We investigated the fatigue crack propagation of base metal, weld metal and heat attected zone in 316L stainless steel. And we analysed acoustic emission signals during the fatigue test by time-frequency analysis method. The specimens of weld metal and HAZ had longer fatigue life and slower rate of crack propagation better than base metal. And as a result of time-frequency was 200-300 kHz was obtained by fatigue crack propagation and 500 kHz was obtained by dimple and separate of inclusion.
The major objective of this study is to investigate the fatigue life evaluation of immovability crossing for railway turnout by the field test. In railway engineering, an appliance is necessary to allow a vehicle to move from one track to another. This appliance came to be known technically as turnout. So, turnout is required very complex railway technologies such as rolling stock, track. Due to the plan under the application of high speed train, turnout are needed more stable far fatigue behaviors. It analyzed the mechanical behaviors of turnout crossing with propose its advanced technical type on the field test and fatigue evaluation far the dynamic fatigue characteristics. As a result, the advanced type crossing are obviously effective for the fatigue damage ratio and dynamic response which is non-modified type. The analytical and experimental study are carried out to investigate the passing path of contact surface and fatigue damage trend decrease dynamic stresses and deflections on advanced crossing type, And the advanced type reduce dynamic fatigue damage ratio and increase fatigue life(about each 38%) more than non-modified type. From the field test results of the servicing turnout crossing, it is evaluated that the modification of contact angle, weight, material and sectional properties is very effective fur ensure against fatigue risks.
Journal of the Korea Academia-Industrial cooperation Society
/
제19권8호
/
pp.456-465
/
2018
This study was conducted to examine the correlations between fatigue, health perception, happiness, and health promoting behaviors, and to identify the influencing factors on health promoting behaviors of clinical nurses in two general hospitals. Data were collected from 153 clinical nurses from February 5 to March 30, 2018. Data were collected through personal interviews using a questionnaire. Data were analyzed using t-test, one-way ANOVA, Pearson's correlation coefficients, and stepwise multiple regression. Fatigue according to the general characteristics showed significant differences in drinking and job stress. Health perception according to the general characteristics showed significant differences in disease. Happiness according to the general characteristics showed significant differences in marital status, type of work, clinical career, nursing unit satisfaction, economic level, and job stress. Health promoting behavior according to the general characteristics showed significant differences in clinical career and economic level. Health promoting behaviors showed significant positive correlations with health perception and happiness, but a significantly negative correlation with fatigue. Happiness and economic level, which accounted for 24% of the variance, were significant predictors influencing health promoting behavior in clinical nurses. To improve health promoting behavior in clinical nurses, it is necessary to develop a program that can raise the happiness considering the economic level.
Transactions of the Korean Society of Mechanical Engineers
/
제12권5호
/
pp.1097-1103
/
1988
This paper deals with surface crack behavior and the fatigue life prediction of notched specimens using the relation between surface crack length, a, and the cycle ratio, $N/N_{f}$. From the $a-N\;/\;N_{f}$ curves, UC(the upper limit curve), LC(the lower limit curve) and MC(the middle limit curve) were assumed and utilized to predict the fatigue life and crack growth rate. The data computed from the three assumed curves were compared with the experimental data. It has been found that in the stable crack growth region ($N/N_{f}=0.3-0.8$) fatigue life can be predicted within 20% errors. Using the characteristics of $a-N\;/\;N_{f}$ curve, it is possible to predict the $da/dN-K_{max}$ curve, the $da/dN-{\Delta}K_{{\varepsilon}_t}$ curve, and the $S-N_{f}$ curve.
As a key reinforcement connection between a tower and a substructure in offshore wind turbine system, the transition piece is inevitably subjected to cyclic dynamic environmental loads such as wind, current and wave. Therefore, well designed transition piece with high strength and good fatigue resistance is of great significance to the structural safety and reliability of offshore wind power systems. In this study, the structural behavior of the transition piece was studied by an extensive sets of finite element analyses. Three widely used types of transition piece were considered. The characteristics of stress development, fatigue life and weight depending on the type of the transition piece were investigated in the ultimate limit state (ULS) and the fatigue limit state (FLS) of a 5-MW offshore wind turbine to be placed in Korea. An optimal form of the transition piece was proposed based on this parametric study.
Transactions of the Korean Society of Mechanical Engineers
/
제12권4호
/
pp.738-746
/
1988
Fatigue crack propagation of duplex stainless steel weldments was studied to develop further phenomenological understanding of the influences of welding heat cycle accompanying microstructural changes. Fatigue tests were carried out under constant amplitude of load in air at room temperature. The results showed that the crack propagation rate was different in base metal, heat affected zone and welding line. The crack propagation behavior in each part of duplex stainless steel was strongly dependent on phase ratio(.gamma../.alpha.) and several factors of microstructure also affected this propagation behavior. The fractographic feature in each part of steel were discussed on crack propagation behaviors.
Proceedings of the Korea Concrete Institute Conference
/
한국콘크리트학회 1997년도 봄 학술발표회 논문집
/
pp.527-533
/
1997
The purpose of this study is to investigate the fatigue behavior of the reinforced concrete beams strengthened with steel plate and CFS(csrbon fiber sheet). In this study, fatigue loads of 60 to 80 percent of the ultimate strength are applied to the specimens. From the results of test the beams strengthened with steel plate show the flexural failure mode, while the specimens strengthened with CFS fail by separation between CFS and concrete surface. In case of the stress level of 70%, strength degradations of the beams with steel plate and CFS in normalized flexural rigidity at 5,000 cycles is 24 and is 24 and 28 percent respectively.
Transactions of the Korean Society of Automotive Engineers
/
제9권3호
/
pp.181-189
/
2001
For the Tailor Welded Blank sheet used fur automobile body panel, the characteristics of fatigue crack propagation behavior were studied. The thickness of specimen was machined to be same (0.9+0.9mm) and different (0.9+2.0mm). As a base test, mechanical properties around welding zone were examined. The results indicated that there were no significant decreases in mechanical properties, but hardness around welding bead is 2.3 times greater than base material. The crack propagation rate was noticeably decreased around welding line and rapidly increased as it passed by welding line. Reviewing the shape of the crack propagation, crack width around welding line was wide around the welding zone due to retardation of crack growth, but it became narrow passing welding line due to decreased toughness. Elasto-Plastic analysis was performed by finite element analysis fur explaining the test results.
The fatigue life of welded joints is associated with crack initiation and propagation life. Theses cannot be easily separated, since the definition of crack initiation is vague due to the initiation of multiple cracks that are distributed randomly along the weld toes. In this paper a method involving a notch strain and fracture mechanical approach, which considers the characteristics of welded joints, e.g. welding residual stress and statistical characteristics of multiple cracks, is proposed, in an attempt to reasonably estimate these fatigue lives. The fatigue crack initiation life was evaluated statistically, e.g. the probability of failure occurrence in 2.3, 50 and $97.7\%$, in which the cyclic response of the local stress/strain hi the vicinity of the weld toes and notch factors derived by the irregular shape of the weld bead are taken into account. The fatigue crack propagation life was simulated by using Monte-Carlo method in consideration of the Ad-factor and the mechanical behavior of mutual interaction/coalescence between two adjacent cracks. The estimated total fatigue life, $(N_T)_{P50\%}$, as a sum of crack initiation and propagation life under the probability of failure occurrence in $50\%$ showed a good agreement with the experimental results. The developed technique for fatigue lift estimation enables to provide a quantitative proportion of crack initiation and propagation life in the total fatigue life due to the nominal stress range, ${\Delta}S$.
In this paper, we investigated the characteristics of fatigue fracture on TB(Tailored Blank) weldment by comparing the fatigue crack propagation characteristics of base metal with those of TB welded sheet used for vehicle body panels. We also investigated the influence of center crack on the fatigue characteristic of laser weld sheet of same thickness. We conducted an experiment on fatigue crack propagation on the base metal specimen of 1.2mm thickness of cold-rolled metal sheet(SPCSD) and 2.0mm thickness of hot-rolled metal sheet(SAPH440) and 1.2+2.0mm TB specimen. We also made an experiment on fatigue crack propagation on 2.0+2.0mm and 1.2+1.2mm thickness TB specimen which had center crack. The characteristics of fatigue crack growth on the base metal were different from those on 1.2+2.0mm thickness TB specimen. The fatigue crack growth rate of the TB welded specimens is slower in low stress intensity factor range $({\Delta}K)$ region and faster in high${\Delta}K$ region than that of the base metal specimens. The slant crack angle slightly influenced the crack propagation of the TB specimen of 2.0+2.0mm thinkness.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.