SF 590A 대형 단조품의 충격특성에 관한 연구 (Impact Behavior of Large SF590A Forged Product)

  • 진상욱;김상식;이영선;이승욱;김남수
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2008년도 춘계학술대회 논문집
    • /
    • pp.61-66
    • /
    • 2008
  • Impact behavior of large SF590A (Fe-0.65C-1.5Mn-0.035P-0.035S-0.3Cr-0.15Mo-0.4Ni-0.3Cu) forged propeller shaft was studied in this study. Charpy impact specimens were prepared from the forged product with different heat number. The impact value of each specimen with different heat number tends to vary greatly depending on the prior austenite grain size and, less significantly, on the amount of sulfur. The dominant metallurgical factors affecting impact behavior of SF590A forged product are discussed based on fractographic and metallographic observations.

  • PDF

P-No. 1 탄소강의 기계적 특성과 미세조직에 미치는 용접후열처리의 영향 (Effect of Post-Weld Heat Treatment on the Mechanical Properties and Microstructure of P-No. 1 Carbon Steels)

  • 이승건;강용준;김기동;강성식
    • Journal of Welding and Joining
    • /
    • 제35권1호
    • /
    • pp.26-33
    • /
    • 2017
  • This study aims to investigate the suitability of requirement for post-weld heat treatment(PWHT) temperature when different P-No. materials are welded, which is defined by ASME Sec. III Code. For SA-516 Gr. 60 and SA-106 Gr. B carbon steels that are typical P-No. 1 material, simulated heat treatment were conducted for 8 h at $610^{\circ}C$, $650^{\circ}C$, $690^{\circ}C$, and $730^{\circ}C$, last two temperature falls in the temperature of PWHT for P-No. 5A low-alloy steels. Tensile and Charpy impact tests were performed for the heat-treated specimens, and then microstructure was analyzed by optical microscopy and scanning electron microscopy with energy-dispersive spectrometry. The Charpy impact properties deteriorated significantly mainly due to a large amount of cementite precipitation when the temperature of simulated heat treatment was $730^{\circ}C$. Therefore, when dissimilar metal welding is carried out for P-No. 1 carbon steel and different P-No. low alloy steel, the PWHT temperature should be carefully selected to avoid significant deterioration of impact properties for P-No. 1 carbon steel.

운전압력 상향을 위한 천연가스배관의 신뢰성 검토 (Reliability Assessment for Pressure Uprating of Natural Gas Transmission Pipelines)

  • 백종현;김우식
    • 한국가스학회지
    • /
    • 제15권5호
    • /
    • pp.1-6
    • /
    • 2011
  • 국내 천연가스 주배관의 가스공급 최대허용운전압력이 6.86 MPa로 제한된 현재 상황에서 배관 관말압력저하를 해소하기 위해서는 배관을 증설 할 수밖에 없는데 이 경우 상당한 비용이 수반된다. 따라서 기존 배관과 설비를 활용한 해결 방안으로 송출압력을 더 높여 배관 운전압력을 상향 조정하여 공급하는 방법을 검토하였다. 배관에 대한 건전성 검토결과, 현재 시공된 배관은 7.85 MPa까지의 운전압력에서도 사용 가능하며, 연성파괴에 대한 저항성을 나타내는 충격흡수에너지는 ASME B31.8에서 요구하는 수치보다 더 높은 값을 가지고 있으며, 외부충격손상시 배관 변형을 위한 소요 하중은 배관 내압 증가에 따라 증가하였다. 그러나 배관의 운전압력이 증가함에 따라 가스 폭발 시 피해범위는 증가한다.

Intra-ply, inter-ply and FG hybrid composites based on basalt and poly-ester fibers: Flexural and impact properties

  • Ehsan Fadayee Fard;Hassan Sharifi;Majid Tehrani;Ehsan Akbari
    • Advances in materials Research
    • /
    • 제12권1호
    • /
    • pp.67-81
    • /
    • 2023
  • Basalt and poly-ester fibers along with epoxy resin were used to produce inter-ply, intra-ply and functionally gradient hybrid composites. In all of the composites, the relative content of basalt fiber to poly-ester fiber was equal to 50 percent. The flexural and charpy impact properties of the hybrid composites are presented with particular regard to the effects of the hybrid types, stacking sequence of the plies, loading direction and loading speed. The results show that with properly choosing the composition and the stacking sequence of the plies; the inter-ply hybrid composites can achieve better flexural strength and impact absorption energy compared to the intra-ply and functionally gradient composites. The flexural strength and impact absorption energy of the functionally gradient hybrid composites is comparable to, or higher than the intra-ply sample. Also, by increasing the loading speed, the flexural strength increases while the flexural modulus does not have any special trend.

35톤급 FRP선박 외판자재의 충격파괴거동에 관한 연구 (A Study on the Impact Fracture Behavior of Side Plate for G/T 35ton Class FRP Vessel)

  • 이진정
    • 선박안전
    • /
    • 통권25호
    • /
    • pp.64-76
    • /
    • 2008
  • This paper describes the failure mechanism and Charpy impact test of Fiber glass Reinforced Plastic composites which it was actually used for side plate of vessel. There are two examinations. The examination I, the specimens which it given temperature range $-25^{\circ}C$-$50^{\circ}C$ and with different initial notch length did impact test and then it compared impact energy(Uc) and impact fracture toughness(GIC). The examination II, the specimens which it putted into fresh water and sea water for scheduled hours did impact test and it compared impact energy(Uc) and impact fracture toughness(GIC). From examination I, it showed that impact energy(Uc) and impact fracture toughness(GIC) were peak at ambient temperature and decrease as temperature reduced. Fracture toughness(GIC) showed increase as initial notch length reduced. From examination II, impact energy(Uc) and impact fracture toughness(GIC) tended to increase which specimens putted in fresh water compared with sea water and maximum tolerance rate tend to decrease as permeation hours will be long.

  • PDF

GF/PP 복합재료의 충격파괴거동에 대한 온도효과 (Temperature Effect on Impact Fracture Behavior of GF/PP Composites)

  • 고성위;엄윤성
    • 수산해양기술연구
    • /
    • 제41권1호
    • /
    • pp.78-84
    • /
    • 2005
  • The main goal of this work is to study the effects of temperature and volume fraction of fiber on the Charpy impact test with GF/PP composites. The critical fracture energy and failure mechanisms of GF/PP composites are investigated in the temperature range of 60^{\circ}C$ to -50^{\circ}C$ by impact test. The critical fracture energy increased as the fiber volume fraction ratio increased. The critical fracture energy shows a maximum at ambient temperature and it tends to decreases as temperature goes up or goes down. Major failure mechanisms can be classified such as fiber matrix debonding, fiber pull-out and/or delamination and matrix deformation.

계장화 충격시험법에 의한 구조용강 용접부의 동적 파괴인성에 관한 연구 (A Study on the Dynamic Fracture Toughness of Welding Structural Steels by Instrumented Impact Testing)

  • 김헌주;김경민;윤의박
    • Journal of Welding and Joining
    • /
    • 제11권1호
    • /
    • pp.42-51
    • /
    • 1993
  • In this study, investigations were conducted in calculating parameters of elastic-plastic fracture mechanics using single specimen. The validity of these testing methods was judged by the confirmation of multiple specimen method of stop block test. The results were as follows: In order to measure a fracture toughness using the instrumented impact test, two general requirement must be considered; One, setting up proper impact velocity considered the effect of loading and the other, the necessity of low blow test for obtaining true energy by the compliance correction. It was possible to detect a crack initiation point by calculating the compliance changing rate from a load-defection curve. Criterion of a stable crack growth, $T_{mat}$ could be estimated by using key-curve method for a base metal. and combining Kaiser's rebound compliance with Paris-Hutchison's $T_{appl}$ equation for the brittled zone of welding heat affected.at affected.d.

  • PDF

Cu를 함유한 HSLA강의 기계적 성질 및 미세 조직에 미치는 시효처리의 영향 (A Study of the Ageing Treatment on the mechanical properties and microstructure of Cu-bearing HSLA steels)

  • 박태원;심인옥;김영우;강정윤
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 1994년도 특별강연 및 춘계학술발표 개요집
    • /
    • pp.39-43
    • /
    • 1994
  • The effects of ageing treatment on the mechanical properties of two Cu-bearing HSLA(High Strength Low Alloy) steels, HSLA-A and HSLA-B ,were studied by means of SEM, TEM, tensile, charpy impact and hardness tests. These steels showed excellent combination in strength and toughness at an ageing of $650^{\circ}C$ by the precipitation of $\varepsilon$-Cu and low carbon alloying. The peak strength was achieved at an ageing of 50$0^{\circ}C$ in both steels, while the impact energy was very low in this peak strength. With ageing temperature above this temperature, strength was decreased whereas impact energy increased. A marked increase in hardness above 675$^{\circ}C$ was associated with the formation of “M-A constituents” which forms during cooling from austenite-ferrite two phase region. The impact transition temperature of HSLA-A and HSLA-B steels were -l$25^{\circ}C$ and -145$^{\circ}C$, respectively.

  • PDF

크롬합금강의 동적파괴인성에 미치는 이온실화처리의 영향 (Influence of Ion-Nitriding on Dynamic Fracture Toughness in Cr Alloy Steels)

  • 오세욱;윤한기;장래웅;김기술
    • 한국해양공학회지
    • /
    • 제2권1호
    • /
    • pp.150-162
    • /
    • 1988
  • The dynamic fracture toughness, $K_{Id}$,is measured in the heat-treated and ion-nitrided Cr-Mo, Ni-Cr-Mo steel using standard and Precracked Charpy specimens an imstrumented impact machine. The value of $K_{Id}$and both the energy of initiate fracture, and the total energy of fracture. Since the $K_{Id}$values of the precraked impact specimens are in accord with their theoretical ones, this testing method is sufficently practical. The effect of ion-nitriding are found to be larger than the heat-treaded specimen.

  • PDF

Mechanical Strength Evaluation of A53B Carbon Steel Subjected to High Temperature Hydrogen Attack

  • Kim, Maan-Won;Lee, Joon-Won;Yoon, Kee-Bong;Park, Jai-Hak
    • International Journal of Safety
    • /
    • 제6권2호
    • /
    • pp.1-7
    • /
    • 2007
  • In this study mechanical strength of A53B carbon steel was analyzed using several types of test specimens directly machined from oil recycling pipe experienced a failure due to hydrogen attack in chemical plants. High temperature hydrogen attack (HTHA) is the damage process of grain boundary facets due to a chemical reaction of carbides with hydrogen, thus forming cavities with high pressure methane gas. Driven by the methane gas pressure, the cavities grow on grain boundaries forming intergranular micro cracks. Microscopic optical examination, tensile test, Charpy impact test, hardness measurement, and small punch (SP) test were performed. Carbon content of the hydrogen attacked specimens was dramatically reduced compared with that of standard specification of A53B. Traces of decarburization and micro-cracks were observed by optical and scanning electron microscopy. Charpy impact energy in hydrogen attacked part of the pipe exhibited very low values due to the decarburization and micro fissure formation by HTHA, on the other hand, data tested from the sound part of the pipe showed high and scattered impact energy. Maximum reaction forces and ductility in SP test were decreased at hydrogen attacked part of the pipe compared with sound part of the pipe. Finite element analyses for SP test were performed to estimate tensile properties for untested part of the pipe in tensile test. And fracture toughness was calculated using an equivalent strain concept with SP test and finite element analysis results.