Friction behavior of controlled low strength material-soil interface

  • Han, WooJin;Kim, Sang Yeob;Lee, Jong-Sub;Byun, Yong-Hoon
    • Geomechanics and Engineering
    • /
    • v.18 no.4
    • /
    • pp.407-415
    • /
    • 2019
  • A controlled low strength material (CLSM) is a highly flowable cementitious material used for trench backfilling. However, when applying vertical loads to backfilled trenches, shear failure or differential settlement may occur at the interface between the CLSM and natural soil. Hence, this study aims to evaluate the characteristics of the interface friction between the CLSM and soils based on curing time, gradation, and normal stress. The CLSM is composed of fly ash, calcium sulfoaluminate cement, sand, silt, water, and an accelerator. To investigate the engineering properties of the CLSM, flow and unconfined compressive strength tests are carried out. Poorly graded and well-graded sands are selected as the in-situ soil adjacent to the CLSM. The direct shear tests of the CLSM and soils are carried out under three normal stresses for four different curing times. The test results show that the shear strengths obtained within 1 day are higher than those obtained after 1 day. As the curing time increases, the maximum dilation of the poorly graded sand-CLSM specimens under lower normal stresses also generally increases. The maximum contraction increases with increasing normal stress, but it decreases with increasing curing time. The shear strengths of the well-graded sand-CLSM interface are greater than those of the poorly graded sand-CLSM interface. Moreover, the friction angle for the CLSM-soil interface decreases with increasing curing time, and the friction angles of the well-graded sand-CLSM interface are greater than those of the poorly graded sand-CLSM interface. The results suggest that the CLSM may be effectively used for trench backfilling owing to a better understanding of the interface shear strength and behavior between the CLSM and soils.

Correlation between Compressive Strength and Unit Weight of Lightweight Foamed Controlled Low Strength Material (CLSM) Using Coal Ash (석탄회를 활용한 경량기포 CLSM의 압축강도와 단위중량의 상관관계)

  • Lee, Jong-Hwi;Lee, Hye-Jin;Chun, Byung-Sik
    • Journal of the Korean Geotechnical Society
    • /
    • v.29 no.1
    • /
    • pp.39-47
    • /
    • 2013
  • With the increase in the application of CLSM using coal ash, we performed a basic research on CLSM material, laying focus on the correlation between compressive strength and unit weight of lightweight foamed CLSM. The unconfined compression strength is a criterion for the judgment of the possibility of re-excavation and an important factor determining the economy, efficiency, and excavation character. However, to know the quantitative compression strength value takes a certain amount of time, because the applicability of unconfined compression strength of CLSM is judged by the standard of 28days. Therefore, in this study the relation between compressive strength and unit weight (foam slurry unit weight, apparent unit weight) is analyzed focusing on lightweight foamed CLSM. We also suggested a formula which can easily predict the 28-day compressive strength only using unit weight value without the need to cure the slurry for 28 days.

A Study on Unconfined Compressive Strength of CLSM with Paper Sludge Ash (제지애쉬가 적용된 CLSM의 일축압축강도 특성에 관한 연구)

  • Park, Jeong-Jun;Lee, In-Hwan;Shin, Eun-Chul;Hong, Gigwon
    • Journal of the Korean Geosynthetics Society
    • /
    • v.18 no.4
    • /
    • pp.253-262
    • /
    • 2019
  • This paper described the evaluation results on unconfined compressive strength characteristics of CLSM with paper sludge ash, in order to develop a CLSM that can prevent sewer pipe damage. The flowability test and the unconfined compressive strength test were performed according to mix design condition of CLSM. The flowability test result showed that the water content, which can satisfy the flowability criteria, was 24% to 32% according to the mix design condition. The results of unconfined compressive strength test showed that the strength incremental ratio was high between 1 and 7 days of curing time, and the strength at this time was more than about 50% of the strength at 28 days of curing time. The strength of CLSM was greatly influenced by fly ash. However, it was analyzed that the mixture of paper sludge ash is required when the reference strength of CLSM is considered. Although the strength of the high cement ratio was higher than that of the low cement, a cement ratio of 5% would be a reasonable mix design condition of CLSM.

Deformation Behavior Underground Pipe with CLSM (유동성 채움재를 이용한 지하 매설관의 변형특성 연구)

  • Park, Jae-Hun;Lee, Kwan-Ho;Jo, Jae-Yun;Sung, Sang-Kyu
    • International Journal of Highway Engineering
    • /
    • v.5 no.2 s.16
    • /
    • pp.25-35
    • /
    • 2003
  • During construction of circular lifeline pipe, the non-proper compaction along the pipe and the decrease of compaction efficiency are the main problems to induce the failure of underground pipe. The use of CLSM(controlled low strength materials) is one of the applications to overcome those problems. In this research, the numerical analysis by PENTAGON FEM program was carried out for 20 cases with the couple of combinations on bedding materials, backfill materials, and pipes. From the FEM analysis, the use of CLSM as backfill materials reduced the settlement of ground surface and the deformation of pipe employed. In case of the vertical deformation on the pipe, common soil backfill for flexible pipes showed 2 times for rigid pipes, but CLSM backfill case did less deformation than the soil backfill for rigid pipes. CLSM backfills for rigid pipes showed the similar results. Judging from the FEM analysis, the use of CLSM increases the structure capacity of the underground pipes.

  • PDF

The Investigation of Application of Reject Ash and Recycled Fine Aggregate to High Flowing CLSM (고유동 CLSM를 위한 Reject Ash 및 순환 잔골재의 활용성 검토)

  • Song, Yong-Won;Yoon, Seob;Kim, Jung-Bin;Jeong, Yong;Park, Chan-Kyu;Lee, Seung-Hoon
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2009.05a
    • /
    • pp.403-404
    • /
    • 2009
  • This study has investigated application of the industrial by-product of reject ash and recycled fine aggregate to consider the economical issue to high flowing CLSM(controled low-strength material). But this high flowing CLSM is required more binder, so it has been estimated the influence of reject ash content, use of recycled fine aggregate and crushed sand, and air content about properties of CLSM.

  • PDF

Durability Characteristics and Environmental Assessment of Controlled tow-Strength Materials Using Bottom Ash (Bottom Ash를 재활용한 저강도 고유동 재료의 내구성 및 환경영향 평가)

  • 원종필;이용수;이존자
    • Journal of the Korea Concrete Institute
    • /
    • v.14 no.2
    • /
    • pp.223-230
    • /
    • 2002
  • The main intent of this research was to determine the feasibility of utilizing recycling bottom ash as CLSM (controlled low-strength material). CLSM is a cementitious material, commonly a blend of portland cement, fly ash, sand, and water, that is usually flowable and self-leveling at the time of placement. The durability characteristics of mixtures made bottom ash we compared with those of fly ash CLSM in order to evaluate the effectiveness and suitability of bottom ash as material in CLSM. A comprehensive evaluation of the bottom ash in CLSM and mix proportions indicated that the bottom ash are capable of performing as CLSM mixtures. The durability characteristic of CLSM incorporating the bottom ash under various physical and chemical causes of deterioration were investigated. Test results indicated that CLSM using bottom ash has acceptable durability performance. CLSM incorporating with bottom ash were also found to be environmentally safe.

A Study on the pH Reduction of Controlled Low Strength Material with Coal Ash (석탄회를 활용한 CLSM의 pH 저감에 관한 연구)

  • Kim, Youngil;Jee, Sunghyun;Chun, Byungsik
    • Journal of the Korean GEO-environmental Society
    • /
    • v.11 no.9
    • /
    • pp.39-45
    • /
    • 2010
  • Controlled low strength material(CLSM) is produced by mixing portland cement, fine aggregates, water and chemical admixtures. Sand is the most commonly used as the fine aggregates in the conventional CLSM. It is getting more and more difficult to obtain sand in Korea so it is required that the alternative materials be developed as the replacement of sand. Since the engineering characteristics of coal ash are similar to the sand, it becomes necessary to examine the application of the coal ash as the alternative material for CLSM and as the environment-friendly material. When the results meet the optimum pH level that plants can live, it can be expanded the scale of application of the study on the plant as the important field. This study was subjected to present the method to reduce the pH range of CLSM to a suitable condition that plants can survive. To verify this method, the care of neutralization was conducted by immersing the specimen to Ammonium monohydrogen phosphate. Before curing and neutralization, the maximum pH of developmental CLSM is approximately 11. However, the pH value of developmental CLSM has under 9.5 after peaceful curing and neutralization management.

Study on Correlation between Compressive Strength and Compressional Wave Velocity for CLSM According to Curing Time (양생시간에 따른 CLSM의 압축강도 및 압축파 속도 상관성 연구)

  • Han, Woojin;Lee, Jongsub;Cho, Samdeok;Kim, Jinhwan;Byun, Yonghoon
    • Journal of the Korean GEO-environmental Society
    • /
    • v.16 no.11
    • /
    • pp.5-11
    • /
    • 2015
  • The development of Controlled Low Strength Material (CLSM), which is a highly flowable material, has been performed for the application of backfill. The objective of this study is to compare the compressive strength and compressive wave velocity of CLSM according to the curing time. To investigate the characteristics of the CLSM consisting of sand, silt, water, flyash, and CSA cement, uniaxial compression test and flow test were carried out. For the measurement of compressional waves, a cell and a couple of transducers were used. The test results show that the compressive strength increases with the curing time, while the increment of compressive strength decreases with the curing time. In addition, the compressive wave velocity increases with the curing time, and the correlation between the compressive wave velocity and compressive strength is similar to exponential function. This study suggests that the correlation between the compressive wave velocity and compressive strength may be effectively used for the estimation of compressive strength of the CLSM at early curing time.

Characteristics of Shear Waves in Controlled Low Strength Material with Curing Time (양생시간에 따른 유동성 채움재의 전단파 특성)

  • Han, Woojin;Lee, Jong-Sub;Byun, Yong-Hoon;Cho, Samdeok;Kim, Juhyong
    • Journal of the Korean GEO-environmental Society
    • /
    • v.17 no.3
    • /
    • pp.13-19
    • /
    • 2016
  • The ultrasonic waves for monitoring concrete materials have been used to investigate the setting and hardening process of concrete. This paper presents the application of bender elements for monitoring the hardening properties of Controlled Low Strength Material (CLSM) and the characterization of shear waves in CLSM according to curing time. To ensure the early age properties and flow, the CLSM consists of CSA cement, sand, silt, water, fly ash, and accelerator. In addition, three different type specimens according to fine contents are mixed. A couple of bender elements are installed at the wall of measurement cell and the CLSM specimen are prepared at the measurement cell for 28 days. Experimental results show that the resonant frequency and shear wave velocities increase with an increase in the curing time, regardless of the fine contents. Up to ten hours, the amplitudes of shear waves also increase, and the resonant frequency and shear wave velocities at the same time increase as the fine contents increase. The shear wave measurement technique using the bender elements may be effectively used to evaluate the hardening properties of CLSM along the curing time.

Confocal laser scanning microscopy image를 이용한 UASB granule의 메탄 생성 능력 측정

  • Lee, Yu-Jin;Kim, Hyo-Seop;An, Yeong-Hui;Park, Seong-Hun
    • 한국생물공학회:학술대회논문집
    • /
    • 2000.04a
    • /
    • pp.365-369
    • /
    • 2000
  • Methanogenic activity of granular sludge was monitored by specific methanogenic activity (SMA) assay and confocal laser scanning microscopy (CLSM) during start-up of a thermophilic UASB reactor. Autofluorescence by CLSM could visualize the methanogenic bacterial population inside sludge granules and its intensity was proportional to SMA. Considering the complex procedures of SMA measurement, fluorescence quantification by CLSM can be suggested as a routine technique measuring methanogenic activity in UASB granules.

  • PDF