• 제목/요약/키워드: Charge/discharge cycle

검색결과 277건 처리시간 0.03초

도전재 종류와 양에 따른 LiMn$_2$O$_4$정극의 충방전 용량 및 Cycle 안정성 (Charge/discharge capacity and cycle salability of LiMn$_2$O$_4$cathode by sorts and volume of conductive agent)

  • 정인성;박계춘;구할본
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1997년도 추계학술대회 논문집
    • /
    • pp.275-278
    • /
    • 1997
  • We investigated effectness of sort and volume of conductive agent to charge/discharge capacity of LiMn$_2$O$_4$. LiMn$_2$O$_4$is prepared by reacting stoichiometric mixture of LiOH . $H_2O$ and MnO$_2$(mole ratio 1 : 2) and heating at 80$0^{\circ}C$ for 24h, 36h, 48h, 60h and 72h. All LiMn$_2$O$_4$cathode active materials show spinel structure. Cathode active materials calcined at 80$0^{\circ}C$ for 36h, charge/discharge characteristics and cycle stability have remarkable advantages. Used that super-s-black and 20wt% as conductive agent in LiMn$_2$O$_4$, it is excellent than property of cathode used Acetylene black or mixture of Super-s-black and acetylene black at charge/discharge capacity and cycle stability. Also, specific efficiency of cathode is excellent as over 98% and that of first cycle is excellent as 92%.

  • PDF

Electrochemical Properties of Coal Tar Pitch based MCMB

  • Suh, Jeong-Kwon;Hong, Ji-Sook;Lee, Jung-Min
    • Carbon letters
    • /
    • 제5권3호
    • /
    • pp.118-126
    • /
    • 2004
  • MCMB (Mesocarbon microbeads) is a kind of anode material for lithium-ion secondary battery. MCMB charge/discharge cycle stability is one of the important criterion at lithium-ion battery operation. In this study, the cycling stability of a lithium-ion secondary battery has been examined. MCMB was made by the direct solvent extraction method. After the MCMB was carbonized and graphitized, the measurement of charge/discharge capacity and efficiency were carried out. In the result, discharge capacity of MCMB in the initial cycle was above 290.0 mAh/g. After the second cycle, efficiency of charge/discharge MCMB was about 98%. These results were similar to the commercial MCMB product.

  • PDF

Microelectromechnical system 소자를 위한 박막형 2차전지용 $SnO_2$ 음극박막의 충방전 특성 평가 (Charge/Discharge Characteristics of $SnO_2$ thin film as an anode of thin film secondary battery for microelectromechanical system device)

  • 남상철;조원일;전은정;신영화;윤영수
    • 한국진공학회지
    • /
    • 제9권1호
    • /
    • pp.36-41
    • /
    • 2000
  • $SnO-2$ thin films for thin film secondary battery anode were deposited n glass substrate with stain-less steel collector and charge/discharge experiments were conducted to investigate feasibility of $SnO-2$ thin film as a new anode material. The as-deposited films were pure $SnO-2$ phase which is not related to deposition condition. The grain size on the surface of as-deposited films increased with increase of oxygen partial pressure. However, the grain size did not show any change above oxygen partial pressure of 80:20. The surface roughness of the as-deposited films increased after decreasing because of resputtering effect of oxygen negative ion in plasma. All films showed typical $SnO-2$ anode characteristics which has a side effect at the first cycle, which is not related to the deposition condition. The charge/discharge experiments of 200cycles indicated that capacity of $SnO-2$ films depended on oxygen contents and surface roughness. The cycle characteristics was determined by initial charge/discharge reaction. The $SnO-2$ film with low initial capacity showed more stable cycle characteristics than film with high initial capacity.

  • PDF

EDLC를 위한 성능시험용 충방전기 개발 (Development of Charger/Discharger to Test Performance for EDLC)

  • 김금수;문종현;조현철;김동희
    • 조명전기설비학회논문지
    • /
    • 제26권7호
    • /
    • pp.16-22
    • /
    • 2012
  • With the increase of consumption of new renewable energy, the use of Electric Double Layer Capacitor(EDLC) is being gradually widened as the next generation energy storage device. In order to expand the market of EDLC which is recently receiving a lot of attraction as a new promising area, development of a charge/discharge cycle tester to measure and test performance, is essential. Therefore, this research designed a circuit to measure capacity and internal resistance and a circuit to measure voltage maintenance properties, based on EDLC's basic charging/discharging properties so it is able to measure the state of charge and discharge at high speed. When evaluating performance characteristics, the 5[V]/100[A] prototype-EDLC charge/discharge testing system developed for this research showed ${\pm}0.1$[%] of accuracy of voltage and current measurement. It was also proved that the developed charge/discharge testing system for EDLC can be applied to the actual industry, when testing the entire system using a program produced for data monitoring and acquisition.

The Surface Modification of Electrode with Solid Electrolyte Interphase for Hybrid Supercapacitor

  • Choi, Min-Geun;Kang, Soo-Bin;Yoon, Jung Rag;Lee, Byung Gwan;Jeong, Dae-Yong
    • Journal of Electrical Engineering and Technology
    • /
    • 제10권3호
    • /
    • pp.1102-1106
    • /
    • 2015
  • A hybrid supercapacitor (HS) is an energy storage device used to enhance the low weight energy density (Wh/kg) of a supercapacitor. On the other hand, a sudden decrease in capacity has been pointed out as a reliability problem after many charge/discharge cycles. The reliability problem of a HS affects the early aging process. In this study, the capacity performance of a HS was observed after charge/discharge. For detailed analysis of the initial charge/discharge cycles, the charge and discharge curve was measured at a low current density. In addition, a solid electrolyte interphase (SEI) layer was confirmed after the charge/discharge. A HC composed of a lithium titanate (LTO) anode and active carbon cathode was used. The charge/discharge efficiency of the first cycle was lower than the late cycles and the charge/discharge rate was also lower. This behavior was induced by SEI layer formation, which consumed Li ions in the LTO lattice. The formation of a SEI layer after the charge/discharge cycles was confirmed using a range of analysis techniques.

MgNi계 수소흡장합금의 충방전특성 (Charge-discharge Characteristic of the Mg-Ni Hydrogen Storage Alloy System)

  • 오명학;정원섭;김인곤
    • 한국수소및신에너지학회논문집
    • /
    • 제10권3호
    • /
    • pp.177-184
    • /
    • 1999
  • The charge-discharge characteristics of the $Mg_2Ni-x$ wt.%Nd (x = 0~3) electrodes were investigated. The electrodes were prepared by the mechanical grinding of the induction-melted $Mg_2Ni$ alloy powders with Ni and/or Nd using planetary ball mill apparatus. The discharge capacity of the $Mg_2Ni$ alloy increased with the increase in the nickel content. The electrode possessing 100 wt.% nickel powder showed the initial capacity of 760 mAh/g and the capacity decay with the cycle number was less than that of the 55 wt.% nickel powder. The Nd was added to this composition. It was found that the $Mg_2Ni-100$ wt.%Ni -0.2 wt.%Nd alloy showed an excellent charge-discharge cycle characteristics compared with the other reported Mg-Ni alloy system. The discharge capacity was 400 mAh/g after 70 cycles. Such an improved cycle life seems to be attributed to the improvement in the corrosion characteristics of the alloy. The anodic polarization curve of the $Mg_2Ni-100$ wt.%Ni-0.2 wt.%Nd alloy exhibited better passivating behavior than that of the $Mg_2Ni-100$ wt.%Ni.

  • PDF

카본을 부극으로 사용하는 $LiMnO_2$ 전지의 전기화학적 특성 (Charge/Discharge Characteristics of $LiMnO_2$ Battery using Carbon as Anode Materials)

  • 김은미;임승규;김남인;구할본
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 추계학술대회 논문집 Vol.21
    • /
    • pp.277-278
    • /
    • 2008
  • Orthorhombic $LiMnO_2$(o-$LiMnO_2$) has attracted public attentions as a cathode materials of Lithium ion battery because it has low cost and high theoretical discharge capacity of 285mAh $g^{-1}$. In our study, o-$LiMnO_2$ is synthesized by quenching method. To verify their phase structure, X-ray diffraction is accomplished. Test cells are assembled to check electrochemical characteristics using acquired o-$LiMnO_2$ cathode and carbon anode. Charge/Discharge cycling was carried out for 50cycles. And impedance was measured at 1, 2, 5, 10, 30, 50cycle. During cycle test, the max discharge capacity was recorded 139mAh $g^{-1}$ at 10cycle.

  • PDF

Li 치환된 $Li[Li_yMn_{2-y}]O_4$ 정극 활물질의 결정 구조와 충방전 용량과의 관계 (The relation of the crystal phase and the charge/discharge capacity of $Li[Li_yMn_{2-y}]O_4$ cathode materials substituted Li)

  • 정인성;구할본;박복기;손명모;이헌수
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2000년도 춘계학술대회 논문집 전자세라믹스 센서 및 박막재료 반도체재료 일렉트렛트 및 응용기술
    • /
    • pp.117-120
    • /
    • 2000
  • The relation of crystal phase and charge/discharge capacity of $Li[Li_yMn_{2-y}]O_4$ were studied for different degrees of Li substitution (y). All cathode material showed spinel phase based on cubic phase in X-ray diffraction. Other peaks didn't show in spite of the increase of y value in $Li[Li_yMn_{2-y}]O_4$. Ununiform of $Li[Li_yMn_{2-y}]O_4$ which calcinated by (111) face and (222) face was more stable than that of pure $LiMn_2O_4$. In addition, At TG analysis, calcined $Li[Li_{0.1}Mn_{1.9}]O_4$ exhibited much mass loss at $800{\mu}m$. The cycle performance of the $Li(Li_yMn_{2-y}]O_4$ was improved by the substitution of $Li^{1+}$ for $Mn^{3+}$ in the octahedral sites. Specially, $Li[Li_{0.08}Mn_{1.92}]O_4$ and $Li[Li_{0.1}Mn_{1.9}]O_4$ cathode materials showed the charge and discharge capacity of about 125mAh/g at first cycle, and about 95mAh/g after 70th cycle. It is excellent than that of pure $LiMn_2O_4$, which 125mAh/g at first cycle, 65mAh/g at 70th.

  • PDF

리튬이온전지의 열화손상에 의한 음향방출 신호 검출 (Detection of Acoustic Signal Emitted during Degradation of Lithium Ion Battery)

  • 최찬양;변재원
    • 비파괴검사학회지
    • /
    • 제33권2호
    • /
    • pp.198-204
    • /
    • 2013
  • 리튬이온전지의 충/방전 열화 과정에서 발생하는 음향방출 신호를 검출하여 누적카운트, 방전용량, 미세손상 사이의 상관관계를 확인하였다. 상용 리튬이온전지를 사용하여 가속 충/방전 싸이클 실험을 하면서 음향방출 신호를 수집하였다. 다수의 음향방출 신호가 전지의 충전 및 방전 과정에서 각각 검출되었다. 충/방전 열화 싸이클이 증가함에 따라 전지 용량은 감소하였고 음향방출 신호의 누적카운트는 증가하는 경향을 보였다. 충/방전 후 전지를 분해하여 내부 전극 손상을 관찰한 결과 전극 계면 박리 및 미소균열이 다수 확인되었으며, 이러한 기계적 손상이 음향방출원인 것으로 판단된다. 전지 방전용량과 음향방출 누적카운트 사이에는 선형의 상관관계가 있었으며, 이로부터 음향방출법을 이용한 리튬이온전지 열화 평가 가능성을 제안하였다.

리튬이온 전지의 충방전 특성에 대한 전산 모델링 (Computational Modeling of Charge-Discharge Characteristics of Lithium-Ion Batteries)

  • 이대현;윤도영
    • 에너지공학
    • /
    • 제20권4호
    • /
    • pp.278-285
    • /
    • 2011
  • 본 연구에서는 리튬이온 전지의 충 방전 특성에 관한 모델링과 전산모사를 수행하였다. 전지의 시스템 구성은 단순화된 2차원 형태의 단일셀에 대하여 모델링하였고, 공학적 편미분방정식 풀이자인 FEMLAB을 이용하여 288 K와 318 K 범위내에서 충방전 특성에 대한 열적 모델링을 수행하였다. 모델링에 채택한 물성치 변수들에 대하여 온도특성을 고려하였으며, 이를 통하여 전지의 특징적인 충방전의 사이클 변화와 충방전 전하량의 변화를 체계적으로 전산모사하였다. 그 결과 충방전 속도에 상관없이 충방전의 주기가 온도가 낮아질수록 짧아짐을 정량적으로 해석할 수 있었다. 이에 부가하여 전지내에서 리튬이온의 물질전달 현상을 해석하여, 전지의 충방전 특성과의 상관관계를 고찰하였다.