The Novel Liquid Crystal Materials for AM-LCDs

  • Yamaguchi, T.;Kibe, S.;Matsui, S.;Yamamoto, H.
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2002년도 International Meeting on Information Display
    • /
    • pp.924-929
    • /
    • 2002
  • We have developed the novel liquid crystal materials with a difluoromethyleneoxy (CF2O) moiety as a linkage group in order to satisfy the diversified various requirements for AM-LCDs. These novel CF2O LC materials have excellent physical properties that are high dielectric anisotropy, low viscosity and wide nematic temperature ranges. Physical properties measurement results that mixtures containing CF2O LC materials have suitable for characteristics for AM-LCDs. The CF2O LC materials are excellent compound for quick response and low driving voltage application.

  • PDF

Optically isotropic liquid crystal composite incorporating with in-plane electric field geometry

  • Yamamoto, Shin-Ichi;Haseba, Yasuhiro;Iwata, Takashi;Higuchi, Hiroki;Choi, Suk-Won;Kikuchi, Hirotsugu
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2009년도 9th International Meeting on Information Display
    • /
    • pp.1593-1595
    • /
    • 2009
  • We demonstrate an intriguing liquid crystal display (LCD) mode that comprises an optically isotropic liquid crystal (LC) composite incorporating with inplane electric field geometry. No surface treatment, such as rubbing, is required to fabricate the LCD mode because it is based on an optically isotropic state. The measured response time was of submillisecond order. The LCD mode has several unique features such as fast response, continuous grayscale capability, and a high contrast ratio.

  • PDF

Advanced Nanoimprinting Material for Liquid Crystal Alignment

  • Gwag, Jin-Seog;Oh-e, Masahito;Yoneya, Makoto;Yokoyama, Hiroshi;Satou, H.;Itami, S.
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2007년도 7th International Meeting on Information Display 제7권1호
    • /
    • pp.534-537
    • /
    • 2007
  • To promote liquid crystal application of nanoimprint lithography, a polymer with new concept is proposed. The material consists of a polyamic acid for good LC alignment and an epoxy resin for good imprinting. The result of sum-frequency generation (SFG) vibrational spectroscopy proves that this material is a functionally gradient material. This material shows excellent capability as a nanoimprinting material as well as an LC alignment layer.

  • PDF

Minamata Disease and the Mercury Pollution of the Globe

  • Harada Masazumi
    • 한국환경보건학회지
    • /
    • 제31권6호
    • /
    • pp.451-456
    • /
    • 2005
  • Minamata disease made its first appearance in the world at Minamata City, Kumamoto Prefecture, in May 1956. In 1962 methyl mercury poisoning through the placenta was found for the first time in the world. This was called congenital Minamata disease. In all cases the clinical symptoms were consistent with those of cerebral palsy. The time and place of outbreak were the same as those for Minamata disease. Their mothers had eaten fish and shellfish during pregnancy. The principal symptoms of congenital Minamata disease are mentalretardation ($100\%$); primitive reflexes ($100\%$); disturbance of coordination ($100\%$); dysarthria ($100\%$); limb deformation (100%); growth disorders ($100\%$); nutritional disorders ($100\%$); chorea-athetose ($95\%$); and hypersalivation ($95\%$). However, today, when the world is polluted by mercury in various places and at various levels, the data we need is not represented by those severe cases, but rather by the chronic milder type. Even in Minamata, the issue of Minamata disease has not been resolved. And likewise, on a global scale the problem of Minamata disease is not yet over.

AFLC 셀을 이용한 반사형 LCD의 설계 및 제작 (Optical configurtion and fabriation for a reflective display using an antiferroelectric liquid crystal cell)

  • 김성철;박원상;이서헌;황용석;이기동;윤태훈;김재창
    • 한국광학회지
    • /
    • 제12권3호
    • /
    • pp.235-239
    • /
    • 2001
  • 본논문에서는 반강유전성 액정의 in-plane tilt 각이 약 $22.5^{\circ}C$인 특성을 가진다는 것을 이용하여 액정의 위상지연을 $\lambda/2$로 설계한 광대역 $\lambda/4$필름을 사용한 단일 편광판 모드 반사형 LCD의 구조를 제안하였으며 이구조의 여러 가지 광특석을 전사모사 해보았다. 실제 실험에서는 in-plane tilt 각이 $\24.9\lambda$인 Chisso상의 CS-4001 반강유전성 액정을 사용하여 액정 셀의 위상지연을 $\lambda/2$로 설계하여 각도에 따른 반사특성과 파장에 따른 분광특성을 측정하였다.

  • PDF

수종의 실란처리 유리섬유를 첨가한 의치상용 레진의 강도변화 및 마모전.후 표면성상분석 (EFFECTS Of VARIOUS SILANE COUPLING AGENTS ON THE STRENGTH AND THE SURFACE ROUGHNESS OF GLASS FIBER-ADDED PMMA RESIN)

  • 이상일;김창회;임영준;김명주;윤석대
    • 대한치과보철학회지
    • /
    • 제45권4호
    • /
    • pp.457-468
    • /
    • 2007
  • Statements of problem: The fracture of acrylic resin dentures remains an unsolved problem. Therefore, many investigations have been performed and various approaches to strengthening acrylic resin, for example, the reinforcement of heat-cured acrylic resin using glass fibers, have been suggested over the years. Silane is important for bonding between glass fiber and resin. Purpose: The aim of the present study was to investigate the effect of various silane on the strength of PMMA resin and roughness of resin-glass fiber complex after abrasion test. Material and methods: 3mm glass fiber (Chopped strand, Hankuk fiber Co., Milyang, Korea) was treated with 3 kinds of silane (MPS, EPS, APS) (Sila-ace, Chisso chemical, Tokyo, Japan) and mixed with PMMA resin(Vertex RS, Vertex Dental B.V., Zeist, Netherlands). Transverse strength and Young's modulus was measured using Instron (Instron model 4466, Instron, Massachusetts, USA). After abrasion test (The 858 Mini Bionix II Test System, MTS System Co., Minnesota, USA) surface roughness was evaluated using tester (Form Talysurf plus, Taylor Hopson Ltd., Leicester England). Examination of scanning electron microscope was also performed. Results: Within this study, the following conclusions were drawn. 1. Surface treatment of glass fiber with MPS and APS increased transverse strength of PMMA resin complex, but surface treatment with EPS decreased transverse strength of PMMA resin complex (p<0.05). 2. Silane treated glass fiber increased Young's modulus of PMMA resin complex compared to desized glass fiber (p<0.05). 3. Roughness increased after abrasion test in case of PMMA resin reinforced with desized glass fiber (p<0.05). 4. Roughness change was not observed after abrasion test in case of PMMA resin reinforced with silane treated glass fiber (p>0.05).