초경합금재의 하드터닝에서 공구재종에 따른 절삭성 (Hard Turning Machinability of V30 Cemented Carbide with PCD, cBN and PcBN Cutting Tool)

  • 허성중
    • 한국정밀공학회지
    • /
    • 제25권12호
    • /
    • pp.47-54
    • /
    • 2008
  • Hard turning process can be defined as a single-point machining process carried out on "hard" materials. The process is intended to replace or limit traditional grinding operations that are expensive, environmentally unfriendly, and inflexible. The purpose of this study is to achieve a systematic understanding of machining characteristics and the effects of machining parameters on cutting force, tool wear shape and chip formation by the outer cutting of a kind of wear resistant tungsten carbide V30. Hard turning experiments were carried out on this alloy using the PCD (Poly Crystalline Diamond), cBN (cubic Boron Nitride) and PcBN (Polycrystalline cubic Boron Nitride) cutting tools. The PcBN and the usual cBN tools were used to be compare with the PCD tool and the dry turning was carried out. The PcBN is attractive as the tool material which replaces the PCD. The tool wear width and cutting force were measured, and the worn tool and chip were observed. The difference of the tool wear mechanism among the three tool materials was investigated.

수종의 BRACKET(DBS)제거방법에 따른 법랑질 표면에 대한 주사전자현미경적 연구 (ENAMEL SURFACE EVALUATION ON VARIOUS REMOVAL TECHNIQUE OF BRACKET (DBS): A STUDY WITH THE SCANNING ELECTRON MICROSCOPY)

  • 송정국;손병화
    • 대한치과교정학회지
    • /
    • 제15권2호
    • /
    • pp.271-277
    • /
    • 1985
  • With modification of the acid etch technique and improvements of the physical and mechanical properties of the acrylic resin, the removal of directly bonded attachments and the finishing of the underlying enamel have become an acute clinical problem. This study was to evaluation the efficacy of recently introduced instrumentation and techniques to remove bonded brackets and residual resin, and restore the affected enamel surface to an acceptable clinical condition. Fortyeight premolar which were scheduled for extraction for orthodontic purposes were bonded with brackets using super-C ortho. Four additional premolars with untreated surfaces were used as controls. After one weak the brackets were removed and the residual resin removed by hand scaler, green stone, green rubber wheel, sandpaper disc, tungsten carbide bur, Sof-lex disc. Half the experimental teeth were given a final pumicing and then all were extracted and stored in 50 percent ethanol. The scanning electron microscopy was used to evaluated the enamel surface. Following results were obtained; 1. A satisfactory result was obtained by means of the Sof-lex disc. 2. The order of the scratch formation was the procedure using hand scaler, green atone, tungsten carbide bur, sandpaper disc, green rubber wheel, and Sof-lex disc. 3. The procedures using green stone and tungsten carbide bur showed many groove formations and the other procedures showed none. 4. final pumicing serves effectively to remove residual adhesive and restore the enamel surface.

  • PDF

발전설비 보일러 튜브용 X20강의 가속열처리에 의한 재질 열화 (Material Degradation of X20 Steel (12Cr-1MoVNi) for Boiler Tube of Power Plant)

  • 최병학;윤기봉;이남혁;김신;이길재;김광호;권동일
    • 대한금속재료학회지
    • /
    • 제46권5호
    • /
    • pp.276-282
    • /
    • 2008
  • Material degradation of Cr steels in boiler tubes was accompanied by the microstructural changes including carbide behavior and crack formation. The microstructural change and the mechanical behavior of hardness and creep properties in accelerated heat-treatments were studied in order to identify the material degradation of the X20 Cr steel. The degradation behavior was occurred in the hardness increasing followed by decreasing due to carbide dissolution and precipitation.

세라믹 가스터빈 환경을 고려한 탄화규소의 입자충격 손상거동-장기간 산화에 따른 산화물층의 영향- (Particle Impact Damage behaviors in silicon Carbide Under Gas Turbine Environments-Effect of Oxide Layer Due to Long-Term Oxidation-)

  • 신형섭
    • 대한기계학회논문집
    • /
    • 제19권4호
    • /
    • pp.1033-1040
    • /
    • 1995
  • To simulate strength reliability and durability of ceramic parts under gas turbine application environments, particle impact damage behaviors in silicon carbide oxidized at 1673 K and 1523 K for 200 hours in atmosphere were investigated. The long-term oxidation produced a slight increase in the static fracture strength. Particle impact caused a spalling of oxide layer. The patterns of spalling and damage induced were dependent upon the property and impact velocity of the particle. Especially, the difference in spalling behaviors induced could be explained by introducing the formation mechanism of lateral crack and elastic-plastic deformation behavior at impact sit. At the low impact velocity regions, the oxidized SiC showed a little increase in the residual strength due to the cushion effect of oxide layer, as compared with the as-received SiC without oxide layer.

버형성 최소화를 위한 스텝드릴 개발 (Development of Step Drill Geometry for Burr Minimization)

  • 장재은;고성림
    • 한국정밀공학회지
    • /
    • 제19권11호
    • /
    • pp.183-191
    • /
    • 2002
  • Drilling tests were carried out using drills with various drill shapes for burr minimization. Final objective of this study is to develop compatible drill shape for minimization of burr formation. For experiments, general carbide drills, round drills, chamfered drills and step drills are designed and manufactured. Burrs are formed by various cutting conditions and in 4 different work materials. Laser sensor is used to measure burr geometries. Cutting forces in drilling are also measured and compared in every drill. As a result of the experiments, step drills with specific step angle and step diameter are suggested for burr minimization.

Synthesis of Silicon Carbide Nanowhiskers from Coconut Fibres and Sol-Gel Derived Silica

  • Raman, V.;Bhatia, G.;Mishra, A.;Saha, M.;Sengupta, P.R.;Srivastava, A.K.
    • Carbon letters
    • /
    • 제7권3호
    • /
    • pp.166-170
    • /
    • 2006
  • Silicon carbide whiskers ($SiC_w$) having the diameter in the range of 20-80 nm were synthesised from coconut fibres through sol-gel process. The coconut fibres were impregnated with tetraethoxysilane and methyltriethoxysilane derived sol and pyrolyzed at $1400^{\circ}C$ in argon. X-ray of the pyrolyzed samples showed the formation of ${\beta}$-SiC.

  • PDF

Ti과 Nb에 의한 HSS 작업롤재의 미세조직 제어 (Microstructural Control of High Speed Steel Roll Material with Titanium and Niobium)

  • 김진수;김동규;최진원;이희춘
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1999년도 제3회 압연심포지엄 논문집 압연기술의 미래개척 (Exploitation of Future Rolling Technologies)
    • /
    • pp.262-271
    • /
    • 1999
  • This work was intended to modify the solidification structure of high speed steel roll material for hot strip mill, by the introduction of alloying elements designed to form primary carbide dispersions via melt treatment procedure. Solidification structure was modified by the melt treatment with titanium and distribution. This modifying effect could be attributed to the fact that the nuclie formed at high temperature upon inoculation induce the formation of fine equiaxed grain and primary carbide during solification, which is also likely to be responsible for the fact that TiC acts as effective nuclie for primary VC solidification.

  • PDF

탄소섬유 강화 복합재 가공용 드릴 공구 개발 및 홀 가공성 평가 (Development of a Drill Tool for CFRP Machining and Evaluation of Drilling Processing)

  • 사민우
    • 한국기계가공학회지
    • /
    • 제19권3호
    • /
    • pp.8-13
    • /
    • 2020
  • Carbon fiber-reinforced plastics (CFRPs) are extremely strong and light fiber-reinforced plastics containing carbon fibers. CFRPs can be expensive to produce, but are commonly used wherever high strength-to-weight ratio and rigidity are required, such as in the aerospace, automotive, and ship superstructure industries. In CFRP drilling, the tool performance greatly varies depending on the tool shapes, cutting conditions, and diamond coating. This study developed a new type of tungsten carbide drill with multi-blade edges to evaluate the surface quality of CFRP materials according to the coating thickness of diamond-coated drills. Experiments on tool wear, surface roughness, and burr formation were conducted. The bore exit quality of a 12 mμ -coated drill was better than that of a 6 mμ -coated drill. The superior effects of the 12 mμ -coated drill and the good surface quality of CFRP were also demonstrated.

고탄소 크롬 베어링 강에서의 잔류 오스테나이트 변화에 따른 회전접촉 피로거동 (A Behavior of Rolling Contact Fatigue on Retained Austenite in High-Carbon Chromium Bearing Steel)

  • 진재관;김동건
    • 열처리공학회지
    • /
    • 제7권3호
    • /
    • pp.190-198
    • /
    • 1994
  • In order to study the effect of retained austenite on rolling contact fatigue in high-carbon chromium bearing steel, retained austenite was controlled by only tempering temperature, individually 200, 220 and $240^{\circ}C$. Among various microstructural alteration during rolling contact fatigue test, plate-like carbide most related to the flaking at sub-surface of contact pressure. The plate-like carbides formed during rolling contact fatigue test decrease with increasing tempering temperature, and fatigue life is much more improved. The retained austenite was decreased with the tempering temperature, and that decreased plate-like carbide formation. Therefore fatigue life is much more improved with decreasing retained austenite.

  • PDF

카올린의 환원 열탄화법에 의한 베타 탄화규소 휘스커의 합성 (Synthesis of $\beta$-SiC Whiskers by the Carbothermal Reduction of Kaolin)

  • 오세정;류종화;조원승;최상욱
    • 한국세라믹학회지
    • /
    • 제35권12호
    • /
    • pp.1249-1256
    • /
    • 1998
  • ${\beta}$-Silicon carbide(${\beta}$-SiC) whiskers could be synthesized by the carbothermal reduction of kaolin at tem-peratures between 1400 and 1500$^{\circ}C$. The whiskers were grown up to about 1150 of aspect ratio by VS mechanism (showing tapering tips) and to about 45 of that by VLS mechanism (showing round droplet tips) respectively. Hydrocarbon like methane in the reaction atmosphere promoted the formation of gaseous il-icon monoxide(SiO) from silicon dioxide(SiO2) and subsequently reacted with it to form whiskers. The for-mation of ${\beta}$-SiC whiskers increased with increasing carbon content(to 30 wt%) and reaction temperatures. The max. yield of ${\beta}$-SiC whiskers was 15% at 1500$^{\circ}C$ under 20%CH4/80%H2.