• Title/Summary/Keyword: Ceramic microstructure

Search Result 1,359, Processing Time 0.028 seconds

Low k Materials for High Frequency High Integration Modules (고주파대응 고집적 모듈용 저유전율 소재)

  • Na, Yoon-Soo;Hwang, Jong-Hee;Lim, Tae-Young;Shin, Hyo-Soon;Kim, Jong-Hee;Cho, Yong-Soo
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.06a
    • /
    • pp.328-328
    • /
    • 2008
  • As a low K material for high frequency high integration modules, glass/ceramic composites were investigated. Glass composition were selected from $SiO_2-B_2O_3-Al_2O_3-R_2O$-RO system which having very low dielectric constant and cordierite was used as a ceramic filler. These composites were sintered at temperature range from $850^{\circ}$ to $950^{\circ}$ and XRD, SEM microstructure analysis of sintered bodies were performed for understanding sintering behavior. Any crystallization was not occurred and dense sintered bodies were attained. Dielectric and mechanical properties of these sintered glass/cordierite composites were analysed by network analyzer and UTM. Glass/ceramic composite with 50 wt% cordierite showing a dielectric constant (${\varepsilon}_r$) of 5.4, Q${\times}f_0$ (Q) of 1600 at 1 GHz and maximum bending strength of 163 MPa was attained.

  • PDF

Analysis of Composite Response Based on Microstructure Details (복합재료의 미시특성에 따른 기계적 특성해석)

  • 김태우
    • Journal of the Korean Ceramic Society
    • /
    • v.40 no.8
    • /
    • pp.784-790
    • /
    • 2003
  • Present investigation shows the analysis results for ceramic reinforced metal matrix composite under uniaxial transverse tensile loading. The resulting deformation, the projected damage type, and stress-strain behavior were computed depending on microstructure details such as the type of periodic reinforcement array, and the type of interface bonding. A two-dimensional finite element analysis was conducted based on the unit-cell of square, hexagonal, or diagonal periodic away For composite with strong interface bonding, the transverse stress vs. strain curve was generally increased with the increase of the ceramic volume fraction. For the composite with weakly bonded interface, however, the transverse stress vs. strain curve was reduced against the ceramic volume fraction. The decrease was caused by the interface debonding-induced stiffness reduction of the composite. For the composite of weakly bonded interface, the relative reduction rate in the final limit stress for hexagonal array was larger than that for square array. Outcome of the present study was compared favorably with the published literature data.

Fabrication and Characteristics of Thermal Barrier Coatings in the La2O3-Gd2O3-ZrO2 System by Using Suspension Plasma Spray with Different Suspension Preparations (서스펜션의 준비방법에 따른 서스펜션 플라즈마 용사를 이용한 La2O3-Gd2O3-ZrO2 계 열차폐코팅의 제조와 특성)

  • Lee, Soyul;Lee, Sung-Min;Oh, Yoon-Suk;Kim, Hyung-Tae;Nahm, Sahn;Kim, Seongwon
    • Journal of the Korean institute of surface engineering
    • /
    • v.49 no.6
    • /
    • pp.595-603
    • /
    • 2016
  • Rare-earth zirconates, including lanthanum zirconate and gadolinium zirconate, have been investigated as ones of the most promising candidates for next-generation thermal barrier coating (TBC) materials due to their excellent properties such as low thermal conductivity, chemical stability at high temperature and so on. In this study, TBCs with three compositions, in the $La_2O_3-Gd_2O_3-ZrO_2$ system with reduced rare-earth contents from $RE_2Zr_2O_7$ compositions, were fabricated by using suspension plasma spray with different suspension preparation methods. The phase formation, microstructure, and thermal properties of TBCs were examined. In particular, each coating exhibited single fluorite phase and a dense, vertically-separated microstructure. The potential of coatings with rare-earth zirconates for TBC applications was also discussed.

Effect of $Al_2O_3$ Particle Size on Thermal Properties of Glass-Ceramics for LTCC Material (저온동시소성용 결정화 유리의 필러 사이즈가 열적 특성에 미치는 영향)

  • Kim, Jin-Ho;Hwang, Seong-Jin;Lee, Sang-Wook;Kim, Hyung-Sun
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2007.11a
    • /
    • pp.281-281
    • /
    • 2007
  • Low Temperature Co-fired Ceramic (LTCC) technology has been used in electronic device for various functions. LTCC technology is to fire dielectric ceramic and a conductive electrode such as Ag or Cu thick film below the temperature of $900^{\circ}C$ simultaneously. The glass-ceramic has been widely used for LTCC materials due to its low sintering temperature, high mechanical properties and low dielectric constants. To obtain the high strength, addition of filler, the microstructure should have various crystals and low pores in a composite. In this study, two glass frits were mixed with different alumina size(0.5, 2, 3.7um) and sintered at the range of $850{\sim}950^{\circ}C$. The microstructure, crystal phases, thermal and mechanical properties of the composites were investigated using FE-SEM, XRD, TG-DTA, Dilatomer. When the particle size of $Al_2O_3$ filler increased, the starting temperatures for the densification of the sintered bodies, onset point of crystallization, peak crystallization temperature in the glass-ceramic composites decreased gradually. After sintered at $900^{\circ}C$, the glass frits were crystallized as $CaAl_2Si_2O_8\;and\;CaMgSi_2O_6$. The purpose of our study is to understand the relationship between the $Al_2O_3$ particle size and thermal properties in composites.

  • PDF

Microstructure and Positive Temperature Coefficient of Resistivity Characteristics of Na2Ti6O13-Doped 0.94BaTiO33-0.06(Bi0.5Na0.5)TiO3 Ceramics (Na2Ti6O13를 도핑한 0.94BaTiO3-0.06(Bi0.5Na0.5)TiO3 세라믹스의 미세구조와 Positive Temperature Coefficient of Resistivity 특성)

  • Cha, Yu-Joung;Jeong, Young-Hun;Lee, Young-Jin;Paik, Jong-Hoo;Lee, Wu-Young;Kim, Dae-Joon
    • Korean Journal of Materials Research
    • /
    • v.20 no.11
    • /
    • pp.575-580
    • /
    • 2010
  • The microstructure and positive temperature coefficient of resistivity (PTCR) characteristics of 0.1 mol%$Na_2Ti_6O_{13}$ doped $0.94BaTiO_3-0.06(Bi_{0.5}Na_{0.5})TiO_3$ (BBNT-NT001) ceramics sintered at various temperatures from $1200^{\circ}C$ to $1350^{\circ}C$ were investigated in order to develop eco-friendly PTCR thermistors with a high Curie temperature ($T_C$). Resulting thermistors showed a perovskite structure with a tetragonal symmetry. When sintered at $1200^{\circ}C$, the specimen had a uniform microstructure with small grains. However, abnormally grown grains started to appear at $1250^{\circ}C$ and a homogeneous microstructure with large grains was exhibited when the sintering temperature reached $1325^{\circ}C$. When the temperature exceeded $1325^{\circ}C$, the grain growth was inhibited due to the numerous nucleation sites generated at the extremely high temperature. It is considered that $Na_2Ti_6O_{13}$ is responsible for the grain growth of the $0.94BaTiO_3-0.06(Bi_{0.5}Na_{0.5})TiO_3$) ceramics by forming a liquid phase during the sintering at around $1300^{\circ}C$. The grain growth of the BBNT-NT001 ceramics was significantly correlated with a decrease of resistivity. All the specimens were observed to have PTCR characteristics except for the sample sintered at $1200^{\circ}C$. The BBNT-NT001 ceramics had significantly decreased $\tilde{n}_{rt}$ and increased resistivity jump with increasing sintering temperature at from $1200^{\circ}C$ to $1325^{\circ}C$. Especially, the BBNT-NT001 ceramics sintered at $1325^{\circ}C$ exhibited superior PTCR characteristics of low resistivity at room temperature ($122\;{\Omega}{\cdot}cm$), high resistivity jump ($1.28{\times}10^4$), high resistivity temperature factor (20.4%/$^{\circ}C$), and a high Tc of $157.9^{\circ}C$.

Preparation and Characterization of SiC Coated Graphite Foam (SiC가 코팅된 그라파이트 Foam의 제조 및 특성 분석)

  • Kyung, Jae-Jin;Kim, Jung-Ju;Kim, Soo-Ryong;Kwon, Woo-Teck;Cho, Kwang-Youn;Kim, Young-Hee
    • Journal of the Korean Ceramic Society
    • /
    • v.44 no.11
    • /
    • pp.622-626
    • /
    • 2007
  • Graphite is widely used in electronic industry due to its excellent electrical and thermal properties. However, graphite starts to oxidize around $400^{\circ}C$ that seriously degrades its properties. SiC coating can be applied to graphite foam to improve its high temperature oxidation resistance. In this research, SiC coating on graphite foam was made via preceramic polymer using a polyphenylcarbosilane. 20% of polyphenylcarbosilane in hexane solution was coated onto graphite by dip coating method. Thermal oxidation was carried out at $200^{\circ}C$ for crosslink of the preceramic polymer and the sample were pyrolysized at $800^{\circ}C{\sim}1200^{\circ}C$ under nitrogen to convert the preceramic polymer to SiC film. The microstructure of the SiC coating after pyrolysis was investigated using FESEM and oxidation resistance up to $800^{\circ}C$ was evaluated.

Structural Analysis and Characterization of PZT Fiber Fabricated by Electrospinning (Electrospinning법으로 제조된 PZT 섬유의 구조분석 및 특성평가)

  • Park, Chun Kil;Yun, Ji Sun;Jeong, Young Hun;Nam, Joong-Hee;Cho, Jeong Ho;Paik, Jong-Hoo;Jeong, Dae Young
    • Journal of the Korean Ceramic Society
    • /
    • v.50 no.6
    • /
    • pp.466-469
    • /
    • 2013
  • Currently, piezoelectric ceramics are being applied in various fields, such as ultrasonic sensors, vibration devices, sound filters, and various energy conversion devices. Flexible piezoelectric ceramics are widely studied in an effort to mitigate the disadvantages of their brittle and inductile properties. Structural damage to piezoelectric fibers is much less than that to thin films when piezoelectric fibers are twisted or bent. Therefore, stretchable devices can be fabricated if piezoelectric fibers are obtained using an elongated substrate. In this study, sintering processes of PZT ($Pb(Zr_{0.53}Ti_{0.47})O_3$) fibers prepared by electrospinning were optimized through the TGA and XRD analyses. The crystal structure and microstructure of the piezoelectric fibers were investigated by XRD, FE-SEM and TEM.

Monte Carlo Simulation of Densification during Liquid-Phase Sintering

  • Lee, Jae Wook
    • Journal of the Korean Ceramic Society
    • /
    • v.53 no.3
    • /
    • pp.288-294
    • /
    • 2016
  • The densification process during liquid-phase sintering was simulated by Monte Carlo simulation. The Potts model, which had been applied to coarsening during liquid-phase sintering, was modified to include vapor particles. The results of two- and threedimensional simulations showed a temporal decrease in porosity, in other words, densification, and an increase in the average size of pores. The results also showed growth of solid grains and the effect of wetting angle on microstructure.

A Study for the Sintering of Boron Carbide ($B_4C$의 소결에 관한 연구)

  • 오정훈;오근호;이종근;김도경;이준근;김종희
    • Journal of the Korean Ceramic Society
    • /
    • v.22 no.1
    • /
    • pp.60-66
    • /
    • 1985
  • Hard shaped bodies are made by sintering a cold-pressed compact of a boron carbide compound which contains a densification aid. Titanium diboride and carbon were used as a densification aid in a range of 1% to 10% by weight. The effects of sintering temperature and additives on linear shrinkage porosity hardness bend strength and microstructure were examined. The initial partical size dependence on the sintered density was also discussed.

  • PDF

Synthesis of Sinter-active $Y_2O_3$ Powders Using Urea (요소를 이용한 활성 이트리아 분말의 합성)

  • 한주환
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.12
    • /
    • pp.1247-1253
    • /
    • 1997
  • Sinter-active yttria powders were prepared by a solution precipitation with using a self-decomposing precipitation agent NH2CONH2(urea). The cold-pressed powders can be sintered to full density and the microstructure of grains less than 200 nm at a temperature as low as 120$0^{\circ}C$. The activity of the yttria powder has been controlled by varying nucleation conditions during precipitation and by minimizing formation of aggregates. The type of precursor is decisive in preparation of a sinter-active oxide powder, and urea is desirable as a precipitation agent for an active yttrium oxide powder.

  • PDF