• 제목/요약/키워드: Casting alloy

검색결과 782건 처리시간 0.028초

Cu-Zr-Ti-Ni-Pd계 비정질 벌크합금의 형성과 성질 (Cu-based Bulk Amorphous Alloys in the Cu-Zr-Ti-Ni-Pd System)

  • 김성규;배차헌
    • 한국주조공학회지
    • /
    • 제22권6호
    • /
    • pp.304-308
    • /
    • 2002
  • The new Cu-Zr-Ti-Ni-Pd amorphous alloy system has been introduced and manufactured using melt-spinning and Cu-mold die casting methods. Amorphous formability, the supercooled liquid region before crystallization and mechanical properties of the alloys were examined. The reduced glass transition temperature(Trg = Tg/Tm) and the supercooled liquid region(${\Delta}$Tx = Tx-Tg) of $Cu_{49}Zr_{30}Ti_{10}Ni_5Pb_6$ alloy were 0.620 and 57 K respectively. $Cu_{49}Zr_{30}Ti_{10}Ni_5Pb_6$ amorphous alloy was produced in the rod shape with 2mm diameter using the Cu-mold die casting. The hardness value of the amorphous bulk alloy was 432 DPN.

분무 주조 과공정 Al-Si계 합금의 응력이완 및 Creep 천이 거동 (Load Relaxation and Creep Transition Behavior of a Spray Cast Hypereutectic Al-Si Based Alloy)

  • 김민수;방원규;박우진;장영원
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2005년도 춘계학술대회 논문집
    • /
    • pp.176-179
    • /
    • 2005
  • Spray casting of hypereutectic Al-Si based alloy has been reported to provide distinct advantages over ingot metallurgy (IM) or rapid solidification/powder metallurgy (RS/PM) process in terms of microstructure refinement. Hypereutectic Al-Si based alloys have been regarded attractive for automotive and aerospace application, due to high specific strength, good wear resistance, low coefficient of thermal expansion, high thermal stability, and good creep resistance. In this study, hypereutectic Al-25Si-2.0Cu-1.0Mg alloy was prepared by OSPREY spray casting process. High temperature deformation behavior of the hypereutectic Al-Si based alloy has been investigated by applying the internal variable theory proposed by Chang et al. The change of strain rate sensitivity and Creep transition were analyzed by using the load relaxation test and constant creep test.

  • PDF

마찰 접촉을 고려한 현수교 PPWS용 소켓의 거동 해석 (Behavior Analysis of PPWS Sockets for Suspension Bridges Considering Frictional Contact)

  • 유훈;이성형;서주원
    • 대한토목학회논문집
    • /
    • 제33권4호
    • /
    • pp.1281-1293
    • /
    • 2013
  • 현수교 주케이블용 평행강선 스트랜드(PPWS) 소켓의 엄밀한 수치해석을 위한 유한요소해석 모델을 제안하였고, 제안된 해석 모델을 이용하여 소켓의 거동을 분석하였다. 개별 강선과 소켓 내부 주입 합금재의 영향을 고려한 직교 이방성 재료 모델을 적용하였고, Coulomb 마찰 및 표면접촉 모델을 도입하여 소켓 내면과 주입 합금재 표면의 접촉 상태를 구현하였다. 인장 실험으로부터 측정된 소켓 외면의 변형율과 유한요소 해석 결과를 비교하여 제안된 유한요소 해석 모델의 타당성을 검증하였고, 마찰계수의 변화에 따른 소켓의 거동을 해석하였다. 해석 결과, 소켓 내면과 주입 합금재 표면의 마찰은 소켓과 주입 합금재에 발생하는 응력 집중을 크게 완화 시켰으며, 소켓 설계법에서 정의된 수직응력식은 소켓 내면과 주입 합금재 표면의 접촉응력 분포에서 상하부 사분위값의 평균을 대표하는 것으로 나타났다.

Co-Cr 합금의 금속-도재 결합 강도 (Bond Strength between Co-Cr Alloy Metal and Ceramic)

  • 김민정;박광식
    • 한국콘텐츠학회논문지
    • /
    • 제21권3호
    • /
    • pp.602-608
    • /
    • 2021
  • 임상에서 사용되는 Co-Cr 합금과 도재 간의 접착 강도를 비교하기 위해 대조군으로 전통적인 주조(Casting) 방법, 실험군으로 Milling(Milling group), SLM(3d printing group) 시편을 제작하여 금속과 도재(ceramic) 간의 접착 강도를 비교 하였다. 합금과 도재간의 접착강도를 측정하기 위해 universal testing machine를 이용하여 3점 굴곡 시험을 시행하고, 결합강도 측정 후 금속-도재간의 계면을 관찰하였다. 금속-도재(ceramic) 간의 실험 결과 casting group 53.59 MPa, milling group 45.90 MPa, 3d printing group 58.34 MPa의 결과값을 보였고, 통계적으로 유의성은 없었다. 파절양상은 두 집단 시편의 대부분이 복합 파절양상(mixed failure)을 보였다. 본 연구는 3D 프린팅로 제작된 합금으로 합금-도재의 결합 강도값을 측정하였을 때 임상적으로 적용 가능한 수치를 보여 주었다.

소실모형주조법으로 제조한 박판형 Al-Si합금에서의 주형 충전 및 기계적 성질 (Mold Filling and Mechanical Properties of Thin Sectioned Al-Si Alloy Fabricated by Lost Foam Casting Process)

  • 김정민;이재철;최진영;조재익;최경환
    • 한국주조공학회지
    • /
    • 제37권6호
    • /
    • pp.186-192
    • /
    • 2017
  • The lost foam casting method was used to fabricate Al-Si alloy thin sheet specimens; the effects of chemical composition and process variables on the mold filling and mechanical properties were investigated. The mold filling capability was observed to be proportional to the pouring temperature, and both the vibration imposed during the casting and the application of a pattern coating had rather negative effects. The mold filling capability also decreased with the addition of Mg or TiB. When the Mg content increased, the tensile strength of the cast alloy was enhanced, but the elongation decreased. However, after T6 heat treatment, both the strength and the elongation were improved. TiB addition for grain refining or pattern coating did not significantly affect the tensile properties.

알루미늄청동의 합금성분 및 냉각속도에 따른 특성변화에 관한 연구 (A Study on the Change of Properties of Al-bronze Due to Alloy Elements and Cooling Rate.)

  • 정운재;김헌주;김동옥;윤의박
    • 한국주조공학회지
    • /
    • 제8권3호
    • /
    • pp.271-281
    • /
    • 1988
  • Al-bronze has a good mechanical property, corrosion resistance and castability, so being highlighted for the new copper alloy. So, effects of alloy composition and cooling rate in the mechaincal properties and solidification behavior have been investigated. The results obtained are as follows; 1) Change in volume on solidification is larger in metal mold casting than in sand mold casting. And it decreases by the addition of Al. 2) The mechanical property in metal mold casting is superior to the one in sand mold casting, and the inclination is obvious up to 9% Al, after heat-treatment ($885^{\circ}C$, $1.5hrs\;{\rightarrow}\;W\;{\cdot}\;Q\;{\rightarrow}\;540^{\circ}C$, 3hrs) 3) By adding Al, the mechanical property is slightly increased up to 9% Al, Above 9% Al, it is increased rapidly, and is accelerated by adding Fe. 4) Cooling rate and hardness, and grain size and cooling rate are related as follows in the range of $1100^{\circ}C$ to $1200^{\circ}C$ pouring temperature. Grain size(${\mu}m$)=$929.6422{\times}cooling\;rate(^{\circ}C\;/\;sec)^{-0.51537}$ Hardness(BHN)=$765.45713{\times}grain\;size({\mu}m)^{-0.31058}$.

  • PDF

용탕단조법에 의한 휘스커강화 Al합금기 복합재료의 고속초소성 (High Strain Rate Superplasticity of Whisker Reinforced Aluminum Alloy Matrix Composites Fabricated by Squeeze Casting)

  • 임석원;유전의칙
    • 한국주조공학회지
    • /
    • 제21권6호
    • /
    • pp.359-365
    • /
    • 2001
  • The superplastic behavior of whisker reinforced aluminum alloy matrix composites fabricated by squeeze casting as one of high pressure routes was investigated. The preforms of ${\alpha}-Si_3N_4$ and ${\beta}-SiC$ whiskers without any binder as a reinforcement were used. The matrix materials were 2024 and 7075 aluminum alloys. For the purpose of optimum superplastic condition, respectively, the whiskers volume fraction, extrusion temperature, tensile test temperature and initial strain rate were changed. Fracture surface of tested specimens were observed by SEM. By the results, it became possible to produce superplastic composites by applying only a hot extrusion process to composites obtained by the squeeze casting. The superplastic composites developed are ${\alpha}-Si_3N_4w/7075$, ${\alpha}-Si_3N_4w/2024$ and ${\beta}-SiCw/2024$ systems at high strain rate.

  • PDF

알루미늄 합금의 소실모형주조 중 기포 형성 기구에 관한 연구 (The Study on the Formation Mechanism of Gas Pore During Lost Foam Casting of Al alloys)

  • 신승렬;한상원;이경환;이진형
    • 한국주조공학회지
    • /
    • 제23권5호
    • /
    • pp.268-275
    • /
    • 2003
  • The mechanism of the hydrogen gas pore formation was investigated in Lost Foam Casting of Al-alloy by reduced pressure test and real casting. The hydrogen gas pick-up was affected by the formed gas during the decomposition of polystyrene in addition to the liquid product. It depended on pouring temperature and a proper temperature of metal front gave the minimum hydrogen pick-up. At a low pouring temperature, the hydrogen went into the melt mainly from entrapped liquid product of polystyrene but pores were formed from the gas as well as the liquid product at a high pouring temperature. The mold flask evacuation down to 710torr decreased the gas porosity down by around 0.4% vol%. The entrapped decomposition product of polystyrene in the melt was observed through the visualization of filling behavior of Al alloy-melt with the high speed camera.

($AlSi_7Mg$알루미늄 합금의 초정 구형화에 대한 주조조건의 영향 (Effect of the Casting Conditions on the Globulization of Primary Al of $AlSi_7Mg$ Alloy)

  • 한요섭;이호인;이재철
    • 한국주조공학회지
    • /
    • 제23권1호
    • /
    • pp.40-46
    • /
    • 2003
  • Semisolid forming requires alloys with non-dendritic microstructure of the thixotropy. Recently, low pouring temperture method without stirring, i.e. liquidus casting has been found out new fabrication method of the semisolid metals. Effects of melt superheat and mold conditions on the globulization of primary Al of $AlSi_7Mg$ alloy were investigated in gravity casting process without stirring. The microstructures of primary Al as function of melt superheat and mold temperature show globular, rosette and dendritic shapes. The conditions for globular microstructure of primary Al were low melt superheat < 35 K and low mold temperature < 500 K. The thermal conditions for globular microstructure of primary Al were undercooled melt at early solidification stages and slow cooling < 0.6 K/s. It was found that the initial microstructure was maintained throughout the solidification and the globules of primary Al can be obtained by high nucleation of fine and spherical nuclei due to enhanced undercooling of melt.

레이저 열원을 이용한 마그네슘 합금의 용접성에 관한 연구 (III) - Pulsed Nd:YAG 레이저를 이용한 사형주조 마그네슘 합금의 맞대기 용접성 - (A Study on the Weldability of Magnesium Alloy by Laser Heat Source (III) - Butt Weldability of Sand Casting Magnesium Alloy using Pulsed Nd:YAG Laser -)

  • 김종도;이정한;이문용
    • Journal of Welding and Joining
    • /
    • 제31권2호
    • /
    • pp.57-62
    • /
    • 2013
  • Magnesium has good castability and limited workability, so its products have been manufactured by almost casting processes. In this study, a pulsed Nd:YAG laser was used to butt-weld the sand casting magnesium alloys. And the effect of welding conditions such as peak power, pulse width, welding speed was evaluated in detail. As a result of this study, large underfill and plenty of spatter taken place under the conditions with high peak power. Thus, it is recommended to use low peak power and long pulse width to obtain good welds with deep penetration. It is also confirmed that the welding speed and pps(pulse per second) are directly connected at weld defects such as underfill, porosity.