
    • 한국표면공학회지
    • /
    • 제31권5호
    • /
    • pp.261-265
    • /
    • 1998
  • We investigated compositional separation of Co-23%Cr magnetic alloy thin films with varying film thicknesses. Saturation magnetization and magnetic microstructures were investigated using vibrating sample magnetometer (VSM) and scanning probe microscope (SPM), respectively. Saturation magnetization was as 700 emu/cc for films below 50 nm-thick, and changed to 430 emu/cc for the ones above 2000 nm-thick. This may be due to increment of molar volume of Cr-enriched phase as film thickness increases. The surface grain size in AFM (atomic force microscope) measurement becomes larger as film thickness increases. The MFM (magnetic force microscope) reveals that magnetic microstructure is changed from the fine spherical domains to the maze type domains as film thickness increases. We conclude that employing thickness of Co-22%Cr films below 50 nm is favorable for high density recording in order to enhance perpendicular saturation magnetization and SNR (signal to noise ratio).

  • PDF

Effects of Magnetic Layer Thickness on Magnetic Properties of CoCrPt/Ti/CoZr Perpendicular Media

  • Hwang, M.S.
    • Journal of Magnetics
    • /
    • 제6권1호
    • /
    • pp.19-22
    • /
    • 2001
  • Change of magnetic properties in CoCrPt/Ti perpendicular media with varying CoCrPt film thickness has been studied. As the CoCrPt film thickness increases from 25 nm, the Ms (saturation magnetization) increases rapidly at first and then more gradually. This Ms behavior is associated primarily with the formation of an "amorphous-like"reacted layer created by intermixing of CoCrPt and Ti at the CoCrPt/Ti interface and secondarily with a change of the Cr segregation mode with varying CoCrPt film thickness. Magnetic domain structure distinctively changes with increasing CsCrPt magnetic layer (ML) thickness. Also the strength of exchange coupling measured from the slope in the demagnetizing region of the M-H loop changes with ML thickness. The expansion of lattice parameters a and c at smaller film thickness suggests that the Cr segregation mode may be connected with the residual stress of the films. Finally, the negative nucleation field (Hn) shows a unique behavior with the change of strength of the exchange interaction.teraction.

  • PDF

Fe-Cr-Mn-X계 합금의 감쇠능 및 플라즈마이온질화 특성에 미치는 합금원소의 영향 [I 감쇠능] (The Effect of Alloy Elements on the Damping Capacity and Plasma Ion Nitriding Characteristic of Fe-Cr-Mn-X Alloys [I Damping Capacity])

  • 손동욱;정상훈;김재환;이종문;김익수;강창룡
    • 동력기계공학회지
    • /
    • 제9권1호
    • /
    • pp.70-75
    • /
    • 2005
  • The damping property of Fe-12Cr-22Mn-X alloys has been investigated to develop high damping and high strength alloy. Particularly, the effect of the phase of austenite, alpha and epsilon martensite, which constitute the structure of the alloys Fe-12Cr-22Mn-X alloys, on the damping capacity at room temperature has been investigated. Various fraction of these phases were formed depending on the alloy element and cold work degree. The damping capacity is strongly affected by ${\varepsilon}$ martensite while the other phase, such as ${\alpha}'$ martensite, actually exhibit little effect on damping capacity. In case of Fe-12Cr-22Mn-3Co alloy, the large volume fraction of ${\varepsilon}$ martensite formed at about 30% cold rolling, and in case of Fe-12Cr-22Mn-1Ti alloy, formed at about 20% cold rolling and showed the highest damping capacity. Damping capacity showed higher value in Fe-12Cr-22Mn-1Ti alloy than one in Fe-12Cr-22Mn-3Co alloy.

  • PDF

자가정렬형 나노구조 Co-22%Cr합금 박막의 기판온도에 따른 미세 도메인 구호 (Magnetic Domain Structures with Substrate Temperatures in Co-22%Cr Alloy Thin Films)

  • 송오성
    • 한국자기학회지
    • /
    • 제11권5호
    • /
    • pp.184-188
    • /
    • 2001
  • DC-스퍼터를 이용하여 기판온도를 실온과 20$0^{\circ}C$로 변화시켜 , 균일한 내부구조를 갖는 구조와 결정립내부에 미세한 자가정렬나노구조(SONS)를 갖는 Co-22%Cr 합금 박막을 각각 제조하고 이들의 미세구조와 도메인구조를 투과전자현미경(TEM)과 자기력현미경(MFM)을 이용하여 확인하였다. Co가 먼저 부식되도록 조치하고 관찰한 투과전자현미경 결과, 실온에서 제작된 박막의 경우에는 결정립 내부가 균일한 조성을 보인 반면, 기판온도가 20$0^{\circ}C$인 Co-22%Cr합금 박막은 결정립 내부에 SONS를 형성하여 판상의 미세 Co-과잉상을 가지는 특이한 미세구조를 가지는 것을 확인하였다. 자기력현미경에 의해 확인된 결과, SONS가 없는 시편(기판온도를 실온으로 유지한 경우)은 주기 5000 정도의 미로형 도메인(domains)이 생겼다. 미로형 도메인은 결정간의 교환에너지가 큰 경우 발생하는 구조로서 고밀도 자기기록이 불리할 것이 예상되었다. 이와 비교해서 SONS가 생성된 (기판온도를 20$0^{\circ}C$로 유지한 경우)시편은 주기 500 정도의 매우 미세한 구형 도메인을 보였다. 미세구형 도메인은 각 도메인간의 교환에너지가 작아 열적 변화에도 데이터가 안정하므로 고밀도 기록에 유리하다고 예상되었다.

  • PDF