도말층 제거와 상아질의 부위가 치수강 내부 상아질에 대한 수종 상아질 결합제의 전단결합성질에 미치는 영향 (THE EFFECT OF SMEAR LAYER REMOVAL AND POSITION OF DENTIN ON SHEAR BOND PROPERTIES OF DENTIN BONDING SYSTEMS TO INTERNAL CERVICAL DENTIN)

  • 임연아;유영대;이용근;이수종;임미경
    • Restorative Dentistry and Endodontics
    • /
    • 제24권3호
    • /
    • pp.465-472
    • /
    • 1999
  • The aim of this study was to determine the shear bond properties of four dentin bonding systems to internal cervical dentin, and to investigate the effect of the pretreatment for removing smear layer and position of dentin on shear bond strength of dentin bonding agents. The materials tested in this study were consisted of four commercially available dentin bonding systems[Allbond 2(AB), Clearfil Linerbond 2(CL), Optibond FL(OP), Scotchbond Multi-purpose(SB)], a restorative light-cured composite resin[Z100]J and a chelating agent[RC-prep(RC)]. Fifty-six freshly extracted human molars were used in this study. Dentin specimens were prepared by first cutting the root of the tooth 1mm below the cementoenamel junction with a diamond bur in a high speed handpiece under air-water coolant, and then removing occlusal part at pulp horn level by means of a second parallel section, The root canal areas were exposed by means of cutting the dent in specimens perpendicular to the root axis. Dentin specimens were randomly assigned to two groups(pretreated group, not-pretreated group) based on the pretreatment method of dentin surface. In pretreated group, RC was applied to dentin surface for 1minute and then rinsed with NaOCl. In not-pretreated group, dentin surface was rinsed with saline Each groups were subdevided into four groups according to dentin bonding systems. Four dentin bonding systems and a restorative resin were applied according to the directions of manufacturer. The dentin-resin specimens were embedded in a cold cure acrylic resin, and were cut with a low speed diamond saw to the dimension of $1{\times}1mm$. The cut specimens were divided into three groups according to the position of internal cervical dentin. The shear bond properties of dentin-resin specimens were measured with Universal testing machine (Zwick, 020, Germany) with the cross head speed of 0.5mm/min. From this experiment. the following results were obtained : 1. In case of shear bond strength, there was no significant difference among dentin bonding systems in not-pretreated groups, whereas in pretreated groups, the shear bond strengths of AB and of SB were statistically significantly higher than those of CL and of OP. 2. The shear bond strengths of AB and of SB in pretreated groups were significantly higher than those in not-pretreated groups. 3. The shear bond strengths of radicular layer of OP were higher than those of occlusal layer of OP in not-pretreated groups, and of AB in pretreated groups. The shear bond strengths of radicular layer of AB and of CL in not-pretreated groups were higher than those in pretreated group.

  • PDF

치주질환으로 발거된 한국인 다근치 치근본체의 특성 (The characteristics of Korean multi-rooted teeth root trunk extracted by periodontal disease)

  • 박현영;조수진;문익상
    • Journal of Periodontal and Implant Science
    • /
    • 제31권3호
    • /
    • pp.573-579
    • /
    • 2001
  • The purpose of this study was to investigate the characteristiss of korean multi-rooted teeth extracted by periodontal disease. A total of 182 extracted multi-rooted teeth were examined. The distance from the cementoenamel junction(CEJ) to the root groove and from the CEJ to the root division was measured. The frequency of the root grooves were calculated. The results are as follows : 1. Distances from CEJ to the root groove were $1.53{\cdot}1.60mm$ for maxillary first premolars mesial${\cdot}$distal sides, $1.26{\cdot}1.38{\cdot}1.75mm$ for maxillary first molars buccal${\cdot}$mesial${\cdot}$distal sides, $1.38{\cdot}1.71{\cdot}1.41mm$ for maxillary second molars buccal${\cdot}$mesial${\cdot}$distal sides, $0.98{\cdot}0.99mm$ for mandibular first molars buccal${\cdot}$lingual sides and $1.28{\cdot}1.35mm$ for mandibular second molars buccal${\cdot}$lingual sides. 2. The frequency of the root grooves were $17.4{\cdot}30.4%$ for maxillary first premolars mesial${\cdot}$distal sides, $44.4{\cdot}84.1{\cdot}67.5%$ for maxillary first molars buccal${\cdot}$mesial${\cdot}$distal sides, $100{\cdot}90.3{\cdot}90.3%$ for maxillary second molars buccal${\cdot}$mesial${\cdot}$distal sides, $42.9{\cdot}77.8%$ for mandibular first molars buccal${\cdot}$lingual sides and 90.6% for mandibular second molars buccal${\cdot}$lingual sides. 3. Distances from CEJ to the root division were $6.8{\cdot}7.2mm$ for maxillary first premolars mesial${\cdot}$distal sides, $3.3{\cdot}4.38{\cdot}4.34mm$ for maxillary first molars buccal${\cdot}$mesial${\cdot}$distal sides, $3.67{\cdot}4.8{\cdot}4.07mm$ for maxillary second molars buccal${\cdot}$mesial${\cdot}$distal sides, $3.1{\cdot}3.89mm$ for mandibular first molars buccal${\cdot}$lingual sides and $3.2{\cdot}4.06mm$ for mandibular second molars buccal${\cdot}$lingual sides.

  • PDF

한국인의 상악 전치부 순측골 두께와 치은 생체형(gingival biotype)의 상관관계 (Relationship between the facial bone thickness and gingival biotype of the anterior maxilla in Koreans)

  • 박지훈;김은강;김형민;주지영;이주연
    • 구강회복응용과학지
    • /
    • 제31권3호
    • /
    • pp.169-177
    • /
    • 2015
  • 목적: 한국인의 상악 전치부 순측골 두께와 치은 생체형(gingival biotype)의 분포 및 상관관계를 평가하는 것이다. 연구 재료 및 방법: 본 연구는 부산대학교치과병원에 내원한 57명의 환자, 335개의 치아를 대상으로 시행되었다. Cone Beam Computed Tomography (CBCT)를 이용하여 백악법랑경계로부터 4 mm, 6 mm, 8 mm 지점의 순측골 두께를 측정하였고, 치은 생체형은 치주탐침자를 이용하여 평가하였다. 결과: 대부분의 대상치아에서 1 mm 이하의 얇은 순측골(4 mm 지점 87%, 6 mm 지점 88%, 8 mm 지점 90%)이 우세하게 관찰되었고, 전체 대상자의 21%에서 얇은 치은 생체형이 확인되었다. 치은 생체형과 순측골 두께 사이의 유의한 상관관계는 존재하지 않았다. 결론: 성공적인 전치부 심미 임플란트 치료를 위해서는 치은 생체형 검사 같은 임상적 검사 이외에 순측골 평가를 위한 추가적 CBCT 등의 방사선 검사가 필수적이다.

근관내 약제가 규산칼슘 기반 재료의 압출 강도에 미치는 영향 (Effect of Intracanal Medicaments on Push-out Bond Strength of Calcium Silicate-based Materials)

  • 정현태;양선미;김선미;최남기;김재환
    • 대한소아치과학회지
    • /
    • 제45권4호
    • /
    • pp.455-463
    • /
    • 2018
  • 이 연구의 목적은 근관 내 약제가 규산칼슘 재료의 압출 강도(Push-out bond strength)에 미치는 영향을 평가하는 것이다. 단일 근관을 가진 40개의 인간 하악 소구치들은 대조군과 수산화칼슘, 이중 항생제, 삼중 항생제를 사용한 군 중 하나로 나뉘어졌다. 근관 세척을 통해 약제를 제거 후, 1 mm 두께로 시편들을 제작하였다. 그 후 ProRoot MTA$^{(R)}$와 Biodentine$^{(R)}$을 근관 내에 적용하였고, 압출 강도 실험과 파절 양상 관찰을 수행하였다. 삼중 항생제와 이중 항생제 군은 대조군과 비교하여 두 종류의 규산칼슘 기반 재료의 상아질 결합력에서 유의한 영향을 미치지 않았고, 수산화칼슘을 사용한 군은 유의한 결합력의 증가를 나타내었다. 대조군과 각각의 실험군 내에서 치근 상아질에 대한 Biodentine$^{(R)}$의 탈락 저항은 ProRoot MTA$^{(R)}$보다 크게 나타났다. 파절 양상에 따라 응집 파절, 혼합 파절, 접착 파절의 순서로 압출 강도의 유의한 감소가 나타났고, 대조군과 비교하여 수산화칼슘을 사용한 군에서는 응집 파절이, 항생제를 사용한 군에서는 접착 파절이 우세하였다.

응축형 복합레진 수복시 유동성 레진 이장이 변연부 미세누출에 미치는 영향 (THE EFFECT OF FLOWABLE RESIN LINING ON THE MARGINAL MICROLEAKAGE OF CONDENSABLE RESIN RESTORATION)

  • 문주훈;고근호
    • Restorative Dentistry and Endodontics
    • /
    • 제26권1호
    • /
    • pp.16-22
    • /
    • 2001
  • The purpose of this study was to evaluate the marginal microleakage of condensable composite resin restorations according to flowable resin lining of internal cavity wall. The eighty extracted human molar teeth without caries and/or restorations are used The experimental teeth were randomly assigned into four groups of ten teeth each. Eighty caries-free extracted human molars were used in this study. The conventional class II cavities (box-shaped on mesial and distal surface, faciolingual width : 3mm, gingival wall depth : 1.5mm) were prepared 1mm below cementoenamel junction with a # 701 carbide bur. The teeth were divided into four groups, and then each group were subdivided into A & B group according to flowable resin & compomer lining ; Group 1-A : Tetric Ceram filling, Group 1-B : Tetric Flow lining and Tetric Ceram filling, Group 2-A Ariston pHc filling, Group 2-B : Tetric Flow lining and Ariston pHc filing, Group 3-A SureFil filling, Group 3-B : Dyract Flow lining and SureFil filling, Group 4-A : Pyramid filling, Group 4-B : Aeliteflo lining and Pyramid filling. To simulate as closely as possible the clinical situation during retoration placement, a "restoration template" was fabricated, and the condensable resin was filled using a three-sited light-curing incremental technique. All the materials used were applied according to the manufacturers' instructions. The specimens were stored in the 100% humidity for 7 days prior to thermocycling (100 thermal cycles of 5~55$^{\circ}C$ water with a 30-second dwell time) The specimens were immersed in 2% metyleneblue dye for 24 hours, and then embedded in transparent acrylic resin and sectioned mesiodistally with diamond wheel saw. The degree of marginal leakage was scored under stereomicroscope ($\times$20) and the data were analyzed by Kruskal-Wallis test and Wilcoxon signed ranks test. The results were as follows : 1. In the gingival margins of all the group, microleakage of subgroup B was less than subgroup A. 2. In the group 1, 2, 4, there was significant differences between subgroup A and B (p<0.05), but in the group 3, there was not significant different between group 3-A (SureFil) and group 3-B (Dyract flow/SureFil) (p>0.05). 3. In the subgroup A and B, there was significant different between all group except group 4 of subgroup A. From the results above, it was suggested that the cavity lining of flowable resin and flowable compomer in condensable resin restoration decrease microleakage at gingival margin, and does improve their ability to seal the gingival margin of class II preparation.

  • PDF

Periodontal healing using a collagen matrix with periodontal ligament progenitor cells in a dehiscence defect model in beagle dogs

  • Yoo, Seung-Yoon;Lee, Jung-Seok;Cha, Jae-Kook;Kim, Seul-Ki;Kim, Chang-Sung
    • Journal of Periodontal and Implant Science
    • /
    • 제49권4호
    • /
    • pp.215-227
    • /
    • 2019
  • Purpose: To histologically characterize periodontal healing at 8 weeks in surgically created dehiscence defects in beagle dogs that received a collagen matrix with periodontal ligament (PDL) progenitor cells. Methods: The bilateral maxillary premolars and first molars in 6 animals were used. Standardized experimental dehiscence defects were made on the buccal side of 3 premolars, and primary culturing of PDL progenitor cells was performed on the molars. Collagen matrix was used as a scaffold and a delivery system for PDL progenitor cells. The experimental sites were grafted with collagen matrix (COL), PDL progenitor cells with collagen matrix (COL/CELL), or left without any material (CTL). Histologic and histomorphometric analyses were performed after 8 weeks. Results: The defect height from the cementoenamel junction to the most apical point of cementum removal did not significantly differ across the CTL, COL, and COL/CELL groups, at $4.57{\pm}0.28$, $4.56{\pm}0.41$, and $4.64{\pm}0.27mm$ (mean ${\pm}$ standard deviation), respectively; the corresponding values for epithelial adhesion were $1.41{\pm}0.51$, $0.85{\pm}0.29$, and $0.30{\pm}0.41mm$ (P<0.05), the heights of new bone regeneration were $1.32{\pm}0.44$, $1.65{\pm}0.52$, and $1.93{\pm}0.61mm$ (P<0.05), and the cementum regeneration values were $1.15{\pm}0.42$, $1.81{\pm}0.46$, and $2.57{\pm}0.56mm$ (P<0.05). There was significantly more new bone formation in the COL/CELL group than in the CTL group, and new cementum length was also significantly higher in the COL/CELL group. However, there were no significant differences in the width of new cementum among the groups. Conclusions: PDL progenitor cells carried by a synthetic collagen matrix may enhance periodontal regeneration, including cementum and new bone formation.

상아질-레진 계면의 공초점 현미경적 형태 및 전단결합강도와의 관계 (CONFOCAL LASER SCANNING MICROSCOPIC MORPHOLOGY OF DENTIN-RESIN INTERFACE AND ITS RELATIONSHIP WITH SHEAR BOND STRENGTH)

  • 최낙원;조병훈;손호현
    • Restorative Dentistry and Endodontics
    • /
    • 제24권2호
    • /
    • pp.310-321
    • /
    • 1999
  • In this in vitro study, confocal laser scanning microscopic morphology of dentin-resin interface and its relationship to shear bond strength were investigated after the exposed dentin surfaces were treated with 3 different kinds of dentin adhesive systems[three-step; Scotchbond Multi-Purpose Plus(SMPP), self-priming bonding resin; Single Bond(SB), self-etching primer; Clearfil Liner Bond 2(LB2)]. 52 extracted human molar teeth without caries and/or restorations. The experimental teeth were randomly divided into three groups of seventeen teeth each. In five teeth of each group, class V cavities(depth: 1.5mm) with 900 cavosurface angles were prepared at the cementoenamel junction on buccal and lingual surfaces. Bonding resins of each dentin adhesive system were mixed with rhodamine B. Primer of SMPP was mixed with fluorescein. In group 1. the exposed dentin was conditioned with etchant, applied with above primer and bonding resin of SMPP. In group 2, with etchant and self-priming bonding agent of SB. In group 3, with self-etching primer and bonding agent of LB2. After treatment with dentin adhesive systems, composite resin were applied and photocured. The experimental teeth were cut longitudinally through the center line of restoration and grounded so that about $90{\mu}m$-thick wafers of buccolingually orientated dentin were obtained. And, $70{\sim}80{\mu}m$-thick wafers sectioned horizontally, thus presenting a dentinal tubules at 900 to the cut surface of a remaining tooth, were obtained. Primer of SMPP mixed with rhodamine B was applied to these wafers. Confocal laser scanning microscopic investigations of these wafers were done within of 24 hours after treatment. To measure shear bond strength, the remaining twelve teeth of each group were grounded horizontally below the dentinoenamel junction, so that no enamel remained. After applying dentin adhesive systems on the dentin surface, composite was applied in the shape of cylinder. The cylinder was 5mm in diameter, and 2mm in thickness. Shear bond strength was measured using Instron with a cross-head speed of 0.5mm/min. It was concluded as follows ; 1. Hybrid layer of SMPP(mean: $4.56{\mu}m$) was thicker than that of any other groups. This value was not statistically significant thicker than that of SB(mean: $3.41{\mu}m$, p>0.05), and significant thicker than that of LB2(mean: $1.56{\mu}m$, p<0.05). There was a statistical difference between SB and LB2(p<0.05). 2. Although there were variations in the length of resin tag even in a sample, and in a group, most samples in SMPP and SB showed resin tags extending above $20{\mu}m$. But samples in LB2 showed resin tags of $10{\mu}m$ at best. 3. Besides primer's infiltration into demineralized peritubular dentin and dentinal tubules, fluorophore of primer was detected in the lateral branches of dentinal tubules. 4. All groups demonstrated statistically significant differences from one another(p<0.05), with shear bond strengths given in descending order as follows: SMPP(18.3MPa), SB(16.0MPa) and LB2(12.4MPa). 5. LB2 having thinnest hybrid layer($1.56{\mu}m$) showed the lowest shear bond strength(12.4MPa).

  • PDF

우로수데옥시콜릭산이 치주질환 억제에 미치는 영향 (A Short-Term Study of the Effects of UDCA on Gingival Inflammation in the Beagle Dog)

  • 박상현;한승민;최상목;구영;류인철;한수부;이학모;김문무;김상년;정종평
    • Journal of Periodontal and Implant Science
    • /
    • 제29권1호
    • /
    • pp.1-14
    • /
    • 1999
  • Ursodeoxycholic acid(UDCA) is a hydrophilic gall bladder acid and has been used as a effective drug for liver disease related to in1munity. This drug inhibits secretions of IL-2, IL-4, and $IFN-{\gamma}$ from T-cells and production of immunoglobulin from B-cells. Also it has been reported that UDCA inhibits production of IL-1 related to the progression of periodontal disease and activation of collagenases. The purpose of the present study was to elucidate the effects of UDCA on inhibition of periodontal disease progression using clinical, microbiological and histometrical parameters. Twelve pure bred, 16 month-old-beagle dogs were used in the study. After ligature-induced periodontal diseases were formed, experimental drugs were applied twice a day and then the results of clinical, microbiological, and histometrical parameters were measured at baselie(initiation of experiment) , 4weeks and 8weeks. The gel with UDCA(concentration 0.5%, 5% 3 dogs in each) was applied to experimental group, chlorhexidine to positive control group(3dogs) and the gel without UDCA(base) to negative control group. After induction of general anesthesia, the maxillary 2nd, 3rd premolars and 1st molar and the mandibular 2nd, 3rd, 4th premolars and 1st molar were ligated in one side selected randomly and were not ligated in the opposite side. The plaque index(PI), gingival index(GI), pocket depth(PD) and gingival crevicular fluid(GCF) volum were measured clinically. The PI and GI were measured at 3 buccal points of all experimental teeth and the GCF was measured only at the 3rd premolar in the maxilla and the 4th premolar in the mandible. In the microbiological study, the samples extracted from the 3rd premolar of the maxilla and the 4th premolar of the mandible at the center of buccal surface were analyzed aerobics, anaerobics and Streptococcus colony forming units, After clinical and microbiological examination at 8weeks, the dogs were sacrificed by carotid artery perfusion. The samples were fixed and sectioned including interproximal area, and the distance from cementoenamel junction(CEJ) to alveolar crest was measured. The results were that PI, GI and PD increased until 4 weeks and decreased at 8 weeks in three groups but the differences between all the groups were not significant. The 0.5% UDCA in non-ligated group showed remarkable decrease of GCF. The experimental group applied 5% UDCA decreased the number of aerobics and anaerobics. The distance from CEJ to alveolar crest was greater in the negative control group on both ligated and non-ligated sides, but the differences were not significant stastically.

  • PDF

심미적 포스트 코어의 종류에 따른 미세누출에 관한 연구 (Microleakage of endodontically treated teeth restored with three different esthetic post and cores)

  • 박지근;박지만;박은진
    • 대한치과보철학회지
    • /
    • 제47권1호
    • /
    • pp.53-60
    • /
    • 2009
  • 연구목적: 오늘날 심미적 요구의 증가로 치아색 포스트 코어에 대한 많은 관심이 모아지고 있으며 다양한 연구가 진행 중이다. 현재 화이버 포스트 (ParaPost fiber White, Coltene Whaledent, Cuyahoga Falls, USA), 지르코니아 포스트 (CosmoPost, Ivoclar Vivadent, Schann, Germany) 등에 관한 논문은 다소 나와 있으나 요즘 여러 분야에서 관심을 받고 있는 CAD/CAM (computer-aided design/computer-aided manufacturing) 방식으로 지르코니아를 가공한 절삭형 지르코니아 포스트 코어에 대한 연구는 많지 않은 실정이다. 이 연구의 목적은 CAD/CAM을 이용한 지르코니아를 비롯하여 근관치료된 치아에서 사용된 세 가지 다른 치아색 포스트 코어에 대해 미세누출 (microleakage)을 비교해 보는 것이다. 연구 재료 및 방법: 발치된 건전한 상악 절치 27개를 채택하여 백악법랑질경계 (CEJ)에서 절단하여 근관치료를 시행하고, 세군 (각 9개)으로 나누었다. 각군들은 화이버 포스트와 콤포짓트 레진 코어 (1군), 지르코니아 포스트와 열가압형 세라믹 코어 (2군), CAD/CAM 절삭형 지르코니아 포스트 코어 (3군)로 수복하였다. $5-55^{\circ}C$ 1000회 열순환 처리 (thermocycling)를 시행하고, 2% 메틸렌 블루로 $37^{\circ}C$에서 24시간 염색하였다. 치아장축과 평행하게 순설방향으로 절단하여 미세누출을 현미경과 컴퓨터 프로그램을 사용하여 분석을 하였다. 데이터는 one-way ANOVA와 Scheffe's multiple range test (${\alpha}=0.05$)로 분석하였다. 결과: 모든 군에서 미세누출을 보였으며, 지르코니아 포스트와 열가압형 세라믹 코어군 (2군)에서 치근계면 입구에서는 다소 많은 미세누출을 보였으나 포스트 끝에 이르러서는 거의 미세누출이 없는 결과를 보였다. 화이버 포스트와 콤포짓트 레진 코어군 (1군)과CAD/CAM 절삭형 지르코니아 포스트 코어군 (3군)에서는 부위별로 균등한 미세누출을 보였다. 결론: 화이버 포스트와 콤포짓트 레진 코어군, 지르코니아 포스트와 열가압형 세라믹 코어군, CAD/CAM 절삭형 지르코니아 포스트 코어군 모두에서 미세누출을 보였고, 이 중에서 지르코니아 포스트와 열가압형 세라믹 코어군이 좀 더 큰 미세누출에 대한 저항성을 보였으며 화이버 포스트와 콤포짓트 레진 코어군, CAD/CAM 절삭형 지르코니아 포스트 코어군은 유사한 양상을 보였으나, 각 실험군 간에 통계적으로 유의한 차이는 인정되지 않았다. (P>.05)

상아질과 Gutta-Percha에 대한 근관충전용 Sealer의 결합강도의 측정 (MEASUREMENT OF ADHESION OF ROOT CANAL SEALER TO DENTINE AND GUTTA-PERCHA)

  • 허미자;유미경;이세준;이광원
    • Restorative Dentistry and Endodontics
    • /
    • 제28권1호
    • /
    • pp.89-99
    • /
    • 2003
  • The purpose of this study was to investigate the bonding of resin- based root canal sealer, AH26 when the sealer was applied as a thin layer between dentine and gutta-percha surface. In this study forty non-caries extracted human molars and resin-based root canal sealer(AH 26, DeTrey/Dentsply, Germany) were used. Disks of gutta-percha, 6mm in diameter.6mm thick (Diadent/Dentsply, Korea) for thermoplastic obturation were used and dentin surfaces were treated with 2% NaOCl(Group 1) or 2%NaOCl+17% EDTA(Group 3). Disks of gutta-Percha, 6mm in diameter.6mm thick (Diadent/Dentsply, Korea) for conventional obturation were used and dentin surface were treated with 2% NaOCl(Group 2) or 2%NaOCl+17% EDTA(Group 4). Enamel was removed by a horizontal section 1mm below the deepest portion of the central occlusal groove by using a watercooled low speed diamond saw. A second horizontal section was done around cementoenamel junction. Exposed dentin surface was cut to approximately $8{\times}8{\;}mm$ rectangular shape and was ground against 320, 400, 600 grade silicon carbide abrasive paper serially. After grinding, the dentine surface were soaked in a solution of 2% NaOCl for 30 minutes and twenty of specimens were treated with 17% EDTA solution for 1 minute. The treated specimens were washed and dried, Root canal sealer, AH26 was prepared according to the manufacture's instructions The Gutta-percha and dentin surface were coated with a thin layer of the freshly mixed seal or. The specimens were left overnight at room temperature. After their initial set, they were transferred to an incubator at $37$^{\circ}C$ for 72 h. After 72 hours, resin blocks were made. The resin block was serially sectioned vertically into stick of $1{\cdot}1mm$. Twenty sticks were prepared from each group. After that, tensile bond strength f3r each stick was measured with Microtensile Tester Failure patterns of the specimens at the interface between gutta-percha and dentin were observed under the SEM(x1000) and Stereomicroscope (LEICA M42O, Meyer Inst., TX U.S.A) at 1.25 x25 magnification. The results were statistically analysed by using a One-way ANOVA and Tukey's test. The results were as follows; 1. Tensile bond strengths($mean{\pm}SD$) were expressed with ascending order as follows: Group 1, $3.09{\pm}$ 1.05Mpa : Group 2, $6.23{\pm}1.16MPa$ : Group 3, $7.12{\pm}1.07MPa$ : Group 4, $10.32{\pm}2.06MPa$. 2. Tensile bond strengths of the group 2 and 4 used disks of gutta-percha for conventional obturation were significantly higher than that of the group 1 and 3 used fir thermoplastic obturation. (p < 0.05). 3. Tensile bond strengths of the group 3 and 4 treated with 2% NaOC1+17% EDTA were significantly higher than that of the group 1 and 2 treated with 2% NaOCl. (p < 0.05). 4. In analysis of failure patterns at the interface between sealer and gutta-percha, there were observed 49 (61%)cases of adhesive failure patterns and 31 (39%) cases of mixed failures patterns.