치과용 Titanium 주조합금의 마멸특성 (Wear Properties of Cast Titanium Alloys for Dental Use)

  • 최석규;김형일;박익민
    • 한국주조공학회지
    • /
    • 제11권6호
    • /
    • pp.482-490
    • /
    • 1991
  • This study presents the wear characteristics of Ti alloys (Pure Ti, Ti-6Al-4V, Ti-5Al-2.5Sn) fabricated by centrifugal precision casting in an Ohara dental titanium casting machine. It was found that the hardness of the surface region is higher than that of the interior region. It is considered that the oxygen adsorption in the surface region during casting, leads to the interstitial solid solution hardening. Wear resistance incerases in the order of pure Ti, Ti-6Al-4V, Ti-5Al-2.5Sn alloys. The interior hardness value increases in the same order. The specific wear rate increases with applied load and increases monotonously with sliding speed. The Fe transfer from the counterpart material was observed on the worn surface of the Ti-5Al-2.5Sn alloy. Oxidative wear occurs at low sliding speeds and mechanical fracture wear occurs at high sliding speeds.

  • PDF

A Fabrication and Antifogging Performance of Random Polypropylene Film Containing Monoglycerides as Antifogging Agent

  • Jo, Wan;Park, Jin Hwan;Hwang, Seok-Ho
    • Elastomers and Composites
    • /
    • 제56권4호
    • /
    • pp.217-222
    • /
    • 2021
  • In this study, random polypropylene (rPP) was compounded with two of monoglycerides, namely, glyceryl monolaurate (GML) and glyceryl monostearate (GMS), as antifogging agents to improve its antifogging performance. rPP film samples were prepared by a film-casting method using a three-roll casting machine after melt blending through a twin screw extruder. With an increase in the monoglyceride content, the melt flow index for rPP films with GML and GMS increased, and their yield strength decreased. The incorporation of GMS in rPP was proven to be more effective in improving its physical properties than was rPP with GML. When GML and GMS were separately added to the rPP film at contents of more than 1 phr and more than 5 phr, respectively, the film exhibited antifogging performance.

전자기 연속 주조법을 이용한 의료용 타이타늄 합금 제작에 관한 연구 (Fabrication of Titanium alloy by Electromagnetic Continuous Casting (EMCC) Method for Medical Applications)

  • 최수지;이현재;백수현;현승균;정현도;문병문
    • 한국주조공학회지
    • /
    • 제38권1호
    • /
    • pp.9-15
    • /
    • 2018
  • Electromagnetic continuous casting (EMCC) was used to fabricate Ti-6Al-4V alloys with properties suitable for medical applications. Ti-6Al-4V alloy ingots fabricated by EMCC were subjected to heat treatment, such as residual stress removing (RRS), furnace cooling after solution treatment (ST-FC) and water-cooling after solution treatment (ST-WC), in order to obtain characteristics suitable for the standard. After component analysis, the microstructure and mechanical properties (tensile strength and elongation) were evaluated by ICP, gas analysis, OM, SEM, a Rockwell hardness tester and universal testing machine. The Ti-6Al-4V alloy ingot fabricated by EMCC was fabricated without segregation, and the lamellar structure was observed in the RRS and ST-FC specimens. The ST-WC specimen showed only martensite structure. As a result of evaluating the mechanical properties based on the microstructure results, we found that the water-cooled heat treatment condition after the solution treatment was most suitable for the Ti-6Al-4V ELI standard.

가속 방사광을 활용한 Fe함유 Al-Si-Cu 주조용 합금의 응고과정 실시간 관찰 및 분석 (Real-time Observation and Analysis of Solidification Sequence of Fe-Rich Al-Si-Cu Casting Alloy by Synchrotron X-ray Radiography)

  • 김봉환;이상환;야스다 히데유키;이상목
    • 한국주조공학회지
    • /
    • 제30권3호
    • /
    • pp.100-110
    • /
    • 2010
  • The solidification sequence and formation of intermetallic phase of Fe-rich Al-Si-Cu alloy were investigated by using real-time imaging of synchrotron X-ray radiation. Effects of cooling rate during uni-directional solidification on the resultant solidification behavior was also studied in a specially constructed vacuum chamber in the SPring-8 facility. The series of radiographic images were complementarily analyzed with conventional analysis of OM and SEM/EDX for phase identification. Detailed solidification sequence and formation mechanisms of various phases were discussed based on real-time image analysis. The growth rates of $\alpha$-AlFeMnSi and ${\beta}-Al_5FeSi$ were measured in order to understand the growth behavior of each phase. It is suggested that real-time imaging technique can be a powerful tool for the precise understanding of solidification behavior of various industrial materials.

Centreless precision grinding of camshafts as an automated operation

  • Petterson, Roger;Lundberg, Torbjorn
    • 오토저널
    • /
    • 제11권3호
    • /
    • pp.8-12
    • /
    • 1989
  • The development of a microprocessor-controlled centreless grinding station has opened the way for the production of automobile camshafts-from raw casting to precision-finished part-as a fully automated operation. This results in manufacture to finer tolerances, with part-to-part consistency and a floor-to-floor time of half that needed for alternative production methods. Shafts with a grinding length of up to 700 mm can be processed.

  • PDF

가압함침법에 의한 $Al_2O_3/Al$ 복합재료의 기공 및 편석의 발생에 대한 분석연구 (Analysis of the Formation of Porosity and Segregation in $Al_2O_3/Al$ Composites by Squeeze Infiltration Method)

  • 서영호;이형국
    • 한국주조공학회지
    • /
    • 제21권3호
    • /
    • pp.163-178
    • /
    • 2001
  • The squeeze infiltration process is potentially of considerable industrial importance. The performance enhancements resulting from incorporation of short alumina fiber into aluminum are well documented. These are particularly significant for certain automobile components. Aluminum matrix composite automotive parts, such as diesel engine pistons or engine blocks are produced using squeeze casting apparatus or pressure die-casting apparatus. But the solidification process gets complicated with manufacturing parameters and the factors for porosity formation have not fully understood yet. In this study the formation of porosity during squeeze infiltration has been studied experimentally to achieve an improved understanding of the squeeze infiltration process for manufacture of short-fiber-reinforced components, particularly the mechanism of porosity formation. Al-based MMCs produced under a range of conditions were examined metallographically and the porosity characterised;a kind of matrix, an initial temperature of melt, and a volume fraction of reinforcement. The densimetry and the microscopic image analysis were done to measure the amount of porosity. A correlation between manufacturing parameters and defects was investigated through these.

  • PDF

주조 형상기억 니켈-티타늄 합금의 초탄성 (SUPERELASTICITY OF CAST SHAPE MEMORY Ni-Ti ALLOY)

  • 최동익;최목균
    • 대한심미치과학회지
    • /
    • 제3권1호
    • /
    • pp.32-43
    • /
    • 1995
  • Ni-Ti alloy has excellent corrosion resistance, biocompatibility, shape memory effect and superelasticity, so it has been used widely in biomedical fields. But it has difficulty in casting due to its high melting temperature and oxygen affinity at high temperature. Recently it has been attempted to cast Ni-Ti alloy using new casting machine and investment. The purpose of this study was to examine the superelastic behavior of cast shape memory Ni-Ti alloy and to compare the mechanical properties of the cast shape memory alloy with those of commercial alloys for removable partial denture framework. Ni-Ti alloy(Ni 50.25%, Ti 49.75% : atomic ratio) was cast with dental argon-arc pressure casting machine and Type IV gold alloy, Co-Cr alloy, Ni-Cr alloy, pure titanium were cast as reference. Experimental cast Ni-Ti alloy was treated with heat($500{\pm}2^{\circ}C$) in muffle furnace for 1 hour. Transformation temperature range of cast Ni-Ti alloy was measured with differential scanning calorimetry. The superelastic behavior and mechanical properties of cat Ni-Ti alloy were observed and evaluated by three point bending test, ultimate tensile test, Vickers microhardness test and scanning electron microscope. The results were as follows : 1. Cast Ni-Ti alloy(Ni 50.25%, Ti 49.75% : atomic ratio) was found to have superelastic behavior. 2. Stiffness of cast Ni-Ti alloy was considerably lesser than that of commercial alloys for removable partial denture. 3. Permanent deformation was observed in commercial alloys for removable partial denture framework at three point bending test over proportional limit(1.5mm deflection), but was not nearly observed in cast Ni-Ti alloy. 4. On the mechanical properties of ultimate tensile strength, elongation and Vickers microhardness number, cast Ni-Ti alloy was similiar to Type IV gold alloy, Co-Cr alloy, Ni-Cr alloy and pure titanium. With these results, cast Ni-Ti alloy had superelastic behavior and low stiffness. Therefore, it is suggested that cast Ni-Ti alloy may be applicated to base metal alloy for removable partial denture framework.

  • PDF

연결방법에 따른 주조체 변위에 관한 3차원적 비교연구 (THREE-DIMENSIONAL COMPARISON OF FRAMEWORK DISPLACEMENTS JOINED BY VARIOUS CONNECTION TECHNIQUES)

  • 임장섭;전영찬;정창모
    • 대한치과보철학회지
    • /
    • 제37권3호
    • /
    • pp.358-374
    • /
    • 1999
  • This study measured the relative displacements of the five-unit fixed partial dentures as cast with the same fixed partial dentures sectioned and assembled by investment-soldering, solder-ing stand-soldering, and cast-joining techniques A total of fifteen specimens using a type IV gold alloy were one-piece cast as control and then sectioned and assembled five test specimens for each method were prepared. A computerized three dimensional coordinate measuring machine and specially designed cylinder for this study were used. Displacement was defined by six displacement variables for the each of cylinders incorporated in each casting: three component displacements(${\Delta}Lx,\;{\Delta}Ly,\;and\;{\Delta}Lz$) and rotational displacements(${\Delta}{\theta}x,\;{\Delta}{\theta}y,\;{\Delta}{\theta}z$). The global displacement was computed using the mathematical formula ${\Delta}R$ = Global displacement =$\sqrt{{(x'-x)}^2+{(y'-y)}^2+{(z'-z)}^2}$ Under the conditions of this study, the following conclusions were drawn: 1. The investment-soldering group showed the largest mean value of final global displacements, followed by stand-soldering group, cast-joining group and one-piece cast group. However, between the mean values of final global displacement for the cast-joining group and one-piece cast group, there was no significant difference. 2. For investment-soldering and stand-soldering groups, the greater global displacements were recorded in soldering phase than in indexing or investing phase. 3. For one-piece cast group, the displacements occured mostly in the casting phase. And for cast-joining group, there was no significant difference in global displacements among the fabricating procedures. 4. Intercentroidal distance decreased in framework-patterning, solder-indexing, solder-standing, and soldering phases, but increased in investment block-investing and casting phases. 5 Specially designed cylinder for touch-trigger type coordinate measuring machine was validated.

  • PDF

연속주조기에서 스트랜드 구동롤의 인발력 분배 제어 (Load Sharing Control of Driven Roll in Continuous Caster)

  • 천창근;김철우
    • 전력전자학회논문지
    • /
    • 제8권4호
    • /
    • pp.321-327
    • /
    • 2003
  • 연속주조 프로세스는 고온의 액체 용강을 고체 금속으로 만드는 프로세스로서, 스트랜드 구동롤의 역할은 운전자가 설정한 주조 속도 제어 패턴에 따라 정확하게 주편을 인발하는 것이다. 기존의 스트랜드 구동롤의 제어는 주조 속도만을 제어하였으나 전동기 드라이버 세팅의 부정확성 및 변동, 연속적인 주조에 의한 구동롤의 마모 및 변형에 의한 롤 직경의 변경, 주조 중 주편 벌징량의 변동 등의 요인에 의해 주조 중 주편을 인발하는 데 소요되는 전체 인발력이 각 구동롤에 적절하게 분배되지 않아 주편 코너부에 수평 크랙을 발생시켜 주조 속도를 증가하는데 있어서 결정적인 장애요인이었다. 본 논문에서는 스트랜드 구동롤에 인가되는 인발력 분포와 주편 품질과의 상관 관계를 도출하고 주조 중에 연속적으로 인발력을 분배할 수 있는 알고리즘을 제안하였다. 제안한 인발력 분배 알고리즘은 각 구동롤 전동기의 절대적인 토크를 제어하는 것이 아니라, 상위제어기에서 결정한 인발력 분배 비율에 따라 각 구동롤 전동기의 토크분 전류를 상호 비교하여 속도 설정치를 조정함으로써 이루어진다. 그리고 인발력 분배 알고리즘의 동작 확인을 위해 광양제척소 1연주공장 4연주기에 적용하여 양호한 결과를 확인하였다.