• Title/Summary/Keyword: Chromium(III)

Search Result 137, Processing Time 0.024 seconds

Selective Removal of Cr (VI) and Cr (III) in Aqueous Solution by Surface Modified Activated Carbon

  • Lee, Jeong-Min;Kim, Min-Il;Lee, Young-Seak
    • Carbon letters
    • /
    • v.9 no.1
    • /
    • pp.23-27
    • /
    • 2008
  • The adsorption and reduction of Cr (VI) to Cr (III) by surface modified activated carbon (AC) in an aqueous solution was studied. The effects of surface modifications on the properties of the carbons were investigated by the analysis of specific surface area, carbon surface pH, acid/base surface values and functional groups. In order to understand the Cr(VI) adsorption and reduction ratio from Cr(VI) to Cr(III), the Cr adsorption capacity of AC was also measured and discussed by using inductively coupled plasma and UV spectrophotometer. The modifications bring about substantial variation in the chemical properties whereas the physical properties such as specific surface area, pore volume and pore size distribution nearly were not changed. Total Cr adsorption efficiency of as-received activated carbon (R-AC) and nitric acid treated activated carbon (N1-AC and N2-AC) were recorded on 98.2, 99.7 and 100%. Cr(III) reduction efficiency of R-AC increased largely from 0.4% to 28.3% compared to N1-AC and N2-AC.

Synthesis, Spectroscopic, and Biological Studies of Chromium(III), Manganese(II), Iron(III), Cobalt(II), Nickel(II), Copper(II), Ruthenium(III), and Zirconyl(II) Complexes of N1,N2-Bis(3-((3-hydroxynaphthalen-2-yl)methylene-amino)propyl)phthalamide (N1,N2-bis(3-((3-hydroxynaphthalen-2-yl)methylene-amino)propyl)phthalamide의 크롬(III), 망간(II), 철(III), 코발트(II), 니켈(II), 구리(II), 루테늄(III) 및 산화 지르코늄(II) 착물에 대한 합성과 분광학 및 생물학적 연구)

  • Al-Hakimi, Ahmed N.;Shakdofa, Mohamad M.E.;El-Seidy, Ahemd M.A.;El-Tabl, Abdou S.
    • Journal of the Korean Chemical Society
    • /
    • v.55 no.3
    • /
    • pp.418-429
    • /
    • 2011
  • Novel chromium(III), manganese(II), iron(III), cobalt(II), nickel(II), copper(II), ruthenium(III), and zirconyl(II) complexes of $N^1,N^2$-bis(3-((3-hydroxynaphthalen-2-yl)methylene-amino)propyl)phthalamide ($H_4L$, 1) have been synthesized and characterized by elemental, physical, and spectral analyses. The spectral data showed that the ligand behaves as either neutral tridentate ligand as in complexes 2-5 with the general formula $[H_4LMX_2(H_2O)]{\cdot}nH_2O$ (M=Cu(II), Ni(II), Co(II), X = Cl or $NO_3$), neutral hexadentate ligand as in complexes 10-12 with the general formula $[H_4LM_2Cl_6]{\cdot}nH_2O$ (M=Fe(III), Cr(III) or Ru(III)), or dibasic hexadentate ligand as in complexes 6-9 with the general formula $[H_2LM_2Cl_2(H_2O)_4]{\cdot}nH_2O$ (M = Cu(II), Ni(II), Co(II) or Mn(II), and 13 with general formula $[H_4L(ZrO)_2Cl_2]{\cdot}8H_2O$. Molar conductance in DMF solution indicated the non-ionic nature of the complexes. The ESR spectra of solid copper(II) complexes 2, 5, and 6 showed $g_{\parallel}$ >g> $g_e$, indicating distorted octahedral structure and the presence of the unpaired electron in the $N^1,N^2$ orbital with significant covalent bond character. For the dimeric copper(II) complex $[H_2LCu_2Cl_2(H_2O)_4]{\cdot}3H_2O$ (6), the distance between the two copper centers was calculated using field zero splitting parameter for the parallel component that was estimated from the ESR spectrum. The antibacterial and antifungal activities of the compounds showed that, some of metal complexes exhibited a greater inhibitory effect than standard drug as tetracycline (bacteria) and Amphotricene B (fungi).

On the Aquation of Dichloro Bis-(Ethylenediamine)-Chromium (III) Cation (Dichloro Bis-(Ethylenediamine)-Chromium (III) 양이온의 수화반응)

  • Jung-Ui Hwang;Jong-Jae Chung;Soung-Oh Bek
    • Journal of the Korean Chemical Society
    • /
    • v.28 no.2
    • /
    • pp.95-101
    • /
    • 1984
  • Aquation reaction kinetics of $[Cr(en)_2Cl_2]^+$complex was carried by the electric conductivity method. Its temperature range was $15^{\circ}C$ to $30^{\circ}C$ and pressure was varied up to 2,000 bars. The reaction rate was increased with increasing temperature, but was reversed to increasing pressure. The activation volume(${\Delta}V^{\neq}$) was increased with increasing temperature and decreased with increasing pressure. At $25^{\circ}C$ and 1 bar it was fairly small positive value, $1.82cm^2/mole$. Activation entropy change(${\Delta}S^{\neq}$) $was calculated as small negative value,-9.019 eu, at $25^{\circ}C$ and 1bar. Referring to the thermodynamic parameters, it was estimated that aquation reaction was proceeded by the interchange-dissociation(Id) mechanism.

  • PDF

TENSILE BOND STRENGTH OF SOLDER JOINT BETWEEN GOLD ALLOY AND NICKEL-CHROMIUM ALLOY (금합금과 Ni-Cr 합금의 납착부 인장강도)

  • Jeong, Jun-Oh;Choi, Hyeon-Mi;Choi, Jeong-Ho;Ahn, Seung-Geun;Song, Kwang-Yeob;Park, Charn-Woon
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.34 no.1
    • /
    • pp.143-150
    • /
    • 1996
  • The purpose of this study was to evaluate the tensile strength of solder joint between gold alloy and nickel-chromium alloy. The specimens were made with type III gold alloys and Ni-Cr-Be alloy and Degular Lot 2 solder. Eighteen paired specimens were made, and subdivided into three groups. Group I specimens were gold alloy-gold alloy combination, Group II specimens were gold alloy-Ni-Cr alloy combination, Group III specimens were Ni-Cr alloy-Ni-Cr alloy combination. Solder block were made with solder investment(Degussa A,G, Germany) and stored in room temperature for 24 hours. To reduce the formation of metallic oxide and increase wetting properties, flux was used before preheating and soldering procedure. The specimens were preheated at $650^{\circ}C$ and flux were applied again and gas-oxygen torch was used to solder the specimen. All soldered specimens were subjected to a tensile force in the Instron universal testing machine : the crosshead speed was 1 mm/mim. Tensile strength values of three soldered joint groups were 1. Gold alloy-Gold alloy solder joint : $$48.8kg/mm^2$$ 2. Gold alloy-Ni-Cr alloy solder joint : $$30.9kg/mm^2$$ 3. Ni-Cr alloy-Ni-Cr alloy solder joint : $$31.8kg/mm^2$$ The microscopic examination of fracture site showed cohesive and combination fracture modes in gold alloy specimens, but showed all adhesive fracture modes in Ni-Cr alloy containing specimens.

  • PDF

Photochemical Reactivity of Chromium(III) Complexes (Chromium(III) 錯物의 光化學的 反應性)

  • Jong-Jae Chung;Jung-Ui Hwang;Jong-Ha Choi
    • Journal of the Korean Chemical Society
    • /
    • v.30 no.2
    • /
    • pp.181-187
    • /
    • 1986
  • It is shown that the substitutive ligand on the photochemical substitution reactions of $trans-Cr^{Ⅲ}N_4XY$ complexes is predicted by considering the total stabilization energy of the hypothetical primary intermediates resulting from the loss of one ligand. The total stabilization energy and one electron energy level of d-orbital are calculated within the framework of angular overlap model. According to the calculated results, the intermediates with larger total stabilization energy are, as expected, more easily produced. Consequently, the relative values of the total stabilization energy are used to decide which of the ligands in $trans-Cr^{Ⅲ}N_4XY$ complexes is preferentially labilized on the lowest energy d-d irradiation. The prediction for the leaving ligand on the photoaquation of $trans-Cr^{Ⅲ}N_4XY$ complexes is consistent.

  • PDF

Chromium(III) Complex Obtained from Dipicolinic Acid: Synthesis, Characterization, X-Ray Crystal Structure and Electrochemical Studies

  • Ghasemi, Khaled;Rezvani, Ali Reza;Razak, Ibrahim Abdul;Moghimi, Abolghasem;Ghasemi, Fatemeh;Rosli, Mohd Mustaqim
    • Bulletin of the Korean Chemical Society
    • /
    • v.34 no.10
    • /
    • pp.3093-3097
    • /
    • 2013
  • The synthesis, X-ray crystallography, spectroscopic (IR, UV-vis), and electrochemical properties of the title compound, $[H_3O][Cr(dipic)_2][H_3O^+.Cl^-]$ (1), ($H_2dipic$ = 2,6-pyridinedicarboxylic acid), are reported. This complex crystallizes in the monoclinic space group Cc with a = 14.9006(10) ${\AA}$, b = 12.2114(8) ${\AA}$, c = 8.6337(6) ${\AA}$, ${\alpha}=90.00^{\circ}$, ${\beta}=92.7460(10)^{\circ}$, ${\gamma}=90.00^{\circ}$, and V = 1569.16(18) ${\AA}^3$ with Z = 4. The hydrogen bonding and noncovalent interactions play roles in the stabilization of the structure. In order to gain a better understanding of the most important geometrical parameters in the structure of the complex, atoms in molecules (AIM) method at B3LYP/6-31G level of theory has been employed.

Effect of Acid Leaching Conditions on the Properties of Cr Powder Produced by Self-propagating High-temperature Synthesis (자전연소합성법을 이용한 Cr 분말 제조시 산세조건에 따른 물성평가)

  • YongKwan Lee;YeongWoo Cho;ShinYoung Choi;SungGue Heo;Ju Won;KyoungTae Park;MiHye Lee;JaeJin Sim
    • Journal of Powder Materials
    • /
    • v.30 no.3
    • /
    • pp.233-241
    • /
    • 2023
  • In this study, we evaluated the effects of acid leaching on the properties of Cr powder synthesized using self-propagating high-temperature synthesis (SHS). Cr powder was synthesized from a mixture of Cr2O3 and magnesium (Mg) powders using the SHS Process, and the byproducts after the reaction were removed using acid leaching. The properties of the recovered Cr powder were analyzed via X-ray diffraction (XRD), scanning electron microscopy (SEM), energy-dispersive X-ray spectroscopy (EDS), particle size analysis (PSA), and oxygen content analysis. The results show that perfect selective leaching of Cr is challenging because of various factors such as incomplete reaction, reaction kinetics, the presence of impurities, and incompatibility between the acid and metal mixture. Therefore, this study provides essential information on the properties under acidic conditions during the production of high-quality Cr powder using a self-propagating high-temperature synthesis method.

Accuracy and Precision of Ion Chromatography/Visible Absorbance Detection for Analyzing Hexavalent Chromium Collected on PVC Filter (Ion Chromatography/Visible Absorbance Detection을 이용한 Cr(VI) 분석의 정확도 및 정밀도 평가)

  • Shin, Yong Chul;Oh, Se Min;Paik, Nam Won
    • Journal of Korean Society of Occupational and Environmental Hygiene
    • /
    • v.7 no.2
    • /
    • pp.223-232
    • /
    • 1997
  • The accuracy and precision of a modified method of NIOSH Method 7600 and EPA method 218.6 was determined for analyzing hexavalent chromium, Cr(VI), collected on PVC filter from workplace air. The method was designed to extract from Cr(VI) on PVC filter with a alkali solution, 2% NaOH/3% $Na_2CO_3$, and to analyze it using ion chromatography/visible absorbance detection(IC/VAD). The results and conclusion are as the following. 1. The peak of Cr(VI) was separated sharply on chromatogram and was linearly related with Cr(VI) concentration in sloution. The correlation coefficient was 0.9999 in a calibration curve. The limit of detection was 0.25 $0.25{\mu}g/sample$. 2. The accuracy(% recovery) was 93.3% in a set of sample($9-50{\mu}g$) stored for a day, and 100.1%($10-60{\mu}g$) in another set of samples stored for 2 hours. It is assumed that the difference in recovery by storage time was due to reduction of Cr(VI) to Cr(III). 3. The precision(coefficient of variation, CV) of the method was 0.015 in spiked samples with Cr(VI) standard solution, and 0.010 in spiked samples with plating solution from a chrome electroplating factory. The overall CV in all types of samples was 0.0013. 4. The Cr(VI) was stable in 2% NaOH/3% $Na_2CO_3$ at least for 10 hours. In conclusion, the IC/VAD method is appropriate for determining low-level Cr(VI) in workplace air containing various interferences.

  • PDF

Fabrication of Cr$_2$O$_3$powder from waste MgO-Cr refractory

  • Lee, Hoon-Ha;Sohn, Jin-Gun;Lee, Jae-Young;Kim, Dae-Young
    • Proceedings of the IEEK Conference
    • /
    • 2001.10a
    • /
    • pp.357-361
    • /
    • 2001
  • The possibility of producing Cr$_2$O$_3$powder from waste magnesia-chromium refractory was investigated by sulfuric acid reaction, alkali fusion, water leaching & purification and heat treatment. The effects of temperature, the amount of NaOH added and the flow rate of air on chromium extraction efficiency in an alkali fusion step were investigated. The fusion product was leached with methanol to solve free-NaOH, and then leached with water to produce a Na$_2$CrO$_4$solution. The purity of chrome(Ⅵ) oxides, prepared both from monochromate with an impurity content and monochromate purified with $CO_2$were also examined. The purified monochromate solution was reduced from Cr(Ⅵ) to Cr(III) with NaHSO$_3$solution. The reduced solution was neutralized with NaOH to produce Cr(OH)$_3$. Water washing was treated to eliminate Na$_2$SO$_4$from neutralized Cr(OH)$_3$slurry. The washed Cr(OH)$_3$was dried and thermally treated to produce Cr$_2$O$_3$powder. The properties like lightness and hue of Cr$_2$O$_3$fabricated in this study were L=47.47, a=-14.40 and b=17.21.

  • PDF