In Vitro Evaluation of Shear Bond Strengths of Zirconia Cerami with Various Types of Cement after Thermocycling on Bovine Dentin Surface (지르코니아 표면 처리와 시멘트 종류에 따른 치면과의 전단 결합 강도 비교 연구)

  • Cho, Soo-Hyun;Cho, In-Ho;Lee, Jong-Hyuk;Nam, Ki-Young;Kim, Jong-Bae;Hwang, Sang-Hee
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.23 no.3
    • /
    • pp.249-257
    • /
    • 2007
  • State of problem : The use of zirconium oxide all-ceramic material provides several advantages, including a high flexural strength(>1000MPa) and desirable optical properties, such as shading adaptation to the basic shades and a reduction in the layer thickness. Along with the strength of the materials, the cementation technique is also important to the clinical success of a restoration. Nevertheless, little information is available on the effect of different surface treatments on the bonding of zirconium high-crystalline ceramics and resin luting agents. Purpose : The aim of this study was to test the effects of surface treatments of zirconium on shear bond strengths between bovine teeth and a zirconia ceramic and evaluate differences among cements Material and methods : 54 sound bovine teeth extracted within a 1 months, were used. They were frozen in distilled water. These were rinsed by tap water to confirm that no granulation tissues have left. These were kept refrigerated at $4^{\circ}C$ until tested. Each tooth was placed horizontally at a plastic cylinder (diameter 20mm), and embedded in epoxy resin. Teeth were sectioned with diamond burs to expose dentin and grinded with #600 silicon carbide paper. To make sure there was no enamel left, each was observed under an optical microscope. 54 prefabricated zirconium oxide ceramic copings(Lava, 3M ESPE, USA) were assigned into 3 groups ; control, airborne-abraded with $110{\mu}m$ $Al_2O_3$ and scratched with diamond burs at 4 directions. They were cemented with a seating force of 10 ㎏ per tooth, using resin luting cement(Panavia $F^{(R)}$), resin cement(Superbond $C&B^{(R)}$), and resin modified GI cement(Rely X $Luting^{(R)}$). Those were thermocycled at $5^{\circ}C$ and $55^{\circ}C$ for 5000 cycles with a 30 second dwell time, and then shear bond strength was determined in a universal test machine(Model 4200, Instron Co., Canton, USA). The crosshead speed was 1 mm/min. The result was analyzed with one-way analysis of variance(ANOVA) and the Tukey test at a significance level of P<0.05. Results : Superbond $C&B^{(R)}$ at scratching with diamond burs showed the highest shear bond strength than others (p<.05). For Panavia $F^{(R)}$, groups of scratching and sandblasting showed significantly higher shear bond strength than control group(p<.05). For Rely X $Luting^{(R)}$, only between scratching & control group, significantly different shear bond strength was observed(p<.05). Conclusion : Within the limitation of this study, Superbond $C&B^{(R)}$ showed clinically acceptable shear bond between bovine teeth & zirconia ceramics regardless of surface treatments. For the surface treatment, scratching increased shear bond strength. Increase of shear bond strength by sandblasting with $110{\mu}m$ $Al_2O_3$ was not statistically different.

Penetration and Microleakage Assessment of Flowable Resin Applied on Carious Fissure Following Various Fissurotomy Techniques (교합면 우식열구에서 열구성형술 방법에 따른 유동성 레진의 침투도와 미세누출 평가)

  • Kwon, Seok;Lee, Sangho;Lee, Nanyoung;Jih, Meongkwan;Yoon, Youngmi
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.45 no.1
    • /
    • pp.90-97
    • /
    • 2018
  • The purpose of this study was to evaluate the effect of fissurotomy on the penetration and microleakage of flowable resins for carious fissures. A total of 250 extracted premolars with early fissure caries were selected and divided into five groups according to the fissurotomy; no fissurotomy (n = 50), fissurotomy with $Fissurotomy^{(R)}$ original bur (n = 50), fissurotomy with $Fissurotomy^{(R)}$ Miro NTF bur (n = 50), fissurotomy with SF104R tapered diamond bur (n = 50), fissurotomy with 1/2 round carbide bur (n = 50). Two types of flowable resins ($UniFil^{(R)}Flow$, $Filtek^{(R)}Flow$) were used as sealing materials. All samples were sectioned and observed using a stereoscopic microscope after thermocycling and immersing in methylene blue solution. The adaptation of flowable resin to the fissure wall was observed using scanning electron microscopy. The penetration of flowable resin into the carious fissure was significantly increased by fissurotomy, which also decreased microleakage. Fissure preparation using different burs showed a significantly different in penetration, but did not show any difference in microleakage. $Unifil^{(R)}Flow$ showed better penetration than $Filtek^{(R)}Flow$, but there was no significant difference in microleakage. Fissurotomy can be used to increase the penetration of flowable resin into carious fissures and decrease microleakage.

Effect of Timing of Light Curing on the Shear Bond Strength of Three Self-adhesive Resin Cements

  • Yoo, Yeon-Kwon;Kim, Sung-Hun;Ryu, Jae-Jun;Ryu, Jae-Jun
    • Journal of Korean Dental Science
    • /
    • v.1 no.1
    • /
    • pp.28-34
    • /
    • 2008
  • Objectives. The objectives of this study were: 1) to compare the effect of varying timing of light curing on shear bond strength, and; 2) to compare the shear bond strength of three self-adhesive cements. Materials and methods. A total of 72 extracted non-carious teeth were divided into 24 for Unicem tests, 24 for Maxcem tests, and 24 for Biscem tests; they were assigned 3 * 2 subgroups of 12 teeth each. The specimens were prepared as follows: 1) The calculus and periodontal ligament were removed from the teeth; 2) The teeth were stored in normal saline; 3) The occlusal enamel of each tooth was removed using high-speed coarse diamond burs under water cooling, and; 4) Finally, the teeth were flattened by 600-grit silicone carbide paper disks. Resin blocks were adhered using either Unicem, Maxcem, or Biscem. Light curing timing was divided into two groups: U10, M10, and B10 were exposed to light after 10 seconds, and; U150, M150, and B150 on the other side were exposed to light after 150 seconds. Shear bond strength was measured by a Universal testing machine with cross head speed of 1mm/min. T-test and One way ANOVA were used for the statistical analysis of data. Results. The shear bond strength of U150 was not significantly higher than that of U10 (U150: 20.55.7Mpa, U10: 18.73.80Mpa). On the other hand, the shear bond strength of M150 was significantly higher than that of M10. The shear bond strength of B150 was also significantly higher than that of B10 (M150:14.45.7Mpa, M10: 9.94.2Mpa, B150: 24.38.3Mpa, B10: 17.27.3Mpa). When the light curing timing was 10sec after bonding, the shear bond strength of Unicem was highest; the shear bond strength of Biscem was highest when the light curing timing was 150sec after bonding (U10: 18.73.80Mpa, B150: 24.38.3Mpa). Significance. Since Unicem is less sensitive based on light curing timing, dentists seem to use it without considering the light curing timing. Maxcem showed the lowest bonding strength (especially M10). Thus, when using Maxcem, dentists need to delay the light curing after adhesion.

  • PDF

Surface Roughness and Cariogenic Microbial Adhesion after Polishing of Smart Chromatic Technology-based Composite Resin (Smart Chromatic Technology 기반 복합 레진의 폴리싱 이후 표면 거칠기 및 우식원성 미생물 부착 )

  • Haesong Kim;Juhyun Lee;Haeni Kim;Howon Park
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.50 no.1
    • /
    • pp.65-74
    • /
    • 2023
  • This study compared the surface roughness and microbial adhesion characteristics of Omnichroma, a novel composite resin developed using "smart chromatic technology", with those of two other conventional composite resins with different filler compositions. A total of 144 specimens were fabricated using 3 types of composite resins: Omnichroma (nano-spherical), Filtek Z350XT (nanofill), and Tetric N-Ceram (nanohybrid) and, divided into 3 groups of 48. Finishing was performed using tungsten carbide burs. Specimens were then divided into 3 subgroups using different polishing methods: Control, SofLex, and PoGo. Surface roughness was analyzed quantitatively and qualitatively using an atomic force microscope and a scanning electron microscope. Microbial adhesion was assessed by culturing Streptococcus mutans on the specimens for 24 hours and then measuring colony-forming units attached to the upper surface. The surface roughness (Ra) of Omnichroma was 0.123 ㎛ after finishing, and it exhibited a smooth surface compared to the other resins. However, after polishing, there were no significant differences in the surface roughness between the three composite groups, regardless of the polishing methods. The surfaces of the Control subgroups were significantly rougher than those of the SofLex subgroups in all 3 composite groups. However, except for Tetric N-Ceram, there were no significant differences between the Control and PoGo subgroups in the other composite groups. Microbial adhesion assessment showed no significant differences between any of the 3 composite resin subgroups; however, Omnichroma exhibited higher microbial adhesion than the other two composites. No significant correlation was observed between surface roughness and microbial adhesion.