CaO 도가니에 의한 Ti-6Al-4V 합금의 용해와 주조결함 (Melting of Ti-6Al-4V Alloy Using CaO Crucible and Internal Defects of its Casting)

  • 세이주우치다;킨야카나타;나오히로타나카;오사무야나기사와
    • 한국주조공학회지
    • /
    • 제24권6호
    • /
    • pp.314-322
    • /
    • 2004
  • The CaO crucible is expected to serve as a useful tool for melting Ti and its alloys due to its thermodynamic stability. However, tjere still remain problems that need to be resolved in the melting of Ti and its alloys to enable commerical use. The cause of the defects of Ti-6AI-4V alloy castings melted in the CaO crucible were examined and compared with induction skull melting. The key factors of the melting technique using the CaO crucible, affecting the quality of Ti-6AI-4V alloy castings, were investigated. Defects of the Ti-6AI-4V alloy castings are caused by the chemical reduction of CaO by Ti. Pressurizing with argon gas in a vacuum induction chamber is effective for reducing the defects. Preheating of the charged material in the crucible and quick pouring into a mold of lower temperature, just after melting down, are important for produsing sound Ti-6AI-4V castings.

대기용해 시 내화물 도가니의 종류가 가돌리늄(Gadolinium)을 함유한 듀플렉스 스테인레스 강의 미세조직에 미치는 영향 (The Effect of Refractory Crucible on Microstructure of Duplex Stainless Steel Cast with Gadolinium during Air Induction Melting)

  • 안지호;임재한;문병문
    • 한국주조공학회지
    • /
    • 제35권5호
    • /
    • pp.114-119
    • /
    • 2015
  • This paper reports the effect of a refractory crucible type on the microstructure of duplex stainless steel (DSS) cast with the addition of gadolinium using air-induction melting. Grade 4A DSSs with 1 wt% of gadolinium (Gd) were fabricated in various crucibles including alumina ($Al_2O_3$), magnesia (MgO), calcia (CaO) coated with yttria ($Y_2O_3$) and graphite. The standard free energies of the formation of calcium and yttrium oxide were lower than those of gadolinium oxide and other crucible elements based oxide. The yield of Gd in DSS using $Al_2O_3$, MgO, CaO-coated $Y_2O_3$ and graphite was 5, 19, 83 and 96%, respectively. As Gd yield increased, the amount of Gd-based inclusions increased, the size of the inclusions were reduced, and the inclusions became evenly distributed.